At least 19 records

Statistical Homogenization of Elastic and Fracture Properties of a Sample Selective Laser Melting Material

Selective laser melting (SLM) is an additive manufacturing technique commonly used in the rapid prototyping of components. The complexity of the SLM microstructure poses a unique challenge to deriving effective mechanical properties at different length scales. Representative volume elements (RVEs) are often used to homogenize the material properties of composites. Instead of RVEs, we use statistical volume elements (SVEs) to homogenize the elastic and fracture properties of the material. This relates the inherent variation of a material’s microstructure to the variation in its mechanical properties at different observation scales. The convergence to the RVE limit is examined from two perspectives: the stability of the mean value as the SVE size increases for the mean-based approach, and the tendency of the normalized variation in homogenized properties to zero as the SVE size increases for the variation-based approach. Fracture properties tend to make the RVE limit slower than do elastic properties from both perspectives. There are also differences between vertical (normal to printing plane) and horizontal (in-plane) properties. While the elastic properties tend to make the RVE limit faster for the horizontal direction, i.e., having a smaller variation and more stable mean value, the fracture properties exhibit the opposite effect. We attributed these differences to the geometry of the melt pools.

36 MATERIALS SCIENCE↗

Critical differences between electron beam melted and selective laser melted Ti-6Al-4 V

Effective optimization of the production of Ti-6Al-4 V using AM requires a fundamental understanding of the relative importance of different microstructural features to the deformation and failure mechanisms, particularly features that vary between production methods. In this study, the tensile response and deformation mechanisms of electron beam melted (EBM) AM Ti-6Al-4 V material loaded in different orientations and produced using various powder sizes were compared to those of selective laser melted (SLM) AM Ti-6Al-4 V material. The density and morphology of pores, phase fractions, prior-β grains, and defect microstructures were evaluated using scanning electron microscopy, X-ray computed tomography, electron backscatter diffraction, and transmission electron microscopy before and after deformation. The results were used to evaluate the relative importance of each feature on strengthening, deformation, and failure initiation mechanisms. Results focused primarily on coarse-powder EBM materials indicated that phase distribution and defect density were most influential for determining material yield strength as well as maximum possible strain to failure. Porosity was lower overall in EBM Ti-6Al-4 V than in SLM, allowing for occasional increases in part strain to failure, but remained a limiting factor determining overall part ductility.

36 MATERIALS SCIENCE↗

High temperature air oxidation behavior of Hastelloy X processed by Electron Beam Melting (EBM) and Selective Laser Melting (SLM)

The microstructure and oxidation behavior of Laser Beam Melted, Electron Beam Melted and wrought Hastelloy X were studied at 950 °C in dry air, 50 h cycles, up to 1000 h. The variability of processing parameters and powder compositions strongly impacted the oxidation and spallation behavior. Finally, the alloys with high Mn and Si were associated with higher oxidation rates, finer Cr 2 O 3 grain microstructure and increased spallation was observed for the alloys with large elongated grain microstructures (aspect ratio of 10 ± 3).

36 MATERIALS SCIENCE↗

Synthesis of precipitation-strengthened Al-Sc, Al-Zr and Al-Sc-Zr alloys via selective laser melting of elemental powder blends

Selective laser melting is used to create Al-1.5Sc, Al-1.5Zr and Al-0.75Sc-0.75Zr (at.%) alloys from blends of elemental Al, Sc, and Zr powders. This study investigates elemental alloying elements (Sc and Zr) which are high-melting and highly reactive, unlike previous work which focused on more concentrated elemental additions of lower-melting, lower-reactivity Cu and Si to aluminum. High-speed in situ synchrotron x-ray imaging and diffraction show that the 20–30 μm Al, Sc, and Zr powders fully melt and sufficiently mix in the molten state to create, on solidification, a homogeneous distribution of primary, micron-size L12 precipitates (Al 3 Sc, Al 3 Zr, and Al 3 (Sc,Zr), respectively) and nucleate micron-size Al matrix grains, as confirmed by SEM imaging of cross-sections. Here, a second laser pass, simulating a realistic additive-manufacturing build condition, fully remelts the initial volume which shows, after solidification, the same Al 3 (Sc,Zr) L1 2 primary micro-precipitates and very fine Al grains. After aging at 300–400°C, the alloys show large increases in hardness, consistent with an exceptionally high number density (1.4 × 10 24 m –3 ) and volume fraction (2.5%) of secondary Al 3 (Sc,Zr) nano-precipitates with a Sc-rich core and Zr-rich shell, as measured via atom-probe tomography.

36 MATERIALS SCIENCE↗

Effect of processing parameters and build orientation on microstructure and performance of AISI stainless steel 304L made with selective laser melting under different strain rates

Selective laser melting (SLM) process brings diverse potentials on geometry flexibility; therefore, it is more and more widespread to be employed in fabrication metal alloys served for industries. Nonetheless, a material characterization study is desired to carry on for better understanding the correlation among process, structure, microstructure, and performance. In the current study, the SLM fabricated AISI stainless steel 304L was fabricated with different process parameters and built orientations (horizontal, inclined, and vertical. The tensile behavior was evaluated under different strain rates (0.0001 /s, 0.001 /s, 0.01 /s, and 0.1 /s) and compared to the commercial cold-rolled and annealed counterpart. Grain structures, tensile strength, elongation-to-failure, strain rate sensitivity, work hardening, and fractographic analysis were evaluated in terms of the effect of energy density, build orientation, and strain rate. The output indicates the tensile strength increases with increasing strain rates. On the contrary, the elongation-to-failure shows a decreasing trend with strain rates. Tensile properties of specimens built in the horizontal and inclined orientations are more sensitive to strain rates due to the smaller dimension of grain structures. Tensile anisotropy depends on the energy input, where a high energy density could yield a strong build orientation-dependent anisotropy. Hall-Petch relationship is validated to explain the mechanical anisotropy in different built orientations for SLM alloys. The strain hardening exponent and work hardening rate are demonstrated to be positively correlated, and they increase with smaller grain sizes. The fine dimple features indicate the ductile fracture mode regardless of strain rates. The size of the ductile dimples seems to depend on the strain rates and build orientations.

36 MATERIALS SCIENCE↗

The Effect of Sulfuric Acid Anodization on the Electrochemical Properties of Aluminum Alloy AlSi 10 Mg Prepared by Selective Laser Melting

Aluminum alloy, AlSi 10 Mg, prepared by selective laser melt (SLM) fabrication was anodized in 9.8% sulfuric acid (Type II) at 15 V for a total of 23 min. Experiments were performed to study the potentiostatic anodization process and its effects on the oxide coating morphology, thickness, and electrochemical properties of the alloy. Prior to anodization, the alloy microstructure is composed of aluminum cells encapsulated in a silicon network. Anodizing the abraded and polished AlSi 10 Mg surface produced a porous oxide layer with a thickness of 5μm. The oxide coating weight was 698 ± 29 mg/ft 2 . The oxide coating forms in the aluminum cells that are isolated from one another by the silicon eutectic phase. In electrochemical tests, the anodic and cathodic potentiodynamic polarization currents were suppressed by factors of 15× and 215×, respectively, as compared to the unanodized controls. The data indicate the anodic oxide coating suppresses the cathodic more than the anodic reaction rate. Linear polarization resistance (R p ) values increased by 279× after anodization. The corrosion current density values (j corr ) decreased by 133× after anodization. Taken together, the electrochemical data indicate the anodic oxide coating (unsealed) increases the corrosion resistance of the SLM alloy by two orders of magnitude.

Electrochemistry↗

Uncertainties Induced by Processing Parameter Variation in Selective Laser Melting of Ti6Al4V Revealed by In-Situ X-ray Imaging

Selective laser melting (SLM) additive manufacturing (AM) exhibits uncertainties, where variations in build quality are present despite utilizing the same optimized processing parameters. In this work, we identify the sources of uncertainty in SLM process by in-situ characterization of SLM dynamics induced by small variations in processing parameters. We show that variations in the laser beam size, laser power, laser scan speed, and powder layer thickness result in significant variations in the depression zone, melt pool, and spatter behavior. On average, a small deviation of only ~5% from the optimized/reference laser processing parameter resulted in a ~10% or greater change in the depression zone and melt pool geometries. For spatter dynamics, small variation (10 μm, 11%) of the laser beam size could lead to over 40% change in the overall volume of the spatter generated. The responses of the SLM dynamics to small variations of processing parameters revealed in this work are useful for understanding the process uncertainties in the SLM process.

36 MATERIALS SCIENCE↗

Effect of heat treatment on the tensile behavior of selective laser melted Ti-6Al-4V by in situ X-ray characterization

Selective Laser Melted Ti-6Al-4V (as-SLMed) exhibits decreased yield strength, increased work hardening, and increased ductility after heat treatment at 730 degrees C (HT-730) or 900 degrees C (HT-900) for 2 h. To understand the change of mechanical properties, in situ high energy X-ray diffraction (HEXRD) is used to examine the phase composition, load partitioning, slip system activity, and dislocation density evolution in all three specimens. The as-SLMed specimen is dominated by martensitic α'. After heat treatment, α' partly or fully decomposes into α+β, reducing the yield strength. In HT-730, beta precipitates with confined size show much higher lattice strain than the α'/α matrix during deformation; in HT-900, the lattice strain difference is mostly eliminated. This is a key reason for the increased ductility in HT-900. From the anisotropic lattice strain development, basal slip is identified as the easiest slip system in α'/α. Using an elasto-plastic self-consistent (EPSC) model, the critical resolved shear stress ratio between prismatic slip and basal slip (CRSS prism /CRSS basal ) is estimated to be 1.31 and 1.16 in the as -SLMed and the HT-900 specimens, respectively. Further, the alpha phase in HT-900 is able to activate multiple slip systems and accumulate more dislocations during plastic deformation. This explains why HT-900 has better ductility and higher work hardening rate than the other two specimens.

36 MATERIALS SCIENCE↗

Selective laser melting of oxide dispersion strengthened MA956 alloy and its surface finishing by magnetic field assisted finishing

Selective laser melting (SLM) is a prominent metal additive manufacturing (AM) capable of processing a myriad of engineering materials with high precision and design freedom. However, similar to other AM processes, poor surface finishing has been an omnipresent problem in SLM technology. In this study, magnetic field assisted finishing (MAF) was used to finish SLM fabricated oxide dispersion strengthened (ODS) MA956, an iron-chromium-aluminum alloy. The effect of laser processing parameters on part density and surface roughness was first studied. Using a multi-objective optimization technique, the optimal parameters to obtain the highest density and lowest surface roughness were determined. Finally, MAF was applied to the parts built with the obtained optimal SLM parameters, but without significant improvement on the surfaces of as-printed samples. Hence, the surfaces of as-printed samples were post-processed (ground) to yield better initial surface conditions prior to MAF. The effect of initial roughness, iron particles size, and abrasive size on MAF performance was studied. Initial roughness had the most dominant effect followed by abrasive size. The underlying mechanism behind the dependency on initial roughness on final surface quality was analyzed by studying the change on the surface profiles with different starting initial roughness. The initial roughness required for MAF to be effective was determined. In conclusion, using the optimal processing conditions, MAF was applied to the post-processed samples to attain the final average surface roughness (R a ) as little as 0.36 μm starting from initial average roughness (R a ) of 1.53 μm.

36 MATERIALS SCIENCE↗

The microstructure of a selective laser melting (SLM)-fabricated NiTi shape memory alloy with superior tensile property and shape memory recoverability

A selective laser melting (SLM)-fabricated NiTi with superior tensile property and shape memory recoverability was obtained by using a unique stripe rotation scanning strategy. Here, the alloy characteristics, formation mechanisms and evolution in terms of twins, dislocations and precipitations of the alloy were systematically studied. Compared to the conventional smelting-followed-by-machining, the SLM fabrication process involves rapid solidification and repeated heating, which confer distinctive characteristics to the microstructures of SLM-fabricated NiTi alloys. Rapid solidification promotes the formation of a supersaturation solid solution matrix containing a high concentration vacancies, which in turn aggregate to generate a high density of dislocations. During subsequent repeated heating stages, these dislocations occur thermal motion along three directions of <001 > , <111> and <110 >, leading to the formation of thermal kinks, helical dislocations and wave morphology. Simultaneously, precipitated particles Ti 3 Ni 4 repeatedly nucleate and heterogeneous grow with the movement of dislocation. Such precipitation behavior, termed repeated precipitation, has not been previously reported in the conventional NiTi alloys, suggesting that it could be a unique characteristic of such alloy. After martensitic transformation, only two twins, {1 1¯ 1} type I twin and compound twin, are detected. The twinning lamellae of these two twins, where precipitation and dislocation pile-ups exist, often have uneven thickness and chaotic arrangement. Besides, the unique self-accommodated microstructures, such as secondary {1 1¯ 1} type I twin and compound twin with “herring-bone’’ lamellae, which often appear in the deformed or nanocrystalline NiTi, can also be observed. These unique microstructures may confer the distinctive properties to the SLM-fabricated NiTi.

36 MATERIALS SCIENCE↗

Effects of Particle Size Distribution with Efficient Packing on Powder Flowability and Selective Laser Melting Process

The powder bed-based additive manufacturing (AM) process contains uncertainties in the powder spreading process and powder bed quality, leading to problems in repeatability and quality of the additively manufactured parts. This work focuses on identifying the uncertainty induced by particle size distribution (PSD) on powder flowability and the laser melting process, using Ti6Al4V as a model material. The flowability test results show that the effect of PSDs on flowability is not linear, rather the PSDs near dense packing ratios cause significant reductions in flowability (indicated by the increase in the avalanche angle and break energy of the powders measured by a revolution powder analyzer). The effects of PSDs on the selective laser melting (SLM) process are identified by using in-situ high-speed X-ray imaging to observe the melt pool dynamics during the melting process. The results show that the powder beds made of powders with dense packing ratios exhibit larger build height during laser melting. The effects of PSD with efficient packing on powder flowability and selective laser melting process revealed in this work are important for understanding process uncertainties induced by feedstock powders and for designing mitigation approaches.

36 MATERIALS SCIENCE↗

Critical pitting temperature of selective laser melted 316L stainless steel: A mechanistic approach

In this work, the critical pitting temperature (CPT) of selective laser melted (SLM) 316 L stainless steel in 1.0 M NaCl was measured and compared with a commercial wrought alloy. Potentiostatic measurements determined a mean CPT value of 16 ± 0.7 °C, 27.5 ± 0.8 °C and 31 ± 1 °C for the wrought alloy, the SLM alloy normal to the build direction and parallel to the build direction, respectively. The lead-in pencil electrode technique was used to study the pit chemistry of the two alloys and to explain the higher CPT values observed for the SLM alloy. A lower critical current density required for passivation in a simulated pit solution was measured for the SLM alloy. Moreover, the ratio of the critical concentration to saturated concentration of dissolving metal cations was found to be higher for the SLM alloy, which was related to its different salt film properties, possibly as a result of the SLM’s distinct microstructure.

36 MATERIALS SCIENCE↗

Selective laser melting of 304L stainless steel: Role of volumetric energy density on the microstructure, texture and mechanical properties

The role of volumetric energy density on the microstructural evolution, texture and mechanical properties of 304L stainless steel parts additively manufactured via selective laser melting process is investigated. 304L is chosen because it is a potential candidate to be used as a matrix in a metal matrix composite with nanoparticles dispersion for energy and high temperature applications. The highest relative density of 99 %±0.5 was achieved using a volumetric energy density of 1400 J/mm 3 . Both XRD analysis and Scheil simulation revealed the presence of a small trace of the delta ferrite phase, due to rapid solidification within the austenitic matrix of 304L. Here, a fine cellular substructure ranged between 0.4–1.8 μm, was detected across different energy density values. At the highest energy density value, a strong texture in the direction of [100] was identified. At lower energy density values, multicomponent texture was found due to high nucleation rate and the existing defects. Yield strength, ultimate tensile strength, and microhardness of samples with a relative density of 99 % were measured to be 540 ± 15 MPa, 660 ± 20 MPa and 254 ± 7 HV, respectively and higher than mechanical properties of conventionally manufactured 304L stainless steel. Heat treatment of the laser melted 304L at 1200 °C for 2 h, resulted in the nucleation of recrystallized equiaxed grains followed by a decrease in microhardness value from 233 ± 3 HV to 208 ± 8 HV due to disappearance of cellular substructure.

304L stainless steel↗

The Electrochemical Behavior of As-Prepared Aluminum Alloy A360 Produced by Selective Laser Melting Fabrication with and without a Trivalent Chromium Process Conversion Coating

In this paper, we report on the electrochemical behavior and corrosion resistance of as-prepared aluminum alloy, A360 (AlSi10Mg), fabricated by additive manufacturing, with and without a trivalent chromium process conversion coating. Selective laser melting was the 3D printing process used for the alloy build. The corrosion suppression provided by the coating system was assessed through electrochemical measurements and accelerated degradation testing during a 14-day continuous neutral salt-spray exposure. The results indicate that the conversion coating can be formed by solution pretreating (degreasing and deoxidation) the alloy (X-Z plane perpendicular to the build plane) with its native surface roughness (as-prepared) followed by immersion for 10, 15 or 20 min in the coating bath. All three immersion times provide an equivalent level of corrosion protection to the alloy. The conversion coating suppresses both anodic and cathodic currents, increases the polarization resistance, and provides both anodic and cathodic corrosion protection to the as-prepared alloy. The conversion-coated specimens exhibit good stand-alone corrosion resistance during a 14-day neutral salt-spray exposure with corrosion intensity values (g/m 2 -year) ~10x lower than values for the uncoated, as-prepared alloy specimens.

36 MATERIALS SCIENCE↗

Property-Graded Stainless Steel 316L by Selective Laser Melting: Characterization & Design

Abstract The purpose of this research work is to characterize and inform the design of (mechanical) property-graded bulk structures made from a single metallic alloy via a laser powder bed fusion (LPBF) process, with an end goal of creating repeatable/reproducible functionally-graded additively manufactured (FGAM) parts. This paper specifically investigates the manufacture of stainless steel (SS) 316L structures via a pulsed selective laser melting (SLM) process, and the underlying causes of property variations (within a functionally-acceptable range) through various material characterization techniques. For this, a design of experiments spanning the volumetric energy density (VED) based process parameter design space was utilized to investigate the range of functionally-acceptable physical/mechanical properties achievable in SS 316L. Five sample conditions (made via different process parameter combinations) were down-selected for in-depth microstructure analysis and mechanical/physical property characterization; these were suitably selected to impart a wide and controllable property range (209–318 HV hardness, 90–99.9% relative density, and 154–211 GPa modulus). It was observed that property variations resulted from combinations of porosity types/amounts, martensitic phase fractions, and grain sizes. Based on these findings, property-graded standard test specimens were designed and manufactured for further investigation—tensile specimens having a monotonic hardness change along its gauge length, four-point bending specimens with varying elastic moduli as a function of the distance from the neutral axis, and Moore’s rotating beam fatigue specimens with moduli variations based on the distance from the center. Altogether, this work lays the foundation for understanding and designing the local and global mechanical performance of FGAM bulk structures.

Engineering↗