Search NASA⌕ Search

SEARCH · Search NASA

Results for “SmCo5”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Effect of different surfactants on the formation and morphology of SmCo5 nanoflakes

The effect of the amount and types of surfactants and milling time on the formation of SmCo5 nanoflakes by surfactant-assisted high-energy ball milling in heptane has been investigated. The majority of the as-milled SmCo5 samples had the shape of flakes with a high degree of texture. Among the surfactants used, oleylamine (OY), trioctylamine (TOA) and oleic acid (OA), OA and OY have similar effects on the formation of SmCo5 nanoflakes, with the highest coercivity of 20.1 kOe obtained after 5 h of milling with 2 wt.% OA. Textured poly-nanocrystalline SmCo5 nanoflakes were formed even with as little as 2 wt.% OA. The coercivity of the specimens prepared with 2-10 wt.% of OA increased from 10.8 to 20.1 kOe when the milling time increased from 0.25 to 5 h. However, the same amount of OA had little effect on the coercivity and grain size when the milling time was kept for 5 h. In the case of TOA, a higher amount of surfactant is required to form the nanoflakes. The evolution of thickness, structure and magnetic properties of SmCo5 flakes with increasing milling time has a similar trend with all surfactants used. The [0 0 1] texture was found to be reduced either with decreasing the amounts of OA from 10 to 2 wt.% when the milling time was 5 h or with increasing the milling time from 0.25 to 5 h when the amount of OA was kept at 5 wt.%. Another interesting result is that the majority of jet-milled SmCo5 powders became more uniform and had a smaller size in the range of 0.3-3 mu m when using milling balls with a single diameter of 4 mm. The small size and uniform nanoflakes are very promising for the development of anisotropic nanocomposite magnets. (C) 2011 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Zheng, LY↗

Effect of ball-milling surfactants on the interface chemistry in hot-compacted SmCo5 magnets

Anisotropic SmCo5 nanoflakes prepared by high-energy ball-milling with surfactants have great potential in applications for high-performance nanocomposite magnets. For such "nanocomposite" applications, the surface structure and chemistry of nanoflakes are crucial for achieving high coercivity. In this study, hot-pressed samples from anisotropic SmCo5 nanoflakes, ball-milled with different surfactants, oleic acid (OA) and oleylamine (OY), were investigated. Interface layers between the SmCo5 nanoflakes were found to consist of samarium oxides and a soft magnetic Co phase. These surface layers contribute to the degradation of hard magnetic performance, which is confirmed by scanning transmission electron microscopy-energy dispersive X-ray spectroscopy analysis of the cross-section of a single flake ball-milled with OA. Samples milled with OY show a much thinner interface layer in compacted samples, which means that the surface degradation during ball-milling with OY is much less than that with OA. The results show clearly that the choice of proper surfactant and the control of processing parameters are the key factors for improving the surface condition of the nanoflakes and the resulting hard magnetic properties. (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Li, WF↗

Materials Data on SmCo5 by Materials Project

SmCo5 crystallizes in the hexagonal P6/mmm space group. The structure is three-dimensional. Sm is bonded in a 6-coordinate geometry to eighteen Co atoms. There are six shorter (2.87 Å) and twelve longer (3.18 Å) Sm–Co bond lengths. There are two inequivalent Co sites. In the first Co site, Co is bonded in a 12-coordinate geometry to three equivalent Sm and six equivalent Co atoms. All Co–Co bond lengths are 2.45 Å. In the second Co site, Co is bonded to four equivalent Sm and eight Co atoms to form a mixture of face, edge, and corner-sharing CoSm4Co8 cuboctahedra. All Co–Co bond lengths are 2.48 Å.

36 MATERIALS SCIENCE↗

Aluminum bonded SmCo5 magnets with enhanced mechanical strength

Despite their versatility and easy manufacturability, polymer-bonded magnets find limited application due to their limited mechanical properties and temperature resistance. In this study, we developed mechanically robust, aluminum-bonded SmCo5 magnets by utilizing a low-temperature, shear-assisted friction consolidation technique. Bonded magnets with varying magnetic phase content were fabricated at processing temperature of 500°C, and their microstructures, magnetic, mechanical, and electrical properties were systematically investigated. The resulting bonded-magnets showed effective consolidation with nanocrystalline microstructures. Magnetic properties were found to be tunable through variations in binder phase content, with coercivity reaching values up to 15.3 kOe (1217.5 kA/m) and maximum magnetic energy product up to 3.6 MGOe (28.7 kJ/m3), which are comparable to other bonded magnets. Electrical resistivities were lower than the polymer-bonded magnets, but comparable to the sintered ones. We observed an average flexural strength of 223 MPa for 60 vol.% SmCo5/Al sample, which is nearly two times higher than the reported values for sintered and bonded Sm-Co magnets. Our research demonstrated an effective approach to fabricate metal-bonded permanent magnets with superior magnetic and mechanical properties potentially applicable for high temperature applications.

Poudel Chhetri, Tej Bahadur↗

The effect of particle size on coercivity and crystallinity of SmCo5

It is observed a turning point in the particle size for which the coercivity H-ci of a Sm-Co alloy reaches a peak. Using a broad size range from 20 nm to 5 mm, the turning point of the flake thickness for SmCo5 nanoflakes is determined in the range of 100-180 nm with H-ci peak at similar to 20 kOe. A lower coercivity at a particle size well below the turning point is likely related to a more detailed nanoscale morphology that controls coercivity. The effect of particle size on crystallinity for high energy milled powder is also discussed with four observations. (C) 2011 American Institute of Physics. [doi:10.1063/1.3607958]

Chen, CH↗

Understanding the origin of magneto-crystalline anisotropy in pure and Fe/Si substituted SmCo 5

In this paper, we report magneto-crystalline anisotropy of pure and Fe/Si substituted SmCo5. The calculations were performed using the advanced density functional theory (DFT) including onsite electron-electron correlation and spin-orbit coupling. Si substitution substantially reduces both the uniaxial magnetic anisotropy and the magnetic moment. Fe substitution with the selective site, on the other hand, enhances the magnetic moment with a limited chemical stability. The magnetic hardness of the SmCo5 is governed by the Sm 4f localized orbital contribution. The 4f density of states (DOS) becomes flat and split with the substitution of Co (2c) with Si/Fe atoms, except with the Fe substitution at 3 g sites. It is also confirmed that Si substitution favors the thermodynamic stability on contrary to the diminished magnetic and anisotropic effects in SmCo5 at either sites.

36 MATERIALS SCIENCE↗

Exchange-coupled nanoscale SmCo/NdFeB hybrid magnets

Nanoscalehybridmagnets containing SmCo5 and Nd2Fe14B hard magnetic phases have been produced via a novel “in-one-pot” processing route. The grain size of the processed bulk composite materials is controlled below 20 nm. The refinement of the nanoscale morphology leads to effective inter-phase exchange coupling that results in single-phase like magnetic properties. Energy product of 14 MGOe was obtained in the isotropic nanocomposite magnets at room temperature. At elevated temperatures, the hybridmagnets have greatly improved thermal stability compared to the Nd2Fe14B single-phase counterpart and have substantially increased magnetization and energy products compared to the single-phase SmCo5 counterpart.

36 MATERIALS SCIENCE↗

Characterisation of Sm-Co-Sn alloys

Cast SmCo{sub 5-x}Sn{sub x} (x = 0.00, 0.01, 0.06 and 0.12) alloys were prepared by arc melting with subsequent thermal homogenisation. Microstructural and x-ray diffraction studies revealed that the alloys were constituted of three phases i.e. SmCo{sub 5}, Sm{sub 2}Co{sub 7} and Sm{sub 2}Co{sub 17}. The addition of Sn caused grain refinement of the alloys. It was found that the Sn addition promoted nucleation of Sm{sub 2}Co{sub 17}, segregation of solute atoms and increase in unit cell volume; consequently, significant augmentation in remanence to maximum magnetization ratios was achieved. - Research Highlights: 1. Tin up to 0.12% was added in a Samarium cobalt-SmCo5 system; discernable changes in the microstructure and phase distribution were achieved; {yields} the nucleation of Sm2Co17 phase, {yields} segregation of Sn and samarium rich Sm2Co7 phase on the grain boundaries {yields} refinement of the microstructure in term of grain size 2. Moreover, addition of Sn caused twofold increase in magnetic properties (Remanence-Mr) of the Sm-Co alloy as compared to the binary SmCo5 system.

36 MATERIALS SCIENCE↗

A solid-state extrusion pathway extensible to upcycling aluminum scrap and end-of-life permanent magnets into ductile Al-6061/SmCo 5 structural magnetic composites

Permanent magnets offer strong potential for multifunctional structural components, but their inherent brittleness limits direct integration. Here, SolidStir® Extrusion (SSE) is used to embed SmCo5 powder into AA6061 in the solid state, and the resulting microstructure, interfacial chemistry, mechanical properties, and magnetic response are systematically characterized. SSE fragments the initial SmCo 5 powder into predominantly fine particles dispersed within an ultrafine Al matrix, with a volume fraction of ∼ 4–6 % in this proof-of-concept study. Interfacial reactions form a continuous Al–Co reaction layer, with local atomic-resolution indexing consistent with Al 13 Co 4 , together with Sm–Si-rich reaction products, while the matrix contains Sm–Co–Si-rich precipitates and Mg 2 Si, producing features from nanometers to micrometers. Compared with an Al extrudate, this architecture increases yield strength by ∼ 42 % and tensile strength by ∼ 31 %, while preserving uniform elongation, and it sustains work hardening in compression from 150 to 400 °C. The composite retained hard-magnetic behavior, with axial magnetization of 12.7 A·m 2 kg −1 at 6 T and intrinsic coercivity of 9.6 kOe. These findings demonstrate that SSE can produce Al-based load-bearing magnetic composites while preserving useful SmCo5 functionality.

36 MATERIALS SCIENCE↗

Magnetism of directly ordered Sm-Co clusters

Sm-Co bulk alloys have shown superior permanent-magnet properties, but research on Sm-Co nanoparticles is challenging because of the need to control particle size, size-distribution, crystalline ordering, and phase purity. In the present study, a cluster-deposition method was used to produce Sm-Co nanoparticles having desired crystal structures without the requirement of subsequent high-temperature thermal annealing. Poorly crystallized SmCo5 nanoparticles exhibit a low room-temperature coercivity of only 100 Oe, whereas crystalline SmCo5 and Sm2Co17 nanoparticles show room-temperature coercivities of 2000 and 750 Oe, respectively. The direct synthesis of Sm-Co nanoparticles having sizes of less than 10 nm and a high degree of atomic ordering is an important step toward creating nanoparticle building blocks for permanent-magnets and other significant applications. (C) 2012 American Institute of Physics. [doi:10.1063/1.3677668]

Balamurugan, B↗

Ultimate intrinsic coercivity samarian-cobalt magnet. An Earth based feasibility study for Space Shuttle missions

Techniques for the electromagnetic containerless reaction of samarium with cobalt for the formation of samarium-cobalt alloys are summarized. The effort expended to reduce and instrument the oxygen partial pressure in the reaction chamber and coolant gas system are described as well as the experiments in which these improvements were shown to be partially effective. A stainless steel glove box capable of being evacuated to low 10 to the -6th torr pressure and refilled with ultra-pure argon was built and installed. Necessary accessories to perform SmCo5 powder preparation, compaction and subsequent encapsulation of the powder inside a hot isostatic pressing cannister were designed, built, and incorporated into the chamber. All accessories were tested for proper functioning inside the chamber. Using the facility, the first batch of densified SmCo5 powder was fabricated to near total density. Analysis of the densified compacts shows that oxygen contamination during fabrication was near zero.

Das, D.↗

Aluminum/SmCo 5 composites for structural and magnetic applications

Metal-bonded magnetic composites (MBMCs) present a promising alternative to dense sintered magnets, particularly for intricate components. Compared to polymer-based bonded magnets, MBMCs have wider applicability in harsh environments. In this paper, we demonstrate a solid-state shear-based manufacturing technique to introduce localized magnetization into a paramagnetic aluminum matrix by embedding SmCo5 permanent magnet particles. Our magnetic composites display hard magnetic behavior with a coercivity of 13 kOe and a remanent magnetization of 4.32 emu/g. In addition to magnetization, we also report a 9% improvement in Young’s modulus. Despite the local temperature rise during processing, the magnetic phases didn’t decompose into unwanted phases, preserving the composite's hard magnetic properties. Creation of an interfacial metallurgical bond with the matrix ensured the suitability of the composites for structural applications. Our study investigates the mechanical, and functional properties of composites, paving the way for lightweight structural magnetic composites with a transformative potential in the aerospace, nuclear, and automotive applications. This work underscores the potential for further optimization and development to drive innovations in magnet and equipment design.

36 MATERIALS SCIENCE↗

Preparation and Magnetic Properties of Sub-Micrometer Sized Sm-Co Powders Prepared From Nanostructured Precursor Oxides

Submicrometer-sized Sm-Co powders have been prepared by the calciothermic reduction and subsequent solid-state diffusion of a nanostructured Sm-Co-O/Co-O precursor. The Sm and Co containing precursor was prepared by an autocombustion process. X-ray diffraction identified the product as a mixture of SmCoO3 and Co-3 O-4. This powder was mixed in a 1:2 mass ratio with CaO (which served as a thermal ballast and aggregation inhibitor) and milled to reduce the particle size below 1 micrometer. Ca metal was added to the mixed powder in amounts between 2 and 6 times those required to reduce the Sm and Co oxides, and sealed in Nb tubes for heat treatment at 900 degrees C for various lengths of time. After cooling to room temperature, metallic Sm-Co particles were isolated from the undesired reaction products by a series of washing steps in acetic acid and ethyl alcohol. The Sm-Co particles were characterized by scanning electron microscopy, vibrating sample magnetometry, and x-ray diffraction. These measurements demonstrated that smaller particle sizes were associated with shorter reaction times and smaller quantities of reducing agent. The formation of hard SmCo5 was systematically associated with either long diffusion times with small amounts of reducing agent, or short diffusion times with large amounts of reducing agent.

Kelly, BG↗

Studies of magnetostriction and spin polarized band structures of rare earth intermetallics

Anisotropic magnetostriction measurements of R6Fe23, R = (Tb, Dy, Ho, and Er) were carried out from 77 K to room temperature. Magnetic fields up to 2.1 Tesla were applied. All the compounds exhibited large magnetostrictions at 77 K, the largest effect being obtained for Tb6Fe23. Saturation magnetostriction values for the compounds were also determined for 77 K and room temperature. Results of the temperature dependence of magnetostriction for Er6Fe23 are in good agreement with Callen and Callen's single ion theory. Therefore, the main sources of magnetostriction in this compound is the Er ion. The spin-up and spin-down electronic energy bands, the density of states and the magnetic moments of YCo5, SmCo5, and GdCo5 were calculated by the spin polarized augmented plane wave technique. The calculations obtained show the origin of the moment, provide good estimates of its magnitude and variation, and the reasons for those variations. They also show the important role of partial charge transfer and of d-d electronic coupling. Calculations for LaNi5 and GdNi5 systems are discussed.

Wallace, W. E.↗

Ultimate intrinsic-coercivity samarium-cobalt magnet: An Earth-based feasibility study for space-shuttle missions

Techniques for containerless melting and solidification of the samarium-cobalt alloy without excessive oxidation were developed. The rationale for extending these experiments in a weightless environment is also discussed. The effect of oxygen content from 0.15 to 0.63 weight percent and grain size in the range of 2 to 10 micrometers has been examined on arc-plasma-sprayed SmCo5 magnets. Contrary to expectations, the larger grain sizes tended to improve the coercivities. This was attributed to an increase in homogeneity resulting from higher temperature treatments used to produce larger grain size. No significant differences in coercivity were observed on the basis of oxygen content in the range examined. It is expected that more meaningful data on the relationship between oxygen content and coercivity will be seen when the oxygen content can be lowered to less than 0.1 weight percent.

Das, D. K.↗

Electromagnetic containerless reaction of samarium with cobalt for the formation of samarium-cobalt alloys

The electromagnetic levitation technique has been used to obtain nearly stoichiometric SmCo5, with the reaction temperature controlled by a gas jet. The results of several experiments carried out at a 450 kHz, 25 kw RF power levitation facility using different reaction times and cooling rates are presented. It is shown that reaction rates achieved with the levitation technique are larger than the expected diffusion rate in the system liquid samarium-solid cobalt. It is also shown that substantial mixing occurs in the RF-levitated melt.

Chang, C. W.↗

Producing Low-Oxygen Samarium/Cobalt Magnet Alloy

Experiments aimed at producing SmCo5 alloy with low oxygen contamination described in report. Two methods of alloying by melting without contact with crucible walls tested. Lowest oxygen contamination, 70 parts per million achieved by dc arc melting on water-cooled, tantalum-clad copper hearth in purified quiescent argon atmosphere. Report includes photographs of equipment, photomicrographs of alloy samples, detailed descriptions of procedures tried, and tables of oxygen contamination and intrinsic coercivities of samples produced.

Das, Dilip K.↗

Design and testing of a coaxial linear magnetic spring with integral linear motor

The design of a coaxial linear magnetic spring which incorporates a linear motor to control axial motion and overcome system damping is presented, and the results of static and dynamic tests are reported. The system has nominal stiffness 25,000 N/m and is designed to oscillate a 900-g component over a 4.6-mm stroke in a Stirling-cycle cryogenic refrigerator being developed for long-service (5-10-yr) space applications (Stolfi et al., 1983). Mosaics of 10 radially magnetized high-coercivity SmCO5 segments enclosed in Ti cans are employed, and the device is found to have quality factor 70-100, corresponding to energy-storage efficiency 91-94 percent. Drawings, diagrams, and graphs are provided.

Patt, P. J.↗