Search NASA⌕ Search

SEARCH · Search NASA

Results for “SiOx Anode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Revealing the aging process of solid electrolyte interphase on SiOx anode

Abstract As one of the most promising alternatives to graphite negative electrodes, silicon oxide (SiO x ) has been hindered by its fast capacity fading. Solid electrolyte interphase (SEI) aging on silicon SiO x has been recognized as the most critical yet least understood facet. Herein, leveraging 3D focused ion beam-scanning electron microscopy (FIB-SEM) tomographic imaging, we reveal an exceptionally characteristic SEI microstructure with an incompact inner region and a dense outer region, which overturns the prevailing belief that SEIs are homogeneous structure and reveals the SEI evolution process. Through combining nanoprobe and electron energy loss spectroscopy (EELS), it is also discovered that the electronic conductivity of thick SEI relies on the percolation network within composed of conductive agents (e.g., carbon black particles), which are embedded into the SEI upon its growth. Therefore, the free growth of SEI will gradually attenuate this electron percolation network, thereby causing capacity decay of SiO x . Based on these findings, a proof-of-concept strategy is adopted to mechanically restrict the SEI growth via applying a confining layer on top of the electrode. Through shedding light on the fundamental understanding of SEI aging for SiO x anodes, this work could potentially inspire viable improving strategies in the future.

25 ENERGY STORAGE↗

Green Electrode Processing Enabled by Fluoro-Free Multifunctional Binders for Lithium-Ion Batteries

The eco-friendly processing of conjugated polymer binder for lithium-ion batteries demands improved polymer solubility by introducing functional moieties, while this strategy will concurrently sacrifice polymer conductivity. Employing the polyfluorene-based binder poly(2,7-9,9 (di(oxy-2,5,8-trioxadecane))fluorene) (PFO), soluble in water-ethanol mixtures, a novel approach is presented to solve this trade-off, which features integration of aqueous solution processing with subsequent controlled thermal-induced cleavage of solubilizing side chains, to produce hierarchically ordered structures (HOS). The thermal processing can enhance the intermolecular π–π stacking of polyfluorene backbone for better electrochemical performance. Notably, HOS-PFO demonstrated a substantial 6–7 orders of magnitude enhancement in electronic conductivity, showcasing its potential as a functional binder for lithium-ion batteries. As an illustration, HOS-PFO protected SiOx anodes, utilizing in situ side chain decomposition of PFO surrounding SiOx particles after aqueous processing are fabricated. HOS-PFO contributed to the stable cycling and high-capacity retention of practical SiOx anodes (3.0 mAh cm -2 ), without the use of any conducting carbon additives or fluorinated electrolyte additives. It is proposed that this technique represents a universal approach for fabricating electrodes with conjugated polymer binders from aqueous solutions without compromising conductivity.

25 ENERGY STORAGE↗

Advanced Anode Manufacturing through Ultra-Thin Li Deposition

During the program's tenure, Applied Materials delivered high-quality (>99.9%) ultra-pure thin lithium metal in sheets and in roll to roll (R2R) formats to program partners for testing, cell builds and evaluation. The thickness range of the deposited Lithium can be controlled between 1-20 μm (<3% nonuniformity). A second R2R tool was commissioned for Li processing and inline CO 2 passivation module was validated. Additionally, S2S deposition tools were used to explore five different surface protection materials for Li-metal. One surface passivation chemistry was down selected for testing and showed improved performance. Key results are summarized in this final report.

25 ENERGY STORAGE↗

Three-Dimensional Mapping of Resistivity and Microstructure of Composite Electrodes for Lithium-Ion Batteries

Nanoparticle silicon–graphite composite electrodes are a viable way to advance the cycle life and energy density of lithium-ion batteries. However, characterization of composite electrode architectures is complicated by the heterogeneous mixture of electrode components and nanoscale diameter of particles, which falls beneath the lateral and depth resolution of most laboratory-based instruments. In this work, we report an original laboratory-based scanning probe microscopy approach to investigate composite electrode microstructures with nanometer-scale resolution via contrast in the electronic properties of electrode components. Applying this technique to silicon-based composite anodes demonstrates that graphite, SiOx nanoparticles, carbon black, and LiPAA binder are all readily distinguished by their intrinsic electronic properties, with measured electronic resistivity closely matching their known material properties. Resolution is demonstrated by identification of individual nanoparticles as small as ~20 nm. Our technique presents future utility in multiscale characterization to better understand particle dispersion, localized lithiation, and degradation processes in composite electrodes for lithium-ion batteries.

25 ENERGY STORAGE↗

Cell-Format-Dependent Mechanical Damage in Silicon Anodes

Strong binders can be counterproductive for silicon anodes. Here, we show that stresses from cycling Si-based electrodes can cause permanent stretching and wrinkling of the current collector. Furthermore, this deformation damages the electrode coating and accelerates cell aging due to the inactivation of Si domains and facilitation of Li plating. Interestingly, we demonstrate that the formation of wrinkles is size-dependent, being present in pouch cells but absent from coin cells. This size-dependent performance decay indicates that, in extreme cases, testing outcomes are highly dependent on scale and that the validation of battery materials may require testing at larger cell formats.

25 ENERGY STORAGE↗

The Role of Oxygen in Lithiation and Solid Electrolyte Interphase Formation Processes in Silicon-Based Anodes

Silicon oxides (SiO x ) have been considered as promising alternatives to pure Si in high energy anodes in lithium-ion batteries (LIBs) due to their improved cycling stability. However, their fundamental lithiation mechanism has not yet been systematically investigated, and potential collateral downsides remain unclear. In this work, we report on the role of oxygen in lithiation/delithiation and solid electrolyte interphase (SEI) formation processes in SiO x thin film model electrodes with different oxygen contents. Here, we show that the SiO x anodes with higher oxygen content experience smaller volume change and form a thinner and more stable SEI, both of which are beneficial for cycling stability. However, these SiO x anodes also show an irreversible lithiation at around 0.7 V attributed to the reduction of Si oxides, leading to lower first cycle coulombic efficiency that is undesirable for practical applications. Overall, these results offer a balanced perspective on the advantages and disadvantages that oxygen brings to Si-based anodes in LIBs.

25 ENERGY STORAGE↗

Enhanced Interfacial Stability of Si Anodes for Li-Ion Batteries via Surface SiO2 Coating

Silicon is a promising alloying anode for lithium-ion batteries owing to its high capacity and low cost. However, its use has been hampered by mechanical failure arising from the large volume change upon cycling and by an insufficiently stable solid-electrolyte interphase (SEI). SEI formation depends on the Si surface, which is often an oxide (SiO x ). In this study we compare three different Si surfaces using Si wafers: 1.3 nm native SiO x , 1.4 nm thermally grown SiO2, and a SiOx-free surface. The oxide-free surface showed the worst electrochemical performance, never exceeding 94% Coulombic efficiency (CE). Furthermore, it also exhibited the thickest SEI and the highest overpotential for lithiation, which correlated with uninhibited electrolyte reduction and the incorporation of P-F species into the SEI. The oxide-coated surfaces performed significantly better, demonstrating a CE above 99% beyond the second cycle, low overpotential for lithiation, and a thinner and more stable SEI. The oxides lower the onset potential for electrolyte reduction, and yield an SEI with fewer P-F species. However, it was found that the CE with the native oxide surface decays from the fifth cycle onwards and correlates with a resurgence of electrolyte reduction. A 1-2 nm thermal SiO 2 coating is optimum for achieving a stable SEI that minimizes side reactions and sustains efficient cycling.

25 ENERGY STORAGE↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Optimal Microstructure of Silicon Monoxide as the Anode for Lithium-Ion Batteries

Because of its metastable nature, silicon monoxide (SiO) consists of Si nanodomains in an amorphous matrix of SiO 2 . The microstructure of SiO, including SiO 2 , Si domains, and interphase (SiO x ) between domains, was modified via an annealing treatment in argon gas and thoroughly characterized by in-situ and ex-situ X-ray diffraction, pair distribution function, and electron energy loss spectroscopy. Two microstructure transformation routes were observed during the annealing process: (1) at a temperature of <800 °C, the annealing treatment was found to affect mainly the structural conformation of the amorphous SiO 2 matrix and the interphase, while (2) an annealing temperature of >800 °C led to significant Si nanodomain growth. Here, we found that the microstructure has a great impact on the electrochemical performance of SiO. The optimized microstructure of SiO appears to be achieved through annealing treatment at 800 °C or less, which results in interphase (SiO x ) reduction without causing significant Si domain growth. This work provides a deep insight into the domain and interphase transformation of SiO upon heat treatment. The improved understanding of the relationship between SiO microstructure and its electrochemical behavior will enable proper design and development of high-energy SiO for lithium-ion batteries.

25 ENERGY STORAGE↗