Search NASA⌕ Search

SEARCH · Search NASA

Results for “Thermal damage”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Lamb Wave Assessment of Fatigue and Thermal Damage in Composites

Among the various techniques available, ultrasonic Lamb waves offer a convenient method of evaluating composite materials. Since the Lamb wave velocity depends on the elastic properties of a structure, an effective tool exists to monitor damage in composites by measuring the velocity of these waves. Lamb wave measurements can propagate over long distances and are sensitive to the desired in-plane elastic properties of the material. This paper describes two studies which monitor fatigue damage and two studies which monitor thermal damage in composites using Lamb waves. In the fatigue studies, the Lamb wave velocity is compared to modulus measurements obtained using strain gage measurements in the first experiment and the velocity is monitored along with the crack density in the second. In the thermal damage studies, one examines samples which were exposed to varying temperatures for a three minute duration and the second includes rapid thermal damage in composites by intense laser beams. In all studies, the Lamb wave velocity is demonstrated to be an excellent method to monitor damage in composites.

Seale, Michael D.↗

Thermal Damage Potential of Electric Vehicles

The main objective is to assess the risk that electric vehicle (EV) battery fires pose regarding thermal damage to other vehicles involved in a crash and to compare EV and internal combustion engine vehicle (ICEV) fires. A literature review of experimental data and statistics are used to perform the assessment. The findings indicate: (1) the heat flux emitted from an EV and ICEV fire are similar due to cabin materials being the main contributor to heat flux, (2) for ICEVs involved in a crash with fuel tank leakage, the thermal damage is significantly more than from an EV fire for equivalent fire durations, (3) the thermal damage potential from ICEV pool fires is at least 5 times higher than EV fires, and (4) EV and ICEV crashes resulting in a fire is about 0.002% and 0.2%, respectively. Thus, EV battery fires have a lower risk than ICEV fires.

33 ADVANCED PROPULSION SYSTEMS↗

Investigation of thermal damage in explosive bridgewire detonators via discrete element method simulations

Exploding bridgewire (EBW) detonators are used to rapidly and reliably initiate energetic reactions by exploding a bridgewire via Joule heating. While the mechanisms of EBW detonators have been studied extensively in nominal conditions, comparatively few studies have addressed thermally damaged detonator operability. We present a mesoscale simulation study of thermal damage in a representative EBW detonator, using discrete element method (DEM) simulations that explicitly account for individual particles in the pressed explosive powder. We use a simplified model of melting, where solid spherical particles undergo uniform shrinking, and fluid dynamics are ignored. The subsequent settling of particles results in the formation of a gap between the solid powder and the bridgewire, which we study under different conditions. In particular, particle cohesion has a significant effect on gap formation and settling behavior, where sufficiently high cohesion leads to coalescence of particles into a free-standing pellet. This behavior is qualitatively compared to experimental visualization data, and simulations are shown to capture several key changes in pellet shape. We derive a minimum and maximum limit on gap formation during melting using simple geometric arguments. In the absence of cohesion, results agree with the maximum gap size. With increasing cohesion, the gap size decreases, eventually saturating at the minimum limit. In conclusion, we present results for different combinations of interparticle cohesion and detonator orientations with respect to gravity, demonstrating the complex behavior of these systems and the potential for DEM simulations to capture a range of scenarios.

cohesive powders↗

The Influence of Carbon Fiber Composite Specimen Design Parameters on Artificial Lightning Strike Current Dissipation and Material Thermal Damage

Previous artificial lightning strike direct effect research has examined a broad range of specimen design parameters. No works have studied how such specimen design parameters and electrical boundary conditions impact the dissipation of electric current flow through individual plies. This article assesses the influence of carbon fiber composite specimen design parameters (design parameters = specimen size, shape, and stacking sequence) and electrical boundary conditions on the dissipation of current and the spread of damage resulting from Joule heating. Thermal-electric finite element (FE) modelling is used and laboratory scale (<1 m long) and aircraft scale (>1 m long) models are generated in which laminated ply current dissipation is predicted, considering a fixed artificial lightning current waveform. The simulation results establish a positive correlation between the current exiting the specimen from a given ply and the amount of thermal damage in that ply. The results also establish that the distance to ground, from the strike location to the zero potential boundary conditions (ground), is the controlling factor which dictates the electric current dissipation in each ply. Significantly, this distance to ground is dependent on each of the specimen shape, dimensions, stacking sequence, and location of ground boundary conditions. Therefore, it is not possible to decouple current dissipation and damage from specimen design and boundary condition setup. However, it is possible to define a specimen size for a given specimen shape, stacking sequence, and waveform which limit the influence of specimen dimensions on the resulting current distribution and damage. For a rectangular specimen design which appears in literature multiple times, as 100 × 150 mm and with a stacking sequence of [45/0/-45/90] 4s , a specimen design of greater than 300 × 200 mm is required to limit the influence of specimen dimensions on current distribution and damage.

36 MATERIALS SCIENCE↗

Evaluating Thermally Damaged Polyimide Insulated Wiring (MIL-W-81381) with Ultrasound

A series of experiments to investigate the use of ultrasound for measuring wire insulation have been conducted. Initial laboratory tests were performed on MIL-W-81381/7,/12, and /21 aviation wire, a wire that has polyimide (Kapton Registered Trademark) layers for insulation. Samples of this wiring were exposed to 370C temperatures for different periods of time to induce a range of thermal damage. For each exposure, 12 samples of each gauge (12, 16, and 20 gauges) were processed. The velocity of the lowest order axisymmetric ultrasonic guided mode, a mode that is sensitive to the geometry and stiffness of the wire conductor and insulation, was measured. The phase velocity for the 20-gauge MIL-W-81381/7 wire had a baseline value of 3023 +/- 78 m/s. After exposure to the high temperatures, the wire's phase velocity rapidly increased, and reached an asymptotic value of 3598 +/- 20 m/s after 100 hours exposure. Similar behavior was measured for the 16 gauge MIL-W-81381/21 wire and 12 gauge MIL-W-81381/12 wire which had baseline values of 3225 +/- 22 m/s and 3403 +/- 33 m/s respectively, and reached asymptotic values of 3668 +/- 19 m/s, and 3679 +/- 42 m/s respectively. These measured velocity changes represent changes of 19, 14, and 8 percent respectively for the 20, 16, and 12 gauge wires. Finally, some results for a wire with an ethylene tetrafluoroethylene insulation are reported. Qualitatively similar behaviors are noted ultrasonically.

Madaras, Eric I.↗

Operability thresholds for thermally damaged EBW detonators

Operability thresholds that differentiate between functional RP-87 exploding bridge wire (EBW) detonators and nonfunctional RP-87 EBW detonators (duds) were determined by measuring the time delay between initiation and early wall movement (function time). The detonators were inserted into an externally heated hollow cylinder of aluminum and fired with current flow from a charged capacitor using an exploding bridge wire (EBW initiated). Functioning detonators responded like unheated pristine detonators when the function time was 4 μs or less. The operability thresholds of the detonators were characterized with a simple decomposition cookoff model calibrated using a modified version of the Sandia Instrumented Thermal Ignition (SITI) experiment. These thresholds are based on the calculated state of the PETN when the detonators fire. The operability threshold is proportional to the positive temperature difference (ΔT) between the maximum temperature within the PETN and the onset of decomposition (~406 K). Furthermore, the temperature difference alone was not sufficient to define the operability threshold. The operability threshold was also proportional to the time that the PETN had been at elevated temperatures. That is, failure was proportional to both temperature and reaction rate. The reacted gas fraction is used in the current work for the reaction correlation. Melting of PETN also had a significant effect on the operability threshold. Detonator failure occurred when the maximum temperature exceeded the nominal melting point of PETN (414 K) for 45±5 s or more.

42 ENGINEERING↗

A liquid stratification model to predict failure in thermally damaged EBW detonators

In previous work, commercially available downward facing exploding bridgewire detonators (EBWs) were exposed to elevated temperatures. These detonators were then initiated using a firing set which discharged a high amplitude short duration electrical pulse into a thin gold bridgewire. Responses of the detonators were measured using photonic doppler velocimetry (PDV) and high-speed photography. A time delay of 4 μs between EBW initiation and first movement of an output flyer separated operable detonators from inoperable detonators or duds. Here, we propose a simple method to determine detonator operability from the calculated state of the detonator at the time the firing set is initiated. The failure criterion is based on the gap distance between the exploding bridgewire (EBW) and the adjacent initiating explosive within the detonator which is low-density pentaerythritol tetranitrate (PETN) that melts between 413-415 K (140-142 ºC). The gap forms as PETN melts and flows to the bottom of the input pellet. Melting of PETN is modeled thermodynamically as an energy sink using a normal distribution spread over a temperature range between the onset temperature of 413 K and the ending temperature of 415 K. The extent of the melt is determined from the average temperature of the PETN. The PETN liquid is assumed to occupy the interstitial gas volume in the lower part of the input pellet. The vacated volume from the relocated liquid forms the gap between the EBW and the PETN. The remaining sandwiched layer consists of solid PETN particles and gas filling interstitial volume. We predict that a threshold gap between 17-27 μm separates properly functioning detonators from duds.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Modeling of the Influence of a Damaged Thermally Grown Oxide (TGO) Layer in an Environmental Barrier Coating System

Environmental barrier coatings (EBC) are an enabling technology for the successful application of ceramic matrix composites (CMCs) in air-breathing gas turbine engines. EBCs are susceptible to a number of failure modes including oxidation/delamination, recessions, chemical attack and dissolution, thermomechanical degradation, erosion, and foreign object impact damage in a combustion environment. Spallation of environmental barrier coating (EBC), induced by a thermally grown oxide (TGO) layer, is a key EBC failure mode. The TGO layer, resulting from steam oxidation, grows either from a silicon bond coat layer (if present) or from a silicon carbide (SiC) based substrate itself. The TGO layer evolves (i.e., thickness increases with time) as water vapor and oxygen gradually diffuse through the EBC, and the EBC spalls off once the TGO layer reaches some critical thickness. The critical thickness of the TGO layer for failure is in the range of 20-30 microns, but it can vary due to exposure temperature, microstructure etc. Current work at NASA Glenn Research Center, under the Revolutionary Tools and Methods (RTM) subproject is aimed at addressing associated failure modes in EBC systems and developing robust analysis tools to aid in the design/analysis of these systems. The objective of the current work is to conduct a sensitivity study to examine the influence of uniformly and non-uniformly grown oxide layers on the associated driving forces leading to spallation of the EBC when subjected to isothermal loading. The effect of damage in the TGO layer on the resulting stress states is also assessed both in uniform and non-uniform TGO layers.

Mital, Subodh K.↗

The effect of thermal damage on the mechanical properties of polymer regrinds

Reprocessed polymers are subjected to high processing temperatures that result in the breakdown of molecular chains and changes in the molecular structures. These phenomena are reflected in the mechanical properties of materials. Practically every regrind is seen as a new material. These experiments deal with the molding, regrinding, and reprocessing of test specimens for the study of their mechanical properties. The comparative test data from each recycled material would give students an insight of the molecular structures and property degradation. Three important rheological and mechanical properties such as melt flow, impact strength, and flexural strength are to be determined. These properties play key roles in the selection of engineering materials. The material selected for demonstration was Makrolon 3000L, a polycarbonate thermoplastic from Bayer AG. The thermal degradation due to repeated processing is reflected in the decrease in molecular weight and breakdown of molecular chains causing increase in melt flow. The Izod-impact resistance and the flexural strength deteriorate gradually.

Kundu, Nikhil K.↗

Determination of Thermal Damage Threshold in THz Photomixers Using Raman Spectroscopy

The increase of device lifetime and reliability of THz photomixers will play an essential role in their possible future application. Therefore, their optimal work conditions/operation range, i.e., the maximal incident optical power should be experimentally estimated. We fabricated and tested THz photomixer devices based on nitrogen-implanted GaAs integrated with a Bragg reflector. Raman spectroscopy was applied to investigate the material properties and to disclose any reversible or irreversible material changes. The results indicate that degradation effects in the photomixer structures/material could be avoided if the total optical power density does not exceed levels of about 0.7 mW/µm 2 for 100 min of operation. Furthermore, the investigations performed during 1000 min of optical exposure on the photomixer devices’ central region comprising interdigitated metal-semiconductor-metal (MSM) structures suggest a reversible “curing” mechanism if the power density level of ~0.58 mW/µm 2 is not exceeded. Long-term operation (up to 1000 h) reveals that the photomixer structures can withstand an average optical power density of up to ~0.4 mW/µm 2 without degradation when biased at 10 V. Besides the decrease of the position of the A1g (LO) Raman mode from ~291 cm -1 down to ~288 cm -1 with increasing optical power density and operation time, broad Raman modes evolve at about 210 cm -1 , which can be attributed to degradation effects in the active photomixer/MSM area. In addition, the performed carrier lifetime and photomixer experiments demonstrated that these structures generated continuous wave sub-THz radiation efficiently as long as their optimal work conditions/operation range were within the limits established by our Raman studies.

36 MATERIALS SCIENCE↗

Comparison of Ultrasound with Tensile Testing of Thermally Damaged Polyimide Insulated Wiring (MIL-W-81381)

Ultrasonic measurements were performed on MIL-W-81381/7, /12, and /21 wire, a polyimide (Kapton) insulated wire. The phase velocity for the 20-gauge MIL-W-81381/7 wire had a baseline value of 3023 plus or minus 78 m/s. After exposure to high temperatures, the wire's phase velocity rapidly increased, and reached an asymptotic value of 3598 plus or minus 20 m/s after 100 hours exposure. Similar responses were measured in other gauges. The baseline measurements of Young's moduli resulted in values of 5636 plus or minus 486, 7714 plus or minus 505, and 8767 plus or minus 292 KSI for the 20 ga, 16 ga, and 12 ga. wires respectively.

Madaras, Eric I.↗

Effects of ply thickness on thermal cycle induced damage and thermal strain

An experimental study was conducted to determine the effects of ply thickness in composite laminates on thermally induced cracking and changes in the coefficient of thermal expansion, CTE. A graphite-epoxy composite material, P75/ERL 1962, in thin (1 mil) and thick (5 mils) prepregs was used to make cross-ply laminates, ((0/90)(sub n))s, with equal total thickness (n=2, n=10) and cross-ply laminates with the same total number of plies (n=2). Specimens of each laminate configuration were cycled up to 1500 times between -250 and 250 F. Thermally induced microdamage was assessed as a function of the number of cycles as was the change in CTE. The results showed that laminates fabricated with thin-plies microcracked at significantly different rates and reached significantly different equilibrium crack densities than the laminate fabricated with thick-ply and n=2. The CTE of thin-ply laminates was less affected by thermal cycling and damage than the CTE of thick-ply laminates. These differences are attributed primarily to differences in interply constraints. Observed effects of ply thickness on crack density was qualitatively predicted by a combined shear-lag stress/energy method.

Tompkins, Stephen S.↗

Sensitivity Study of Impact Risk Model Results to Thermal Radiation Damage Model for Large Objects

NASA’s Probabilistic Asteroid Impact Risk (PAIR) assessment model assesses the likelihood of potential damage for asteroid impact scenarios. Fast-running models are used to capture the effects of different hazards. This paper looks specifically at local ground damage hazards, including blast overpressure and thermal radiation damage, for large object impact scenarios. A sensitivity study is conducted to determine which parameters, and over what ranges, cause impact risks to become sensitive to thermal damage. Two additional thermal models with different approaches are used for comparison. The study determined the current thermal model is most sensitive to the luminous efficiency parameter that reflects the model’s uncertainty in the amount of energy contributing to the thermal radiation damage. This sensitivity was most apparent for the highest severity damage levels. Comparisons of the three models showed that in addition to sensitivities within the models, the impact risks are also sensitive to the choice of thermal model. The study results were applied to the 2023 PDC hypothetical asteroid impact scenario and parameter ranges of interest determined. At the serious damage level, luminous efficiencies above 0.006 showed a small chance of thermal playing an important role, while luminous efficiencies above 0.0008 led to thermal playing a significant role at the unsurvivable damage severity level. Study results are used to identify key areas where additional model refinement and better knowledge of asteroid properties may be important for improving damage estimates.

SMD↗

Sensitivity Study of Impact Risk Model Results to Thermal Radiation Damage Model for Large Objects

NASA’s Probabilistic Asteroid Impact Risk (PAIR) assessment model assesses the likelihood of potential damage for asteroid impact scenarios. Fast-running models are used to capture the effects of different hazards. This paper looks specifically at local ground damage hazards, including blast overpressure and thermal radiation damage, for large object impact scenarios. A sensitivity study is conducted to determine which parameters, and over what ranges, cause impact risks to become sensitive to thermal damage. Two additional thermal models with different approaches are used for comparison. The study determined the current thermal model is most sensitive to the luminous efficiency parameter that reflects the model’s uncertainty in the amount of energy contributing to the thermal radiation damage. This sensitivity was most apparent for the highest severity damage levels. Comparisons of the three models showed that in addition to sensitivities within the models, the impact risks are also sensitive to the choice of thermal model. The study results were applied to the 2023 Planetary Defense Conference hypothetical asteroid impact scenario and parameter ranges of interest determined. At the serious damage level, luminous efficiencies above 0.006 showed a small chance of thermal playing an important role, while luminous efficiencies above 0.0008 led to thermal playing a significant role at the unsurvivable damage severity level. Study results are used to identify key areas where additional model refinement and better knowledge of asteroid properties may be important for improving damage estimates.

SMD↗

Modeling nuclear waste disposal in crystalline rocks at the Forsmark and Olkiluoto repository sites – Evaluation of potential thermal–mechanical damage to repository excavations

We conduct coupled thermo-hydro-mechanical modeling of a KBS-3V repository design in crystalline rocks, using data and conditions from the Forsmark in Olkiluoto repository sites in Sweden and Finland. The study focuses on repository performance related to the impact of thermal and hydraulic evolution on the potential for thermal–mechanical damage to underground repository excavations. For the designs and conditions considered at the Forsmark and Olkiluoto repository sites, the simulations show a peak temperature well under the adopted performance target of a 100°C maximum temperature, whereas there is still a high potential for thermal–mechanical damage to the KBS-3V waste deposition holes. The thermal–mechanical damage is much more likely if rock permeability is so low that it delays saturation and swelling of bentonite-clay-based backfill beyond the time for the thermal–mechanical peak, which occurs 50 to 100 years after nuclear waste deposition. We also found that sidewalls of the KBS-3V emplacement tunnels are vulnerable to tensile fracturing due to the combined effect of thermal stressing and backfill swelling. The study highlights a strong interaction between bentonite-based backfill and host rock through capillary suction along with induced rock desaturation. A careful design and selection of the bentonite-clay-based backfill materials for KBS-3V tunnels and deposition holes can facilitate a timely saturation and backfill swelling that in turn can minimize thermal–mechanical damage.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

TPS In-Flight Health Monitoring Project Progress Report

Progress in the development of new thermal protection systems (TPS) is reported. New approaches use embedded lightweight, sensitive, fiber optic strain and temperature sensors within the TPS. Goals of the program are to develop and demonstrate a prototype TPS health monitoring system, develop a thermal-based damage detection algorithm, characterize limits of sensor/system performance, and develop ea methodology transferable to new designs of TPS health monitoring systems. Tasks completed during the project helped establish confidence in understanding of both test setup and the model and validated system/sensor performance in a simple TPS structure. Other progress included complete initial system testing, commencement of the algorithm development effort, generation of a damaged thermal response characteristics database, initial development of a test plan for integration testing of proven FBG sensors in simple TPS structure, and development of partnerships to apply the technology.

Kostyk, Chris↗

An investigation of the thermal cycling damage of 25 vol. pct SiCw/alumina ceramic matrix composite

An investigation was made of the thermal cycling damage of a 25 vol pct SiC whisker/alumina (SiCw/Al2O3) composite. Thermal cycling tests were conducted by subjecting a composite specimen to two different fluidized beds. After thermal cycling the composite specimens were subjected to elastic modulus and effective fracture toughness measurements. The thermal cycled specimens were investigated with SEM and TEM studies. It was found that this composite has a relatively high resistance to thermal cycling.

Armstrong, William D.↗