Search NASA⌕ Search

SEARCH · Search NASA

Results for “Type 304L Stainless Steel”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Microstructural Evolution During a Solid State Tube Pinch Weld of Type 304l Stainless Steel

Microstructure development is examined for a specialized spot weld that is used as a solid-state closure process for austenitic stainless steel tubing, referred to as pinch welding. In order to elucidate the microstructural evolution of the weld, a series of test welds were made at nominal conditions using tubing and production like components. These pinch welds normally terminate after twelve cycles of a 60 Hz AC weld process. In this study, production tubes were welded from one to twelve cycles and the microstructure and weld variables after each individual weld cycle number were characterized using radiography and optical metallography. Two electrochemical etchants were used to highlight different microstructural features. The study revealed that: (1) this type pinch weld is largely complete after about six cycles of 60 Hz AC current, half the weld time utilized; (2) the resistance, deformation, and closure length approach “steady-state” conditions after six cycles; and (3) both oxalic and nitric acid electrolytic etchants are useful for highlighting specific microstructural attributes of type 304 L stainless steel. Finally, two distinct microstructural regions can be identified for these welds: the edge of the weld, which is driven by concentrated deformation, recrystallization, and grain growth, and the center region, which is more typical of forge welding and micro-asperity breakdown followed by diffusion and grain-growth.

36 MATERIALS SCIENCE↗

Distribution of Tritium in the Near Surface of Candidate Structural Materials for Fusion Reactors. Type 304L Stainless Steel, Inconel, Hastelloy, Eurofer-97, Oxide Dispersion-Strengthened Alloy 14YWT

Five different candidate structural materials for fusion have undergone pure tritium gas soaking at room temperature and at 310-mbar(a) pressure. The tritium uptake on the surface and in the bulk of the alloys has been analyzed using surface leaching, chemical etching, and thermal desorption. The nickel-based alloys: Inconel-X-750 and Hastelloy-X, absorbed the least amount of total tritium compared with austenitic stainless steel AISI 304L, reduced activation ferritic-martensitic (RAFM) Eurofer-97, and advanced nanoferritic alloy 14YWT. Microstructural analyses using electron backscatter diffraction (EBSD) indicate that the number of grains and mean grain size is not a dominant factor in near surface tritium uptake. The quantity of iron dissolved in the surface oxide appears to be the major factor in encouraging tritium absorption.

O'Callaghan, James↗

2021 Report - SRNL Aging and Lifetimes program tritium aging studies on structural alloys

This report documents work performed in fiscal year 2021 at SRNL in support of the Aging and Lifetimes program. This work is part of an on-going collaboration between SRNL and SNL to understand tritium embrittlement of structural metals used in Gas Transfer System reservoirs, thereby informing lifetime assessments and predictions. In this effort, test coupons are pre-charged with tritium and allowed to age in a freezer to minimize tritium diffusion and off-gassing while allowing for born-in helium levels to systematically increase. Coupons are then removed periodically and tested to develop an understanding of how mechanical properties degrade as helium levels increase. This report summarizes test results from coupons which are in various stages of aging as they were tritium pre-charged in previous years. Tests were performed on 304L that was previously tritium pre-charged and allowed to age to nominally 300 appm helium. Specimens from this study were previously tested at 100 appm nominal helium content, and this new test point expands that study. Tensile testing of these heat treated 304L tubes (and welded tubes) aged to 100 appm helium were completed which provided a unique study of a diverse set of microstructures and yield strengths ranging from 200-800 MPa. Additionally, 304L notched and smooth tensile specimens aged to 300 appm helium were tensile tested to predetermined strains to provide for a systematic microscopy investigation of aging effects on microstructural damage in partnership with SNL. Testing was performed on 304L electron beam (EB) weld coupons as well as 21-6-9 annealed coupons that were thermally pre-charged in 2020. Tests on the EB welds were completed at 100 appm helium contents, and tests on the annealed 21-6-9 material were completed at 100, 200, and 300 appm helium. Table 0-1 provides the status of the ongoing tritium coupon aging studies. The table includes the year tritium pre-charging took place, the material, and the targeted helium concentrations (appm) for testing.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

2020 Report - SRNL Aging and Lifetimes program tritium aging studies on structural alloys

This report documents work performed in calendar year 2020 at SRNL in support of the Aging and Lifetimes program. This work is part of an on-going collaboration between SRNL and SNL to understand tritium embrittlement of structural metals in Gas Transfer System reservoirs which informs lifetime assessments and lifetime predictions. In this effort, test coupons are precharged with tritium and allowed to age in a freezer to minimize tritium egress and allow for born-in helium levels to systematically increase. Coupons are then removed periodically and tested to develop an understanding of how mechanical properties degrade as helium levels increase. This report summarizes test results from coupons which are in various stages of aging as they were tritium precharged in previous years.

36 MATERIALS SCIENCE↗

2022 Report - SRNL Aging and Lifetimes program tritium aging studies on structural alloys

This report documents work performed in fiscal year 2022 at SRNL in support of the Aging and Lifetimes program. This work is an enduring collaboration between SRNL and SNL to study tritium embrittlement of structural metals used in Gas Transfer System reservoirs. The measured data inform component lifetime assessments and predictions. Test coupons are thermally pre-charged with tritium and allowed to age at cryogenic temperatures to freeze out tritium diffusion and minimize off-gassing while allowing for decay helium levels to build. Coupons are removed and tested at planned intervals to measure how mechanical properties degrade as helium levels increase. This report summarizes test results from coupons which are in various stages of aging as they were tritium pre-charged in previous years, as well as documenting one new charging run.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Influence of Residual Stress on Fatigue Crack Growth Rates in Stainless Steel Processed by Different Additive Manufacturing Methods

The properties and microstructure of Type 304L stainless steel produced by two additive manufacturing (AM) methods—directed energy deposition (DED) and powder bed fusion (PBF)—are evaluated and compared. Localized heating and steep temperature gradients of AM processes lead to significant residual stress and distinctive microstructures, which may be process-specific and influence mechanical behavior. Test data show that materials produced by DED and PDF have small differences in tensile strengths but clear differences in residual stress and microstructural features. Measured fatigue crack growth rates (FCGRs) for cracks propagating parallel to and perpendicular to the build directions differ between the two AM materials. To separate the influences of residual stress and microstructure, K-control test procedures with decreasing and constant stress intensity factor ranges are used to measure FCGRs in the near-threshold regime (crack growth rates ≤ 1 × 10 −8 m/cycle). Residual stress is quantified by the residual stress intensity factor, K res , measured by the online crack compliance method. Correcting the FCGR data for differences in K res brings results for specimens of the two AM materials into agreement with each other and with results for wrought specimens, when the latter are corrected for crack closure. Differences in microstructure and tensile strength have an insignificant influence on FCGRs in these tests.

additive manufacturing↗

Tritium Aging Effects on Fracture Toughness of Stainless Steel Weldments

The long-term embrittlement effects of tritium and decay helium on the structural properties of stainless steels have been studied for years at Savannah River to provide required data for establishing safe operating conditions and lifetimes of pressure vessels used to contain tritium gas. In this study, the fracture toughness properties of the longest-aged tritium-precharged stainless-steel base metals and weldments tested at Savannah River were measured and compared to earlier results. The fracture toughness values were the lowest recorded here for tritium-exposed stainless steel. As-forged and as-welded specimens were thermally precharging with tritium gas at 34.5 MPa and 623 K, then aged for up to 17 years to buildin decay helium prior to testing. ASTM J-Integral fracture mechanics analyses, transmission electron microscopy (TEM), and small angle neutron scattering (SANS) examinations were conducted to characterize the effects of tritium and its radioactive decay product, helium-3. Results show that the fracture toughness values were reduced to less than 2-4% of the as-forged values for specimens with more than 1300 appm helium from tritium decay. The trend of decreasing fracture toughness values with increasing helium content was consistent with earlier observations, and the data show that Type 304L stainless steel is more resistant to tritium-induced cracking than Type 21-6-9 stainless at similar decay helium levels. The fracture toughness properties of long-aged weldments were also affected, but the reductions were not as severe over time because weldments did not retain as much tritium as did the base metals. TEM observations were used to characterize the effects of decay helium bubbles on the deformation substructures, but nanometer-sized helium bubbles were not easily resolved because of high dislocation densities within the forged microstructures. SANS results are presented that suggest the technique can provide information on decay helium bubble size, spacing, and distribution in these steels.

36 MATERIALS SCIENCE↗

Localized Corrosion of Chromium-Containing Conventional and Multiprincipal Element Alloys in Methanol and Aqueous Chloride Environments

The localized corrosion behavior of Type 304L stainless steel (UNS S30400), Alloy 625 (UNS N06625), and three experimental NiCoCrMo multiprincipal element alloys (MPEA), exposed to methanol/lithium chloride solutions with different water contents, is examined in this paper. Cyclic potentiodynamic polarization tests indicated that water increased the pitting and repassivation potentials and the critical temperature at which localized corrosion occurred in chloride solutions. The effect of water on repassivation potential in methanol-chloride solution depended on the chloride concentration and alloy content. At lower chloride concentration and higher alloy content, water had a greater inhibiting effect on repassivation potential, suggesting a competitive reaction between chloride and water on the metal surface in the pit. The localized corrosion resistance of the MPEAs followed the same trend as that of commercial stainless steels and Ni-base alloys in terms of the effect of alloying elements. The implications of these results on the mechanisms of localized corrosion are discussed.

Materials Science↗

2019 accomplishments: degradation of mechanical properties in structural metals and welds for FTS reservoirs

This report documents work in 2019 at SRNL in support of the Aging and Lifetimes program. Specimens for fracture toughness testing were prepared in prior years by thermally pre-charging samples, provided by Sandia National Laboratories, of welded types 304L and 21-6-9 stainless steels. These samples were pre-charged in 2017. The fracture toughness of the first aged specimens was measured and compared to historical data. The measurements of the 304L and 21-6-9 weld and particularly HAZ represent some of the first fracture data relevant to modern GTS reservoirs. This work represents an on-going collaboration between SRNL and SNL to understand tritium embrittlement of structural metals in Gas Transfer System reservoirs which informs lifetime assessments. Continued testing was conducted on ongoing historical studies, including the effects of very long-term aging, and the relative performance of differently forged stockpile relevant 304L and 316L samples. New samples were pre-charged with tritium and placed in a freezer for an aging study to allow helium to build into the material. The precharged samples consist of smooth and notched tensile samples of 304L stainless steel, as well as tube tensile samples of different thermal treatments supplied by Sandia National Laboratories. Their charging marks the beginning of a new sequence of studies to explore fundamental deformation mechanisms underpinning tritium embrittlement. At predesignated times, samples will be removed from aging and tested to provide data which will help develop an understanding of material degradation with increasing aging time. Also documented is progress in employing various advanced characterization techniques including high resolution electron microscopy, thermally programed desorption, and small angle x-ray scattering, as well as facilities renovations and equipment procurements in support of sustained tritium impacts on materials program at SRNL.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Molecular Iodine Interactions with Metal Substrates: Towards the Understanding of Iodine Interactions in the Environment Following a Nuclear Accident

In order to evaluate the potential impacts to the public from radioiodine in a nuclear event, it is vital to expand our understanding of the interaction of molecular iodine with various surfaces. There are many potential surfaces that iodine could interact with in and around a nuclear facility, including stainless steel. This study, carried out at ambient temperature, pressure and humidity, demonstrates the highly adsorptive nature of molecular iodine on two types of austenitic stainless steel, 304L and 316L. In the authors review of available literature, Fe is the only metal in stainless steel that is assumed to react with gas-phase molecular iodine. By using a novel approach which combines Inductively Coupled Plasma-Optical Emission Spectroscopy (ICP-OES) with surface Energy Dispersive X-ray Spectroscopy (EDS) there is evidence of the formation of metal iodides that have not previously been verified or quantified. Samples exposed to gaseous molecular iodine formed an iodine containing corrosion product visible by scanning electron microcopy (SEM). Evaluation of the metals in the corrosion region using EDS was compared to a water leach of the same samples analyzed using ICP-OES. A comparison of the results provide evidence that the water leachate is representative of the corrosion layer and not the base material. Furthermore, it provides confirmation of metal iodide formation with minor stainless-steel constituents including: FeI2, NiI2, MnI2 and CrI2.

Beck, Chelsie L.↗

Effect of microstructural and environmental variables on ductility of austenitic stainless steels

Austenitic stainless steels are used extensively in harsh environments, including for high-pressure gaseous hydrogen service. However, the tensile ductility of this class of materials is very sensitive to materials and environmental variables. While tensile ductility is generally insufficient to qualify a material for hydrogen service, ductility is an effective tool to explore microstructural and environmental variables and their effects on hydrogen susceptibility, to inform understanding of the mechanisms of hydrogen effects in metals, and to provide insight to microstructural variables that may improve relative performance. In this study, hydrogen precharging was used to simulate high-pressure hydrogen environments to evaluate hydrogen effects on tensile properties. Several austenitic stainless steels were considered, including both metastable and stable alloys. Room temperature and subambient temperature tensile properties were evaluated with three different internal hydrogen contents for type 304L and 316L austenitic stainless steels and one hydrogen content for XM-11. Significant ductility loss was observed for both metastable and stable alloys, suggesting the stability of the austenitic phase is not sufficient to characterize the effects of hydrogen. Internal hydrogen does influence the character of deformation, which drives local damage accumulation and ultimately fracture for both metastable and stable alloys. While a quantitative description of hydrogen-assisted fracture in austenitic stainless steels remains elusive, these observations underscore the importance of the hydrogen-defect interactions and the accumulation of damage at deformation length scales.

36 MATERIALS SCIENCE↗

Fatigue and Fracture Behavior of Additively Manufactured Austenitic Stainless Steel

Additive manufacturing (AM) includes a diverse suite of innovative manufacturing processes for producing near-net shape components, typically from powder or wire feedstock. Reported mechanical properties of AM materials vary significantly depending on the details of the manufacturing process and the characteristics of the processing defects (namely, lack of fusion defects). However, an excellent combination of strength, ductility and fracture resistance can be achieved in AM type 304L and 316L austenitic stainless steels by minimizing processing defects. It is also important to recognize that localized solidification processing during AIVI produces microstructures more analogous to weld microstructures than wrought microstructures. Consequently, the mechanical behavior of AM austenitic stainless steels in harsh environments can diverge from the performance of wrought materials. This report gives an overview of the fracture and fatigue response of type 304L materials from both directed energy deposition (DED) and powder bed fusion (PBF) techniques. In particular, the mechanical performance of these materials is considered for high-pressure hydrogen applications by evaluating fatigue and fracture resistance after thermally precharging of test specimens in high-pressure gaseous hydrogen. The mechanical behaviors are considered with respect to previous reports on hydrogen-assisted fracture of austenitic stainless steel welds and the unique characteristics of the AM microstructures. Fatigue crack growth can be relatively insensitive to processing defects, displaying similar behavior as wrought materials. Fracture resistance of dense AM austenitic stainless steel, on the other hand, is more consistent with weld metal than with compositionally-similar wrought materials. Hydrogen effects in the AM materials are generally more severe than in wrought materials, but comparable to measurements on welded austenitic stainless steels in hydrogen environments. While hydrogenassisted fracture manifests differently in welded and AM austenitic stainless steel, the fracture process appears to have a common origin in the compositional microsegregation intrinsic to solidification processes.

additive manufacturing, austenitic stainless steel↗

Corrosion of Ferrous Structural Alloys in Biomass Derived Fuels and Organic Acids

This work investigated the corrosivity of biomass-derived liquid fuels and organic acids associated with bio-oils and conducted a corrosion compatibility evaluation of several structural ferrous alloys in the fuels and acids. Here, the acidity parameters and solution conductivity values were higher in raw pyrolysis bio-oils than postprocessed oils with significant corrosion attack for carbon steel and Fe-2.25Cr-1Mo. However, higher-grade stainless steels, ferritic Fe-15Cr (15Cb) and austenitic types 304L and 316L, showed negligible corrosion loss, whereas lower-Cr ferritic grades 409, 410, and 416 were attacked. Metal leaching tests and electrochemical impedance spectroscopy measurements revealed superior corrosion resistance of 316 over 410 stainless steels in solutions of formic and oxalic acids that can be present in bio-oils. The corrosion evaluation methods utilized in this work provide effective screening tools to identify the compatible structural alloys for bio-oils.

09 BIOMASS FUELS↗

FY23 Simulation of Elastic-Plastic Failure Propagation

This memo summarizes the simulation of ductile failure propagation work conducted under the ASC project “V&V of Ductile Failure” conducted during FY 23. Physically, the failure propagation consists of crack propagation in the material. In the numerical setting—specifically in a finite element model—propagation can be accomplished through element death when critical conditions occur locally at an element that is then deleted from the simulation. The validation of the finite element models is evaluated by direct comparison between the experimental and simulation results regarding the rate of crack growth and its influence on the load-deflection response of the specimens tested. This work considers two geometries that display stable crack propagation under displacement-controlled conditions. The first geometry consists of hat specimens loaded in compression with nominally identical geometries but made with three different materials: Steel A286, Al 7075-T651 and 304L stainless steel. The three materials represent a range of ductility values that affect the response and crack propagation within the specimen. The crack induced propagates under an essentially mode-II type of deformation. The second geometry consists of a pre-cracked 304L stainless steel compact tension test specimen loaded so as to induce a mode-I deformation at the crack.

36 MATERIALS SCIENCE↗

Cold Spray Deposition of 304L Stainless Steel to Mitigate Chloride-Induced Stress Corrosion Cracking in Canisters for Used Nuclear Fuel Storage

A feasibility study of the cold spray deposition process of 304L stainless steel on 304L stainless steel substrates as a mitigation method for chloride-induced stress corrosion cracking (CISCC) has been investigated under various substrate conditions. The study is aimed at the application of this technology to mitigate CISCC that may potentially occur in or nearthe fusion welded regions of stainless steel canisters in Dry Cask Storage System (DCSS) for used nuclear fuels. Spherical gas-atomized 304L stainless steel powder, in the size range of 25 µm to 44 µm, was used as a feedstock powder for the cold spray process. The powder was deposited on four types of 304L substrates with various surface conditions: as-polished, oxidized, cold-rolled, plates with prototypical CISCC. The effects of cold spray parameters on quality of cold spray coatings were investigated. Thickness, porosity, and phases in the as-deposited materials were evaluated using scanning electron microscopy (SEM) and X-ray diffraction (XRD), and correlated with microhardness and adhesion strength measured via micro-indentation and ASTM C633 pulling test, respectively. XRD analysis of the coatings was also conducted to examine the effects of cold spray condition on residual stress state in the coating. Detailed cross-sectional examination of coating/substrate interfaces was performed with transmission electron microscopy (TEM) equipped with energy dispersive spectroscopy (EDS). Dense and continuous coatings with good adhesion strength and hardness were produced for the various substrate conditions by adjusting cold spray parameters. The results demonstrate that cold spray stainless steel coating is a viable option to provide a physical barrier against CISCC in fusion weld regions of stainless steel in corrosive chloride salt-bearing environments.

Dry Cask Storage Systems, cold spray, 304L stainle↗

Experimental and Computational Studies of Stress Corrosion Cracking of Alloys 308/309 and 82/182 Weldments in Corrosive and Radiation Environment

The goal of the project was to determine factors that influence SCC and IASCC in weldments found in LWR nuclear power plants. We focused on a SA508-304L SS weldment fabricated by EPRI using gas tungsten arc welding and used an aggressive BWR normal water chemistry (NWC) immersion environment. This weldment used 309L butter and 308L groove filler material. The microstructure of the 309L butter was non-uniform, exhibiting a 20–30μm thick martensitic layer closest to the SA508 interface, a 1–4 mm thick single γ austenite phase dilution zone, and a γ–δ duplex region extending to the 308L groove filler. The 308L groove filler had an entirely γ–δ duplex microstructure. Two approximately 1-inch thick 304L and SA508 plates approximately 12 by 6 square inches were joined using standard nuclear grade welding techniques. This included a post weld heat treatment of the 309L butter after application, a 0.32 cm fit-up root opening, and 57 bead lines of 308L groove filler applied in 18 layers. A 60 degree weld bevel angle was used and the 309L butter was 1.5 cm thick. Displacement cascade damage was induced using proton irradiation at the Michigan Ion Beam Laboratory. The incident proton energy was 2 MeV, the sample temperature was 360 ºC, and the calculated dpa value at 10 μm (60% of the Bragg peak depth of ~18 μm) was 5 dpa using the quick Kinchin-Pease model. Proton irradiation to this damage level required approximately 125 hours of beam time. Two types of samples were irradiated, tensile specimens and TEM bars. Samples were selected from all regions of the weldment, including the SA508-309L butter interface, the 309L-308L interface, and 308L-304L interface. The stainless steel alloys (304L, 308L, and 309L) within the heat affected zone are characterized by a duplex skeletal morphology of δ-ferrite and γ-austenite resulting from the recrystallization associated with weld fabrication. Approximately 7 to 8 mm of length along the specimen was irradiated. The gauge volume surfaces were mechanically polished and then electro-polished to remove mechanical damage from the mechanical polishing step prior to irradiation. Immersion tests were performed in a recirculating autoclave under BWR NWC conditions (2000 ppb wt. dissolved oxygen, neutral pH, 288 ºC, 10 MPa, and inlet water conductivity <100 nS/cm) to accelerate corrosion. Constant strain rate tests were performed either to failure or to approximately 5% strain. Strain rates of 10 -7 to 10 -6 mm/mm/s were used and typical immersion testing required four to six weeks to achieve failure or strains near 5%. Analysis primarily used advanced electron microscopy techniques of FIB lift out specimens.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Crystallographic effects on transgranular chloride-induced stress corrosion crack propagation of arc welded austenitic stainless steel

Abstract The effect of crystallography on transgranular chloride-induced stress corrosion cracking (TGCISCC) of arc welded 304L austenitic stainless steel is studied on >300 grains along crack paths. Schmid and Taylor factor mismatches across grain boundaries (GBs) reveal that cracks propagate either from a hard to soft grain, which can be explained merely by mechanical arguments, or soft to hard grain. In the latter case, finite element analysis reveals that TGCISCC will arrest at GBs without sufficient mechanical stress, favorable crystallographic orientations, or crack tip corrosion. GB type does not play a significant role in determining TGCISCC cracking behavior nor susceptibility. TGCISCC crack behaviors at GBs are discussed in the context of the competition between mechanical, crystallographic, and corrosion factors.

36 MATERIALS SCIENCE↗