Search NASA⌕ Search

SEARCH · Search NASA

Results for “Tensile”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

The tensile and tensile-creep deformation behavior of Ti–8Al–1Mo–1V(wt%)

The deformation behavior of titanium (Ti) can be complex due to the lower crystal symmetry of the hexagonal α phase compared with metals based on cubic phases. The tensile and tensile-creep deformation behavior of a Ti–8Al–1Mo–1V(wt%) alloy with a weak crystallographic texture was investigated in-situ straining scanning electron microscopy. Tensile experiments were performed at room temperature (RT), 260°C, 455°C, and 650°C, while tensile-creep experiments were performed at 370°C and 455°C. Electron backscattered diffraction (EBSD) was performed both before and after the deformation, and slip trace analysis was used to identify the activation of the slip modes as a function of temperature and the associated global-stress-state Schmid factors. While extensive slip was characterized during the tensile tests, no twinning was observed. During the RT tensile tests the majority of the slip observed was on prismatic planes, while the relative activity of basal slip increased with temperature, such that at 455°C, basal slip and prismatic slip were equally active. Some grain boundary and triple point cracking occurred during the elevated-temperature tensile deformation, while less slip activity and more grain boundary ledge formation were observed during the tensile-creep deformation. In conclusion, during tensile-creep, basal slip was more prevalent than prismatic slip and some transgranular cracks formed.

36 MATERIALS SCIENCE↗

Tensile properties, strain rate sensitivity, and activation volume of additively manufactured 316L stainless steels [Tensile properties of 316L stainless steels made by laser powder-bed-fusion additive manufacturing]

The tensile properties of additively manufactured (AM) metals and alloys are among the most important variables that impact the potential applications of these materials. Here we examine and report on the tensile properties of AM 316L stainless steels fabricated by the laser powder-bed-fusion (L-PBF) technique, via twelve sets of optimized laser processing parameters that produce materials with density >98.8 ± 0.10%. A heterogeneous microstructure is observed in all L-PBF samples, including microscopic features such as dislocations, cellular walls, elemental segregations, local misorientations, impurities, precipitates, and a large fraction of low-angle grain boundaries (2-10°, ~40–60%). The derived average grain size defined by high-angle grain boundaries (>10°) is ~30–50 μm. Tensile testing reveals a yield strength ranging from 552 to 635 MPa and a tensile-elongation-to-failure (TEF) of 0.09–0.42 for directly-printed samples, whereas these values are 592–690 MPa and 0.29–0.50 for samples machined from the as-built rectangular thin plates. In all samples, we observe a variation of tensile yield strength within ~15% but not the TEF, suggesting marginal microstructural changes despite a wide range of laser processing parameters. The large scatter of TEF in directly-printed samples originates from the sensitivity of thin gauge geometry (~2 mm 2 cross-section area) to the built-in flaws. We measured a substantially higher strain rate sensitivity (m~0.02–0.03) of L-PBF 316L compared to the coarse-grained counterparts (~0.006), together with a small activation volume of ~20–30b3 (where b is the Burgers vector of 316L). In conclusion, these deformation kinetics parameters suggest that the tensile plasticity of L-PBF 316L is controlled by a much finer microstructural length scale than the measured grain size, consistent with the high strength and juxtaposed nano- to macro-structures seen in these materials. Strategies to optimize the tensile properties of AM materials are discussed.

36 MATERIALS SCIENCE↗

Analysis of Tensile Deformation and Failure in Austenitic Stainless Steels: Part II- Irradiation Dose Dependence

Irradiation effects on stable and unstable deformations and fracture behaviors in irradiated austenitic stainless steels (SSs) have been studied in detail based on the equivalent true stress versus true strain curves. An iterative technique in finite element simulation was used to obtain the equivalent true stress-true strain data from experimental tensile curves. It was shown that the strain hardening rate was retained at a high level on unstable deformation after significant irradiation and was independent of the irradiation dose up to the initiation of a localized necking. The equivalent fracture stress was nearly independent of irradiation dose before the damage (embrittlement) mechanism changed. In low dose range (< ~ 2dpa), the fracture strain and tensile fracture energy decreased rapidly with dose and at higher doses they decreased gradually to saturated levels, which were still high for irradiated materials. It was also found that the fracture properties for EC316LN SS were less sensitive to irradiation dose than those for 316 SS, although their uniform tensile properties showed almost the same dose dependencies. It was confirmed that the dose dependence of tensile fracture properties evaluated by the linear approximation model for nominal stress was accurate enough for practical use without elaborate calculations.

36 MATERIALS SCIENCE↗

A novel indirect tensile test method to measure the biaxial tensile strength of concretes and other quasibrittle materials

A novel indirect tensile test method, the biaxial flexure test (BFT) method, has been developed to measure the biaxial tensile strength of concretes. The classical modulus of rupture (MOR) test has been generalized to three dimensions. In this method, we use a circular plate as the new test specimen. This plate is supported by an annular ring. We apply an external load to this specimen through a circular edge. The centers of the specimen, the loading device and the support are identical. The biaxial tensile strength measured by this new method is about 19% greater than the uniaxial tensile strength obtained from the classical modulus of rupture test as reported by other researchers. However, at the same time, we also found that the stochastic deviation of the biaxial tensile strength is about 63% greater than the uniaxial strength.

36 MATERIALS SCIENCE↗

Strain partition and rupture analysis of notched tensile multilayered steel specimens

Highlights: • In situ SEM tensile experiments were performed to investigate the fracture processes. • In situ synchrotron x-ray diffraction were carried out to study the microscopic deformation in MLS steel. • The changing trends of the strain in the austenite layer and martensitic layer have been revealed. - Abstract: Multilayered steel composites consisting of alternating martensitic and austenite layers were successfully fabricated with a combination of high strength and ductility. In situ SEM tensile experiments were performed to investigate the fracture processes. Results indicated that the martensitic layer distributed between two ductile austenite layers has better deformation ability, and the dimple fracture mode dominated the fracture of the whole specimen. In situ synchrotron microbeam X-ray diffraction experiments were carried out to study the microscopic deformation in austenitic layer and martensitic layer ahead of notch root under incremental tensile loading. Results indicated that for austenite layer, the maximum strain is located in the middle of the layer at the lower applied load. When at the higher applied load, larger strain is concentrated on the notch root. For martensitic layer, uniform strain is distributed at the region at the lower applied load, with increasing the applied load, small strain appears in the middle of martensitic layer. However, the variation in the strain in the martensitic layer is relatively smaller, which is actually affected by both the notch and the ferrite content in the martensitic layer. The changing trends of the strain in the austenite layer and martensitic layer can still show the better combination of brittle martensitic phase and ductile austenite phase.

36 MATERIALS SCIENCE↗

Low and room temperatures tensile properties of a nanoprecipitate-strengthened (FeCoCr)40Ni40Al10Cu10 high-entropy alloy

Highlights: • We designed a (FeCoCr){sub 40}Ni{sub 40}Al{sub 10}Cu{sub 10} high entropy alloy (HEA) strengthened by exclusive L1{sub 2} nano-precipitates. • The present HEA exhibited excellent combination of tensile strength (~1200MPa) and elongation (~36%) at 233 K. • The coherent nano-precipitates, deformation twinning and immobile LC locks made a joint contribution to the optimal mechanical property. - Abstract: We report the tensile properties and microstructural evolution of a high entropy alloy (FeCoCr){sub 40}Ni{sub 40}Al{sub 10}Cu{sub 10} deformed at low temperature (233K) and room temperature (293 K). The alloy presented a superior combination of tensile strength (~1200 MPa) and elongation (~36%) at 233 K than at 293 K. Transmission electron microscopy revealed that the enhanced tensile properties at low temperature were due to deformation twinning, the formation of immobile Lomer-Cottrell dislocation locks, and the high density coherent nano-precipitates.

36 MATERIALS SCIENCE↗

Beam current effect as a potential challenge in SEM-EBSD in situ tensile testing

Highlights: • In situ SEM-EBSD tensile tests were conducted using 304L steels with 8 and 10.4% Ni. • KAM and GROD evolution, twinning, and phase instability were investigated. • Phase transformation in 8% Ni-steel was sensitive to the electron beam current. In situ mechanical tensile tests coupled with electron backscatter diffraction (EBSD) analysis were conducted using specimens of two 304L steels with ~8 and 10.4% Ni content, respectively. Twinning was observed in steel with 10.4% Ni content, whereas steel with 8% Ni content demonstrated martensitic transformation. Testing showed that the kinetics of martensitic transformation in steel with 8% Ni content was influenced by the electron beam current used during EBSD scans. Continuous scanning using 32 nA nominal beam current led to suppression of the phase instability in the near-surface layer, but acceptable comparable-to-the-bulk results were obtained using 8 nA beam current. The exact mechanism of the beam current role is unclear, but it appears to be neutral regarding Kernel Average Misorientation behavior and deformation-induced twinning.

36 MATERIALS SCIENCE↗

Investigation of thermal aging effects on the tensile properties of Alloy 617 by in-situ synchrotron wide-angle X-ray scattering

The nickel-base Alloy 617 has been considered as the lead candidate structural material for the intermediate heat exchanger (IHX) of the Very-High-Temperature Reactor (VHTR). In order to assess the long-term performance of Alloy 617, thermal aging experiments up to 10,000 h in duration were performed at 1000 degrees C. Subsequently, in-situ synchrotron wide-angle X-ray scattering (WAXS) tensile tests were carried out at ambient temperature. M23C6 carbides were identified as the primary precipitates, while a smaller amount of M6C was also observed. The aging effects were quantified in several aspects: (1) macroscopic tensile properties, (2) volume fraction of the M23C6 Phase, (3) the lattice strain evolution of both the matrix and the M23C6 precipitates, and (4) the dislocation density evolution during plastic deformation. The property-microstructure relationship is described with a focus on the evolution of the M23C6 phase. For aging up to 3000 h, the yield strength (YS) and ultimate tensile strength (UTS) showed little variation, with average values being 454 MPa and 787 MPa, respectively. At 10,000 h, the YS and UTS reduced to 380 MPa and 720 MPa, respectively. The reduction in YS and UTS is mainly due to the coarsening of the M23C6 Precipitates. After long term aging, the volume fraction of the M23C6 phase reached a plateau and its maximum internal stress was reduced, implying that under large internal stresses the carbides were more susceptible to fracture or decohesion from the matrix. Finally, the calculated dislocation densities were in good agreement with transmission electron microscopy (TEM) measurements. The square roots of the dislocation densities and the true stresses displayed typical linear behavior and no significant change was observed in the alloys in different aging conditions.

Alloy 617↗

Tensile Testing of Aged TR-55 Silicone Rubber (Gamma Radiation Under Tensile Strain): Load/Unload Cycling Followed by Strain to Failure

TR-55 silicone rubber samples were previously subjected to an aging process consisting of the application of a tensile strain of approximately 0, 67, 100, 133, or 167% elongation (axial stretch ratio λ 1 = 1.00, 1.67, 2.00, 2.33, or 2.67) during exposure to gamma radiation doses of 0, 5, 10, or 17 Mrad under vacuum. Two rectangular specimens were cut from each sample for uniaxial tensile testing. Each specimen was subjected to four load/unload cycles followed immediately by strain to failure and stress-strain curves were generated. The Young’s (elastic) modulus was calculated based on the initial slope of the stressstrain curve of the first loading segment. Tensile strength and failure strain were determined.

36 MATERIALS SCIENCE↗

Static tensile and tensile creep testing of five ceramic fibers at elevated temperatures

Static tensile and tensile creep testing of five ceramic fibers at elevated temperature was performed. J.P. Stevens, Co., Astroquartz 9288 glass fiber, Nippon Carbon, Ltd., (Dow Corning) Nicalon NLM-102 silicon carbide fiber, and 3M Company Nextel 312, 380, and 480 alumina/silica/boria fibers were supplied in unsized tows. Single fibers were separated from the tows and tested in static tension and tensile creep. Elevated test temperatures ranged from 400 to 1300 C and varied for each fiber. Room temperature static tension was also performed. Computer software was written to reduce all single fiber test data into engineering constants using ASTM Standard Test Method D3379-75 as a reference. A high temperature furnace was designed and built to perform the single fiber elevated temperature testing up to 1300 C. A computerized single fiber creep apparatus was designed and constructed to perform four fiber creep tests simultaneously at temperatures up to 1300 C. Computer software was written to acquire and reduce all creep data.

Zimmerman, Richard S.↗

Static tensile and tensile creep testing of five ceramic fibers at elevated temperatures

Static tensile and tensile creep testing of five ceramic fibers at elevated temperature was performed. J.P. Stevens, Co., Astroquartz 9288 glass fiber; Nippon Carbon, Ltd., (Dow Corning) nicalon NLM-102 silicon carbide fiber; and 3M Company Nextel 312, 380, and 480 alumina/silica/boria fibers were supplied in unsized tows. Single fibers were separated from the tows and tested in static tension and tensile creep. Elevated test temperatures ranged from 400 C to 1300 C and varied for each fiber. Room temperature static tension was also performed. Computer software was written to reduce all single fiber test data into engineering constants using ASTM Standard Test Method D3379-75 as a reference. A high temperature furnace was designed and built to perform the single fiber elevated temperature testing up to 1300 C. A computerized single fiber creep apparatus was designed and constructed to perform four fiber creep tests simultaneously at temperatures up to 1300 C. Computer software was written to acquire and reduce all creep data.

Zimmerman, Richard S.↗