Mechanical properties and determination of slip systems of the B2 YZn intermetallic compound

Single crystal specimens of YZn (B2) were tested in tension at room temperature. Specimens with a [1 0 1] tensile axis orientation exhibited {r_brace}0 1 1{l_brace} <100> primary slip and an ultimate tensile strength of 365MPa at 3.7% elongation. Specimens with [0 0 1] and [1 1 1] tensile axis orientations showed no slip lines and fractured at a stress of 180MPa at 3.3% and 130MPa at 2.9% elongation, respectively. Transmission electron microscopy (TEM) examination of the Burger's vector of dislocations in tensile tested specimens revealed <1 0 0>-type dislocations. TEM analysis suggested that a secondary slip system, {l_brace}0 0 1{r_brace}<1 0 0>, may be active. Banded features with a {l_brace}0 2 1{r_brace} orientation were observed in deformed YZn; these may be slip traces produced by the cross-slip of <1 0 0> dislocations. Acting together, {l_brace}0 1 1{r_brace} <1 0 0> and {l_brace}0 0 1{r_brace} <1 0 0> slip provide only three independent slip systems, and no extra independent systems are provided by the cross-slip. This finding is consistent with the low ductility of YZn.

36 MATERIALS SCIENCE↗

Materials Data on YZn by Materials Project

YZn is Halite, Rock Salt structured and crystallizes in the cubic Fm-3m space group. The structure is three-dimensional. Y is bonded to six equivalent Zn atoms to form a mixture of corner and edge-sharing YZn6 octahedra. The corner-sharing octahedral tilt angles are 0°. All Y–Zn bond lengths are 2.96 Å. Zn is bonded to six equivalent Y atoms to form a mixture of corner and edge-sharing ZnY6 octahedra. The corner-sharing octahedral tilt angles are 0°.

36 MATERIALS SCIENCE↗

Materials Data on YZn by Materials Project

YZn is Tetraauricupride structured and crystallizes in the cubic Pm-3m space group. The structure is three-dimensional. Y is bonded in a body-centered cubic geometry to eight equivalent Zn atoms. All Y–Zn bond lengths are 3.11 Å. Zn is bonded in a body-centered cubic geometry to eight equivalent Y atoms.

36 MATERIALS SCIENCE↗

Experimental and calculated phases in two as-cast and annealed Mg-Zn-Y alloys

The CALPHAD (Calculation of Phase Diagram) method was used to select ternary alloys from Mg-Zn-Y system, aimed at determining the role of precipitates in the microstructure and texture evolution of Mg during and after deformation. The selected alloys are Mg-6Zn-1.2Y and Mg-5Zn-2Y. The constituent phases in the as-cast Mg-6Zn-1.2Y alloy are {alpha}-Mg solid solution phase and I (Mg{sub 3}YZn{sub 6}) intermetallic phase. The as-cast Mg-5Zn-2Y alloy is composed of {alpha}-Mg, I and W (Mg{sub 3}Y{sub 2}Zn{sub 3}) phases. The intermetallics in the two alloys form by eutectic reaction, which in Mg-5Zn-2Y alloy results in initially W-phase formation and ultimately I-phase formation during solidification. After heat treatment, the Mg-6Zn-1.2Y and Mg-5Zn-2Y alloys contain nearly the same amount of ternary intermetallics (I and W phases, respectively) in equilibrium with {alpha}-Mg solid solution phase. The main solute in {alpha}-Mg phase is Zn with the same amount in the two alloys. The type and quantity of the phases obtained experimentally disagree with the results obtained from the thermodynamic database. One important discrepancy is that, in Mg-6Zn-1.2Y alloy, the I phase is not stable at the temperature of 430 Degree-Sign C, and that the W phase is the stable phase at this temperature. The differences in the experimental and calculated data indicate that the Mg-Zn-Y system requires to be reassessed with more experimental data. - Highlights: Black-Right-Pointing-Pointer Mg-6Zn-1.2Y and Mg-5Zn-2Y alloys were selected by FactSage Trade-Mark-Sign Thermodynamic software. Black-Right-Pointing-Pointer The I and W intermetallics in the two alloys form by eutectic reaction. Black-Right-Pointing-Pointer The alloys contain similar amounts of different intermetallics in equilibrium with {alpha}-Mg. Black-Right-Pointing-Pointer In Mg-6Zn-1.2Y, the I phase is not stable at the temperature of 430 Degree-Sign C. Black-Right-Pointing-Pointer The hardness of W phase is determined to be lower than that of I phase.

36 MATERIALS SCIENCE↗

Structure and microwave dielectric properties of Ba{sub 3}(VO{sub 4}){sub 2}–Zn{sub 2−x}SiO{sub 4−x} ceramic composites

Highlights: ► New Ba{sub 3}(VO{sub 4}){sub 2}–Zn{sub 1.87}SiO{sub 3.87} microwave dielectric composite ceramic was reported. ► The single-phase willemite was obtained by controlling of ZnO deficiency. ► The composite with 40 wt% Zn{sub 1.87}SiO{sub 3.87} exhibited excellent τ{sub f} value of 0.4 ppm/°C. - Abstract: Microwave dielectric ceramic composites with compositions of (1 − y)Ba{sub 3}(VO{sub 4}){sub 2}–yZn{sub 2−x}SiO{sub 4−x} (y = 0.4–0.6, x = 0.13) have been prepared by firing mixtures of Ba{sub 3}(VO{sub 4}){sub 2} and Zn{sub 1.87}SiO{sub 3.87}. The X-ray diffraction (XRD) analysis revealed that Zn{sub 2}SiO{sub 4} with a willemite phase can be obtained by appropriately controlling the ZnO deficiency. The starting Zn{sub 1.87}SiO{sub 3.87} powder should be thus composed of the ZnSiO{sub 4} crystal phase and redundant SiO{sub 2} amorphous phase at room temperature. The scanning electron microscopy studies demonstrated the coexistence of Zn{sub 2}SiO{sub 4} and Ba{sub 3}(VO{sub 4}){sub 2} phases in the sintered bodies, as further confirmed by the XRD and Raman results. The near-zero temperature coefficients of the resonant frequency (τ{sub f}) could be achieved by adjusting the relative content of the two phases owing to their opposite τ{sub f} values. The existence of a slight amount of secondary phases, element interdiffusion and non-stoichiometry such as Zn deficiency altogether made the predicted property values deviate from the experimentally measured ones. The composite ceramics with 40 wt% Zn{sub 1.87}SiO{sub 3.87} sintered at 1100 °C exhibited desirable microwave dielectric properties of the quality factor Q × f ∼ 23,000 GHz, dielectric constant ε{sub r} ∼ 9.3, and τ{sub f} ∼ 0.4 ppm/°C.

36 MATERIALS SCIENCE↗