Key Degradation Products in Nitroplasticizer Thermal Aging

Upon thermal aging, nitroplasticizer (NP) can thermally degrade and release numerous degradation products depending on aging conditions. In this report, we summarize our recent findings, a library of key degradation products in the NP thermal aging is provided. The library contains 25 identified species with their corresponding MS/MS spectrum and intensity profiles, which are derived from our 44-month thermal aging experiment of NP conducted in air, nitrogen, and water at room temperature (RT), 38, 45, 55, and 64°C. To provide a comprehensive yet simplified overview of NP degradation, we summarized the proposed mechanisms of HONO elimination and decomposition, acid generation, PBNA nitrosation and nitration, acid-catalyzed hydrolyses of NP and polynitrated PBNAs, as well as the formation of NP degradants. As the last part of a series of publications and reports on the investigation of NP degradation mechanisms, this work further unfolds complex chemistry that occurs in the entire aging process of NP.

36 MATERIALS SCIENCE

Probing the fatigue enhancement in a thermally aged cast duplex stainless steel by in situ neutron diffraction

After long-term thermal aging at 400 °C for 3000 h and 10,000 h, a cast duplex stainless steel exhibits promoted fatigue performance, including enhanced three-stage cyclic hardening and prolonged fatigue life. Utilizing in situ neutron diffraction, the phase-specific stresses are resolved, and their evolutions over entire fatigue cycling reveal the underlying mechanisms of the fatigue enhancement. It is found that the ferrite phase bears a much higher stress than the austenite matrix under both as-received and aged conditions. The enhanced cyclic hardening in Stage I is attributed to the strengthening of both phases due to thermal aging, while the enhancement in Stage III results from the martensitic transformation induced strengthening. The fatigue life is prolonged thanks to the cyclic hardening and the delay of martensitic transformation in the austenite phase after thermal aging.

Yu, Dunji

Long-term thermal aging behavior and strength reduction in a laser powder bed fusion 316H stainless steel

The long-term thermal stability of structural alloys is essential for ensuring the safe and reliable operation of nuclear reactors and other power plants. While extensive research has explored the effects of thermal aging on conventional stainless steels, the behavior of additively manufactured (AM) alloys remains less understood. This study examines the thermal aging response of laser powder bed fusion (LPBF) 316H stainless steel (SS) at temperatures ranging from 550 °C to 750 °C over durations of up to 10,000 h (approximately 1.14 years). Advanced characterization techniques, including electron microscopy and synchrotron X-ray diffraction, were used to investigate dislocation recovery and phase evolution. Based on these findings, a time-temperature-precipitation (TTP) diagram was developed for LPBF 316H SS, revealing a 10- to100-fold acceleration in precipitation kinetics compared to wrought 316H SS. A physics-informed model was calibrated using the short-term experimental data, enabling predictions of average precipitate sizes, volume fractions of M 23 C 6 and Laves phases, and changes in molybdenum solute concentration for aging up to 1 × 10⁶ h (114 years). These microstructural insights were further utilized to estimate yield strength and extrapolate strength reduction factors over the extended aging period. Despite the accelerated aging kinetics, LPBF 316H SS demonstrated superior yield strength retention compared to its wrought counterpart. In conclusion, this study establishes a framework for evaluating long-term performance using short-term experimental data and supports the accelerated qualification of AM materials for high-temperature structural applications.

Laser powder bed fusion

Thermal aging effects on crosslinked polyethylene cable insulation with decabromodiphenyl ether flame retardant alternative

Decabromodiphenyl ether (decaBDE) has been extensively used as a flame retardant in several applications, including nuclear electrical cable insulation. However, decaBDE has been identified as a persistent, bioaccumulative and toxic (PBT) substance, leading to regulatory scrutiny. The Environmental Protection Agency (EPA) published a regulation on January 6, 2021, aimed at phasing out the manufacturing, processing, and distribution of decaBDE. This rule set a compliance deadline of March 8, 2021, for the manufacture and processing of decaBDE, and an extended deadline of January 6, 2023, for specific applications including wire and cable insulation in nuclear power generation facilities. In response to such regulations, RSCC, a major supplier of safety-related electrical cables and associated products to the U.S. nuclear industry updated the formula of their crosslinked polyethylene (XLPE) insulation to replace the historically used decaBDE flame retardant with an acceptable alternative. This change from the previous decaBDE-containing XLPE prompted interest in comparative performance of the two material formulations, especially with respect to characteristics relevant to safety-related function such as thermal and radiation resistance. RSCC graciously provided samples of wire insulated with the decaBDE-containing XLPE formulation and corresponding wire insulated with XLPE of the new formulation, containing a decaBDE alternative. In this work we compare characteristics of the two formulations and a previously produced commercial version of the RSCC decaBDE-containing XLPE insulation subjected to thermal aging at 150 °C and 165 °C. The comparison was focused on mechanical durability, thermal stability in the oxidative environment, and chemical structures. Briefly, • Tensile elongation at break (EAB) results showed loss of mechanical elasticity with longer aging time, as expected. Aging time dependence of EAB did not differ between the decaBDE-containing and decaBDE-alternative samples. • Subtle differences between the two materials can be detected from Fourier-transform infrared spectroscopy (FTIR) absorbance spectra in the range below 1700 cm -1 , are assumed to be related to decomposition of flame retardant additives during thermal aging. • The oxidation induction time (OIT) data seemed to show that the unaged decaBDE-containing XLPE material is more thermally stable than the unaged decaBDE-alternative material, but the discrepancy in OIT decreased with aging time and the OIT values of the two materials became similar starting with the 4 th day of aging at 165 °C. This thermal aging investigation confirmed that the mechanical durability, a key property monitored for cable qualification, was not significantly affected by the modification of the formulation with a decaBDE alternative flame-retardant system in the investigated thermal aging conditions. Further studies on the same sets of materials exposed to thermal and gamma radiation aging would further inform comparison of the materials safety-related function.

36 MATERIALS SCIENCE

Effect of Thermal Aging on Microstructure and Stress Corrosion Cracking Behavior of an Alloy 152 1st Layer Butter Weldment

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40- 80 years. Likewise, water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is critical for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for different durations up to 75,000h (equivalent to 60 years of reactor service). The microstructural characterization by means of synchrotron X-ray conducted in small, 0.2 mm - step line scans in the high-deformation regions of the weld root – covering areas spanning from the weld heat affected zone (HAZ) in Alloy 690 to the weld and weld butter on LAS - did not show evidence of LRO in any of the three Alloy 152 heats aged at 370°C and 450°C to an equivalent of 60 years of service. However, the first weld butter layer has high levels of deformation and is highly susceptible to SCC even in its non-aged condition. Nanohardness testing confirmed the extreme hardening with aging (ΔHV ≅ 100) at two locations within this weldment. In absence of LRO, hardening is suspected to be due to thermally-induced Cr carbide precipitation and coarsening. Testing in a primary water environment of the 1st layer of Alloy 152 weld butter aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloys. Similarly, the SCC CGR response of the aged weld butter does not appear to show a deterioration in performance, however, the difficult-to-test weldment geometry may affect the test results.

22 GENERAL STUDIES OF NUCLEAR REACTORS

Latent Pitfalls in Microstructure-Based Modeling for Thermally Aged 9Cr-1Mo-V Steel (Grade 91)

A case study was conducted on a mechanistic model development that predicted tensile strength deterioration with thermal aging of 9Cr-1Mo-V steel in supporting the 60-year design life expected for advanced nuclear reactors. For property prediction beyond practical testing times, mechanistic modeling is highly desired, as it taps into the physics of structure–property relationships and therefore can generate reliable results for extrapolation. Meanwhile, as mechanistic models are often complicated, reflecting the intricacy of microstructure and strengthening mechanisms, pitfalls that are difficult to detect often exist. Here, this paper discusses latent pitfalls that are common in mechanistic modeling or specific in this 9Cr-1Mo-V case development through using the American Society of Mechanical Engineers verification and validation in computational solid mechanics (ASME V&V 10) standard for evaluating credibility of modeling in materials engineering. Suggestions are also made for enhancing reliability of microstructure-based modeling.

36 MATERIALS SCIENCE

Microstructure and Mechanical Properties of Scaled Thermally Aged LPBF 316H SS Builds

As part of the US Department of Energy’s Advanced Materials and Manufacturing Technologies program’s mission to accelerate qualification of advanced manufacturing pathways for nuclear applications, laser powder bed fusion (LPBF) 316H stainless steel (SS) has been selected as a model system to develop a rapid code case framework. This effort directly addresses the grand challenges of (1) expanding the limited portfolio of materials currently codified for elevated-temperature nuclear structural service under Section III, Division 5 of the American Society of Mechanical Engineers’ Boiler and Pressure Vessel Code; and (2) significantly reducing qualification timelines that traditionally exceed a decade. The strategic importance of LPBF 316H lies in its immediate industrial relevance, existing data foundation from wrought 316H, and alignment with ongoing code case development for LPBF 316L. Prior work revealed accelerated precipitation of deleterious secondary phases and reduced creep ductility in as-printed LPBF 316H. Building on that prior research, FY 2025 activities focused on establishing an understanding of the key failure mechanisms of crept 316H specimens to aid in code case development and on evaluating stress relief (SR) parameters on the high-temperature performance and thermal aging induced degradation of tensile and fracture behavior in LPBF 316H.

36 MATERIALS SCIENCE

Microstructure & Mechanical Properties of Scaled Thermally Aged LPBF 316H SS Builds

As part of the US Department of Energy’s Advanced Materials and Manufacturing Technologies program’s mission to accelerate qualification of advanced manufacturing pathways for nuclear applications, laser powder bed fusion (LPBF) 316H stainless steel (SS) has been selected as a model system to develop a rapid code case framework. This effort directly addresses the grand challenges of (1)expanding the limited portfolio of materials currently codified for elevated-temperature nuclear structural service under Section III, Division 5of the American Society of Mechanical Engineers’ Boiler and Pressure Vessel Code; and (2) significantly reducing qualification timelines that traditionally exceed a decade. The strategic importance of LPBF 316H lies in its immediate industrial relevance, existing data foundation from wrought 316H, and alignment with ongoing code case development for LPBF 316L.Prior work revealed accelerated precipitation of deleterious secondary phases and reduced creep ductility in as-printed LPBF 316H. Building on that prior research, FY2025activities focused on establishing an understanding of the key failure mechanisms of crept 316H specimens to aid in code case development and on evaluating stress relief (SR) parameters on the high-temperature performance and thermal aging-induced degradation of tensile and fracture behavior in LPBF316H.

36 MATERIALS SCIENCE

The Effect of Thermal Aging on the Performance of High-Cr Ni-based Alloys in Primary Water Environment

Nickel-based Alloy 690, and the associated weld Alloys 52 and 152, are used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels. They are chosen for their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate beyond their first or second license renewal (e.g., 40 to 60 years or beyond 60 years). Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants. Moreover, Ni-Cr alloys are being considered for high-level radioactive waste disposal containers that will be required to contain the waste for at least 10,000 years.

22 GENERAL STUDIES OF NUCLEAR REACTORS

FY24 progress report on A709 mechanical properties data development and A709 thermal aging status

The report provides the status of the creep, fatigue, and creep-fatigue testing to date conducted at Idaho National Laboratory to generate the data package. This data package evaluates the material performance from three commercial heats to support the Alloy 709 qualification in American Society of Mechanical Engineers, Boiler and Pressure Vessel Code, Section III, Division 5. First procured heat was manufactured by G.O. Carlson with heat number 58776. Second and third heats were fabricated by ATI Specialty Rolled Products with heat numbers 529900 and 530843, respectively. A series of creep and cyclic specimens were fabricated from these three heats and tests were performed. A list of finished, ongoing, and planned test are presented for creep, fatigue, and creep-fatigue tests. Cyclic properties of three commercial heats are compared.

36 MATERIALS SCIENCE

FY24 progress report on A709 mechanical properties data development and A709 thermal aging status

The report provides the status of the creep, fatigue, and creep-fatigue testing to date conducted at Idaho National Laboratory to generate the data package. This data package evaluates the material performance from three commercial heats to support the Alloy 709 qualification in American Society of Mechanical Engineers, Boiler and Pressure Vessel Code, Section III, Division 5. First procured heat was manufactured by G.O. Carlson with heat number 58776. Second and third heats were fabricated by ATI Specialty Rolled Products with heat numbers 529900 and 530843, respectively. A series of creep and cyclic specimens were fabricated from these three heats and tests were performed. A list of finished, ongoing, and planned test are presented for creep, fatigue, and creep-fatigue tests. Cyclic properties of three commercial heats are compared.

36 - MATERIALS SCIENCE

Initial Testing of an In Situ Load Retention Aging Vessel

A thermal aging vessel instrumented with load cells was fabricated. The primary function of the vessel is to continuously monitor the in situ load retention of up to three compressed polymer coupons undergoing thermally accelerated aging under nitrogen. A secondary function is to enable gas sampling of the vessel headspace during thermal aging. Heating of the vessel is achieved using a custom heater jacket. To improve upon our conventional aging study methods which require periodic interruption of aging to perform load testing in an Instron machine at room temperature, this technology aims to automate/facilitate data acquisition/analysis, improve data quality, and enable uninterrupted compression of the polymer which represents the service condition. As an example case to assess functionality of the in situ vessel, the load retention of a siloxane elastomer material additively manufactured by direct-ink-writing (DIW) was measured at three different isothermal aging temperatures for ~1 month. Initial compression of the coupons while near the aging temperature was achieved by temporarily opening the heated vessel to access the interior chamber and manually tightening four nuts to drive the heated compression plate down onto the heated coupons. Initial testing demonstrated achievement of the primary load retention monitoring function. Unfortunately, the vessel leaked which prevented gas sampling; an active purge was used to maintain a nitrogen atmosphere. Welded or otherwise sealed joints, which could be implemented in a future design, would likely eliminate leak paths. To apply time-temperature superposition (TTS), a technique used to provide long-term prediction of the load retention from short-term isothermal data, the load retention needed to be calculated relative to the load at an estimated “equilibrium” time, after most of the transient viscoelastic physical relaxation occurred. The peak load immediately after compression could not be used as the load retention basis for two reasons: (1) age-related changes must be isolated from non-age-related physical relaxation before applying TTS and (2) the manual mechanism used to compress the specimens at the aging temperature was neither smooth nor repeatable which affected the peak load value. To better understand the effect of the mode of initial compression on the measured load, and possibly better estimate “equilibrium” physical relaxation times, systematic stress relaxation experiments were performed using an Instron machine with a thermal chamber. At a given temperature, the DIW polymer was compressed to a fixed strain in either a stepped or continuous manner at two different rates, then held at that strain for 24 hrs. The results indicated that, at a given temperature, the different stress relaxation curves appeared to converge to the same curve at some “equilibrium” time when the non-age-related physical relaxation was mostly complete. Though this observation suggests that the discontinuous manual compression employed by the vessel is feasible, a compression mechanism that is rapid, smooth, and repeatable would enhance its use.