Investigation of Weibull statistics in fracture analysis of cast aluminum

The fracture strengths of two large batches of A357-T6 cast aluminum coupon specimens were compared by using two-parameter Weibull analysis. The minimum number of these specimens necessary to find the fracture strength of the material was determined. The applicability of three-parameter Weibull analysis was also investigated. A design methodology based on the combination of elementary stress analysis and Weibull statistical analysis is advanced and applied to the design of a spherical pressure vessel shell. The results from this design methodology are compared with results from the applicable ASME pressure vessel code.

Holland, Frederic A., Jr.↗

Investigation of Weibull statistics in fracture analysis of cast aluminum

The fracture strengths of two large batches of A357-T6 cast aluminum coupon specimens were compared by using two-parameter Weibull analysis. The minimum number of these specimens necessary to find the fracture strength of the material was determined. The applicability of three-parameter Weibull analysis was also investigated. A design methodolgy based on the combination of elementary stress analysis and Weibull statistical analysis is advanced and applied to the design of a spherical pressure vessel shell. The results from this design methodology are compared with results from the applicable ASME pressure vessel code.

Holland, F. A., Jr.↗

Fiber Breakage Model for Carbon Composite Stress Rupture Phenomenon: Theoretical Development and Applications

Stress rupture failure of Carbon Composite Overwrapped Pressure Vessels (COPVs) is of serious concern to Science Mission and Constellation programs since there are a number of COPVs on board space vehicles with stored gases under high pressure for long durations of time. It has become customary to establish the reliability of these vessels using the so called classic models. The classical models are based on Weibull statistics fitted to observed stress rupture data. These stochastic models cannot account for any additional damage due to the complex pressure-time histories characteristic of COPVs being supplied for NASA missions. In particular, it is suspected that the effects of proof test could significantly reduce the stress rupture lifetime of COPVs. The focus of this paper is to present an analytical appraisal of a model that incorporates damage due to proof test. The model examined in the current paper is based on physical mechanisms such as micromechanics based load sharing concepts coupled with creep rupture and Weibull statistics. For example, the classic model cannot accommodate for damage due to proof testing which every flight vessel undergoes. The paper compares current model to the classic model with a number of examples. In addition, several applications of the model to current ISS and Constellation program issues are also examined.

Murthy, Pappu L. N.↗

Statistical study of thermal fracture of ceramic materials in the water quench test

The Weibull statistical theory of fracture was applied to thermal shock of ceramics in the water quench test. Transient thermal stresses and probability of failure were calculated for a cylindrical specimen cooled by convection. The convective heat transfer coefficient was calibrated using the time to failure which was measured with an acoustic emission technique. Theoretical failure probability distributions as a function of time and quench temperature compare favorably with experimental results for three high-alumina ceramics and a glass.

Rogers, Wayne P.↗

A Reliability Model for Ni-BaTiO3-Based (BME) Ceramic Capacitors

The evaluation of multilayer ceramic capacitors (MLCCs) with base-metal electrodes (BMEs) for potential NASA space project applications requires an in-depth understanding of their reliability. The reliability of an MLCC is defined as the ability of the dielectric material to retain its insulating properties under stated environmental and operational conditions for a specified period of time t. In this presentation, a general mathematic expression of a reliability model for a BME MLCC is developed and discussed. The reliability model consists of three parts: (1) a statistical distribution that describes the individual variation of properties in a test group of samples (Weibull, log normal, normal, etc.), (2) an acceleration function that describes how a capacitors reliability responds to external stresses such as applied voltage and temperature (All units in the test group should follow the same acceleration function if they share the same failure mode, independent of individual units), and (3) the effect and contribution of the structural and constructional characteristics of a multilayer capacitor device, such as the number of dielectric layers N, dielectric thickness d, average grain size r, and capacitor chip size S. In general, a two-parameter Weibull statistical distribution model is used in the description of a BME capacitors reliability as a function of time. The acceleration function that relates a capacitors reliability to external stresses is dependent on the failure mode. Two failure modes have been identified in BME MLCCs: catastrophic and slow degradation. A catastrophic failure is characterized by a time-accelerating increase in leakage current that is mainly due to existing processing defects (voids, cracks, delamination, etc.), or the extrinsic defects. A slow degradation failure is characterized by a near-linear increase in leakage current against the stress time; this is caused by the electromigration of oxygen vacancies (intrinsic defects). The two identified failure modes follow different acceleration functions. Catastrophic failures follow the traditional power-law relationship to the applied voltage. Slow degradation failures fit well to an exponential law relationship to the applied electrical field. Finally, the impact of capacitor structure on the reliability of BME capacitors is discussed with respect to the number of dielectric layers in an MLCC unit, the number of BaTiO3 grains per dielectric layer, and the chip size of the capacitor device.

reliability↗

Microstructural, Chemical and Mechanical Characterization of Polymer-Derived Hi-Nicalon Fibers with Surface Coatings

Room temperature tensile strengths of as-received Hi-Nicalon fibers and those having BN/SiC, p-BN/SiC, and p-B(Si)N/SiC surface coatings, deposited by chemical vapor deposition, were measured using an average fiber diameter of 13.5 microns. The Weibull statistical parameters were determined for each fiber. The average tensile strength of uncoated Hi-Nicalon on was 3.19 +/- 0.73 GPa with a Weibull modulus of 5.41. Strength of fibers coated with BN/SiC did not change. However, coat with p-BN/SiC and p-B(Si)N/SiC surface layers showed strength loss of approx. 10 and 35 percent, respectively, compared with as-received fibers. The elemental compositions of the fibers and the coatings were analyzed using scanning Auger microprobe and energy dispersive x-ray spectroscopy. The BN coating was contaminated with a large concentration of carbon and some oxygen. In contrast, p-BN, p-B(Si)N, and SiC coatings did not show any contamination. Microstructural analyses of the fibers and the coatings were done by scanning electron microscopy (SEM), transmission electron microscopy (TEM), and selected area electron diffraction. Hi-Nicalon fiber consists of the P-SIC nanocrystals ranging in size from 1 to 30 nm embedded in an amorphous matrix. TEM analysis of the BN coating revealed four distinct layers with turbostatic structure. The p-BN layer was turbostratic and showed considerable preferred orientation. The p-B(Si)N was glassy and the silicon and boron were uniformly distributed. The silicon carbide coating was polycrystalline with a columnar structure along the growth direction. The p-B(Si)N/SiC coatings were more uniform, less defective and of better quality than the BN/SiC or the p-BN/SiC coatings.

Bansal, Narottam P.↗

Measuring the Weibull modulus of microscope slides

The objectives are that students will understand why a three-point bending test is used for ceramic specimens, learn how Weibull statistics are used to measure the strength of brittle materials, and appreciate the amount of variation in the strength of brittle materials with low Weibull modulus. They will understand how the modulus of rupture is used to represent the strength of specimens in a three-point bend test. In addition, students will learn that a logarithmic transformation can be used to convert an exponent into the slope of a straight line. The experimental procedures are explained.

Sorensen, Carl D.↗

Mechanical, Chemical and Microstructural Characterization of Monazite-Coated Silicon Carbide Fibers

Tensile strengths of as-received Hi-Nicalon and Sylramic fibers and those having monazite surface coatings, deposited by atmospheric pressure chemical vapor deposition, were measured at room temperature and the Weibull statistical parameters determined. The average tensile strengths of uncoated Hi-Nicalon and Sylramic fibers were 3.19 +/- 0.73 and 2.78 +/- 0.53 GPa with a Weibull modulus of 5.41 and 5.52, respectively. The monazite-coated Hi-Nicalon and Sylramic fibers showed strength loss of approx. 10 and 15 percent, respectively, compared with the as-received fibers. The elemental compositions of the fibers and the coatings were analyzed using scanning Auger microprobe and energy dispersive X-ray spectroscopy. The LaPO4 coating on Hi-Nicalon fibers was approximately stoichiometric and about 50 nm thick. The coating on the Sylramic fibers extended to a depth of about 100 to 150 nm. The coating may have been stoichiometric LaPO4 in the first 30 to 40 nm of the layer. However, the surface roughness of Sylramic fiber made this profile somewhat difficult to interpret. Microstructural analyses of the fibers and the coatings were done by scanning electron microscopy, transmission electron microscopy, and selected area electron diffraction. Hi-Nicalon fiber consists of fine beta-SiC nanocrystals ranging in size from 1 to 30 mn embedded in an amorphous matrix. Sylramic is a polycrystalline stoichiometric silicon carbide fiber consisting of submicron beta-SiC crystallites ranging from 100 to 300 nm. Small amount of TiB2 nanocrystallites (approx. 50 nm) are also present. The LaPO4 coating on Hi-Nicalon fibers consisted of a chain of peanut shape particles having monazite-(La) structure. The coating on Sylramic fibers consisted of two layers. The inner layer was a chain of peanut shape particles having monazite-(La) structure. The outer layer was comprised of much smaller particles with a microcrystalline structure.

Bansal, N. P.↗

The effects of surface finish and grain size on the strength of sintered silicon carbide

The effects of surface treatment and microstructure, especially abnormal grain growth, on the strength of sintered SiC were studied. The surfaces of sintered SiC were treated with 400, 800 and 1200 grit diamond wheels. Grain growth was induced by increasing the sintering times at 2050 C. The beta to alpha transformation occurred during the sintering of beta-phase starting materials and was often accompanied by abnormal grain growth. The overall strength distributions were established using Weibull statistics. The strength of the sintered SiC is limited by extrinsic surface flaws in normal-sintered specimens. The finer the surface finish and grain size, the higher the strength. But the strength of abnormal sintering specimens is limited by the abnormally grown large tabular grains. The Weibull modulus increases with decreasing grain size and decreasing grit size for grinding.

You, Y. H.↗

The analysis of Gemini 7 EEG data by three different computer oriented methods

The problem in assessment of electroencephalograms has been the subject element in visual evaluations of such records as well as the need for extensive training (2 or 3 years) before suitable candidate is capable to perform this task. There have been variety of computer type analyses of EEG during the past ten years or more, and we are still searching for a reliable, inexpensive, online data processing procedure for this task. We are aware our Soviet colleagues are routinely using computer assessment of EEGs, using relatively inexpensive hardware. In our report we endeavor to show how four different assessment procedures (visual assessment, zero crossing technique, smoothing and peak counting technique, and Weibull Statistic) may be utilized, and indicate the advantages and disadvantages peculiar to each. We wish to point out that in the Gemini 7 EEG analog records supplied to the Henry Ford Hospital, Channel II (mid-line central to mid-line occipital electrodes) could not be assessed reliably after approximately 26 hours of flight. Channel I (left central to left occipital electrodes) provided the more assessable EEG up to approximately 54 hours of flight. These channels were compared during the first 26 hours of flight, and no significant difference was found by our various assessment procedures. We, therefore, have limited this report to the findings on the analyses of Channel I during its approximate 54 hours of flight.

Proctor, L. D.↗

Effect of production processes on the fracture strength of silicon solar cells

Fracture of Czochralski silicon wafers during processing is an important factor in solar cell yield and cost. A fracture-mechanics test and analysis program was developed to evaluate fracture strength changes in the in-process wafer-to-cell processing at different stages on a manufacturer's production line. The strength data were described by Weibull statistical analysis and can be interpreted with the surface-flaw distribution of each of the process steps.

Chen, C. P.↗

Fracture strength of GaAs solar cells as a function of manufacturing process steps

Fracture of single crystal GaAs substrate during the solar cell processing is an important factor in solar cell yield and cost. Fracture mechanics technique was utilized to evaluate cell cracking characteristics and changes in fracture strength of GaAs solar cells in a present state-of-the-art of manufacturing process for GaAs solar cells from wafer to complete cell of a typical production line. Considerable change in the fracture strength of GaAs solar cells as a function of cell processing was found. The strength data were described by Weibull statistical analysis and can be interpreted with the change of flaw distribution of each of the manufacturing process steps.

Chen, C. P.↗

Monolithic ceramic analysis using the SCARE program

The Structural Ceramics Analysis and Reliability Evaluation (SCARE) computer program calculates the fast fracture reliability of monolithic ceramic components. The code is a post-processor to the MSC/NASTRAN general purpose finite element program. The SCARE program automatically accepts the MSC/NASTRAN output necessary to compute reliability. This includes element stresses, temperatures, volumes, and areas. The SCARE program computes two-parameter Weibull strength distributions from input fracture data for both volume and surface flaws. The distributions can then be used to calculate the reliability of geometrically complex components subjected to multiaxial stress states. Several fracture criteria and flaw types are available for selection by the user, including out-of-plane crack extension theories. The theoretical basis for the reliability calculations was proposed by Batdorf. These models combine linear elastic fracture mechanics (LEFM) with Weibull statistics to provide a mechanistic failure criterion. Other fracture theories included in SCARE are the normal stress averaging technique and the principle of independent action. The objective of this presentation is to summarize these theories, including their limitations and advantages, and to provide a general description of the SCARE program, along with example problems.

Manderscheid, Jane M.↗

Transmission overhaul and replacement predictions using Weibull and renewel theory

A method to estimate the frequency of transmission overhauls is presented. This method is based on the two-parameter Weibull statistical distribution for component life. A second method is presented to estimate the number of replacement components needed to support the transmission overhaul pattern. The second method is based on renewal theory. Confidence statistics are applied with both methods to improve the statistical estimate of sample behavior. A transmission example is also presented to illustrate the use of the methods. Transmission overhaul frequency and component replacement calculations are included in the example.

Savage, M.↗

Transmission overhaul and replacement predictions using Weibull and renewal theory

A method to estimate the frequency of transmission overhauls is presented. This method is based on the two-parameter Weibull statistical distribution for component life. A second method is presented to estimate the number of replacement components needed to support the transmission overhaul pattern. The second method is based on renewal theory. Confidence statistics are applied with both methods to improve the statistical estimate of sample behavior. A transmission example is also presented to illustrate the use of the methods. Transmission overhaul frequency and component replacement calculations are included in the example.

Savage, M.↗

Transmission overhaul estimates for partial and full replacement at repair

Timely transmission overhauls increase in-flight service reliability greater than the calculated design reliabilities of the individual aircraft transmission components. Although necessary for aircraft safety, transmission overhauls contribute significantly to aircraft expense. Predictions of a transmission's maintenance needs at the design stage should enable the development of more cost effective and reliable transmissions in the future. The frequency is estimated of overhaul along with the number of transmissions or components needed to support the overhaul schedule. Two methods based on the two parameter Weibull statistical distribution for component life are used to estimate the time between transmission overhauls. These methods predict transmission lives for maintenance schedules which repair the transmission with a complete system replacement or repair only failed components of the transmission. An example illustrates the methods.

Savage, M.↗

Scale effects on the transverse tensile strength of graphite epoxy composites

The influence of material volume on the transverse tensile strength of AS4/3501-6 graphite epoxy composites was investigated. Tensile tests of 90 degree laminates with 3 different widths and 5 different thicknesses were conducted. A finite element analysis was performed to determine the influence of the grip on the stress distribution in the coupons and explain the tendency for the distribution of failure locations to be skewed toward the grip. Specimens were instrumented with strain gages and extensometers to insure good alignment and to measure failure strains. Data indicated that matrix dominated strength properties varied with the volume of material that was stressed, with the strength decreasing as volume increased. Transverse strength data were used in a volumetric scaling law based on Weibull statistics to predict the strength of 90 degree laminates loaded in three point bending. Comparisons were also made between transverse strength measurements and out-of-plane interlaminar tensile strength measurements from curved beam bending tests. The significance of observed scale effects on the use of tests for material screening, quality assurance, and design allowables is discussed.

Obrien, T. Kevin↗

Long-life assessment of graphite epoxy materials for Space Station Freedom pressure vessels

Graphite/epoxy composite overwrapped pressure vessels are being considered for use on Space Station Freedom because of their light weight and high efficiency. These composite pressure vessels weigh roughly one-third of comparable all-metal aluminum pressure vessels, and could result in a 15,000-lb weight saving for the propulsion and fluid management and distribution systems. These vessels must resist failures under sustained pressure loads for crew safety considerations and adequate protection of the space structure during their 30-yr life. Weibull statistical analysis techniques have been applied, and a model developed, for predicting long-term stress-rupture behavior based on published short-term test data on composite strands and pressure vessels. Graphite/epoxy materials are calculated to have a 99.99-percent probability of surviving stress rupture for 30 yr under a sustained load of 50 percent ultimate failure strength. Stress-rupture lifetimes are predicted to increase as the size of the pressure vessels increases in support of the viscoelastic load-transfer mechanism proposed for stress rupture of fiber/epoxy composite materials.