Search NASA⌕ Search

SEARCH · Search NASA

Results for “TZM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K

Here, in this study, the corrosion behaviours of molybdenum (Mo) and a Mo-based alloy (TZM) were investigated using a static immersion corrosion technique. Weight loss, surface microstructure, and corrosion depth of Mo and the TZM alloy were correlated with elements. The compatibility of Mo and the TZM alloy in static liquid Li was suitable. Mo demonstrated uniform corrosion with a homogenous dissolution of free C and Mo, and TZM alloy exhibited a nonuniform corrosion behaviour with a preferential grain boundary attack caused by the selective dissolution of free C, Ti, and Zr. When the surface oxidation layer of the samples was consumed, free C from Mo and TZM diffused into molten Li to form Li 2 C 2 and then was captured by Zr, Ti, and Mo to form thermodynamically stable carbides, which resulted in the enrichment of the C layer near the sample surfaces. In addition, Ti and Zr acted as N-trappers in liquid Li; the formation of Zr and Ti nitrides resulted in the enrichment of N, Ti, and Zr elements on the surface and led to TZM corrosion increase. Thus, Zr and Ti depletion, pitting, and grain boundary corrosion were problematic for TZM under long-term exposure to liquid Li. Reducing the content of free C and nonmetallic N and increasing the amount of Ti and Zr carbides on the surface of and inside the raw TZM alloy helped improve the corrosion resistance of TZM in liquid Li.

36 MATERIALS SCIENCE↗

Development of Hydrogen Permeation Barrier and Matrix Interaction Protection Coatings for TZM Enclosure of Hydride Moderators (Microreactor Program M3 Report)

It is important to develop a high-performance enclosure solution for hydride-based microreactor moderation components to effectively suppress hydride thermal decomposition and prevent hydrogen loss in harsh in-reactor environments. Currently, the DOE-NE Microreactor Program (MR program) is investigating the titanium-zirconium-molybdenum (TZM) canned yttrium hydride (YH 2-x ) solution, which provides acceptable hydrogen retainment performance up to ~700 °C. However, improvements in the enclosure are necessary for increasing long-term operation temperature beyond 700 °C and enhancing short-term survivability at even higher temperatures during power transients. One potential solution is the addition of a dedicated hydrogen permeation barrier, which can potentially improve the enclosure's performance. Furthermore, the hydride moderator components will be inserted into the microreactor matrix, which may consist of materials that are not chemically inert against TZM. Therefore, the TZM might need to be protected from the external environment through the application of another surface protection coating. To address these critical issues, two types of barrier coatings optimized for TZM-based moderator enclosure has been developed. A multilayer coating approach has been used to identify TZM-compatible barrier materials. Behavior of these coating designs against H 2 permeation and long-term high-temperature graphite matrix interactions has been examined in detail. Additionally, the developed coatings' behavior when exposed to both high-temperature thermal cycling and heavy-ion irradiation has also been investigated. Overall, the development of these barrier coatings is essential for achieving maturity for the metal hydride moderator technology. The results in this report will provide crucial insights into the behavior of the developed coatings and their potential for improving the long-term performance of TZM-based moderator enclosures.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Thermal stability of oxidized ultrathin Li films on TZM for plasma facing components

For improved understanding of the behavior of Li plasma facing components (PFCs) in the presence of oxygen impurities, we report on the thermal stability of ultrathin (up to 1.0 nm) LiO x films on a titanium-zirconium-molybdenum (TZM) alloy substrate over the temperature range of 310–1400 K. LiO x films were prepared by either post-oxidation of Li films or Li films deposited on an oxygen-precovered TZM surface. Thermal stability of these films was studied using a combination of temperature programmed desorption (TPD), X-ray photoelectron spectroscopy (XPS), and low-energy ion scattering (LEIS). For post-oxidized Li films, TPD showed that no Li desorption occurred until temperatures above 620 K, and then Li desorbed from the surface via at least three desorption peaks. The O 1s XPS spectra on the post-oxidized films at 310 K indicate the formation of lithium oxide (Li2O) and peroxide/hydroxide (Li 2 O 2 /LiOH). The peroxide/hydroxide converts to oxide after heating to 680 K with no desorption of Li or O 2 , and then this film decomposes to liberate Li into the gas phase while leaving oxygen at the TZM surface. Heating the LiO x films to 1070 K led to a solid-state reaction with surface Mo atoms of the substrate to form a condensed binary lithium molybdenum oxide (LixMoOy) phase, which upon further heating decomposed to liberate gas phase binary lithium molybdenum oxide species. Li deposition on an oxygen-precovered TZM surface formed a complex, highly stable, oxygen rich, Li-O-Mo interfacial oxide. Li desorption from multilayer Li films on oxygen-precovered TZM surfaces occurred in a metallic Li multilayer peak and three other oxide-derived peaks. These results support the improved thermal stability of oxidized lithium as compared to metallic Li and have implications for Mo impurity transport into the plasma at high temperatures.

36 MATERIALS SCIENCE↗

Fabrication of a Mo based high temperature TZM alloy by non-consumable arc melting technique

High temperature structural materials are in great demand for power, chemical and nuclear industries which can perform beyond 1000 °C as super alloys usually fail. In this regard, Mo based TZM alloy is capable of retaining strength up to 1500 °C with excellent corrosion compatibility against molten alkali metals. Hence, currently this alloy is considered an important candidate material for high temperature compact nuclear and fusion reactors. Due to reactive nature of Mo and having high melting point, manufacturing this alloy by conventional process is unsuitable. Powder metallurgy technique has limited success due to restriction in quantity and purity. This paper deals with fabrication of TZM alloy by nonconsumable tungsten arc melting technique. Initially a ternary master alloy of Mo-Ti-Zr was prepared which subsequently by dilution method, was converted into TZM alloy gradually by external addition of Mo and C in various proportions. A number of melting trials were conducted to optimize the process parameters like current, voltage and time to achieve desired alloy composition. The alloy was characterized with respect to composition, elemental distribution profile, microstructure, hardness profile and phase analysis. Well consolidated alloy button was obtained having desired composition, negligible material loss and having microstructure as comparable to standard TZM alloy. (author)

36 MATERIALS SCIENCE↗

Results from a new flowing liquid Li limiter with TZM substrate during high confinement plasmas in the EAST device

A third generation flowing liquid lithium (FLiLi) limiter with a substrate made of TZM, an alloy with >99% Mo, was fabricated by conventional manufacturing techniques. TZM has a high corrosion resistance, a high sputtering threshold, and a good wettability to Li, as compared to stainless steel (SS), which had been used as an FLiLi substrate surface in 2014 and 2016. The third generation FLiLi was inserted into the edge in EAST H-mode plasmas in an upper single-null configuration with an ion grad-B drift toward the upper divertor with a limiter temperature of 330–380 °C and an auxiliary heating power of about 2–8 MW. Analysis has shown that by using TZM FLiLi, fuel particle recycling continuously decreased and near-complete edge localized mode elimination was achieved in H-mode plasmas with RF-only heating. The main impurities during the initial FLiLi discharges were Mo, Fe, and W resulting from strong plasma interaction at the Mo plate side, the SS collector, and the upper W divertor. Plasma stored energy increased by about 10 kJ in subsequent FLiLi discharges due to decreased impurity radiation. Engineering analysis shows a uniform lithium flow with an ~80% Li coverage ratio on the limiter surface, similar to the second FLiLi, even though only one of two J × B pumps was functioning. Despite technical difficulties, the FLiLi gen.3 improved the overall plasma performance, providing support for flowing liquid Li plasma facing component applications in present and future devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Investigation of welding and brazing of molybdenum and TZM alloy tubes

This effort involved investigating the welding and brazing techniques of molybdenum tubes to be used as cartridges in the crystal growth cartridge. Information is given in the form of charts and photomicrographs. It was found that the recrystallization temperature of molybdenum can be increased by alloying it with 0.5 percent titanium and 0.1 percent zirconium. Recrystallization temperatures for this alloy, known as TZM, become significant around 2500 F. A series of microhardness tests were run on samples of virgin and heat soaked TZM. The test results are given in tabular form. It was concluded that powder metallurgy TZM may be an acceptable cartridge material.

Lundblad, Wayne E.↗

The Change in the hardness of LCAC. TZM, and ODS molybdenum in the post-irradiated and annealed conditions

Hardness measurements were performed on wrought Low Carbon Arc Cast (LCAC), TZM, and Oxide Dispersion Strengthened (ODS) molybdenum in the post-irradiated and post-irradiated + annealed condition to determine the recovery kinetics. Irradiations performed in the High Flux Isotope Reactor (HFIR) at nominally 300 C and 600 C to neutron fluence levels that range from 10.5 to 246 x 10{sup 24} n/m{sup 2} (E > 0.1 MeV) resulted in relatively large increases in hardness (77-109%), while small increases in hardness (<18%) were observed for irradiations at 870-1100 C. The hardness recovery for ODS and LCAC irradiated at 300 C and 600 C were shown to be complete at 980 C and {approx} 1100-1250 C, respectively. Isothermal annealing at 700 C was used to determine the activation energy for recovery of LCAC and ODS (3.70-4.88 eV {+-} 0.28-0.77 eV), which is comparable to values reported in the literature for molybdenum vacancy self-diffusion. This suggests that recovery of LCAC and ODS is controlled by the solid-state diffusion of vacancies in the bulk, and that the finer grain size and particle size ODS does not affect this mechanism. TZM exhibited slower recovery kinetics, which can be explained by the solute atoms (titanium and zirconium) inhibiting vacancy diffusion.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Post-Irradiation Fracture Toughness of Unalloyed Molybdenum, ODS molybdenum, and TZM molybdenum following irradiation at 244C to 507C

Commercially available unalloyed molybdenum (Low Carbon Arc Cast (LCAC)), Oxide Dispersion Strengthened (ODS) molybdenum, and TZM molybdenum were neutron irradiated at temperatures of nominally 244 C, 407 C, and 509 C to neutron fluences between 1.0 to 4.6x1025 n/m2 (E>0.1 MeV). Post-irradiation fracture toughness testing was performed. All alloys exhibited a Ductile to Brittle Transition Temperature that was defined to occur at 30 4 MPa-m1/2. The highest post-irradiated fracture toughness values (26-107 MPa-m1/2) and lowest DBTT (100-150 C) was observed for ODS molybdenum in the L-T orientation. The finer grain size for ODS molybdenum results in fine laminates that improve the ductile laminate toughening. The results for ODS molybdenum are anisotropic with lower post-irradiated toughness values (20-30 MPa-m1/2) and higher DBTT (450-600 C) in the T-L orientation. The results for T-L ODS molybdenum are consistent or slightly better than those for LCAC molybdenum (21-71 MPa-m1/2 and 450-800 C DBTT). The fracture toughness values measured for LCAC and T-L ODS molybdenum at temperatures below the DBTT were determined to be 8-18 MPa-m1/2. Lower non-irradiated fracture toughness values were measured for TZM molybdenum that are attributed to the large carbide precipitates serving as preferential fracture initiation sites. The role of microstructure and grain size on post-irradiated fracture toughness was evaluated by comparing the results for LCAC molybdenum and ODS molybdenum.

Cockeram, Brian V↗

Effects of temperature and surface contamination on D retention in ultrathin Li films on TZM

Here in this work, we investigate deuterium retention at the Mo-Li interface by studying thin Li films three monolayers thick on a TZM Mo alloy. Li films at temperatures between 315 and 460 K were exposed to a deuterium ion beam and D retention was measured using temperature programmed desorption. In the absence of oxygen, D is retained as LiD, and the relative amount of retained D decreases with increasing substrate temperature. In three-monolayer thick lithium oxide films, the amount of D retained was 2.5 times higher than the amount retained as LiD in the metallic Li film. However, oxygen reduces the thermal stability of D in the film, causing D 2 O and D 2 to be released from the surface at temperatures 150-200 K below the LiD decomposition temperature. These results highlight the importance of maintaining a metallic Li layer for high D retention in Li films on TZM at elevated temperatures.

36 MATERIALS SCIENCE↗

Development of explosively bonded TZM wire reinforced Columbian sheet composites

Methods of producing TZM molybdenum wire reinforced C129Y columbium alloy composites by explosive welding were studied. Layers of TZM molybdenum wire were wound on frames with alternate layers of C129Y columbium alloy foil between the wire layers. The frames held both the wire and foils in place for the explosive bonding process. A goal of 33 volume percent molybdenum wire was achieved for some of the composites. Variables included wire diameter, foil thickness, wire separation, standoff distance between foils and types and amounts of explosive. The program was divided into two phases: (1) development of basic welding parameters using 5 x 10-inch composites, and (2) scaleup to 10 x 20-inch composites.

Otto, H. E.↗

Irradiation of TZM: Uranium dioxide fuel pin at 1700 K

A fuel pin clad with TZM and containing solid pellets of uranium dioxide was fission heated in a static helium-cooled capsule at a maximum surface temperature of 1700 K for approximately 1000 hr and to a total burnup of 2.0 percent of the uranium-235. The results of the postirradiation examination indicated: (1) A transverse, intergranular failure of the fuel pin occurred when the fuel pin reached 2.0-percent burnup. This corresponds to 1330 kW-hr/cu cm, where the volume is the sum of the fuel, clad, and void volumes in the fuel region. (2) The maximum swelling of the fuel pin was less than 1.5 percent on the fuel-pin diameter. (3) There was no visible interaction between the TZM clad and the UO2. (4) Irradiation at 1700 K produced a course-grained structure, with an average grain diameter of 0.02 centimeter and with some of the grains extending one-half of the thickness of the clad. (5) Below approximately 1500 K, the irradiation of the clad produced a moderately fine-grained structure, with an average grain diameter of 0.004 centimeter.

Mcdonald, G. E.↗

Effects of long-term aging on ductility of the columbium alloys C-103, Cb-1Zr, and Cb-752 and the molybdenum alloy Mo-TZM

A program was conducted to determine if aging embrittlement occurs in the columbium alloys C-103, CB-1Zr, and Cb-752 or in the molybdenum alloy Mo-TZM. Results showed that aging embrittlement does not occur in C-103, Cb-1Zr, or Mo-TZM during long-term (1000 hr) aging at temperatures in the range 700 to 1025 C. In contrast, aging embrittlement did occur in the Cb-752 alloy after similar aging at 900 C. A critical combination of the solute additions W and Zr in Cb-752 led to Zr segregation at grain boundaries during long-term aging. This segregation subsequently resulted in embrittlement as indicated by an increase in the ductile-brittle transition temperature from below -1960 C to about -150 C.

Stephens, J. R.↗

The Design and Use of Tungsten Coated TZM Molybdenum Tile Inserts in the DIII-D Tokamak Divertor

Future tokamak devices are envisioned to utilize a high-Z metal divertor with tungsten as theleading candidate. However, tokamak experiments with tungsten divertors have seen significantdetrimental effects on plasma performance. The DIII-D tokamak presently has carbon as theplasma facing surface but to study the effect of tungsten on the plasma and its migration aroundthe vessel, two toroidal rows of carbon tiles in the divertor region were modified with high-Zmetal inserts, composed of a molybdenum alloy (TZM) coated with tungsten. A dedicated twoweek experimental campaign was run with the high-Z metal inserts. One row was coated withtungsten containing naturally occurring levels of isotopes. The second row was coated withtungsten where the isotope 182W was enhanced from the natural level of 26% up to greater than90%. The different isotopic concentrations enabled the experiment to differentiate between thetwo different sources of metal migration from the divertor. Various coating methods wereexplored for the deposition of the tungsten coating, including chemical vapor deposition,electroplating, vacuum plasma spray, and electron beam physical vapor deposition. The coatingswere tested to see if they were robust enough to act as a divertor target for the experiment. Testsincluded cyclic thermal heating using a high power laser and high-fluence deuterium plasmabombardment. The issues associate with the design of the inserts (tile installation, thermal stress,arcing, leading edges, surface preparation, etc.), are reviewed. The results of the tests used toselect the coating method and preliminary experimental observations are presented.

Holtrop, Kurt↗

Explosive bonded TZM-wire-reinforced C129Y columbium composites

Technique consists of positioning layers of TZM metal filaments between thin C129Y columbium sheets and joining multiple sheet stacks by single explosive joining operation. Metallurgical bonds are excellent, external heat is not required, process is relatively inexpensive, and resulting composites are considerably stronger than base alloy.

Reece, O. Y.↗