Search NASA⌕ Search

SEARCH · Search NASA

Results for “ZnSb”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Computational and experimental analysis on Te-doped ZnSb thermoelectric material

Highlights: • Combined theoretical and experimental work on the Te-doping of thermoelectric ZnSb. • DFT calculation predict the influence of oxygen impurity on doping. • Experimental observation shows that Te-doped Zn4Sb3 is initially formed. • Transient Potential-Seebeck Microprobe scanning (T-PSM) used as a doping sensor. • An inert processing chain is a prerequisite for production of n-type ZnSb. - Abstract: We report a combined theoretical and experimental work on the tellurium doping of thermoelectric ZnSb. We investigated the influence of tellurium on the phase’s stabilities by DFT calculations. During experimental validation by SEM and EPMA characterization “needlelike” areas of Te-doped ZnSb were identified. The experimental results also highlight that for the compositions Zn{sub 0.5} Sb{sub 0.5-x} Te{sub x} the system reaches a non-equilibrium state where ZnSb, ZnTe and Te-doped ZnSb are simultaneously present. The determination of the doping mechanism has demonstrated the formation of Te-doped Zn{sub 4}Sb{sub 3} after quenching, leading to the formation of Te-doped ZnSb due to the zinc diffusion during annealing. Presumed from experimental observation oxygen prevents the tellurium diffusion. These results lead to the conclusion of an inert processing chain as a prerequisite for production of n-type ZnSb, which puts hurdles on a cheap and easily scalable tellurium doping for homogeneous and competitive products.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Reliable density functional calculations for the electronic structure of thermoelectric material ZnSb

In this paper, we present the results of systematic test calculations for the electronic structure of thermoelectric material ZnSb using a first-principles full-potential all electron computational method. We used a linear combination of atomic orbitals (LACO) formalism, based on density functional theory (DFT). The exchange-correlation interaction potential of the many electron system was described by using a generalized gradient approximation (GGA). We compared the calculated indirect and direct band gaps as well as the effective masses of holes and electrons in ZnSb with experimental measurement results. The calculated indirect band gap of ZnSb is 0.56 eV, which agrees very well with the experimentally measured values of 0.50 eV ~ 0.61 eV. The calculated direct band gap at X point is 0.89 eV. The calculated effective masses of electrons and holes in ZnSb also agree with experimental data. The systematical test calculations as well as the comparisons of the calculated results with experimental measurements show that the obtained electronic structure of ZnSb would be reliable. We did not observe a major deficiency of the first-principles DFT calculation for the electronic structure of ZnSb, using full-potential all electron LACO method. The reported electronic structure of single crystal ZnSb from this work may provide a fundamental knowledge base for further research and applications for this important thermoelectric material.

36 MATERIALS SCIENCE↗

Enhancement of thermoelectric properties by energy filtering: Theoretical potential and experimental reality in nanostructured ZnSb

Energy filtering has been suggested by many authors as a means to improve thermoelectric properties. The idea is to filter away low-energy charge carriers in order to increase Seebeck coefficient without compromising electronic conductivity. This concept was investigated in the present paper for a specific material (ZnSb) by a combination of first-principles atomic-scale calculations, Boltzmann transport theory, and experimental studies of the same system. The potential of filtering in this material was first quantified, and it was as an example found that the power factor could be enhanced by an order of magnitude when the filter barrier height was 0.5 eV. Measured values of the Hall carrier concentration in bulk ZnSb were then used to calibrate the transport calculations, and nanostructured ZnSb with average grain size around 70 nm was processed to achieve filtering as suggested previously in the literature. Various scattering mechanisms were employed in the transport calculations and compared with the measured transport properties in nanostructured ZnSb as a function of temperature. Reasonable correspondence between theory and experiment could be achieved when a combination of constant lifetime scattering and energy filtering with a 0.25 eV barrier was employed. However, the difference between bulk and nanostructured samples was not sufficient to justify the introduction of an energy filtering mechanism. The reasons for this and possibilities to achieve filtering were discussed in the paper.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Materials Data on Tl(ZnSb)2 by Materials Project

Tl(ZnSb)2 crystallizes in the tetragonal I4cm space group. The structure is three-dimensional and consists of two Tl ribbons oriented in the (0, 0, 1) direction and one ZnSb framework. In each Tl ribbon, Tl1+ is bonded in a 2-coordinate geometry to two equivalent Tl1+ atoms. Both Tl–Tl bond lengths are 3.74 Å. In the ZnSb framework, Zn2+ is bonded to four equivalent Sb+2.50- atoms to form a mixture of corner and edge-sharing ZnSb4 tetrahedra. There are a spread of Zn–Sb bond distances ranging from 2.67–2.74 Å. Sb+2.50- is bonded to four equivalent Zn2+ atoms to form a mixture of corner and edge-sharing SbZn4 tetrahedra.

36 MATERIALS SCIENCE↗

From the Ternary Phase Ca 14 Zn 1+δ Sb 11 (δ ≈ 0.4) to the Quaternary Solid Solutions Ca 14– x RE x ZnSb 11 (RE = La–Nd, Sm, Gd, x ≈ 0.9). A Tale of Electron Doping via Rare-Earth Metal Substitutions and the Concomitant Structural Transformations

In this work, the ternary compound Ca 14 Zn 1.37(1) Sb 11 and its six rare-earth metal substituted derivatives Ca 14–x RE x ZnSb 11 (RE = La–Nd, Sm, Gd; x ≈ 0.90±0.06) have been synthesized and structurally characterized by single-crystal X-ray diffraction methods. All com-pounds formally crystallize in the tetragonal Ca 14 AlSb 11 structure type (space group $I$4 1 $/ acd$, No. 142, $Z$ = 8). The crystal structure of Ca 14 Zn 1.37(1) Sb 11 subtly differs from the structure of the remaining six, as well as from the structure of the archetype, due to the presence of a partially occupied interstitial Zn position. The extra zinc atom is needed in this structure to alleviate the unfavorable number of valence electrons in the imaginary Ca 14 ZnSb 11 . Electron doping, via substitution of RE 3+ ions on Ca 2+ sites is shown as an alternative route to achieve electron balance in these Zn-based analogs of the Ca 14 AlSb 11 structure, which does not require the in-corporation of interstitial atoms. Electrical resistivity measurements done on single-crystalline samples are in agreement with the notion that Ca 14–x RE x ZnSb 11 behave as either bad metals or heavily-doped semi-conductors. Magnetization measurements show Curie-Weiss paramagnetic behavior related to the local-moment magnetism of the RE 3+ ions.

36 MATERIALS SCIENCE↗

On the tin impurity in the thermoelectric compound ZnSb: Charge-carrier generation and compensation

The technique for measuring the Hall coefficient and electrical conductivity in the thermal cycling mode is used to study the effect of the Sn impurity on the microstructure and properties of pressed ZnSb samples. Tin was introduced as an excess component (0.1 and 0.2 at %) and as a substitutional impurity for Zn and Sb atoms in a concentration of (2–2.5) at % The temperature dependences of the parameters of lightly doped samples are fundamentally like similar curves for ZnSb with 0.1 at % of Cu. The highest Hall concentration, 1.4 × 10{sup 19} cm{sup –3} at 300 K, is obtained upon the introduction of 0.1 at % of Sn; the dimensionless thermoelectric figure of merit attains its maximum value of 0.85 at 660 K. The experimental data are discussed under the assumption of two doping mechanisms, which are effective in different temperature ranges, with zinc vacancies playing the decisive role of acceptor centers. In two ZnSb samples with SnSb and ZnSn additives, the charge-carrier compensation effect is observed; this effect depends on temperature and markedly changes with doping type. As in p-type A{sup IV}–B{sup VI} materials with a low Sn content, hole compensation can be attributed to atomic recharging Sn{sup 2+} → Sn{sup 4+}. Types of compensating complexes are considered.

36 MATERIALS SCIENCE↗

ZnSb Polymorphs with Improved Thermoelectric Properties

Zn$_x$Sb$_{1–x}$ systems are one of the most promising materials for thermoelectric applications due to their low cost, low toxicity, and high thermoelectric figure of merit. We report the discovery and characterization of novel ZnSb polymorphs with improved thermoelectric properties from a systematic $ab initio$ structural search. The putative ground state at low temperature is a structure with $Pbca$ symmetry. Corresponding electron and phonon transport properties are computed, where the lattice thermal conductivity was accurately obtained through third-order interatomic force constants. At 500 K, both the reduced figure of merit $S^2/L$ as well as the lattice thermal conductivity are superior to any previously reported numbers on ZnSb polymorphs, rendering the $Pbca$ phase a promising candidate for an exceptionally good thermoelectric material.

36 MATERIALS SCIENCE↗

Optimum operating-temperature range and lifetime estimate for ZnSb:0.1 at % Cu thermoelectrics

The temperature dependences of concentration and mobility are investigated in 300–700–300 K thermal cycles at different durations of low-temperature annealing of a ZnSb:0.1 at % Cu sample before the onset of every thermal cycle. Concurrently, the material is annealed for 1500 hours at a temperature difference of 310–670 K, and, then, its thermoelectric parameters are measured. The results are analyzed taking into account the features of the crystalline structure and the covalent nature of the chemical bonds in ZnSb. The operating range and lifetime of this composition are estimated on the basis of a model of the interaction of impurity defects with a decrease in their acceptor activity and an increase in the hole-scattering cross section at low temperatures.

36 MATERIALS SCIENCE↗

Temperature dependence of the atomic structure and electrical activity of defects in ZnSb thermoelectric lightly doped with copper

A model for describing the temperature dependence of the defect microstructure in high-efficiency ZnSb thermoelectric with a copper content of 0.1 at % is chosen. The temperature dependences of the chargecarrier density and mobility for thermal cycle I (300–700–300 K) are analyzed taking into account the features of the crystal structure and covalent chemical bond in ZnSb. The basic defect structure (at temperatures of T = 560–605 K) is the state when all Cu atoms are equally distributed between sites of both sublattices and behave as acceptors, and the number of intrinsic donor and acceptor defects is much smaller. The effect of the latter becomes noticeable when the temperature goes beyond the above-mentioned range. At T > 605 K, extra acceptors (antisite Zn{sub Sb}) occur; upon cooling below 560 K, Cu{sub 2} dimers arise and the electrical activity of the impurity lowers. Dimer decay upon heating leads to growth in the concentration with temperature up to saturation in the above-mentioned range. Additional thermal cycles II–VIII are performed; the observed changes in the temperature dependences of the hole concentration and mobility are discussed in the context of the investigated model.

36 MATERIALS SCIENCE↗

Materials Data on ZnSb by Materials Project

ZnSb is SC16 CuCl, stable at 5GPa structured and crystallizes in the orthorhombic Pbca space group. The structure is three-dimensional. Zn2+ is bonded to four equivalent Sb2- atoms to form a mixture of distorted corner and edge-sharing ZnSb4 tetrahedra. There are a spread of Zn–Sb bond distances ranging from 2.69–2.91 Å. Sb2- is bonded in a 5-coordinate geometry to four equivalent Zn2+ and one Sb2- atom. The Sb–Sb bond length is 2.84 Å.

36 MATERIALS SCIENCE↗

Materials Data on Mg(ZnSb)2 by Materials Project

Mg(ZnSb)2 crystallizes in the trigonal P-3m1 space group. The structure is three-dimensional. Mg2+ is bonded to six equivalent Sb3- atoms to form MgSb6 octahedra that share corners with twelve equivalent ZnSb4 tetrahedra, edges with six equivalent MgSb6 octahedra, and edges with six equivalent ZnSb4 tetrahedra. All Mg–Sb bond lengths are 3.05 Å. Zn2+ is bonded to four equivalent Sb3- atoms to form ZnSb4 tetrahedra that share corners with six equivalent MgSb6 octahedra, corners with six equivalent ZnSb4 tetrahedra, edges with three equivalent MgSb6 octahedra, and edges with three equivalent ZnSb4 tetrahedra. The corner-sharing octahedra tilt angles range from 11–56°. There are three shorter (2.74 Å) and one longer (2.80 Å) Zn–Sb bond lengths. Sb3- is bonded to three equivalent Mg2+ and four equivalent Zn2+ atoms to form a mixture of distorted edge and corner-sharing SbMg3Zn4 pentagonal bipyramids.

36 MATERIALS SCIENCE↗

A study of transport properties in Cu and P doped ZnSb

ZnSb samples have been doped with copper and phosphorus and sintered at 798 K. Electronic transport properties are interpreted as being influenced by an impurity band close to the valence band. At low Cu dopant concentrations, this impurity band degrades the thermoelectric properties as the Seebeck coefficient and effective mass are reduced. At carrier concentrations above 1 × 10{sup 19 }cm{sup −3}, the Seebeck coefficient in Cu doped samples can be described by a single parabolic band.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Zintl-phase Eu 2 ZnSb 2 : A promising thermoelectric material with ultralow thermal conductivity

Zintl compounds are considered to be potential thermoelectric materials due to their “phonon glass electron crystal” (PGEC) structure. A promising Zintl-phase thermoelectric material, 2-1-2–type Eu 2 ZnSb 2 ( P 6 3 / mmc ), was prepared and investigated. The extremely low lattice thermal conductivity is attributed to the external Eu atomic layers inserted in the [Zn 2 Sb 2 ] 2- network in the structure of 1-2-2–type EuZn 2 Sb 2 ( P 3 ¯ m 1 ) , as well as the abundant inversion domain boundary. By regulating the Zn deficiency, the electrical properties are significantly enhanced, and the maximum ZT value reaches ∼1.0 at 823 K for Eu 2 Zn 0.98 Sb 2 . Our discovery provides a class of Zintl thermoelectric materials applicable in the medium-temperature range.

30 DIRECT ENERGY CONVERSION↗

Materials Data on Ba(ZnSb)2 by Materials Project

BaZn2Sb2 crystallizes in the orthorhombic Pnma space group. The structure is three-dimensional. Ba2+ is bonded in a 7-coordinate geometry to seven Sb3- atoms. There are a spread of Ba–Sb bond distances ranging from 3.53–3.78 Å. There are two inequivalent Zn2+ sites. In the first Zn2+ site, Zn2+ is bonded to four Sb3- atoms to form a mixture of edge and corner-sharing ZnSb4 tetrahedra. There are a spread of Zn–Sb bond distances ranging from 2.71–2.80 Å. In the second Zn2+ site, Zn2+ is bonded to four Sb3- atoms to form a mixture of edge and corner-sharing ZnSb4 tetrahedra. There are a spread of Zn–Sb bond distances ranging from 2.69–2.85 Å. There are two inequivalent Sb3- sites. In the first Sb3- site, Sb3- is bonded in a 7-coordinate geometry to three equivalent Ba2+ and four Zn2+ atoms. In the second Sb3- site, Sb3- is bonded in a 4-coordinate geometry to four equivalent Ba2+ and four Zn2+ atoms.

36 MATERIALS SCIENCE↗

Materials Data on Ca(ZnSb)2 by Materials Project

CaZn2Sb2 crystallizes in the trigonal P-3m1 space group. The structure is three-dimensional. Ca2+ is bonded to six equivalent Sb3- atoms to form CaSb6 octahedra that share corners with twelve equivalent ZnSb4 tetrahedra, edges with six equivalent CaSb6 octahedra, and edges with six equivalent ZnSb4 tetrahedra. All Ca–Sb bond lengths are 3.23 Å. Zn2+ is bonded to four equivalent Sb3- atoms to form ZnSb4 tetrahedra that share corners with six equivalent CaSb6 octahedra, corners with six equivalent ZnSb4 tetrahedra, edges with three equivalent CaSb6 octahedra, and edges with three equivalent ZnSb4 tetrahedra. The corner-sharing octahedra tilt angles range from 19–53°. There are three shorter (2.72 Å) and one longer (2.82 Å) Zn–Sb bond lengths. Sb3- is bonded to three equivalent Ca2+ and four equivalent Zn2+ atoms to form a mixture of distorted edge and corner-sharing SbCa3Zn4 pentagonal bipyramids.

36 MATERIALS SCIENCE↗

Materials Data on Sr(ZnSb)2 by Materials Project

SrZn2Sb2 crystallizes in the trigonal P-3m1 space group. The structure is three-dimensional. Sr2+ is bonded to six equivalent Sb3- atoms to form SrSb6 octahedra that share corners with twelve equivalent ZnSb4 tetrahedra, edges with six equivalent SrSb6 octahedra, and edges with six equivalent ZnSb4 tetrahedra. All Sr–Sb bond lengths are 3.37 Å. Zn2+ is bonded to four equivalent Sb3- atoms to form ZnSb4 tetrahedra that share corners with six equivalent SrSb6 octahedra, corners with six equivalent ZnSb4 tetrahedra, edges with three equivalent SrSb6 octahedra, and edges with three equivalent ZnSb4 tetrahedra. The corner-sharing octahedra tilt angles range from 23–51°. There are three shorter (2.74 Å) and one longer (2.83 Å) Zn–Sb bond lengths. Sb3- is bonded to three equivalent Sr2+ and four equivalent Zn2+ atoms to form a mixture of distorted edge and corner-sharing SbSr3Zn4 pentagonal bipyramids.

36 MATERIALS SCIENCE↗