Search NASA⌕ Search

SEARCH · Search NASA

Results for “ZrC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Revisiting W–ZrC interfaces: A first principles study

We investigate W–ZrC interfaces using first-principles calculations based on the density functional theory. There have been theoretical and experimental studies exploring W–ZrC interfaces, however, the debate regarding the most stable interface continues to persist. In this study, we systematically simulated various W–ZrC interfaces merging W and ZrC surfaces with different orientations. Subsequently, we evaluated their stabilities and explained the corresponding stabilities in terms of the nature of bonding and charge-transfer processes at the interface. We find ZrC(111)–W(110) is the most stable interface with higher adhesive energy than the other interfaces. The additional stability associated with the ZrC(111)–W(110) results from significant interface reconstruction. Three layers of W and ZrC adjacent to the interface are involved in the charge-transfer process leading to stronger ionic bonds in ZrC(111)–W(110) as compared to the other potential candidate: ZrC(100)–W(100). The C and W atoms are found to be displaced from their symmetric position during the reconstruction process at the interface to facilitate stronger bonds with shorter W–C and W–Zr bonds in ZrC(111)–W(110) as compared to ZrC(100)–W(100). This leads to stronger covalent bonds in ZrC(111)–W(110) than that in ZrC(100)–W(100). Therefore, we conclude that the stronger covalent and ionic forces in ZrC(111)–W(110) than those in ZrC(100)–W(100) are responsible for making ZrC(111)–W(110) to be the most stable interface. In conclusion, this study addresses the long-standing question of the most stable W–ZrC interface and derives a number of implications for other W-transition metal carbide interfaces which are potential candidates for improving the mechanical properties of plasma facing materials.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Microstructure and Mechanical Properties of W-ZrC Composites Synthesized by Reactive Melt Infiltration of Zr{sub 2}Cu into Porous Preforms from Partially Carburized W Powders

W-ZrC composites with different W contents from 48 to 73 vol.% have been synthesized by reactive melt infiltration of Zr{sub 2}Cu melt into porous preforms from partially carburized W powders at 1300 °C for 1 h in vacuum. The influences of carbon content and porosity in the preforms on microstructure and mechanical properties of W-ZrC composites are investigated. Cold isostatic pressing followed by pre-sintering process is used to produce porous preforms with suitable porosities of 53.6-47% under a pressure of 100 MPa to allow sufficient penetration of Zr{sub 2}Cu melt into the preforms. Small amounts of Cu-rich phases form in the synthesized W-ZrC composites after a complete reaction of y/2xZr{sub 2}Cu(l) + WC{sub y}(s) = y/xZrC{sub x}(s) + W(s) + y/2xCu(l). These Cu-rich phases are distributed not only at the phase boundaries of W matrix and ZrC grains, but also in the interior of ZrC{sub x} grains. With decreasing W content from 73 to 48 vol.% in the W-ZrC composites, the flexural strength and fracture toughness increase from 519 to 657 MPa and from 9.1 to 10.6 MPa m{sup 1/2}, respectively.

36 MATERIALS SCIENCE↗

Hydrogen embrittlement and mechanical response of 304L steel with ZrC additions

While stainless steels are widely used for hydrogen storage infrastructure, they can still be vulnerable to hydrogen embrittlement justifying the need to further improve their hydrogen resiliency. Here, we investigate the potential for transition metal carbide additions to improve the hydrogen compatibility of austenitic stainless steels. ZrC nanoparticles were dispersed in contents of 0.01–10 wt% in 304 L stainless steel powder, mixed via high energy ball milling, and subsequently consolidated using direct current sintering. To assess hydrogen compatibility, the tensile properties of similarly processed 304 L without ZrC nanoparticles were compared to 304 L with the ZrC additions; both materials were evaluated prior to and after hydrogen exposure (non-charged and H-precharged, respectively). Depending upon the ZrC phase fraction, the yield strengths varied from ∼325 to 560 MPa in the non-charged condition and from ∼375 to 550 MPa in the H-precharged condition. Strain at failure varied from ∼5 to 90 % and from ∼5 to 35 % in the non-charged and hydrogen-precharged conditions, respectively. Results from stress-strain profiles demonstrate limited efficacy of ZrC as a method to mitigate hydrogen embrittlement entirely but does demonstrate the potency of ZrC inclusions as strengthening addition to 304 L alloys without a loss of ductility.

08 HYDROGEN↗

W-ZrC composites prepared by reactive melt infiltration of Zr 2 Cu alloy into binder jet 3D printed WC preforms

W-ZrC composites were successfully prepared by reactive melt infiltration (RMI) of stoichiometric and excess amounts of Zr 2 Cu into sintered and un-sintered WC preforms made from binder jet 3D printing. The focus of this work was to study the conversion of reactant powders and liquid infiltrant with varying preform density and infiltrant amount by controlling the processing time to reach high conversion yield while understanding the phase composition, microstructure, and hardness. To investigate the effect of time, the reactive melt infiltration was conducted at 1400 °C for 2, 4 and 8 h in a furnace with 96% Ar - 4% H2 gas atmosphere. The increase in reaction time from 2 to 8 h increased the W and W 2 C phase contents and decreased the ZrC phase content when using sintered WC preforms. Samples prepared from un-sintered WC preforms exhibited improved reactive melt infiltration compared to sintered samples, and there was no detectable W 2 C phase and nearly full consumption of WC. Similar to sintered WC samples, the content of W and ZrC phases increased with the increase in time from 2 to 8 h. The interfaces and phases at reaction interfaces were investigated using electron diffraction analysis and S/TEM-EDS to understand material stability; the phases were identified and consistent with XRD analysis. Additionally, there was no Cu present at the interfaces. Increasing the amount of infiltrant led to better reactive melt infiltration. In general, the hardness increased with reaction time and the highest Vickers hardness was found in the W-ZrC sample formed from sintered WC reacted with excess Zr 2 Cu. Finally, this research addresses the critical comparison of sintering and RMI time and shows that by using un-sintered samples for 8 h we are able to achieve W-ZrC composites with fewer undesired phases.

36 MATERIALS SCIENCE↗

Acetylene adsorption on δ-MoC(001), TiC(001) and ZrC(001) surfaces: A comprehensive periodic DFT study

A comprehensive study of acetylene adsorption on δ-MoC(001), TiC(001) and ZrC(001) surfaces was carried out by means of calculations based on periodic density functional theory, using the Perdew–Burke–Ernzerhof exchange–correlation functional. It was found that the bonding of acetylene was significantly affected by the electronic and structural properties of the carbide surfaces. The adsorbate interacted with metal and/or carbon sites of the carbide. The interaction of acetylene with the TiC(001) and ZrC(001) surfaces was strong (binding energies higher than $-$3.5 eV), while moderate acetylene adsorption energies were observed on δ-MoC(001) ($-$1.78 eV to –0.66 eV). Adsorption energies, charge density difference plots and Mulliken charges suggested that the binding of the hydrocarbon to the surface had both ionic and covalent contributions. According to the C–C bond lengths obtained, the adsorbed molecule was modified from acetylene-like into ethylene-like on the δ-MoC(001) surface (desired behavior for hydrogenation reactions) but into ethane-like on TiC(001) and ZrC(001). The obtained results suggest that the δ-MoC(001) surface is expected to have the best performance in selective hydrogenation reactions to convert alkynes into alkenes. Another advantage of δ-MoC(001) is that, after C 2 H 2 adsorption, surface carbon sites remain available, which are necessary for H 2 dissociation. Furthermore, these sites were occupied when C 2 H 2 was adsorbed on TiC(001) and ZrC(001), limiting their application in the hydrogenation of alkynes.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermal conductivity profile determination in proton-irradiated ZrC by spatial and frequency scanning thermal wave methods

Using complementary thermal wave methods, the irradiation damaged region of zirconium carbide (ZrC) is characterized by quantifiably profiling the thermophysical property degradation. The ZrC sample was irradiated by a 2.6 MeV proton beam at 600 °C to a dose of 1.75 displacements per atom. Spatial scanning techniques including scanning thermal microscopy (SThM), lock-in infrared thermography (lock-in IRT), and photothermal radiometry (PTR) were used to directly map the in-depth profile of thermal conductivity on a cross section of the ZrC sample. The advantages and limitations of each system are discussed and compared, finding consistent results from all techniques. SThM provides the best resolution finding a very uniform thermal conductivity envelope in the damaged region measuring ∼52 ± 2 μm deep. Frequency-based scanning PTR provides quantification of the thermal parameters of the sample using the SThM measured profile to provide validation of a heating model. Measured irradiated and virgin thermal conductivities are found to be 11.9 ± 0.5 W m{sup −1} K{sup −1} and 26.7 ±1 W m{sup −1} K{sup −1}, respectively. A thermal resistance evidenced in the frequency spectra of the PTR results was calculated to be (1.58 ± 0.1) × 10{sup −6} m{sup 2} K W{sup −1}. The measured thermal conductivity values compare well with the thermal conductivity extracted from the SThM calibrated signal and the spatially scanned PTR. Combined spatial and frequency scanning techniques are shown to provide a valuable, complementary combination for thermal property characterization of proton-irradiated ZrC. Such methodology could be useful for other studies of ion-irradiated materials.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Response of ZrC to swift heavy ion irradiation

Zirconium carbide (ZrC) is commonly used for energy sector research, as well as a surrogate for the proposed advanced nuclear fuel candidate uranium carbide. Here this study investigates structural modifications to nanocrystalline and microcrystalline ZrC resulting from dense electronic excitations induced by swift heavy ion exposure. Samples were irradiated with 946 MeV Au ions to various fluences up to 6 × 10 13 ions cm –2 and characterized using synchrotron-based x-ray diffraction. The evolution of the unit-cell parameter and heterogeneous microstrain were evaluated as a function of fluence and compared with those of nanocrystalline and microcrystalline CeO 2 (a surrogate for UO 2 fuel) irradiated under identical conditions. Distinct differences were observed in the radiation responses of the carbide and oxide across both grain sizes. Most notably, microcrystalline ZrC exhibits swelling characterized by two distinct regimes, which does not result in saturation at the ion fluences achieved. This contrasts with CeO 2 , which exhibits the well-documented direct-impact defect accumulation mechanism, reaching a steady-state saturation of swelling at higher fluences. Nanocrystalline CeO 2 undergoes more pronounced swelling compared with microcrystalline CeO 2 , in contrast to nanocrystalline ZrC, which exhibits only minimal unit-cell changes. These results demonstrate that swift heavy ion-induced structural changes can be quite different in carbides and oxides, which must be considered when extrapolating fission-fragment type damage in current fuels to advanced fuels.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Pre- and post-irradiation characterization and properties measurements of ZrC coated surrogate TRISO particles

Zirconium carbide is a candidate to either replace or supplement silicon carbide as a coating material in TRISO fuel particles for high temperature gas-cooled reactor fuels. Six sets of ZrC coated surrogate microsphere samples, fabricated by the Japan Atomic Energy Agency using the fluidized bed chemical vapor deposition method, were irradiated in the High Flux Isotope Reactor at the Oak Ridge National Laboratory. These developmental samples available for the irradiation experiment were in conditions of either as-fabricated coated particles or particles that had been heat-treated to simulate the fuel compacting process. Five sets of samples were composed of nominally stoichiometric compositions, with the sixth being richer in carbon (C/Zr = 1.4). The samples were irradiated at 800 and 1250 C with fast neutron fluences of 2 and 6 dpa. Post-irradiation, the samples were retrieved from the irradiation capsules followed by microstructural examination performed at the Oak Ridge National Laboratory's Low Activation Materials Development and Analysis Laboratory. This work was supported by the US Department of Energy Office of Nuclear Energy's Advanced Gas Reactor program as part of International Nuclear Energy Research Initiative collaboration with Japan. This report includes progress from that INERI collaboration, as well as results of some follow-up examination of the irradiated specimens. Post-irradiation examination items included microstructural characterization, and nanoindentation hardness/modulus measurements. The examinations revealed grain size enhancement and softening as the primary effects of both heat-treatment and irradiation in stoichiometric ZrC with a non-layered, homogeneous grain structure, raising serious concerns on the mechanical suitability of these particular developmental coatings as a replacement for SiC in TRISO fuel. Samples with either free carbon or carbon-rich layers dispersed in the ZrC coatings experienced negligible grain size enhancement during both heat treatment and irradiation. However, these samples experienced irradiation induced softening similar to stoichiometric ZrC samples.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Improving the Strength of the ZrC-SiC and TC4 Brazed Joint Through Fabricating Graded Double-Layered Composite Structure on TC4 Surface

In order to improve the ZrC-SiC ceramic and TC4 brazed joint property, graded double-layered SiC particles (SiCp)-reinforced TC4-based composite structure (named as GLS for convenience) was designed to relieve the residual stress in the joint. The GLS was successfully fabricated on TC4 substrate by double-layered laser deposition technology before the brazing process. The investigation of the GLS shows that the volume fraction of SiCp in the two composite layers was graded (20 and 39 vol pct, respectively). Ti{sub 5}Si{sub 3} and TiC phases formed in the GLS due to the reaction of SiCp and TC4. The laser power-II (the laser power for the second deposition layer) affected the microstructure of the GLS significantly. Increasing the laser power-II would promote the reaction between the SiCp and TC4. But the high laser power-II made the layer I remelt completely and the two layers became homogeneous rather than graded structure. In the ZrC-SiC and TC4 brazed joint, the CTE (coefficient of thermal expansion) was graded from the TC4 to the ZrC-SiC due to the GLS, and the strength of the joint with the GLS (91 MPa) was higher than that without the GLS (43 MPa).

36 MATERIALS SCIENCE↗

Helium induced microstructure damage, nano-scale grain formation and helium retention behaviour of ZrC

Transition-metal ultra-high temperature ceramics are promising materials for nuclear structural applications. However, an understanding of their response to high-temperature irradiation and helium is vastly limited. This paper presents a study of helium effects in zirconium carbide (ZrC) by performing room temperature 3 MeV 3 He + ion irradiations up to 5 × 10 20 ions m –2 (~1.8 at.% at peak) and high-temperature annealing (1273–1873 K), coupled with state-of-art characterization using transmission electron microscopy (TEM), scanning electron microscopy (SEM) and nuclear reaction analysis (NRA). We reveal that ZrC is susceptible to irradiation damage in terms of helium bubble formation. After annealing at 1373 K, tiny bubbles (1–2 nm) formed aligned clusters which were highly over-pressurized, producing strain contrast in TEM. At 1773 K, significant bubble growth occurred. Additionally, at 1773 K, a combined TEM/SEM analysis revealed dramatic matrix damage due to helium-induced surface blistering. Underneath blister caps, the microstructure evolved into ultra-fine nano-scale grains similar to high burn-up structures observed in nuclear fuels, but consisting of numerous nano-cracks. We hypothesize that such structures are formed due to high gas pressure build-up and its subsequent release. This phenomenon initiated at the grain boundaries. Blister top surface consisted of inter-granular and trans-granular cracks. NRA depth profiling revealed that helium was present as double peaks with major portion lying at the end-of-the-range (EOR) and the rest as TEM invisible clusters in a shoulder extending to the surface. ZrC started releasing helium after 1373 K. As a result, helium release increased significantly at higher temperatures, with majority helium loss occurring from EOR rather than from near-surface regions.

36 MATERIALS SCIENCE↗

Characterization of fusion welded ceramics in the SiC-ZrB 2 -ZrC system

Various SiC-ZrB 2 -ZrC ceramics were joined by fusion welding to determine the maximum silicon carbide content that could be joined. Commercial powders were hot pressed, machined, and preheated to 1450 °C before joining with a tungsten inert gas welding torch at 160–200 A. Resulting welds were cross-sectioned and analyzed to determine which compositions were weldable and to characterize microstructural evolution in welded samples. As compositions approached the ternary eutectic, the welds had smaller SiC grains and exhibited better weldability. Penetration depth of welds was controlled by a combination of current input and welding speed. Here, the ternary eutectic in the system was found at 36.9 ± 1.3 vol% SiC, 42.7 ± 1.5 vol% ZrB 2 , and 20.4 ± 1.9 vol% ZrC and its melting temperature was 2330 ± 23 °C. A ternary phase diagram for the SiC-ZrB 2 -ZrC was constructed and proposed via microstructural analysis of arc melted pellets on binary joins between each binary eutectic and the ternary eutectic in the system.

36 MATERIALS SCIENCE↗

Thermochemical Assessment of Oxygen Gettering by SiC or ZrC in PuO2-x TRISO Fuel

Particulate nuclear fuel in a modular helium reactor is being considered for the consumption of excess plutonium and related transuranics. In particular, efforts to largely consume transuranics in a single-pass will require the fuel to undergo very high burnup. This deep burn concept will thus make the proposed plutonia TRISO fuel particularly likely to suffer kernel migration where carbon in the buffer layer and inner pyrolytic carbon layer is transported from the high temperature side of the particle to the low temperature side. This phenomenon is oberved to cause particle failure and therefore must be mitigated. The addition of SiC or ZrC in the oxide kernel or in a layer in communication with the kernel will lower the oxygen potential and therefore prevent kernel migration, and this has been demonstrated with SiC. In this work a thermochemical analysis was performed to predict oxygen potential behavior in the plutonia TRISO fuel to burnups of 50% FIMA with and without the presence of oxygen gettering SiC and ZrC. Kernel migration is believed to be controlled by CO gas transporting carbon from the hot side to the cool side, and CO pressure is governed by the oxygen potential in the presence of carbon. The gettering phases significantly reduce the oxygen potential and thus CO pressure in an otherwise PuO2-x kernel, and prevent kernel migration by limiting CO gas diffusion through the buffer layer. The reduction in CO pressure can also reduce the peak pressure within the particles by ~50%, thus reducing the likelihood of pressure-induced particle failure. A model for kernel migration was used to semi-quantitatively assess the effect of controlling oxygen potential with SiC or ZrC and did demonstrated the dramatic effect of the addition of these phases on carbon transport.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of fluidized bed chemical vapor deposition ZrC coatings on PyC/YSZ kernels deposited under differing conditions

In this study, coated fuel particle architectures with ZrC coatings are candidate fuels for advanced power reactors and space nuclear propulsion (SNP) concepts. Owing to its relevance to SNP, the composition, microstructure, and mechanical properties of eight ZrC coatings prepared by fluidized bed chemical vapor deposition were evaluated. Evaluation by SEM and EBSD showed that all grains were columnar. Across the various examined samples, minor axis diameters varied between 0.3 and 1.1 μm, and major axis diameters varied between 0.4 and 2.3 μm. Major and minor diameters increased with thickness particularly at higher deposition temperatures in which the major grain axis (from an ellipse fit to the grain shape) increased by 2.5 μm over the entire coating. Coatings with higher reactive gas flows and Zr/C concentrations closer to 1 were observed to contain nanocrystalline graphite deposits. Reactive gas flow doubling led to increases in coating thickness from around 10–15 μm to around 22–27 μm.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The effect of powder feedstock and heat treatment on the thermal and mechanical properties of binder jet printed ZrC

In this study, zirconium carbide (ZrC) disks were fabricated using binder jet printing to study the effect of powder feedstock, print parameters, and heat treatment on flowability and final materials properties. A median volumetric particle size smaller than 10 μm was shown to cause the powder to stop flowing during printing. Disks were printed using ZrC with suitable flowability and then heat-treated at temperatures between 1800°C and 2200°C for 1 or 5h. The density, part shrinkage, thermal diffusivity, and fracture strength all increased with increasing temperature and time. The heat-treated disks were then heated to 2200°C for 5h and the properties converged for disks of the same particle size, indicating the hottest temperature and longest time of exposure dictates the final properties. Lastly, it was shown that larger particles produce lower density materials with worse thermal diffusivity, most likely because of poor connectivity between particles after heat treatment.

36 MATERIALS SCIENCE↗