Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K

Here, in this study, the corrosion behaviours of molybdenum (Mo) and a Mo-based alloy (TZM) were investigated using a static immersion corrosion technique. Weight loss, surface microstructure, and corrosion depth of Mo and the TZM alloy were correlated with elements. The compatibility of Mo and the TZM alloy in static liquid Li was suitable. Mo demonstrated uniform corrosion with a homogenous dissolution of free C and Mo, and TZM alloy exhibited a nonuniform corrosion behaviour with a preferential grain boundary attack caused by the selective dissolution of free C, Ti, and Zr. When the surface oxidation layer of the samples was consumed, free C from Mo and TZM diffused into molten Li to form Li 2 C 2 and then was captured by Zr, Ti, and Mo to form thermodynamically stable carbides, which resulted in the enrichment of the C layer near the sample surfaces. In addition, Ti and Zr acted as N-trappers in liquid Li; the formation of Zr and Ti nitrides resulted in the enrichment of N, Ti, and Zr elements on the surface and led to TZM corrosion increase. Thus, Zr and Ti depletion, pitting, and grain boundary corrosion were problematic for TZM under long-term exposure to liquid Li. Reducing the content of free C and nonmetallic N and increasing the amount of Ti and Zr carbides on the surface of and inside the raw TZM alloy helped improve the corrosion resistance of TZM in liquid Li.

36 MATERIALS SCIENCE↗

Development of Hydrogen Permeation Barrier and Matrix Interaction Protection Coatings for TZM Enclosure of Hydride Moderators (Microreactor Program M3 Report)

It is important to develop a high-performance enclosure solution for hydride-based microreactor moderation components to effectively suppress hydride thermal decomposition and prevent hydrogen loss in harsh in-reactor environments. Currently, the DOE-NE Microreactor Program (MR program) is investigating the titanium-zirconium-molybdenum (TZM) canned yttrium hydride (YH 2-x ) solution, which provides acceptable hydrogen retainment performance up to ~700 °C. However, improvements in the enclosure are necessary for increasing long-term operation temperature beyond 700 °C and enhancing short-term survivability at even higher temperatures during power transients. One potential solution is the addition of a dedicated hydrogen permeation barrier, which can potentially improve the enclosure's performance. Furthermore, the hydride moderator components will be inserted into the microreactor matrix, which may consist of materials that are not chemically inert against TZM. Therefore, the TZM might need to be protected from the external environment through the application of another surface protection coating. To address these critical issues, two types of barrier coatings optimized for TZM-based moderator enclosure has been developed. A multilayer coating approach has been used to identify TZM-compatible barrier materials. Behavior of these coating designs against H 2 permeation and long-term high-temperature graphite matrix interactions has been examined in detail. Additionally, the developed coatings' behavior when exposed to both high-temperature thermal cycling and heavy-ion irradiation has also been investigated. Overall, the development of these barrier coatings is essential for achieving maturity for the metal hydride moderator technology. The results in this report will provide crucial insights into the behavior of the developed coatings and their potential for improving the long-term performance of TZM-based moderator enclosures.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Thermal stability of oxidized ultrathin Li films on TZM for plasma facing components

For improved understanding of the behavior of Li plasma facing components (PFCs) in the presence of oxygen impurities, we report on the thermal stability of ultrathin (up to 1.0 nm) LiO x films on a titanium-zirconium-molybdenum (TZM) alloy substrate over the temperature range of 310–1400 K. LiO x films were prepared by either post-oxidation of Li films or Li films deposited on an oxygen-precovered TZM surface. Thermal stability of these films was studied using a combination of temperature programmed desorption (TPD), X-ray photoelectron spectroscopy (XPS), and low-energy ion scattering (LEIS). For post-oxidized Li films, TPD showed that no Li desorption occurred until temperatures above 620 K, and then Li desorbed from the surface via at least three desorption peaks. The O 1s XPS spectra on the post-oxidized films at 310 K indicate the formation of lithium oxide (Li2O) and peroxide/hydroxide (Li 2 O 2 /LiOH). The peroxide/hydroxide converts to oxide after heating to 680 K with no desorption of Li or O 2 , and then this film decomposes to liberate Li into the gas phase while leaving oxygen at the TZM surface. Heating the LiO x films to 1070 K led to a solid-state reaction with surface Mo atoms of the substrate to form a condensed binary lithium molybdenum oxide (LixMoOy) phase, which upon further heating decomposed to liberate gas phase binary lithium molybdenum oxide species. Li deposition on an oxygen-precovered TZM surface formed a complex, highly stable, oxygen rich, Li-O-Mo interfacial oxide. Li desorption from multilayer Li films on oxygen-precovered TZM surfaces occurred in a metallic Li multilayer peak and three other oxide-derived peaks. These results support the improved thermal stability of oxidized lithium as compared to metallic Li and have implications for Mo impurity transport into the plasma at high temperatures.

36 MATERIALS SCIENCE↗

Fabrication of a Mo based high temperature TZM alloy by non-consumable arc melting technique

High temperature structural materials are in great demand for power, chemical and nuclear industries which can perform beyond 1000 °C as super alloys usually fail. In this regard, Mo based TZM alloy is capable of retaining strength up to 1500 °C with excellent corrosion compatibility against molten alkali metals. Hence, currently this alloy is considered an important candidate material for high temperature compact nuclear and fusion reactors. Due to reactive nature of Mo and having high melting point, manufacturing this alloy by conventional process is unsuitable. Powder metallurgy technique has limited success due to restriction in quantity and purity. This paper deals with fabrication of TZM alloy by nonconsumable tungsten arc melting technique. Initially a ternary master alloy of Mo-Ti-Zr was prepared which subsequently by dilution method, was converted into TZM alloy gradually by external addition of Mo and C in various proportions. A number of melting trials were conducted to optimize the process parameters like current, voltage and time to achieve desired alloy composition. The alloy was characterized with respect to composition, elemental distribution profile, microstructure, hardness profile and phase analysis. Well consolidated alloy button was obtained having desired composition, negligible material loss and having microstructure as comparable to standard TZM alloy. (author)

36 MATERIALS SCIENCE↗

Results from a new flowing liquid Li limiter with TZM substrate during high confinement plasmas in the EAST device

A third generation flowing liquid lithium (FLiLi) limiter with a substrate made of TZM, an alloy with >99% Mo, was fabricated by conventional manufacturing techniques. TZM has a high corrosion resistance, a high sputtering threshold, and a good wettability to Li, as compared to stainless steel (SS), which had been used as an FLiLi substrate surface in 2014 and 2016. The third generation FLiLi was inserted into the edge in EAST H-mode plasmas in an upper single-null configuration with an ion grad-B drift toward the upper divertor with a limiter temperature of 330–380 °C and an auxiliary heating power of about 2–8 MW. Analysis has shown that by using TZM FLiLi, fuel particle recycling continuously decreased and near-complete edge localized mode elimination was achieved in H-mode plasmas with RF-only heating. The main impurities during the initial FLiLi discharges were Mo, Fe, and W resulting from strong plasma interaction at the Mo plate side, the SS collector, and the upper W divertor. Plasma stored energy increased by about 10 kJ in subsequent FLiLi discharges due to decreased impurity radiation. Engineering analysis shows a uniform lithium flow with an ~80% Li coverage ratio on the limiter surface, similar to the second FLiLi, even though only one of two J × B pumps was functioning. Despite technical difficulties, the FLiLi gen.3 improved the overall plasma performance, providing support for flowing liquid Li plasma facing component applications in present and future devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

The Change in the hardness of LCAC. TZM, and ODS molybdenum in the post-irradiated and annealed conditions

Hardness measurements were performed on wrought Low Carbon Arc Cast (LCAC), TZM, and Oxide Dispersion Strengthened (ODS) molybdenum in the post-irradiated and post-irradiated + annealed condition to determine the recovery kinetics. Irradiations performed in the High Flux Isotope Reactor (HFIR) at nominally 300 C and 600 C to neutron fluence levels that range from 10.5 to 246 x 10{sup 24} n/m{sup 2} (E > 0.1 MeV) resulted in relatively large increases in hardness (77-109%), while small increases in hardness (<18%) were observed for irradiations at 870-1100 C. The hardness recovery for ODS and LCAC irradiated at 300 C and 600 C were shown to be complete at 980 C and {approx} 1100-1250 C, respectively. Isothermal annealing at 700 C was used to determine the activation energy for recovery of LCAC and ODS (3.70-4.88 eV {+-} 0.28-0.77 eV), which is comparable to values reported in the literature for molybdenum vacancy self-diffusion. This suggests that recovery of LCAC and ODS is controlled by the solid-state diffusion of vacancies in the bulk, and that the finer grain size and particle size ODS does not affect this mechanism. TZM exhibited slower recovery kinetics, which can be explained by the solute atoms (titanium and zirconium) inhibiting vacancy diffusion.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Post-Irradiation Fracture Toughness of Unalloyed Molybdenum, ODS molybdenum, and TZM molybdenum following irradiation at 244C to 507C

Commercially available unalloyed molybdenum (Low Carbon Arc Cast (LCAC)), Oxide Dispersion Strengthened (ODS) molybdenum, and TZM molybdenum were neutron irradiated at temperatures of nominally 244 C, 407 C, and 509 C to neutron fluences between 1.0 to 4.6x1025 n/m2 (E>0.1 MeV). Post-irradiation fracture toughness testing was performed. All alloys exhibited a Ductile to Brittle Transition Temperature that was defined to occur at 30 4 MPa-m1/2. The highest post-irradiated fracture toughness values (26-107 MPa-m1/2) and lowest DBTT (100-150 C) was observed for ODS molybdenum in the L-T orientation. The finer grain size for ODS molybdenum results in fine laminates that improve the ductile laminate toughening. The results for ODS molybdenum are anisotropic with lower post-irradiated toughness values (20-30 MPa-m1/2) and higher DBTT (450-600 C) in the T-L orientation. The results for T-L ODS molybdenum are consistent or slightly better than those for LCAC molybdenum (21-71 MPa-m1/2 and 450-800 C DBTT). The fracture toughness values measured for LCAC and T-L ODS molybdenum at temperatures below the DBTT were determined to be 8-18 MPa-m1/2. Lower non-irradiated fracture toughness values were measured for TZM molybdenum that are attributed to the large carbide precipitates serving as preferential fracture initiation sites. The role of microstructure and grain size on post-irradiated fracture toughness was evaluated by comparing the results for LCAC molybdenum and ODS molybdenum.

Cockeram, Brian V↗

Effects of temperature and surface contamination on D retention in ultrathin Li films on TZM

Here in this work, we investigate deuterium retention at the Mo-Li interface by studying thin Li films three monolayers thick on a TZM Mo alloy. Li films at temperatures between 315 and 460 K were exposed to a deuterium ion beam and D retention was measured using temperature programmed desorption. In the absence of oxygen, D is retained as LiD, and the relative amount of retained D decreases with increasing substrate temperature. In three-monolayer thick lithium oxide films, the amount of D retained was 2.5 times higher than the amount retained as LiD in the metallic Li film. However, oxygen reduces the thermal stability of D in the film, causing D 2 O and D 2 to be released from the surface at temperatures 150-200 K below the LiD decomposition temperature. These results highlight the importance of maintaining a metallic Li layer for high D retention in Li films on TZM at elevated temperatures.

36 MATERIALS SCIENCE↗

The Design and Use of Tungsten Coated TZM Molybdenum Tile Inserts in the DIII-D Tokamak Divertor

Future tokamak devices are envisioned to utilize a high-Z metal divertor with tungsten as theleading candidate. However, tokamak experiments with tungsten divertors have seen significantdetrimental effects on plasma performance. The DIII-D tokamak presently has carbon as theplasma facing surface but to study the effect of tungsten on the plasma and its migration aroundthe vessel, two toroidal rows of carbon tiles in the divertor region were modified with high-Zmetal inserts, composed of a molybdenum alloy (TZM) coated with tungsten. A dedicated twoweek experimental campaign was run with the high-Z metal inserts. One row was coated withtungsten containing naturally occurring levels of isotopes. The second row was coated withtungsten where the isotope 182W was enhanced from the natural level of 26% up to greater than90%. The different isotopic concentrations enabled the experiment to differentiate between thetwo different sources of metal migration from the divertor. Various coating methods wereexplored for the deposition of the tungsten coating, including chemical vapor deposition,electroplating, vacuum plasma spray, and electron beam physical vapor deposition. The coatingswere tested to see if they were robust enough to act as a divertor target for the experiment. Testsincluded cyclic thermal heating using a high power laser and high-fluence deuterium plasmabombardment. The issues associate with the design of the inserts (tile installation, thermal stress,arcing, leading edges, surface preparation, etc.), are reviewed. The results of the tests used toselect the coating method and preliminary experimental observations are presented.

Holtrop, Kurt↗

Laser Powder Bed Fusion Additive Manufacture Nb1Zr Development

Next generation fission and fusion nuclear reactors require materials that can withstand operating temperatures greater than 500 °C, neutron irradiation doses of up to 200 displacements per atom (dpa), and potentially corrosive coolants such as the alkali liquid metals sodium, lithium, and NaK (Na33K eutectic alloy). Refractory alloys, such as Nb1Zr (Nb-1wt%Zr) and Molybdenum alloy TZM (Mo-0.5wt%Ti-0.08wt%Zr) have been traditionally considered viable candidates for advanced fission and fusion reactor concepts. However, it is relatively difficult to generate complex geometries of interest from these alloys using traditional manufacturing methods. In addition, there needs to be a concentrated effort to address refractory metal challenges at elevated temperature operation. In order to generate complex geometries of interest, modern manufacturing techniques are considered to increase the technological readiness level (TRL), cost-effectiveness, and schedule savings. This work focused on the continued development of laser powder bed fusion (L-PBF) additive manufacturing (AM) to improve both design flexibility, evaluate microstructure and properties, and ultimately accelerate the TRL and qualification of these processes and alloys for components to potentially be put into service. Niobium alloy Nb1Zr was identified through a down-selection process outlined in previous reports as a candidate to develop in L-PBF AM. Historically, Nb1Zr had been explored for high temperature fast spectrum fission reactors for both terrestrial and space applications. Molybdenum alloy TZM has also been considered for these reactor concepts due to exceptional high-temperature strength, creep resistance, and stability under irradiation. L-PBF AM of TZM has previously been investigated at LANL under the Microreactor program, NASA, ORNL, and in academia. However, due to the crack prone nature of TZM, L-PBF AM of TZM resulted in significant microcracking and additional development is required to pursue viable maturation. Other AM methods have been found to be more successful in printing TZM, and those alternatives approaches are discussed in this effort. The efforts detailed in this report focused on continued development of Nb1Zr through L-PBF and development of TZM via L-PBF and electron powder bed fusion (E-PBF). The objective of this work was to further the development of these AM techniques for the chosen refractory alloys, elucidating and addressing associated challenges through characterization of several demonstration builds. At LANL, Nb1Zr builds were completed using an EOS M290 and M400 machines, and a refractory alloy-dedicated L-PBF system, the Xact Metal XM200G, was installed. The XM200G primary purpose was to do the Nb1Zr parameter development process; however, due to difficulties associated with the machine installation and qualification process, it was decided to pivot development to the larger M400 and M290 machines. Although the supply of Nb1Zr powder was limited, it was sufficient to generate sub-scale metallographic specimens for the purpose of parameter development. This was first accomplished on the EOS M400 then the M290 due to machine schedule availability. Further development of TZM has been initiated at the University of Texas El Paso (UTEP) under contract with LANL to use both a heated build envelope L-PBF machine and E-PBF machine that have been found in the literature to mitigate microcracking. UTEP was provided with TZM powder and build plates to support parallel TZM parameter development across both machines. As part of the contract, UTEP will also be conducting microstructural characterization once optimized process parameters have been identified. The optimized process parameters for each machine will be used to generate a series of metallographic, mechanical, and surface finish specimens for subsequent characterization and testing. In the next section, we provide a detailed discussion of the methodology used for investigating the feasibility of leveraging these alloys for use in advanced reactor applications.

36 MATERIALS SCIENCE↗