Search NASA⌕ Search

SEARCH · Search NASA

Results for “anode solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Unraveling Morphology and Chemistry Dynamics in Fluoroethylene Carbonate Generated Silicon Anode Solid Electrolyte Interphase Across Delithiated and Lithiated States: Relative Cycling Stability Enabled by an Elastomeric Polymer Matrix

The silicon solid electrolyte interphase (SEI) faces cyclical cracking and reconstruction due to the ∼350% volume expansion. Understanding the SEI dynamic morphology and chemistry evolution from delithiated to lithiated states is thereby paramount to engineering a stable Si anode. Fluoroethylene carbonate (FEC) is a preferred additive with widely demonstrated enhancement of the Si cycling. Thus, insights into the dynamics of the FEC-SEI may provide hints toward engineering the Si interface. Herein, complementary ATR-FTIR, AFM, tip IR, and XPS probing reveal the presence of an elastomeric polycarbonate-like matrix in the FEC-generated SEI which is absent from the FEC-free SEI. Adding FEC to the baseline 1 M LiPF 6 in EC:EMC (1:1) electrolyte promotes formation of a thinner and more conformal SEI, and subdues morphology and chemistry changes between consecutive half-cycles. From AFM, morphological stabilization of the FEC-SEI occurs earlier. Furthermore, conventional SEI biproducts such as Li 2 CO 3 and LiEDC appear in reduced quantities in the FEC-SEI implying a reduced quantity of Li-consuming species. The thin polymeric FEC-SEI enables deeper (de)lithiation of silicon. In conclusion, the enhanced mechanical compliance, chemical invariance, and reduced Li inventory consumption of the FEC-SEI are logically the key features underlying the Si cycling enhancement by FEC.

25 ENERGY STORAGE↗

Recent progress in understanding solid electrolyte interphase on lithium metal anode

Lithium (Li) metal batteries (LMBs) are among the most promising candidates of next-generation high-energy-density rechargeable batteries. Solid electrolyte interphase (SEI) on Li metal anode plays a significant role which influences the Li deposition morphology and the cycle life of LMBs. Although SEI is the most important part, a thorough understanding of SEI is inadequate. In this review, we focus on the progresses of understanding on structures, properties and influencing factors of SEI as well as efficient strategies of tailoring SEI. First, the compositions, models and recent progresses on characterizing atomic structure of SEI are summarized. Second, the properties of SEI, including electronic conduction, ionic conduction, stability and mechanical properties are elucidated. Structures and properties of SEI are greatly influenced by multiple factors such as solvent, salt, additive, solvation structure, impurity, current density, temperature, pressure and capacity utilization. Thus, interactions between these factors and SEI are comprehensively discussed. Correlations of SEI with Li deposition morphology, rate capability and cycle life are further summarized. Moreover, efficient strategies of tailoring SEI with desired properties, including in-situ SEI and ex-situ SEI are also reviewed. Despite the significant progresses that have been achieved in the researches of SEI, better understanding of SEI is still highly demand. Finally, future directions especially in-operando techniques, multi-modality approaches for characterization of SEI and artificial intelligence assisted understanding of correlation between electrolyte components and SEI properties are proposed.

Wu, Haiping↗

Quantifying Lithium Ion Exchange in Solid Electrolyte Interphase (SEI) on Graphite Anode Surfaces

Solid Electrolyte Interphase (SEI) has been identified as the most important and least understood component in lithium-ion batteries. Despite extensive studies in the past two decades, a few mysteries remain: what is the chemical form of and degree of mobility of Li + in the interphase? What fraction of Li + is permanently immobilized in the SEI, while the rest are still able to participate in the cell reactions via the ion-exchange process with Li + in the electrolyte? This study attempted to answer, in part, these questions by using 6 Li and 7 Li-isotopes to label SEIs and electrolytes, and then quantifying the distribution of permanently immobilized and ion-exchangeable Li + with solid-state NMR and ToF-SIMS. The results showed that the majority of Li + were exchanged after one SEI formation cycle, and a complete exchange after 25 cycles. Ion exchange by diffusion based on concentration gradient in the absence of applied potential also occurred simultaneously. This knowledge will provide a foundation for not only understanding but also designing better SEIs for future battery chemistries.

25 ENERGY STORAGE↗

Direct in situ measurements of electrical properties of solid–electrolyte interphase on lithium metal anodes

The solid–electrolyte interphase (SEI) critically governs the performance of rechargeable batteries. An ideal SEI is expected to be electrically insulative to prevent persistently parasitic reactions between the electrode and the electrolyte and ionically conductive to facilitate Faradaic reactions of the electrode. However, the true nature of the electrical properties of the SEI remains hitherto unclear due to the lack of a direct characterization method. Here we use in situ bias transmission electron microscopy to directly measure the electrical properties of SEIs formed on copper and lithium substrates. We reveal that SEIs show a voltage-dependent differential conductance. A higher rate of differential conductance induces a thicker SEI with an intricate topographic feature, leading to an inferior Coulombic efficiency and cycling stability in Li||Cu and Li||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells. Further, our work provides insight into the targeted design of the SEI with desired characteristics towards better battery performance.

25 ENERGY STORAGE↗

Mechanical studies of the solid electrolyte interphase on anodes in lithium and lithium ion batteries

A stable solid electrolyte interphase (SEI) layer is key to high performing lithium ion batteries for metrics such as calendar and cycle life. The SEI must be mechanically robust to withstand large volumetric changes in anode materials such as lithium and silicon, so understanding the mechanical properties and behavior of the SEI is essential for the rational design of artificial SEI and anode form factors. The mechanical properties and mechanical failure of the SEI are challenging to study, because the SEI is thin at only ~ 10 – 200 nm thick and is air sensitive. Furthermore, the SEI changes as a function of electrode material, electrolyte and additives, temperature, potential, and formation protocols. A variety of in situ and ex situ techniques have been used to study the mechanics of the SEI on a variety of lithium ion battery anode candidates; however, there hasn't been a succinct review of the findings thus far. Because of the difficultly of isolating the true SEI and its mechanical properties, there have been a limited number of studies that can fully de-convolute the SEI from the anode it forms on. A review of past research will be helpful for culminating current knowledge and helping to inspire new innovations to better quantify and understand the mechanical behavior of the SEI. This review will summarize the different experimental and theoretical techniques used to study the mechanics of SEI on common lithium ion battery anodes and their strengths and weaknesses.

25 ENERGY STORAGE↗

Interfacial Issues and Modification of Solid Electrolyte Interphase for Li Metal Anode in Liquid and Solid Electrolytes

Abstract The high energy density required for the next generation of lithium batteries will likely be enabled by a shift toward lithium metal anode from the conventional intercalation‐based anode such as graphite. However, several critical challenges for Li metal originate from its highly reactive nature and the hostless reaction of deposition and stripping impede the practical use of Li metal as an anode. The role of the solid electrolyte interphase (SEI) is very important for the Li metal anode where the SEI must protect the dynamically changing surface of the Li metal. Since the SEI‐generating reaction mechanisms for the two different electrolyte systems, liquid and solid, are considerably different, the SEI layers formed between the Li metal and the electrolytes in the two electrolyte systems have substantially different properties, causing different interfacial issues. Inhibition of the interfacial problems requires different strategies to reinforce the SEI layer for each of the electrolyte systems. However, the differences in the two electrolyte systems have not been clearly compared in the prior literature. In this report, the interfacial issues for the two different electrolyte systems are compared and different strategies for SEI modification are provided to overcome the issues.

25 ENERGY STORAGE↗

Topological Considerations in Electrolyte Additives for Passivating Silicon Anodes with Hybrid Solid–Electrolyte Interphases

Unlike most anodes used in high energy density batteries, lithiated Si does not form long-lasting passivating solid-electrolyte interphases (SEI) during formation or on charge due to SEI delamination, reconstruction, or dissolution. As a result, electrolyte degradation is continuous and results in a permanent loss of the Li inventory, shortening the useful life of the battery. Here, in this study, we show that perfluoroether electrolyte additives featuring either sulfonyl fluorides or trifluorovinyl ethers, when introduced in prescribed amounts to locally superconcentrated electrolytes, exhibit preferential reactivity at Si during formation due to their higher reduction potential than salts and solvents, creating a hybrid SEI that is simultaneously enriched with LiF and organics tethered to the reactive functionality. While both reactive motifs are effective in creating a hybrid SEI, perfluoroether additives bearing sulfonyl fluorides show more substantial integration. More important, however, is the combined influence of additive topology on anchoring efficacy and tether flexibility between anchoring sites on SEI resiliency. Top-performing Si|LFP cells featuring ditopic additive-enriched SEI improve capacity retention by as much as 45% over 100 cycles when compared to additive-free cells.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Binary Cation Matrix Electrolyte and Its Effect on Solid Electrolyte Interphase Suppression and Evolution of Si Anode

An unstable solid electrolyte interphase (SEI) has been recognized as one of the biggest challenges to commercializing silicon (Si) anodes for high-energy-density batteries. This work thoroughly investigates a binary cation matrix of Mg 2+ +Li + electrolyte and its role in SEI development, suppression, and evolution of a Si anode. Findings demonstrate that introducing Mg ions dramatically reduces the SEI growth before lithiation occurs, primarily due to the suppression of solvent reduction, particularly ethylene carbonate (EC) reduction. The Mg 2+ alters the Li + cation solvation environment as EC preferably participates in the oxophyllic Mg 2+ solvation sheath, thereby altering the solvent reduction process, resulting in a distinct SEI formation mechanism. The initial SEI formation before lithiation is reduced by 70% in the electrolyte with the presence of Mg 2+ cations. While the SEI continues to develop in the postlithiation, the inclusion of Mg ions results in an approximately 80% reduction in the postlithiation SEI growth. Continuous electrochemical cycling reveals that Mg 2+ plays a crucial role in stabilizing the deep-lithiated Si phases, which effectively mitigates side reactions, resulting in controlled SEI growth and stable interphase while eliminating complex Li x Si y formation. Mg ions promote the development of a notably more rigid and homogeneous SEI, characterized by a reduced dissipation (ΔD) in the Mg 2+ +Li + ion matrix compared to the solely Li + system. In conclusion, this report reveals how the Mg 2+ +Li + ion matrix affects the SEI evolution, viscoelastic properties, and electrochemical behavior at the Si interface in real time, laying the groundwork for devising strategies to enhance the performance and longevity of Si-based next-generation battery systems.

25 ENERGY STORAGE↗

Enhanced Reversibility of Iron Metal Anode with a Solid Electrolyte Interphase in Concentrated Chloride Electrolytes

Iron is a promising candidate for a cost-effective anode for large-scale energy storage systems due to its natural abundance and well-established mass production. Recently, Fe-ion batteries (FeIBs) that use ferrous ions as the charge carrier have emerged as a potential storage solution. The electrolytes in FeIBs are necessarily acidic to render the ferrous ions more anodically stable, allowing a wide operation voltage window. However, the iron anode suffers severe hydrogen evolution reaction with a low Coulombic efficiency (CE) in an acidic environment, shortening the battery cycle life. Herein, a hybrid aqueous electrolyte that forms a solid-electrolyte interphase (SEI) layer on the Fe anode surface is introduced. The electrolyte mainly comprises FeCl 2 and ZnCl 2 as cosalts, where the Zn-Cl anionic complex species of the concentrated ZnCl 2 allows dimethyl carbonate (DMC) to be miscible with the aqueous ferrous electrolyte. SEI derived from DMC's decomposition passivates the iron surface, which leads to an average CE of 98.3% and much-improved cycling stability. As a result, this advancement shows the promise of efficient and durable FeIBs.

25 ENERGY STORAGE↗

A Facile Potential Hold Method for Fostering an Inorganic Solid‐Electrolyte Interphase for Anode‐Free Lithium‐Metal Batteries

Abstract Anode‐free lithium batteries are regarded as an ultimate form of high‐energy‐density lithium‐ion batteries. Unfortunately, irreversible lithium loss during cycling plays a major role in degrading the overall cell performance in the anode‐free configuration. To alleviate the deterioration, building a robust solid‐electrolyte interface on an anode current collector is an indispensable requirement. Here, we present a facile in‐situ electrochemical method of a potential hold during the first charge to guide more salt‐derived (less solvent‐derived) decomposition on the anode interface. We show the distinctive decomposition potential of lithium salts and ether/carbonate solvents, where the Li‐solvation structures with salt contact‐ion‐pairs preferentially decompose to form LiF‐rich and less organic components, leading to enhanced lithium Coulombic efficiency in Li||Cu cells as well as mitigating the capacity fade of Cu||LiFePO 4 and Cu||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells.

Shin, Woochul↗

Insights into Spontaneous Solid Electrolyte Interphase Formation at Magnesium Metal Anode Surface from Ab Initio Molecular Dynamics Simulations

Spontaneous chemical reactivity at multivalent (Mg, Ca, Zn, Al) electrode surfaces is critical to solid electrolyte interphase (SEI) formation, and hence, directly affects the longevity of batteries. Here, we report an investigation of the reactivity of 0.5 M Mg(TFSI)2 in 1,2-dimethoxyethane (DME) solvent at a Mg(0001) surface using ab initio molecular dynamics (AIMD) simulations and detailed Bader charge analysis. Based on the simulations, the initial degradation reactions of the electrolyte strongly depend on the structure of the Mg(TFSI)2 species near the anode surface. At the surface, the dissociation of Mg(TFSI)2 species occurs via cleavage of the N-S bond for the solvent separated ion pair (SSIP) and via cleavage of the C-S bond for the contact ion pair (CIP) configuration. In the case of the CIP, both TFSI anions undergo spontaneous bond dissociation reactions to form atomic O, C, S, F, and N species adsorbed on the surface of the Mg anode. These products indicate that the initial SEI layer formed on the surface of the pristine Mg anode consists of a complex mixture of multiple components such as oxides, carbides, sulfides, fluorides, and nitrides. We believe that the atomic level insights gained from these simulations will lay the groundwork for the rational design of tailored and functional interphases that are critical for the success of multivalent battery technology.

Agarwal, Garvit↗

Identification of LiH and nanocrystalline LiF in the solid–electrolyte interphase of lithium metal anodes

A comprehensive understanding of the solid–electrolyte interphase (SEI) composition is crucial to developing high-energy batteries based on lithium metal anodes. A particularly contentious issue concerns the presence of LiH in the SEI. In this work, we report on the use of synchrotron-based X-ray diffraction and pair distribution function analysis to identify and differentiate two elusive components, LiH and LiF, in the SEI of lithium metal anodes. LiH is identified as a component of the SEI in high abundance, and the possibility of its misidentification as LiF in the literature is discussed. LiF in the SEI is found to have different structural features from LiF in the bulk phase, including a larger lattice parameter and a smaller grain size (<3 nm). These characteristics favour Li + transport and explain why an ionic insulator, like LiF, has been found to be a favoured component for the SEI. Finally, pair distribution function analysis reveals key amorphous components in the SEI.

36 MATERIALS SCIENCE↗

On the dynamics of the fluoroethylene carbonate generated solid electrolyte interphase on silicon anodes during calendar life aging

Here, the widespread use of silicon (Si)-rich anodes in lithium-ion batteries (LIBs) is impeded by an unstable solid electrolyte interphase (SEI) incurring insufficient cell life. Fluoroethylene carbonate (FEC) additive in the electrolyte significantly improves cycle life. However, the gains on calendar life remain unclear; the SEI structure still undergoes detrimental alterations at rest. Thus, elucidating the SEI dynamics during calendar aging is critical to mitigating time-dependent capacity degradation. ATR-FTIR, XPS, and ToF-SIMS are used herein to investigate the SEI structure before and after calendar aging. Si cycled without FEC exhibits no notable SEI chemistry changes Pre- and Post-aging, leaving poor passivation as the main failure pathway. Conversely, the FEC-SEI starts as short oligomeric species from FEC/EC electroreduction prior to aging; after calendar aging, polymerized carbonates become consistently more prominent. Unexpectedly, the deposition of self-polymerized FEC species results from time exposure to the delithiated Si specifically as opposed to the lithiated surface. This unexpected finding is supported by another recent Si calendar-aging research, which albeit not investigating FEC, finds global failure of the SEI upon delithiation resulting in ∼247 fold more reactive surface compared to the lithiated.

Batteries↗

Excellent cycling stability of sodium anode enabled by a stable solid electrolyte interphase formed in ether-based electrolytes

Sodium (Na)-ion batteries have been considered as one of the most promising power sources beyond Li-ion batteries. Although Na metal anode exhibits a high theoretical capacity of 1165 mAh g-1, its application on Na batteries is largely hindered by dendrite growth and low Coulombic efficiency. Herein, we demonstrate that an electrolyte consists of 1 M sodium tetrafluoroborate in Tetraglyme can enable excellent cycling efficiency (99.9 %) of Na metal anode for more than 1000 cycles. This high reversibility of Na anode can be attributed to a stable solid electrolyte interphase formed on Na surface as revealed by cryogenic transmission electron microscopy and X-ray photoelectron spectroscopy. These electrolytes also enabled excellent cycling stability of Na||hard carbon cells and Na||Na2/3Co1/3Mn2/3O2 cells at high rate with very high coulombic efficiencies.

sodium metal, TEGDME, solid electrolyte interphase↗

Solid electrolyte interphase (SEI) application on anode of fluoride ion/shuttle batteries

The present disclosure is directed to fluoride (F) ion batteries and F shuttle batteries comprising an anode with a solid electrolyte interphase (SEI) layer, a cathode comprising a core shell structure, and a liquid fluoride battery electrolyte. According to some aspects, the components therein enable discharge and recharge at room-temperature.

Xu, Qingmin↗