Corrosion and corrosion prevention in gas turbines

The conditions governing the corrosion behavior in gas turbines are surveyed. Factors such as temperature, relative humidity, the presence of sulfur and nitrogen dioxide, and fuel quality are discussed. Electromechanical corrosion at relatively low temperature in compressors; oxidation; and hot corrosion (sulfidation) at high temperature in turbines are considered. Corrosion prevention by washing and rinsing, fueld additives, and corrosion resistant materials and coatings are reviewed.

Mom, A. J. A.↗

Effects of surface chemistry on hot corrosion life

Burner rig tests were conducted under the following conditions: 900 C, hourly thermal cycling, 0.5 ppm sodium as MaCl in the gas stream, velocity 0.3 Mach. The alloys are Udiment 700, Rene 80, uncoated and with RT21, Codep, or NiCoCrAlY coatings. These tests were completed for specimens in the as-processed condition and after aging at 1100 C in oxidizing or inert evnivronments for time up to 600 hours. Coil inductance changes used for periodic nondestructive inspection of specimens were useful in following the course of corrosion. Typical sulfidation was observed in all cases, structurally similar to that observed for service-run turbine components. Aging at cuased a severe decrease in hot corrosion life of RT21 and Codep coatings and a significant but less decrease in the life of the NiCoCrAlY coating. The extent of these decreases was much greater for all three coatings on U700 substrates than on Rene 80 substrates. Coating/substrate interdiffusion rather than by surface oxidation.

Fryxell, R. E.↗

Effects of surface chemistry on hot corrosion life

Burner rig tests were conducted under the following conditions: 900 C, hourly thermal cycling, 0.5 ppm sodium as NaCl in the gas stream, and Mach 0.3 velocity. The alloys tested were Udimet 700 (U700) and Rene 80, uncoated and with RT21, Codep, or NiCoCrAlY coatings. The tests, up to 1000 hours, included specimens in the as-processed condition and after aging at 1100 C in oxidizing or inert environments for up to 600 hours. Coil-inductance changes were measured for periodic nondestructive inspection of speciments and found useful in the following course of corrosion. Typical sulfidation observed in all cases was similar to that observed in service-run turbine components. Aging at 1100 C caused severe decrease in the hot corrosion life of RT21 and Codep coatings and a significant but lesser decrease in the life of NiCoCrAlY coatings. The extent of these decreases was much greater for all three coatings on U700 than on Rene substrates. A coating hot corrosion life-predicitin model was proposed. The model requires time/temperature information for a turbine component at takeoff conditions as well as environmental contaminant information.

Fryxell, R. E.↗

Hot corrosion of S-57, 1 cobalt-base alloy

A cobalt base alloy, S-57, was hot corrosion tested in Mach 0.3 burner rig combustion gases at maximum alloy temperatures of 900 and 1000 C. Various salt concentrations were injected into the burner: 0.5, 2, 5, and 10 ppm synthetic sea salt and 4 ppm sodium sulfate (Na2SO4). S-57 underwent accelerated corrosion only under the most severe test conditions, for example, 4 ppm Na2SO4 at 900 C. The process of the accelerated corrosion was primarily sulfidation.

Santoro, G. J.↗

Improved PFB operations: 400-hour turbine test results

A pressurized fluidized bed (PFB) coal-burning reactor was used to provide hot effluent gases for operation of a small gas turbine. Preliminary tests determined the optimum operating conditions that would result in minimum bed particle carryover in the combustion gases. Solids were removed from the gases before they could be transported into the test turbine by use of a modified two stage cyclone separator. Design changes and refined operation procedures resulted in a significant decrease in particle carryover, from 2800 to 93 ppm (1.5 to 0.05 grains/std cu ft), with minimal drop in gas temperature and pressure. The achievement of stable burn conditions and low solids loadings made possible a 400 hr test of small superalloy rotor, 15 cm (6 in.) in diameter, operating in the effluent. Blades removed and examined metallographically after 200 hr exhibited accelerated oxidation over most of the blade surface, with subsurface alumina penetration to 20 micron m. After 400 hours, average erosion loss was about 25 micron m (1 mil). Sulfide particles, indicating hot corrosion, were present in depletion zones, and their presence corresponded in general to the areas of adherent solids deposit. Sulfidation appears to be a materials problem equal in importance to erosion.

Rollbuhler, R. J.↗

Corrosion of metals and alloys in sulfate melts at 750 C

The corrosion of Ni, Co, Ni-10Cr, Co-21Cr, and IN738 was studied at 750 C in the presence of molten sulfate mixtures (Na2SO4-Li2SO4 and Na2SO4-CoSO4) and in an atmosphere consisting of O2 + 0.12 percent SO2-SO3. The corrosion was observed to be similar for both Na2SO4-Li2SO4 and Na2SO4-CoSO4 melts. The corrosion of Ni and Co took place by the formation of a mixed oxide plus sulfide scale, very similar to the corrosion in SO2 or SO3 alone. The initial stage for the corrosion of Ni-10Cr involved the formation of a thick NiO + Ni3S2 duplex scale, and Cr sulfide was formed during the later stages. A pitting type of morphology was observed for both Co-21Cr and IN738. The pit was Cr sulfide at the beginning, and subsequently the sulfides oxidized to Cr2O3. A base-metal oxide layer was present above the pit, and this was observed to be formed very early in the corrosion process. A mechanism is proposed to explain this. In general, the formation of sulfides appears to be the primary mode of degradation in mixed sulfide melts.

Misra, A. K.↗

Effects of SO2 and SO3 on the Na2SO4 induced corrosion of nickel

The effects of SO2 and SO3 in the environment on the hot-corrosion behavior of Ni in the temperature range 750-950 C has been studied. Below the melting point of Na2SO4 (884 C), rapid corrosion takes place by formation of a Na2SO4-NiSO4 melt which can penetrate the porous oxide scale and give rise to sulfide information by coming in contact with the metal. The distribution of the sulfides depends on the SO2 level in the ambient gas. Continued corrosion occurs by a sulfidation-oxidation mechanism. At temperatures above the melting point of Na2SO4, accelerated degradation occurs via dissolution of the surface scale, followed by reprecipitation of the oxide in a nonprotective form.

Misra, A. K.↗

Sodium sulfate-induced corrosion of pure nickel and superalloy Udimet 700 in a high velocity burner rig at 900 C

Sodium sulfate-induced corrosion of pure nickel and a commercial nickel-base superalloy, Udimet 700 (U-700), were studied at 900 C in a Mach 0.3 burner rig with different Na levels in the combustor. The corrosion rate of Ni was independent of the Na level in the combustor and considerably lower than that measured in laboratory salt spray tests. The lower rates are associated with the deposition of only a small amount of Na2SO4 on the surface of the NiO scale. Corrosion of U-700 was observed to occur in two stages. During the first stage, the corrosion proceeds by reaction of Cr2O3 scale with the Na2SO4 and evaporation of the Na2CrO4 reaction product from the surface of the corroding sample. Cr depletion in the alloy occurs and small sulfide particles are formed in the Cr depletion zone. Extensive sulfidation occurs during the second state of corrosion, and a thick scale forms. The relationship between the corrosion rate of U-700 and the Na level in the combustor gives a good correlation in the range of 0.3 to 1.5 ppm by weight Na. Very low levels of Na in the combustor cause accelerated oxidation of U-700 without producing the typical hot corrosion morphology.

Misra, A. K.↗

Corrosion Prevention in Copper Combustion Chamber Liners of Liquid Oxygen/Methane Booster Engines

Prior research conducted by United Technologies Research Center and Rockwell International Rocketdyne Division encountered severe copper corrosion while flowing hydrocarbon fuels through copper cooling tubes. These experimental results have very important implications for the development of low-cost, regeneratively cooled, oxygen/hydrocarbon bipropellant booster engines. Aerojet TechSystems undertook a program sponsored by NASA/Lewis Research Center in 1986 with two objectives: (1) to define the corrosive interaction process that occurs between hydrocarbon fuels and copper combustion chamber liner materials, using both static and dynamic test methods, and (2) to identify and demonstrate protective measures against this corrosive process. The results of the first program task demonstrated that the most damaging corrosive process was caused by trace amounts of sulfur-containing impurities in the hydrocarbon fuel which react with the copper chamber liner material to form cuprous sulfide (Cu2S), as reported in Paper No. AlAA 88-3215. Experiments were conducted which demonstrated this corrosive process with Mil-Spec RP-1, propane, and methane fuels in contact with OFHC, NASA-Z, and ZrCu coppers. The preliminary results of the second program task demonstrated that electrodeposited gold and platinum coatings held promise of preventing corrosion of copper chamber liners by methane contaminated with sulfur-containing impurities, as reported in Paper No. AIAA 89-2738. Experiments were conducted which demonstrated greatly reduced corrosion of copper by hydrogen sulfide (H2S) and methyl mercaptan (CH3SH) as measured impurities in methane. This paper presents the concluding, confirmatory results from the second program task. The efficacy of a protective gold coating on NASA-Z copper cooling channel walls was conclusively demonstrated. Tests were conducted in the Aerojet Carbothermal Test Facility which provide realistic simulations of booster engine cooling channel conditions such as temperature, pressure, flow velocity, and heat flux. Dynamic test series were performed with methane containing 5 and 10 ppm (by volume) hydrogen sulfide. Gold-plated and unplated copper alloy specimens were evaluated. The tests demonstrated that gold coatings were effective in preventing corrosion of the copper. Posttest metallographic examinations of the unplated specimens showed severe corrosion as a result of reaction with the sulfur containing contaminant in the fuel. In contrast, posttest metallographic examination of the gold-coated specimens showed no corrosion under similar operating conditions. The findings from metallurgical and chemical analyses of the copper specimens, chemical analysis of the methane, and description of all test conditions are provided. Conclusions are reached as to the efficacy of the plating methods and the effectiveness of the metal coatings in the prevention of corrosion in hydrocarbon-fueled booster engine combustion chamber liners.

S D Rosenberg↗

Mechanism of Na2SO4-induced corrosion of molybdenum containing nickel-base superalloys at high temperatures. I - Corrosion in atmospheres containing O2 only. II - Corrosion in O2 + SO2 atmospheres

Kinetics of the Na2SO4-induced corrosion of the molybdenum-containing nickel-base superalloys, B-1900 and Udimet 700, coated with Na2MoO4, has been studied in oxygen atmosphere at temperatures ranging from 750 to 950 C. Because the gas turbine atmosphere always contains some SO2 and SO3, the effect of atmospheric SO2 content on corrosion of Udimet-700 has also been studied. It was found that in the O2 atmosphere the melt in the catastrophic corrosion phase consists of Na2MoO4 plus MoO3, with the onset of the catastrophic corrosion coinciding with the appearance of MoO3. In the presence of low levels of atmospheric SO2 (below 0.24 percent), the melt during catastrophic corrosion contains, in addition to Na2MoO4 and MoO3, some quantities of Na2SO4. At the levels of SO2 above 1 percent, no catastrophic corrosion was observed. At these SO2 levels, internal sulfidation appears to be the primary mode of degradation.

Misra, A. K.↗

Burner Rig Hot Corrosion of Five Ni-Base Alloys Including Mar-M247

The hot corrosion resistance of four new Ni-base superalloys was compared to that of Mar-M247 by testing in a Mach 0.3 burner rig at 900 C for 300 1-hr cycles. While the Al content was held the same as in the Mar-M247, the Cr and Co levels in the four new alloys were decreased while other strengthening elements (Re, Ta) were increased. Surprisingly, despite their lower Cr and Co contents, the hot corrosion behavior of all four new alloys was superior to that of the Mar-M247 alloy. The Mar-M247 alloy began to lose weight almost immediately whereas the other four alloys appeared to undergo an incubation period of 50-150 1-hr cycles. Examination of the cross-sectional microstructures showed regions of rampant corrosion attack (propagation stage) in all five alloys after 300 1-hr cycles . This rampant corrosion morphology was similar for each of the alloys with Ni and Cr sulfides located in an inner subscale region. The morphology of the attack suggests a classic "Type I", or high temperature, hot corrosion attack.

Nesbitt, James A.↗

Studies on the hot corrosion of a nickel-base superalloy, Udimet 700

The hot corrosion of a nickel-base superalloy, Udimet 700, was studied in the temperature range of 884 to 965 C and with different amounts of Na2SO4. Two different modes of degradation were identified: (1) formation of Na2MoO4 - MoO3 melt and fluxing by this melt, and (2) formation of large interconnected sulfides. The dissolution of Cr2O3, TiO2 in the Na2SO4 melt does not play a significant role in the overall corrosion process. The conditions for the formation of massive interconnected sulfides were identified and a mechanism of degradation due to sulfide formation is described. The formation of Ns2MoO4 - MoO3 melt requires an induction period and various physiochemical processes during the induction period were identified. The factors affecting the length of the induction period were also examined. The melt penetration through the oxide appears to be the prime mode of degradation whether the degradation is due to the formation of sulfides or the formation of the Na2MoO4 - MoO3 melt.

Misra, A. K.↗

Studies on the hot corrosion of a nickel-base superalloy, Udimet 700

The hot corrosion of a nickel-base superalloy, Udimet 700, was studied in the temperture range of 884 to 965 C and with different amounts of Na2SO4. Two different modes of degradation were identified: (1) formation of Na2MoO4-MoO3 melt and fluxing by this melt, and (2) formation of large interconnected sulfides. The dissolution of Cr2O3, TiO2 in the Na2SO4 melt does not play a significnt role in the overall corrosion process. The conditions for the formation of massive interconnected sulfides were identified and a mechanism of degradation due to sulfide formation is described. The formation of Na2MoO4-MoO3 melt requires an induction period and various physiochemical processes during the induction period were identified. The factors affecting the length of the induction period were also examined. The melt penetration through the oxide appears to be the prime mode of degradation whether the degradation is due to the formation of sulfides or the formation of the Na2MoO4-MoO3 melt.

Misra, A. K.↗

Effects of surface chemistry on hot corrosion life

Baseline burner rig hot corrosion with Udimet 700, Rene' 80; uncoated and with RT21, Codep, or NiCoCrAlY coatings were tested. Test conditions are: 900C, hourly thermal cycling, 0.5 ppm sodium as NaCl in the gas stream, velocity 0.3 Mach. The uncoated alloys exhibited substantial typical sulfidation in the range of 140 to 170 hours. The aluminide coatings show initial visual evidence of hot corrosion at about 400 hours, however, there is no such visual evidence for the NiCoCrAlY coatings. The turbine components show sulfidation. The extent of this distress appeared to be inversely related to the average length of mission which may, reflect greater percentage of operating time near ground level or greater percentage of operation time at takeoff conditions (higher temperatures). In some cases, however, the location of maximum distress did not exhibit the structural features of hot corrosion.

Fryxell, R. E.↗

Hydrocarbon-fuel/combustion-chamber-liner materials compatibility

The results of dynamic tests using methane and NASA-Z copper test specimen under conditions that simulate those expected in the cooling channels of a regeneratively cooled LOX/hydrocarbon booster engine operating at chamber pressures up to 3000 psi are presented. Methane with less than 0.5 ppm sulfur contamination has little or no effect on cooling channel performance. At higher sulfur concentrations, severe corrosion of the NASA-Z copper alloy occurs and the cuprous sulfide Cu2S, thus formed impedes mass flow rate and heat transfer efficiency. Therefore, it is recommended that the methane specification for this end use set the allowable sulfur content at 0.5 ppm (max). Bulk high purity liquid methane that meets this low sulfur requirement is currently available from only one producer. Pricing, availability, and quality assurance are discussed in detail. Additionally, it was found that dilute sodium cyanide solutions effectively refurbish sulfur corroded cooling channels in only 2 to 5 minutes by completely dissolving all the Cu2S. Sulfur corroded/sodium cyanide refurbished channels are highly roughened and the increased surface roughness leads to significant improvements in heat transfer efficiency with an attendant loss in mass flow rate. Both the sulfur corrosion and refurbishment effects are discussed in detail.

Homer, G. David↗

Corrosion of 310 stainless steel in H2-H2O-H2S gas mixtures: Studies at constant temperature and fixed oxygen potential

Corrosion of SAE 310 stainless steel in H2-H2O-H2S gas mixtures was studied at a constant temperature of 1150 K. Reactive gas mixtures were chosen to yield a constant oxygen potential of approximately 6 x 10 to the minus 13th power/cu Nm and sulfur potentials ranging from 0.19 x 10 to the minus 2nd power/cu Nm to 33 x 10 to the minus 2nd power/cu Nm. The kinetics of corrosion were determined using a thermobalance, and the scales were analyzed using metallography, scanning electron microscopy, and energy dispersive X-ray analysis. Two corrosion regimes, which were dependent on sulfur potential, were identified. At high sulfur potentials (p sub S sub 2 less than or equal to 2.7 x 10 to the minus 2nd power/cu Nm) the corrosion rates were high, the kinetics obeyed a linear rate equation, and the scales consisted mainly of sulfide phases similar to those observed from pure sulfication. At low sulfur potentials (P sub S sub 2 less than or equal to 0.19 x 10 to the minus 2nd power/cu Nm) the corrosion rates were low, the kinetics obeyed a parabolic rate equation, and scales consisted mainly of oxide phases.

Rao, D. B.↗

The hot corrosion of Co-25Cr-10Ni-5Ta-3Al-0.5Y alloy /S-57/

A cobalt-base alloy, Co-25Cr-10Ni-5Ta-3Al-0.5Y (S-57), was subjected to hot corrosion in Mach 0.3 burner-rig combustion gases at maximum alloy temperatures of 900 and 1000 C. Various salt concentrations were injected into the burner: 0.5, 2,5, and 10 parts per million synthetic sea salt and 4 parts per million sodium sulfate (Na2SO4). The extent of corrosion was determined by measuring the maximum depth of corrosion in the alloy, and the corrosion process was studied by metallography, X-ray diffraction, scanning electron microscopy, and electron microprobe analysis. While S-57 was found to possess only moderate oxidation resistance at these temperatures, this alloy resisted significant hot corrosion attack under all but the most severe test conditions. The process of hot corrosion attack under the most severe conditions of this study was primarily sulfidation.

Santoro, G. J.↗

Reactions occurring during the sulfation of sodium chloride deposited on alumina substrates

The reaction between solid NaCl and air containing 1 pct SO2 has been studied between 500 and 700 C. The reaction product, Na2SO4, forms not only on the surface of the NaCl but also on surrounding areas of the substrate due to the volatility of the NaCl at these temperatures. At the higher temperatures, the vapor pressure of NaCl is so high that the majority of the reaction product is distributed on the substrate. Above 625 C, the reaction product is a liquid solution of NaCl and Na2SO4 that exists only so long as NaCl is supplied from the original crystal source. Eventually, the liquid solidifies by constitutional solidification as the NaCl is converted to Na2SO4. While it exists, the liquid NaCl-Na2SO4 solution is shown to be highly corrosive to Al2O3 and, on a scale of Al2O3 growing on alloy HOS 875, particularly attacks the grain boundaries of the scale at preferred sites where chromium and iron oxides and sulfides rapidly develop. This is proposed as one mechanism by which NaCl deposition contributes to the initiation of low temperature hot corrosion.

Wu, C. S.↗