Search NASA⌕ Search

SEARCH · Search NASA

Results for “SOLUTION HEAT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Effect of Solution Heating Rate on Quasi-static and Dynamic Mechanical Properties of Al-Mg-Si-Cu Alloy

The effect of solution heating rate on quasi-static and dynamic mechanical properties of Al-Mg-Si-Cu alloy in bake hardening state was investigated through mechanical properties, microstructure and fracture morphology characterization in the present study. The results show that solution heating rate has a strong influence on microstructure, quasi-static and dynamic mechanical properties. As solution heating rate rises, the grain microstructure transforms from the elongated grains to equiaxed grains and the fraction of low-angle grain boundaries (LAGBs) also decreases. Moreover, the equivalent average grain size first decreases, and then increases. The relationship between solution heating rate and mechanical property is monotonic, not depending on strain rate. As solution heating rate rises, the yield strength, ultimate tensile strength and elongation decrease. In contrast to quasi-static loading, dynamic loading always tends to improve strengths and elongation. In addition, compared with the quasi-static tensile specimens, the dynamic tensile specimens possess a larger number of dislocations. Regardless of strain rate and solution heating rate, all the tensile specimens exhibit the ductile fracture mode. As solution rate rises, the dimples decrease and become shallow gradually. The dimples in dynamic fracture zone are larger and deeper than those in the quasi-static fracture zone.

36 MATERIALS SCIENCE↗

Solid-state transformation of Fe-rich intermetallic phases in Al–5.0Cu–0.6Mn squeeze cast alloy with variable Fe contents during solution heat treatment

The Al–5.0 wt.% Cu–0.6 wt.% Mn alloys with a variable Fe content were prepared by squeeze casting. Optical microscopy (OM), Deep etching technique, scanning electron microscopy(SEM), X-ray diffraction (XRD) and transmission electron microscopy (TEM) were used to examine the solid-state transformation of Fe-rich intermetallics during the solution heat treatment. The results showed that the Chinese script-like α-Fe, Al{sub 6}(FeMn) and needle-like Al{sub 3}(FeMn) phases transform to a new Cu-rich β-Fe (Al{sub 7}Cu{sub 2}(FeMn)) phase during solution heat treatment. The possible reaction and overall transformation kinetics of the solid-state phase transformation for the Fe-rich intermetallics were investigated. - Graphical abstract: Display Omitted - Highlights: • The α-Fe, Al{sub 6}(FeMn) and Al{sub 3}(FeMn) phases change to the β-Fe phases. • Possible reactions of Fe phases during solution heat treatment are discussed. • The overall fractional transformation rate follows an Avrami curve.

36 MATERIALS SCIENCE↗

The Effect of Solution Heat Treatment on an Advanced Nickel-Base Disk Alloy

Five heat treat options for an advanced nickel-base disk alloy, LSHR, have been investigated. These included two conventional solution heat treat cycles, subsolvus/oil quench and supersolvus/fan cool, which yield fine grain and coarse grain microstructure disks respectively, as well as three advanced dual microstructure heat treat (DMHT) options. The DMHT options produce disks with a fine grain bore and a coarse grain rim. Based on an overall evaluation of the mechanical property data, it was evident that the three DMHT options achieved a desirable balance of properties in comparison to the conventional solution heat treatments for the LSHR alloy. However, one of the DMHT options, SUB/DMHT, produced the best set of properties, largely based on dwell crack growth data. Further evaluation of the SUB/DMHT option in spin pit experiments on a generic disk shape demonstrated the advantages and reliability of a dual grain structure at the component level.

Gayda, J.↗

Solution heat-treatment of Nb-modified MAR-M247 superalloy

MAR-M247 superalloy has excellent mechanical properties and good oxidation resistance at elevated temperatures. Niobium is an element known as {gamma} Prime phase hardener in nickel-based superalloys, besides promoting homogeneous distribution of MC carbides. This work is inserted in a project that aims to evaluate the total replacement of tantalum by niobium atoms in MAR-M247 superalloy (10.2 Co, 10.2 W, 8.5Cr, 5.6 Al, 1.6 Nb, 1.4 Hf, 1.1 Ti, 0.7 Mo, 0.15 C, 0.06 Zr, 0.015 B, Ni balance-wt.%). Based on microstructural characterizations (SEM and FEG-SEM, both with EDS) of the as-cast material and heat-treated materials as well as utilizing Thermocalc simulations and experiments of differential thermal analysis (DTA), heat-treatment at 1260 Degree-Sign C for 8 h was chosen as an ideal condition for the solution of Nb-modified MAR-M247 superalloy. The hardness of as-cast and ideally solution treated materials was 390 {+-} 14 HV and 415 {+-} 6 HV, respectively. - Highlights: Black-Right-Pointing-Pointer DTA and microstructure of MAR-M247(Nb) showed a good agreement with Thermocalc. Black-Right-Pointing-Pointer An ideal condition for solution heat-treatment of MAR-M247(Nb) is 1260 Degree-Sign C for 8 h. Black-Right-Pointing-Pointer It was an observed evidence of incipient melting in samples heat-treated at 1280 Degree-Sign C.

36 MATERIALS SCIENCE↗

System and method for forming material substrate printer

A method is disclosed for manufacturing a part via an additive manufacturing process. A solution is used which has a volatile component within which is suspended particles of a powdered material. The solution is heated until it at least one of begins boiling or is about to begin boiling. The heated solution is then deposited at least at one location on a substrate to help form a layer of the part. The volatile component then evaporates, leaving only the particles of powdered material. The particles are then heated to the melting point. The deposition and heating operations are repeated to successively form a plurality of layers for the part. The evaporation of the volatile component helps to cool the part.

36 MATERIALS SCIENCE↗

System and method for forming material substrate printer

A method is disclosed for manufacturing a part via an additive manufacturing process. A solution is used which has a volatile component within which is suspended particles of a powdered material. The solution is heated until it at least one of begins boiling or is about to begin boiling. The heated solution is then deposited at least at one location on a substrate to help form a layer of the part. The volatile component then evaporates, leaving only the particles of powdered material. The particles are then heated to the melting point. The deposition and heating operations are repeated to successively form a plurality of layers for the part. The evaporation of the volatile component helps to cool the part.

Demuth, James A.↗

Revisiting the Analytical Solutions of Heat Transport in Fractured Reservoirs Using a Generalized Multirate Memory Function

Numerous analytical solutions have been developed for modeling thermal perturbations to underground formations caused by deep-well injection of fluids. Each solution has been derived for a specific boundary value problem and a simplified flow network with one set of parallel fractures. In this paper, new generalized solutions G*( x, s ) are developed using (existing) global transfer functions G$^*_0(x,s)$ and a new memory function g*( s ), where x and s are the space and Laplace variable. The memory function represents the solutions of conductive heat exchange between fractures and matrix blocks and between fractured aquifers and unfractured aquitards. The memory function is developed to account for multirate exchange induced by different shapes, sizes, properties, and volumetric fractions of matrix blocks bounded by multiple sets of orthogonal fractures with different spacing. The global transfer functions represent the fundamental solutions to convective, convective-conductive, and convective-dispersive heat transport in fractures (or aquifers) without exchange and are available for various (1-D linear, 1-D radial, 2-D dipole, and single-well injection-withdrawal) flow fields. The new solutions with exchange are developed using $G^*(x,s) = B^*(s)G^*_0{x, s[1 + Θg^*(s)]}$, thereby greatly simplifying solution development in a novel way, where Θ and B*( s ) are a fracture-matrix scaling factor and the boundary condition function. As a result, the new solutions are applied to several example problems, showing that heat transport in fractured aquifers is significantly impacted by (1) thermal dispersion in fractures that is rarely considered, (2) multirate heat exchange with a wide range of size and anisotropy of rectangular matrix blocks, and (3) heat exchange between aquifers and aquitards.

58 GEOSCIENCES↗

Stress corrosion cracking of several solution heat-treated Mg–X alloys

Here we studied the stress corrosion cracking (SCC) behaviour of solution heat-treated as-cast Mg0.1Zr, Mg1Mn, Mg0.1Sr, Mg0.3Si, Mg5Sn, Mg5Zn and Mg0.3Ca in distilled water (DW) using the linearly increasing stress test (LIST). SCC susceptibility was related to the stress rate for all the Mg–X alloys except for Mg0.1Sr. At ~7.0 × 10 ₋4 MPa s ₋1 , Mg0.3Si and Mg5Sn were immune to SCC; Mg0.1Zr, Mg1Mn and Mg0.1Sr suffered medium SCC; Mg5Zn and Mg0.3Ca suffered relatively more serious SCC. At ~7.0 × 10 ₋5 MPa s ₋1 , Mg5Zn and Mg0.3Ca suffered the most serious transgranular SCC, whilst the other Mg–X alloys suffered medium SCC.

36 MATERIALS SCIENCE↗

Heat Treatment of Friction-Stir-Welded 7050 Aluminum Plates

A method of heat treatment has been developed to reverse some of the deleterious effects of friction stir welding of plates of aluminum alloy 7050. This alloy is considered unweldable by arc and high-energy-density beam fusion welding processes. The alloy can be friction stir welded, but as-welded workpieces exhibit low ductility, low tensile and yield strengths, and low resistance to stress corrosion cracking. Heat treatment according to the present method increases tensile and yield strengths, and minimizes or eliminates stress corrosion cracking. It also increases ductility. This method of heat treatment is a superior alternative to a specification-required heat treatment that caused the formation of large columnar grains, which are undesired. Workpieces subjected to the prior heat treatment exhibited elongations <2 percent, and standard three-point bend specimens shattered. The development of the present heat treatment method was guided partly by the principles that (1) by minimizing grain sizes and relieving deformation stresses, one can minimize or eliminate stress corrosion cracking and (2) the key to maximizing strength and eliminating residual stresses is to perform post-weld solution heating for as long a time as possible while incurring little or no development of large columnar grains in friction stir weld nuggets. It is necessary to perform some of the solution heat treatment (to soften the alloy and improve machine welding parameters) before welding. The following is an example of thickness- dependent pre- and post-weld heat treatments according to the present method: For plates 0.270 in. (approx.6.86 mm) thick milled from plates 4.5 in. (114.3 mm) thick, perform pre-weld solution heating at 890 F (477 C) for 1 hour, then cool in air. After friction stir welding, perform solution heating for 10 minutes, quench, hold at room temperature for 96 hours, then age at 250 F (121 C) for 5 hours followed by 325 F (163 C) for 27 hours.

Petter, George E.↗

Shear Assisted Processing and Extrusion (ShAPE) of Aluminum Alloy 7075, 2024, and Al-12.4TM

The most common aluminum alloys utilized in the aerospace industry are 7075 and 2024 due to their high strength-to-weight ratio compared to advanced high strength steels and other aluminum alloys. Despite excellent performance, these aluminum alloys have seen limited use outside of the aerospace industry due in part to high cost. If high-performance aluminum extrusions could be made more cost effectively by eliminating energy intensive process steps typical of conventional extrusion, then numerous opportunities exist for more widespread adoption. A key reason for the high cost of 7075 and 2024 extrusions (25-75% higher than 6061) is their slow extrusion speed. 7075 and 2024 are limited to 2 m/min and 3.5 m/min respectively, in contrast to 6061 which can be extruded at 20–80 m/min. In addition to slow speed, aluminum alloys require numerous thermal treatments throughout the extrusion process including homogenization and pre-heating prior to extrusion, and solution heat treating and artificial aging after extrusion. Each of these steps contribute to the total energy consumed during manufacturing of extruded components. This project investigates the use of ShAPE to improve extrusion speed and reduce, or even eliminate, the typical thermal treatments for high strength aluminum alloys, all while improving material performance. The overarching goal of this project was to demonstrate that Shear Assisted Processing and Extrusion (ShAPE) can manufacture high-performance aluminum alloy tubing with lower manufacturing energy and improved mechanical properties compared to conventional extrusion. Unlike conventional extrusion where the billet is rammed against a stationary die using a strictly linear motion, the ShAPE process superimposes a rotational shear force by spinning the die while the billet is plunged. Compared to conventional linear extrusion, the ShAPE process imparts significantly more strain into the feedstock material, which enables the formation of novel microstructures. These microstructures manifest an array of property and process improvements for extrusion of high-performance aluminum alloys. The following accomplishments were achieved for this project: Extrusion of 7075 at 12.2 meters/min compared to 2 meters/min for conventional extrusion; Elimination of 7075 billet homogenization (430 °C for 20 hours) which is required prior to conventional extrusion; Elimination of 7075 billet pre-heating (400 °C for 1 hour) in a separate furnace which is required prior to conventional extrusion; Achieved 7075-T6with yield strength = 595 MPa, ultimate tensile strength = 531MPa, and elongation = 17.4% for extrusions made from unhomogenized billets. Exceeds the ASTM and ASM standard, and typical industry values; Achieved 7075-T5 (i.e., no solution heat treatment) with yield strength = 588 MPa, ultimate tensile strength = 535 MPa, and elongation = 14.8% for extrusions made from homogenized billets; Extrusion of 2024 at 7.4 meters/min compared to 3.5 meters/min for conventional extrusion; Achieved 2024-T8510 yield strength = 522 MPa, ultimate strength = 510MPa, and elongation = 7.1% for extrusions made from wrought billets. Exceeds the ASTM and ASM standard, and typical industry values; Extrusion of Al-12.4TM high-performance aluminum powder directly into tubing, in a single step, which eliminates process steps typical of powder metallurgy extrusion.

36 MATERIALS SCIENCE↗

Finite analytic numerical solution of heat transfer and flow past a square channel cavity

A numerical solution of flow and heat transfer characteristics is obtained by the finite analytic method for a two dimensional laminar channel flow over a two-dimensional square cavity. The finite analytic method utilizes the local analytic solution in a small element of the problem region to form the algebraic equation relating an interior nodal value with its surrounding nodal values. Stable and rapidly converged solutions were obtained for Reynolds numbers ranging to 1000 and Prandtl number to 10. Streamfunction, vorticity and temperature profiles are solved. Local and mean Nusselt number are given. It is found that the separation streamlines between the cavity and channel flow are concave into the cavity at low Reynolds number and convex at high Reynolds number (Re greater than 100) and for square cavity the mean Nusselt number may be approximately correlated with Peclet number as Nu(m) = 0.365 Pe exp 0.2.

Chen, C.-J.↗

Effects of Post-Weld Heat Treatment on the Mechanical Properties of Similar- and Dissimilar-Alloy Friction Stir Welded Blanks

Friction stir welding is a solid state joining process with relatively low welding temperatures. Nevertheless, the mechanical properties of friction stir welded blanks are degraded after welding. Indeed, both strength and ductility of the welds are decreased after welding. Often, the resulting friction stir welded blanks need to be formed to their final structural shape. Therefore, the formability of friction stir welded blanks is of primary importance in the manufacturing of structural parts. This paper studies how the mechanical properties and particularly formability of friction stir welded blanks can be improved by applying a post weld heat treatment. Two aluminum alloys from 2000 and 7000 series, namely 2024-T3 and 7075-T6, are selected for the study. The sheet thickness of both materials is 2,0 mm. The selected alloys are welded in three configurations: 2024-T3 and 2024-T3, 7075-T6 and 7075-T6, and 2024-T3 and 7075-T6. The resulting welds are naturally aged for a few months. Three sets of standard dog bone shape tensile test specimens are then machined from the welds. The first set of the specimens is tested without any heat treatment. The second set of the specimens is solution heat treated and quenched before testing. The third set of the specimens is solution heat treated, quenched, and naturally aged for a week before testing. The mechanical properties of the three different sets of specimens are compared with each other. It is shown that careful selection of post weld heat-treatment can greatly improve the formability of friction stir welded blanks.

36 MATERIALS SCIENCE↗

The measurement of heats of solution of high melting metallic systems in an electromagnetic levitation field

A method was tested for measuring the enthalpies of mixing of liquid metallic alloying systems, involving the combination of two samples in the electromagnetic field of an induction coil. The heat of solution is calculated from the pyrometrically measured temperature effect, the heat capacity of the alloy, and the heat content of the added sample. The usefulness of the method was tested experimentally with iron-copper and niobium-silicon systems. This method should be especially applicable to high-melting alloys, for which conventional measurements have failed.

Frohberg, M. G.↗

Forging of Advanced Disk Alloy LSHR

The powder metallurgy disk alloy LSHR was designed with a relatively low gamma precipitate solvus temperature and high refractory element content to allow versatile heat treatment processing combined with high tensile, creep and fatigue properties. Grain size can be chiefly controlled through proper selection of solution heat treatment temperatures relative to the gamma precipitate solvus temperature. However, forging process conditions can also significantly influence solution heat treatment-grain size response. Therefore, it is necessary to understand the relationships between forging process conditions and the eventual grain size of solution heat treated material. A series of forging experiments were performed with subsequent subsolvus and supersolvus heat treatments, in search of suitable forging conditions for producing uniform fine grain and coarse grain microstructures. Subsolvus, supersolvus, and combined subsolvus plus supersolvus heat treatments were then applied. Forging and subsequent heat treatment conditions were identified allowing uniform fine and coarse grain microstructures.

Gabb, Timothy P.↗