Search NASA⌕ Search

SEARCH · Search NASA

Results for “Spark Plasma Sintering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Selective laser sintering and spark plasma sintering of (Zr,Nb,Ta,Ti,W)C compositionally complex carbide ceramics

Abstract Two advanced manufacturing processes, spark plasma sintering (SPS) and selective laser sintering (SLS), have been developed for synthesis of (Zr,Nb,Ta,Ti,W)C compositionally complex carbide (CCC) via reactive sintering of a powder mixture of constitute monocarbides. X‐ray diffraction analysis confirmed that the single‐phase CCC can be formed by both SPS and SLS. While a homogenous microstructure with uniform metal element distributions was developed during SPS, three‐layer microstructures with a thin TiC‐rich layer and two TaC‐rich layers along with a TiO 2 ‐rich surface layer containing W nanoparticles were formed during SLS. In addition, cellular structures with W, Zr, and Ti element segregation and dislocations on cell boundaries were observed in the SLS‐CCC sample, indicating the effect of nonequilibrium conditions on microstructure formation during laser melting followed by rapid cooling and solidification process. Compared to the SPS‐CCC sample, the SLS‐CCC showed enhanced hardness and reduced thermal conductivity, which may be related to their unique cellular structures.

36 MATERIALS SCIENCE↗

Microstructure refinement of hot deformed Dy-free NdFeB magnets through a novel cold sintering approach by pressure-assisted spark plasma sintering

Anisotropic fine-grained Dy-free NdFeB high-performance magnets were produced using a novel cold sintering approach by pressure-assisted spark plasma sintering (SPS). The NdFeB nanocrystalline ribbon powders were subjected to cold sintering below 450 °C using pressure-assisted SPS, followed by hot deformation at 710 °C and 810 °C via SPS. Results indicate that cold sintering below 450 °C effectively restricts grain growth in the NdFeB magnets, yielding sub-100 nm scale grains across both fine-grained regions and most coarse-grained regions. The refined grain structure achieved through cold sintering allows for a lower hot deformation temperature as compared with the magnet by conventional sintering, as finer grains allow easier deformation and grain sliding/rotation. This process produces a highly fine-grained and anisotropic microstructure to achieve high magnetic performance (i.e., high intrinsic coercivity, remanence, and maximum energy product) in the magnets. The cold sintering (at 350 °C) and lower hot deformation temperatures required (e.g., 710 °C) help control grain coarsening and limit grain size that is commensurate with the size of a single magnetic domain of the Nd 2 Fe 14 B magnetic matrix phase, resulting in high intrinsic coercivity (H ci =11.4 kOe). Furthermore, the reduced hot deformation temperature mitigates the formation of coarse grain bands, leading to improved magnetic properties, specifically an increased remanence (B r = 14.3 kGs) and a high maximum energy product ((BH) max = 48 MGOe). In conclusion, cold sintered hot deformed NdFeB magnet also shows good thermal stability with reversible temperature coefficient α(B r )= -0.097 %/K and α(H ci )= -0.616 %/K at elevated temperatures up to 400 K.

Cold Sintering↗

Manufacturing porous U-10Zr metallic fuels with controllable microstructure by volume control spark plasma sintering

In this paper, the volume control spark plasma sintering tool has been designed and applied to sinter porous U-10Zr metallic fuels, by which the sintered sample volume can be precisely controlled. Ethanol and NH 4 HCO 3 are used to control the powder compact or as pore formers to control the pore size and pore structure. Without pore formers, the fuel pellet displays an inhomogeneous microstructure consisting of highly porous and highly densified areas. Uneven powder stacking in the green body results in a non-uniform microstructure, and in the closed-packed area, Joule heating accelerates the neck formation and densification. The addition of ethanol reduces the friction between the powders, resulting in isolated pores formed by the stacking of powders during the sintering. By adding NH 4 HCO 3 , the pore size, and structure can be well controlled, and an interconnected pore structure can be obtained upon the decomposition of the NH 4 HCO 3 . Further, a uniform microstructure and pore distributions can be achieved through the U-10Zr fuel pellets by controlling current flow during the volume control SPS sintering. The microstructure and phase characterization of the sintered porous U-10Zr pellets show major phases of α-U and α-Zr for the sample with short dwelling. For the sample with long dwelling (30 min), the ω UZr 2 in the Zr-enriched area has been observed. The strategy of volume control SPS sintering with the assistance of pore formers could be used to fabricate porous U-10Zr metallic fuels to mimic the microstructure evolution of irradiated metallic fuels (including porosity) and could enable a possible solution for the design of new sodium-free metallic fuels for high burnup.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Additive manufacturing of high‐density silicon carbide ceramics through post‐processing spark plasma sintering

This research advances the field of additive manufacturing (AM) of silicon carbide (SiC) ceramics by integrating spark plasma sintering (SPS) to enhance material density, mechanical strength, and thermal properties. Traditional AM techniques struggle to achieve the high‐density SiC required for demanding applications, such as aerospace engineering, where high thermal conductivity and mechanical strength are paramount. Here, our study addresses these challenges by incorporating SPS as a post‐processing step, achieving near‐theoretical maximum densities and significantly reducing porosity, thereby resulting in outstanding thermal conductivity in SiC ceramics. We developed a specialized SiC ink optimized for 3D printing, ensuring structural integrity after deposition through tailored rheological properties. The application of SPS facilitates rapid, uniform sintering, essential for attaining superior density, mechanical properties, and thermal performance. Our experimental results, confirmed through scanning electron microscopy analysis, demonstrate significant microstructural properties, mechanical strength, and thermal conductivity, showcasing the effectiveness of integrating SPS in AM processes. This innovative approach not only expands the capabilities of AM in producing complex, high‐density ceramic structures but also broadens the potential applications of SiC in demanding environments.

36 MATERIALS SCIENCE↗

Solid-state reaction mediated microstructural evolution in a spark plasma sintered in situ Ti–B 4 C composite

For this study, a novel porosity-free in situ Ti–B 4 C composite was fabricated via spark plasma sintering (SPS). Detailed analysis of the phase evolution, coupling results from XRM, XRD and SEM-EBSD-EDS, indicate that primarily TiB 2 precipitates formed due to the in-situ reactions between the boron-carbide and titanium powders. The precipitation of TiB 2 resulted in the formation of a graphitic C-rich thin layer circumscribing the partially reacted B 4 C particles. Further progression of the in-situ reaction leads to the out-diffusion of the excess carbon from the B 4 C particles, across the graphite and TiB 2 phases, forming TiC upon reacting with the titanium matrix. Therefore, the final microstructure primarily consisted of TiB 2 , TiC, and partially reacted B 4 C phases, with small amounts of TiB, α-Ti, and graphite. Furthermore, the microstructure in these SPS processed in situ composites appeared to be the product of a solid-state Ti–B 4 C diffusion couple, substantially different from their fusion-based additively manufactured counterparts. Nano-indentation tests revealed a remarkably high average hardness of ~25 GPa for this SPS-processed Ti–B 4 C composite and comparable (with literature) phase-specific hardness and modulus values for the constituent TiB 2 , TiC, and B 4 C phases.

36 MATERIALS SCIENCE↗

Uniaxial compressive creep tests by spark plasma sintering of 70% theoretical density α -uranium and U-10Zr

Metallic fuels hold numerous advantages over conventional uranium dioxide fuels and are a key component of several liquid metal-cooled advanced reactor concepts including sodium fast reactors. These fuels undergo rapid swelling during early burnup; consequently, they spend most of their reactor lifetime in a porous state. The presence of this porosity alters many of the mechanical properties of the fuel including creep impacting fuel deformation during axial swelling. This work investigates the creep behavior of the porous fuel using a spark plasma sintering technique. Creep tests were performed for the first time on porous α-phase uranium and uranium with 10 wt. % zirconium (U-10Zr) samples. The samples of α-phase uranium and U-10Zr were fabricated from depleted uranium by spark plasma sintering and subjected to uniaxial compressive creep testing. Calculated stress exponents were found to be 2.6±1.6 and 5.7±1.4 for α-U and U-10Zr, respectively, and calculated activation energies were found to be 61.6±1.1kJ/mol for α-U. The creep data were also used to evaluate existing porosity inclusive in creep models.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High density UO2 and high thermal conductivity UO2 composites by spark plasma sintering (SPS)

Embodiments of the invention are directed to a method for production of a nuclear fuel pellet by spark plasma sintering (SPS), wherein a fuel pellet with more than 80% TD or more than 90% TD is formed. The SPS can be performed with the imposition of a controlled uniaxial pressure applied at the maximum temperature of the processing to achieve a very high density, in excess of 95% TD, at temperatures of 850 to 1600° C. The formation of a fuel pellet can be carried out in one hour or less. In an embodiment of the invention, a nuclear fuel pellet comprises UO 2 and a highly thermally conductive material, such as SiC or diamond.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Spark plasma sintering of fuel meats for U 3 O 8 based dispersion fuels

Research and test reactors often use dispersion-type fuel due to its increased thermal conductivity and burn-up capabilities compared to conventional fuel. Al-U 3 O 8 (aluminumtriuranium octaoxide) dispersion fuels have several advantages over their competitors, such as higher service temperature and better stability of oxygen stoichiometry. However, the two-step fabrication of dispersion fuel causes undesirable porosity in cold-pressed fuel meats that is preserved in co-extruded fuel plates. To combat this, spark plasma sintering (SPS) was used for the fabrication of Al-15, 20, and 30 vol% U 3 O 8 and 8 and 12 vol% Mo-U 3 O 8 fuel meats for the Al-U 3 O 8 time. The in situ SPS data was used to construct and validate Master Sintering Curves (MSCs) with accuracies in Al fuels at 0.02 g/cm 3 , and Mo fuels at 0.07 and 0.17 g/cm 3 . The as-sintered fuel meats were characterised using x-ray diffraction (XRD) and scanning electron microscopy (SEM) to understand chemical and physical changes following the SPS process. The pellets exhibited very high relative densities, the U 3 O 8 was observed to undergo reduction to UO 2 .

Aluminium↗

Graded microstructure and mechanical properties of spark plasma sintered Fe-Cr alloys

Developing graded microstructure and mechanical properties is critical for accelerating the design and optimization of structural materials for a wide range of applications. Here, in this study, Fe-Cr alloys were fabricated by spark plasma sintering (SPS) technique. The microstructure, microhardness, and tensile properties of the as-fabricated and thermally annealed variants were investigated. Graded grain structures were created in the as-fabricated cylinders along both axial and radial directions. Grain size was gradually reduced from the sample periphery to the center. Microhardness measurements reveal a gradual decrease of hardness towards the periphery of the samples. The as-fabricated Fe-Cr alloys show a desired combination of tensile strength and elongation, primarily due to the formation of a high density of oxides, voids, dislocations, and grain boundaries. After in-situ thermal annealing at 600 °C under 60 MPa for 2 h using SPS, the Fe-Cr alloys underwent minimal grain growth, and the graded grain structures were retained. The hardness was more uniformly distributed in the annealed variants, and the tensile strength was reduced with an increase in the total elongation, which is attributed to the dissolution of nano-sized oxide particles and the relief of the residual stress. This study demonstrates that SPS coupled with subsequent heat treatment can tailor the graded microstructure and control the mechanical properties of Fe-Cr alloys, showing potential applications in other alloy systems.

36 MATERIALS SCIENCE↗

Manufacturing Bulk Nanocrystalline Al-3Mg Components Using Cryomilling and Spark Plasma Sintering

In the current study, pure aluminum (Al) powders were cryomilled with and without 3 wt.% pure magnesium (Mg) dopant for varying durations followed by spark plasma sintering (SPS) of powders to prepare bulk components with superior mechanical properties. The crystallite sizes were determined for powders and the bulk components by analyzing the X-ray diffraction (XRD) spectrum. The calculations indicated a reduction in crystallite size with the increase in the cryomilling duration. The results also showed a more significant decrease in the crystallite sizes for Al-3Mg samples than that of pure Al. The changes in the surface morphology of powders were characterized using scanning electron microscopy (SEM). The elemental mapping analysis at nanoscale was carried out using Energy-dispersive X-ray spectroscopy (EDX) in Scanning transmission electron microscopy (STEM). The mechanical properties of the bulk components were assessed using a Vickers Microhardness tester. The test results demonstrated an improvement in the hardness of Mg-doped components. Higher hardness values were also reported with an increase in the cryomilling duration. This article discusses the mechanisms for the reduction in crystallite size for pure Al and Al-3Mg and its subsequent impact on improving mechanical properties.

36 MATERIALS SCIENCE↗

Manufacturing Li 2 TiO 3 -based tritium breeder materials by volume-controlled spark plasma sintering with an optimized microstructure

Multifunctional ceramic breeder materials are highly desirable for the deuterium-tritium fusion to achieve high efficiency in breeding tritium through neutron irradiation of lithium-containing blankets. Li 2 TiO 3 displays unique attributes as a potential ceramic breeder material. An optimized microstructure with three-dimensional interconnected pore structure is required for rapid transport of the tritium for effective fuel cycle, which however enviably results in the degradation of the thermal-mechanical properties of the breeding materials. In this work, nanocrystalline porous Li 2 TiO 3 ceramic pellets with controlled porosities of 14% and 20% are manufactured by volume-controlled spark plasma sintering. An optimized 3D interconnected pore structure is achieved consisting of both micro-sized pores and nano-sized pores embedded in nanocrystalline matrix, which could be beneficial to facilitate easy removal of bred T and He. Further, the 3D interconnected porous structure is well maintained upon isothermal annealing of the SPS-fabricated pellets at relevant operation temperature of the solid breeding materials. Single-phasic porous pellets also display enhanced thermal-mechanical properties, superior to current state-of-the-art materials which establish their potential as a promising tritium breeder material for nuclear fusion applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effect of V Content on Corrosion Behavior of Al-V Alloys Produced by Mechanical Alloying and Subsequent Spark Plasma Sintering

Al-V alloys produced via high-energy ball milling have been reported to show simultaneous improvement of corrosion resistance and mechanical properties compared to traditional Al alloys. In these alloys, V content plays a crucial role in increasing or decreasing the corrosion resistance. Therefore, the effect of V and microstructure on corrosion of high-energy ball milled and subsequently spark plasma sintered Al-xV alloys (x = 2, 5, 10 at%) has been studied. Cyclic potentiodynamic polarization tests and electrochemical impedance spectroscopic analysis revealed the increment of V content up to 5 at% enhanced the corrosion resistance of the alloy. However, highly heterogeneous microstructure in Al-10 at%V resulted in significant localized corrosion over the immersion time. The electrochemical impedance spectroscopy studies over 14 days of immersion revealed underlying corrosion mechanisms.

36 MATERIALS SCIENCE↗

Spark plasma sintered, MoNbTi-based multi-principal element alloys with Cr, V, and Zr

MoNbTi, MoNbTiZr, CrMoNbTiZr, and MoNbTiVZr multi-principal element alloys (MPEAs) were fabricated via spark plasma sintering (SPS) and investigated for use in high-strength applications. The fabrication method by SPS and powder metallurgy differs from those presented in the prior literature, where most MPEAs are fabricated using arc melting (AM) methods. Here cryogenic milling was used to maximize potential defect sinks (grain boundaries) for radiation resistance and to increase ultimate tensile strength through the Hall-Petch effect. SPS was chosen for consolidation in order to maintain a fine-grained structure during densification. Each alloy was characterized using x-ray diffraction and scanning electron microscopy for phase identification and compositional homogeneity. The base ternary alloy MoNbTi presented a predominantly single BCC system with minor cubic phases. The introduction of additional alloying elements—Zr, V, and Cr—heightened the phase complexity and increased the fractions of a secondary BCC phase and an HCP phase from Zr. The addition of Cr induced a larger fraction of the Laves phase to form. The addition of V caused the precipitation of small Mo inclusions. Thermodynamic analysis was performed to understand the separation of phases in each alloy. Discrepancies among the phase predictions generated by thermodynamic models, phases previously presented in the literature, and the characterization results suggest that MPEA fabrication methods, especially solid-state methods, require significant investigation to ensure that alloys can remain stable throughout their anticipated service lifetimes.

36 MATERIALS SCIENCE↗

Pelletization with Spark Plasma Sintering and Characterization of Metal Iodides: An Assessment of Long-Term Radioiodine Immobilization Options

Four promising iodine “getter” materials (Ag, Cu, Bi, and Sn) for radioiodine capture were assessed in their pure metal-iodide (MI x ) pelletized forms to compare relative chemical durabilities. To study chemical durability, commercial MI x compounds of AgI, BiI 3 , BiOI, CuI, and SnI 4 were converted to dense monolithic pellets using spark plasma sintering. Semidynamic leach testing in the form of modified ASTM C1308 tests was then performed on the pellets in two different forms including unmounted (as-pressed) specimens (i.e., “U”) and epoxy-mounted specimens (i.e., “M”) with polished surfaces. The chemical durability results and sample characterizations showed that three of the five MI x compounds tested (i.e., AgI, CuI, and BiOI) displayed moderate to high leach resistances. Further, the remaining two MI x compounds (i.e., BiI 3 and SnI 4 ), which are both desirable iodine waste forms due to their high iodine loading capacities, readily decomposed during leach testing, indicated by crystallographic changes in the specimens as well as large amounts of iodine detected in the leachate solutions. The instabilities of BiI 3 and SnI 4 raise uncertainties for using the base metals/cations (i.e., Bi 0 /Bi 3+ and Sn 0 /Sn 4+ , respectively) as viable getters for radioiodine capture due to likely poor waste form chemical durabilities after capture and consolidation into waste forms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Formation and Consolidation of UN Nanostructures in U-Mo Fuel via Mechanical Alloying and Spark Plasma Sintering

Uranium-molybdenum (U-Mo) alloys show promise as a nuclear fuel system due to their high thermal conductivity and high fuel loading capability. However, U-Mo systems suffer from irradiation induced swelling ultimately affecting the cladding via mechanical and chemical interaction. To address these shortcomings, this thesis investigated the formation of uranium mononitride (UN) nanoparticles within a U-10Mo matrix. To promote the formation of UN, U-10Mo powders were mechanically alloyed under a high purity nitrogen cover gas (99.9995%) atmosphere. Variations were made in stainless steel milling media size, duration of milling, and number of times the milling jar was re-aerated with nitrogen gas. UN nanoparticulates were successfully formed within the U-Mo matrix and was characterized utilizing light element analysis, X-ray diffractometry, scanning and transmission-electron microscopy, electron energy loss spectroscopy, and atom probe tomography. Presence of the UN nanoparticles was found as early as 1-hour into the mechanical alloying process, and significant iron contamination found after 10-hours of milling. The U-Mo/UN powders were compacted using spark plasma sintering techniques in order to stabilize the nanostructure. U-Mo/UN compacts containing small amounts of neodymium and helium were analyzed to observe the defect migration tendencies of fission products within the fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase stability and magnetic and electronic properties of a spark plasma sintered CoFe – P soft magnetic alloy

More efficient power conversion devices are able to transmit greater electrical power across larger distances to satisfy growing global electrical needs. A critical requirement to achieve more efficient power conversion are the soft magnetic materials used as core materials in transformers, inductors, and motors. To that effect it is well known that the use of non-equilibrium microstructures, which are, for example, nanocrystalline or consist of single phase solid solutions, can yield high saturation magnetic polarization and high electrical resistivity necessary for more efficient soft magnetic materials. In this work, we synthesized CoFe – P soft magnetic alloys containing nanocrystalline, single phase solid solution microstructures and studied the effect of a secondary intermetallic phase on the saturation magnetic polarization and electrical resistivity of the consolidated alloy. Single phase solid solution CoFe – P alloys were prepared through mechanically alloying metal powders and phase decomposition was observed after subsequent consolidation via spark plasma sintering (SPS) at various temperatures. The secondary intermetallic phase was identified as the orthorhombic (Co x Fe 1-x ) 2 P phase and the magnetic properties of the (Co x Fe 1-x ) 2 P intermetallic phase were found to be detrimental to the soft magnetic properties of the targeted CoFe – P alloy.

36 MATERIALS SCIENCE↗

Synthesis of Hf 6 Ta 2 O 17 superstructure via spark plasma sintering for improved oxidation resistance of multi-component ultra-high temperature ceramics

Ultra-high temperature ceramics (UHTCs) have shown aspiration to overcome challenges in the thermal protection system (TPS) by designing new materials referred to as multi-component UHTCs (MC-UHTCs) in the compositional space. MC-UHTCs have shown remarkable improvement in oxidation resistance due to the formation of the Hf6Ta2O17 superstructure during plasma exposure. Herein, the Hf 6 Ta 2 O 17 superstructure is synthesized via a solid-state reaction between HfO 2 and Ta 2 O 5 powder mixtures during spark plasma sintering (SPS). The compositions chosen are 50 vol% of HfO 2 -50 vol% of Ta 2 O 5 (50HO-50TO) and 70 vol% of HfO 2 -30 vol% of Ta 2 O 5 (70HO-30TO). The phase quantification via Rietveld analysis showed Hf 6 Ta 2 O 17 as a principal phase with some residual Ta 2 O 5 phase in both the samples. The high-temperature thermal stability of the samples was evaluated using high-velocity plasma jet exposure for up to 3 min. 50HO-50TO was able to withstand the intense plasma condition, which is attributed to the higher content of the Hf 6 Ta 2 O 17 phase (~84%) and lower strain in the Ta 2 O 5 phase. The augmentation in the Hf 6 Ta 2 O 17 phase to 94.7% (in 50HO-50TO) post plasma exposure has been attributed to the invariant transformation from a liquid state to Hf 6 Ta 2 O 17 at temperatures >2500 °C during testing. The mechanical integrity is elucidated from the insignificant change in the hardness ~13.3 GPa before and 11.2 GPa after plasma exposure of the 50HO-50TO sample. As a result, the Hf 6 Ta 2 O 17 superstructure's thermo-mechanical stability suggests developing novel oxidation-resistant MC-UHTCs in compositional space for reusable space vehicle applications.

36 MATERIALS SCIENCE↗

Review of Solid State Consolidation Processing Techniques of ODS Steels (Hot Extrusion, Hot Isostatic Pressing, Spark Plasma Sintering, and Stir Friction Consolidation): Resulting Microstructures and Mechanical Properties

This paper reviews the solid-state consolidation processing techniques for Oxide Dispersion Strengthened steels and compares them in terms of the resulting microstructure and reported mechanical properties. Synthesis techniques include hot extrusion, hot isostatic pressing, spark plasma sintering and friction consolidation. The effects of process parameters on the resulting microstructures and performance are discussed for each technique. Average oxide size, average grain size, and porosity are compared across techniques, as well as mechanical strength and ductility. Across consolidation techniques where temperature can be controlled, a low sintering temperature with a high sintering pressure is favorable for keeping oxide sizes, grain sizes, and porosity low. The use of yttrium and titanium for oxide formation has been evidenced to reduce oxide sizes, and tungsten additions have been shown to improve strength. Current literature suggests that the more mature hot extrusion technique produces stronger steel with consistently fine oxides, while other alternative solid-state consolidation, while promising, offer margin for improvement.