Mesoscale Evaluation of Titanium Silicide Monolayer as a Cathode Host Material in Lithium–Sulfur Batteries
Not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not provided.
Effect of initial massive type structure of a gamma-TiAl based alloy on its hot deformed and stabilized microstructure was investigated. A gamma alloy with composition of Ti-47Al-12Nb-0.5Si was subjected to rapid quenching from alpha phase field. The quenched sample was deformed at high temperature. Further post deformation heat treatment was conducted to stabilize the as-deformed structure. It was shown that Nb and Si have important roles in grain refinement of the final product. Presence of niobium in the alloy made the diffusion controlled eutectoid reaction sluggish and assisted the formation of massive type gamma phase (gamma{sub m}) by rapid cooling from alpha phase field. Silicon addition assisted the microstructural refinement by forming hard and finely dispersed titanium silicide particles. These particles act as preferred sites for dynamic recrystallization during hot deformation. Massive gamma phase tends to deform uniformly and decompose to equilibrium phases after final heat treatment and results in a very fine grained microstructure.
The mechanism of heat transfer and the contribution of electron-phonon coupling to thermal conductance of a metal-semiconductor interface remains unclear in the present literature. We report ab initio simulations of a technologically important titanium silicide (metal)–silicon (semiconductor) interface to estimate the Schottky barrier height, and the strength of electron-phonon and phonon-phonon heat transfer across the interface. The electron and phonon dispersion relations of TiSi{sub 2} with C49 structure and the TiSi{sub 2}-Si interface are obtained using first-principles calculations within the density functional theory framework. These are used to estimate electron-phonon linewidths and the associated Eliashberg function that quantifies coupling. We show that the coupling strength of electrons with interfacial phonon modes is of the same order of magnitude as coupling of electrons to phonon modes in the bulk metal, and its contribution to electron-phonon interfacial conductance is comparable to the harmonic phonon-phonon conductance across the interface.
A process for the production of a corrosion resistant coating on graphite and carbon bodies is described. The carbon or graphite body is coated or impregnated with titanium silicide under the addition of a metal containing wetting agent in a nitrogen free atmosphere, so that a tight coating is formed.
Several composite systems made of titanium matrix reinforced with silicon carbide fiber were investigated to obtain a better understanding of composite-degradation mechanisms and to develop techniques to minimize loss of mechanical properties during fabrication and in service. Emphasis was on interface control by fiber or matrix coatings. X-ray diffraction studies on planar samples showed that the formation of titanium silicides was greatly inhibited by the presence of aluminum or Ti3A1 layers at the fiber-matrix interface, with the Ti3A1 being more effective in reducing the reactions. Fiber studies showed that coating the fiber with a 1-micron-thick layer of aluminum improved the as-fabricated strength of a stoichiometric SiC fiber and reduced the fiber degradation during exposure to composite-fabrication conditions. Applying an interfacial barrier by coating the matrix foils instead of the fibers was found to be an effective method for improving composite strength. Reducing the fabrication temperature also resulted in significant improvements in composite strengths. Good-quality, well-consolidated composites were fabricated at temperatures well below those currently used for SiC-Ti composite fabrication.
Nanotechnology has created a demand for new fabrication methods with an emphasis on simple, low-cost techniques. Directional solidification of eutectics (DSE) is an unconventional approach in comparison to low-temperature biomimetic approaches. A technical challenge for DSE is producing microstructural architectures on the nanometer scale. In both processes, the driving force is the minimization of Gibb's free energy. Selfassembly by biomimetic approaches depends on weak interaction forces between organic molecules to define the architectural structure. The architectural structure for solidification depends on strong chemical bonding between atoms. Constituents partition into atomic-level arrangements at the liquid-solid interface to form polyphase structures, and this atomic-level arrangement at the liquid-solid interface is controlled by atomic diffusion and total undercooling due to composition (diffusion), kinetics, and curvature of the boundary phases. Judicious selection of the materials system and control of the total undercooling are the keys to producing structures on the nanometer scale. The silicon-titanium silicide (Si-TiSi2) eutectic forms a rod structure under isothermal cooling conditions. At the NASA Glenn Research Center, directional solidification was employed along with a thermal gradient to promote uniform rods oriented with the thermal gradient. The preceding photomicrograph shows the typical transverse microstructure of a solidified Si-TiSi2 eutectic composition. The dark and light gray regions are Si and TiSi2, respectively. Preferred rod orientation along the thermal gradient was poor. The ordered TiSi2 rods have a narrow distribution in diameter of 2 to 3 m, as shown. The rod diameter showed a weak dependence on process conditions. Anisotropic etch behavior between different phases provides the opportunity to fabricate structures with high aspect ratios. The photomicrographs show the resulting microstructure after a wet chemical etch and a dry plasma etch. The wet chemical etches the silicon away, exposing the TiSi2 rods, whereas plasma etching preferentially etches the Si-TiSi2 interface to form a crater. The porous architectures are applicable to fabricating microdevices or creating templates for part fabrication. The porous rod structure can serve as a platform for fabricating microplasma devices for propulsion or microheat exchangers and for fabricating microfilters for miniatured chemical reactors. Although more work is required, self-assembly from DSE can have a role in microdevice fabrication.
An antifuse is disclosed which has an electrically-insulating region sandwiched between two electrodes. The electrically-insulating region has a single layer of a non-hydrogenated silicon-rich (i.e. non-stoichiometric) silicon nitride SiN.sub.X with a nitrogen content X which is generally in the range of 0<X.ltoreq.1.2, and preferably 0.5.ltoreq.X.ltoreq.1.2. The breakdown voltage V.sub.BD for the antifuse can be defined to be as small as a few volts for CMOS applications by controlling the composition and thickness of the SiN.sub.X layer. The SiN.sub.X layer thickness can also be made sufficiently large so that Poole-Frenkel emission will be the primary electrical conduction mechanism in the antifuse. Different types of electrodes are disclosed including electrodes formed of titanium silicide, aluminum and silicon. Arrays of antifuses can also be formed.
Silicides and germanides are compounds consisting of a metal and silicon or germanium. In the microelectronics industry, silicides are the material of choice for contacting silicon based devices (over the years, CoSi{sub 2}, C54-TiSi{sub 2}, and NiSi have been adopted), while germanides are considered as a top candidate for contacting future germanium based electronics. Since also strain engineering through the use of Si{sub 1−x}Ge{sub x} in the source/drain/gate regions of MOSFET devices is an important technique for improving device characteristics in modern Si-based microelectronics industry, a profound understanding of the formation of silicide/germanide contacts to silicon and germanium is of utmost importance. The crystallographic texture of these films, which is defined as the statistical distribution of the orientation of the grains in the film, has been the subject of scientific studies since the 1970s. Different types of texture like epitaxy, axiotaxy, fiber, or combinations thereof have been observed in such films. In recent years, it has become increasingly clear that film texture can have a profound influence on the formation and stability of silicide/germanide contacts, as it controls the type and orientation of grain boundaries (affecting diffusion and agglomeration) and the interface energy (affecting nucleation during the solid-state reaction). Furthermore, the texture also has an impact on the electrical characteristics of the contact, as the orientation and size of individual grains influences functional properties such as contact resistance and sheet resistance and will induce local variations in strain and Schottky barrier height. This review aims to give a comprehensive overview of the scientific work that has been published in the field of texture studies on thin film silicide/germanide contacts.
The adherence, friction, and wear properties of thin hard refractory compound coatings applied to 440C bearing steel by radiofrequency sputtering were investigated. Friction and wear tests were done with nonconforming pin on disk specimens. The compounds examined were chromium carbide, molybdenum silicide, and titanium carbide. The adherence, friction, and wear were markedly improved by the application of a bias voltage to the bearing steel substrate during coating deposition. Analysis by X-ray photoelectron spectroscopy indicated that the improvement may be due to a reduction in impurities in bias deposited coatings. A fivefold reduction in oxygen concentration in MoSi2 coating by biasing was noted. Chromium carbide was not effective as an antiwear coating. Molybdenum silicide provided some reduction in both friction and wear. Titanium carbide exhibited excellent friction and antiwear properties at light loads. Plastic flow and transfer of the coating material onto the pin specimen appears to be important in achieving low friction and wear.
The complex permittivity for Pt, Pd, Ni, and Ti-silicide films as well as heavily doped p- and n-type silicon were determined by ellipsometry over the energy range 0.031 eV to 4.0 eV. Fits to the Drude model gave bulk plasma and relaxation frequencies. Rutherford backscattering spectroscopy, X-ray diffraction, scanning electron microscopy, secondary ion mass spectrometry, and four-point probe measurements complemented the optical characterization. Calculations from measured permittivities of waveguide loss and mode confinement suggest that the considered materials are better suited for long-wavelength surface-plasmon-polariton waveguide applications than metal films.
The thermal stability of epitaxial SrTiO{sub 3} thin films grown by molecular-beam epitaxy on Si (001) has been studied using x-ray diffraction (XRD), optical microscopy (OM), scanning electron microscopy (SEM), and thermodynamic calculations. Our studies focus on the stability of the SrTiO{sub 3}/Si structures under the conditions typically employed in the pulse laser deposition (PLD) growth of complex metal oxide heteroepitaxy on Si. We observe additional Bragg peaks in thermally treated SrTiO{sub 3} buffered Si structures, corresponding to possibly TiSi{sub 2} and/or SrSiO{sub 3}, reaction products which are consistent with the reaction schemes we propose. In addition, OM and SEM reveal microstructures that are not readily accounted for solely by the solid state reactions as put forth by previous workers but can be reasonably explained by our proposed reaction schemes. Using our observations and thermodynamic analysis, we argue that reactions involving the gaseous species SiO(g), the reactivity of which has not been previously considered in this system, are important. We attribute the onset of degradation of the SrTiO{sub 3} film at high temperatures, to the circular void forming reaction Si(s)+SiO{sub 2}(s){yields}2SiO(g) at the interface and suggest that the reactions considered by previous workers involving all solid state reactants occurs only at the conclusion of degradation. Our results points to the need for keeping the PLD temperature as low as possible to minimize the production of reactive SiO(g) in avoiding the deleterious reactions.
Zr-modified silicide coatings were prepared on Ti-6Al-4 V alloy by pack cementation process to enhance its wear resistance. The microstructure and wear properties of the substrate and the coatings were comparatively investigated using GCr15 and Al{sub 2}O{sub 3} as the counterparts under different sliding loads. The obtained Zr-modified silicide coating had a multilayer structure, consisting of a thick (Ti,X)Si{sub 2} (X represents Al, Zr and V elements) outer layer, a TiSi middle layer and a Ti{sub 5}Si{sub 4} + Ti{sub 5}Si{sub 3} inner layer. The micro-hardness of the coating was much higher than the substrate and displayed a decrease tendency from the coating surface to the interior. Sliding against either GCr15 or Al{sub 2}O{sub 3} balls, the coatings showed superior anti-friction property to the Ti-6Al-4 V alloy, as confirmed by its much lower wear rate under each employed sliding condition.
Ti{sub 5}Si{sub 3}, Ti{sub 5}Si{sub 3}/TiC, and Ti{sub 5}Si{sub 3}/Ti{sub 3}SiC{sub 2} have been electrochemically synthesized from the Ti-bearing blast furnace slag/TiO{sub 2} and/or C mixture precursors at a cell voltage of 3.8 V and 1223 K to 1273 K (950 °C to 1000 °C) in molten CaCl{sub 2}. The pressed porous mixture pellets were used as the cathode, and a solid oxide oxygen-ion-conducting membrane (SOM)-based anode was used as the anode. The phase composition and morphologies of the cathodic products were systematically characterized. The final products possess a porous nodular microstructure due to the interconnection of particles. The variations of impurity elements, i.e., Ca, Mg, and Al, have been analyzed, and the result shows that Ca and Mg can be almost completely removed; however, Al cannot be easily removed from the pellet due to the formation of Ti-Al alloys during the electroreduction process. The electroreduction process has also been investigated by the layer-depended phase composition analysis of the dipped/partially reduced pellets to understand the detailed reaction process. The results indicate that the electroreduction process of the Ti-bearing blast furnace slag/TiO{sub 2} and/or C mixture precursors can be typically divided into four periods, i.e., (i) the decomposition of initial Ca(Mg,Al)(Si,Al){sub 2}O{sub 6}, (ii) the reduction of Ti/Si-containing intermediate phases, (iii) the removal of impurity elements, and (iv) the formation of Ti{sub 5}Si{sub 3}, TiC, and Ti{sub 3}SiC{sub 2}. It is suggested that the SOM-based anode process has great potential to be used for the direct and facile preparation of Ti alloys and composites from cheap Ti-containing ores.
In order to improve the ZrC-SiC ceramic and TC4 brazed joint property, graded double-layered SiC particles (SiCp)-reinforced TC4-based composite structure (named as GLS for convenience) was designed to relieve the residual stress in the joint. The GLS was successfully fabricated on TC4 substrate by double-layered laser deposition technology before the brazing process. The investigation of the GLS shows that the volume fraction of SiCp in the two composite layers was graded (20 and 39 vol pct, respectively). Ti{sub 5}Si{sub 3} and TiC phases formed in the GLS due to the reaction of SiCp and TC4. The laser power-II (the laser power for the second deposition layer) affected the microstructure of the GLS significantly. Increasing the laser power-II would promote the reaction between the SiCp and TC4. But the high laser power-II made the layer I remelt completely and the two layers became homogeneous rather than graded structure. In the ZrC-SiC and TC4 brazed joint, the CTE (coefficient of thermal expansion) was graded from the TC4 to the ZrC-SiC due to the GLS, and the strength of the joint with the GLS (91 MPa) was higher than that without the GLS (43 MPa).
Vacuum brazing of TC4 alloy and SiO{sub 2} ceramic was achieved using a nano-AgCuNi braze alloy. The melting temperature of nano-AgCu powders was analyzed by differential scanning calorimeter. Furthermore, the effects of the Ni content on the microstructure and mechanical properties of the joints were studied. The results showed that the melting temperature of the nano-AgCu filler was 774 °C. A decrease in the melting temperature of 6 °C was observed, compared with the general AgCu filler, and this decrease enabled the interfacial reaction of the joint to begin earlier. The typical interfacial microstructure of the TC4/nano-AgCuNi/SiO{sub 2} ceramic joint brazed at 950 °C for 10 min was TC4/α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure/Ti{sub 2}(Cu,Ni) compound with α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure/Ti{sub 4}O{sub 7} + TiSi{sub 2}/SiO{sub 2} ceramics. The homogeneous microstructure of α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectoid structure primarily existed in the diffusion layer. Additionally, the refined α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure created via a eutectic reaction and Ti{sub 2}(Cu,Ni) compound was distributed in the brazing seam. The Ni content could influence the formation of Ti-Cu-Ni ternary intermetallic compounds (IMCs). An increase in Ni led to an increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure in the brazing seam. The shear strength of the brazed joints first increased and then decreased with the increase in the nano-Ni content, and the optimal shear strength of 30.1 MPa was achieved at 10 wt.% Ni. The increase in the α-Ti + Ti{sub 2}(Cu,Ni) + Ti{sub 2}(Ni,Cu) hypereutectic structure and the decrease in brittle compounds enhanced the shear strength of the joint. Fracture analysis of the joints brazed at 950 °C for 10 min indicated that the cracks mainly occurred in SiO{sub 2} ceramic.
During investigations of novel material types with uses in future nuclear technologies (ITER/DEMO and GenIV fission reactors), ternary carbides with compositions Ti{sub 3}AlC{sub 2} and Ti{sub 3}SiC{sub 2} have been irradiated with high Xe fluences, 6.25 x 10{sup 15} ions cm{sup -2} ({approx}25-30 dpa), using the IVEM-TANDEM facility at Argonne National Laboratory. Both compositions show high tolerance to damage, and give indications that they are likely to remain crystalline to much higher fluences. There is a visible difference in tolerance between Ti{sub 3}AlC{sub 2} and Ti{sub 3}SiC{sub 2} that can be related to the changes in bonding within each material. These initial findings provide evidence for a novel class of materials (+200 compounds) with high radiation resistance, while, significantly, both of these materials are composed of low-Z elements and hence exhibit no long-term activation.
The structural stabilities, elastic and electronic properties of Ti{sub 5}X{sub 3} (X=Si, Ge, Sn, Pb) compounds with D8{sub 8} structure have been systematically investigated within the frame work of density functional theory. With increase of atomic number of the element X, the calculated lattice constants of Ti{sub 5}X{sub 3} compounds are found to increase, while stabilities of these compounds decrease because the formation enthalpies increase. Moreover, with exception of C{sub 12}, the calculated elastic constants C{sub ij} are reduced with increase of atomic number of element X, the bulk, shear, Young's modulus and Debye temperature are also lowered, while Poisson's ratio is larger, and the ductility is slightly improved. The elastic anisotropies were further studied, especially the 3D direction dependence of these elastic modulus was visually described. The density of states and charge density distribution reveal bonding feature of Ti{sub 5}X{sub 3}. Especially, the X-X and Ti-X covalent bonding strength is found to decrease with increase of atomic number of element X. - Graphical abstract: The charge density contour plots on the (0 0 0 1) plane for Ti{sub 5}Si{sub 3} (a), Ti{sub 5}Ge{sub 3} (b), Ti{sub 5}Sn{sub 3} (c) and Ti{sub 5}Pb{sub 3} (d). Highlights: Black-Right-Pointing-Pointer The elastic constants except C{sub 12} were lowered with increase of atomic number of X. Black-Right-Pointing-Pointer The bulk and shear modulus as well as Young's modulus was also decreased. Black-Right-Pointing-Pointer The elastic anisotropies of Ti{sub 5}X{sub 3} were further studied visually. Black-Right-Pointing-Pointer The X-X and Ti-X covalent bonding strength was lowered.
The aim of the present work is to determine the kinetics of reaction between TiSi{sub 2} powder and gaseous nitrogen. Isothermal nitridation of TiSi{sub 2} powders with fine (1.4 µm) and medium (4.5 µm) particle size has been studied in pure nitrogen atmosphere from 1000 to 1200 °C for duration up to 50 h. The isothermal nitridation kinetics of TiSi{sub 2} powders were investigated by thermogravimetry. The nitridation rate strongly depends on the particle size and temperature. Smaller size particle exhibits higher nitridation rate due to its larger surface area. The conversion process is complex with nucleation and growth of TiN at the surface of the grain and Si{sub 3}N{sub 4} inside the grain promoted by the Kirkendall effect with an influence of the volume increase. - Graphical abstract: Backscattered electrons image of a transverse TiSi{sub 2} grain nitrurated at 1100 °C for 50 h. - Highlights: • Influence of grain size on TiSi{sub 2} powder nitridation. • Influence of temperature on TiSi{sub 2} powder nitridation. • Experimental measurements of the nitridation kinetics. • An explanation of the nitridation mechanism.