Search NASA⌕ Search

SEARCH · Search NASA

Results for “anode-free cells”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Battery detectives: Uncovering cathode impact on anode-free Li cell performance by operando NMR

Here, Anode-free Li-ion batteries could attain new levels of energy density, but challenges remain in controlling deposition and managing degradation. In this issue of Chem, Kwon et al. probe Li metal growth using operando NMR to unravel how cathode materials impact performance and establish criteria for the high-energy/low-cost design tradeoff.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revisiting the Impact of Anion Selection on Sulfur Redox Reaction Kinetics for High Sulfur Loading Lithium–Sulfur Batteries

Lithium bis(trifluoromethane)sulfonimide (LiTFSI) is widely used in lithium–sulfur (Li–S) battery electrolytes due to its stability with lithium polysulfides (LiPSs) and moderate compatibility with lithium metal anodes. However, LiTFSI presents environmental concerns due to its association with per- and polyfluoroalkyl substances (PFAS), which are environmentally persistent and potentially toxic, raises sustainability concerns. This research also reveals that LiTFSI limits sulfur redox reactions (SRRs), making it less effective than other lithium salts. Additionally, some salts previously considered incompatible with Li-S systems due to their reactivity with LiPSs are demonstrated to perform effectively. For the first time, a protective, porous cathode electrolyte interphase (CEI) formed in situ through reactions between salt anions and LiPS is reported. The cells delivered a high specific capacity of 1230.8 mAh g −1 at 0.05 C with a sulfur loading of ≈6 mg cm −2 , limited lithium anode, maintaining a capacity retention of 76.2% after 100 cycles at 0.1 C. Under harsh conditions, such as high sulfur loading, lean electrolyte conditions (3 µL mg −1 ), and in anode-free cells, the cells continued to deliver outstanding capacity. This work provides valuable guidelines for understanding and selecting lithium salts to advance electrolyte design for Li–S batteries.

high loading batteries↗

Impact of Salt Chemistry and Interlayer Architecture on Solid Electrolyte Interphase Composition and Performance

Reversible lithium metal anodes require interphases that are chemically stable, mechanically robust, and compatible with scalable processing. Here, we use slot-die-coated, salt-rich PEO interlayers to design SEI nanolayers on Cu current collectors and isolate how salt anion chemistry controls interphase composition and lithium plating/stripping behavior in architectures relevant to Li plating and anode-free cells. Mesoscale modeling shows that dendrite initiation at SEI defects is governed by a tradeoff among interphase thickness, ionic conductivity, and stiffness through defect-driven current focusing, motivating controlled formation from thin precursor layers. Using UHV-transferred XPS and ToF-SIMS depth profiling after controlled Li deposition, we find that fluorinated sulfonylimide salts (LiTFSI, LiFSI) form mixed inorganic/organic interphases containing LiF and PEO-derived alkoxides, with LiFSI producing a more LiF-dominant Li-facing surface than LiTFSI under identical conditions. In contrast, LiNO 3 -containing interlayers yield a comparatively thick nitrate-derived interphase that reduces upon Li contact to an N-rich inorganic layer (Li–N/N 3− , LiN x O y ). In Cu| |Li cells, these designed interlayers reduce interfacial resistance and improve Coulombic efficiency (CE) and critical current density (CCD) relative to uncoated controls, with LiFSI- and LiNO 3 -based interlayers providing the highest CE/CCD. Overall, the results demonstrate a manufacturing-relevant approach to engineer SEI nanolayers by salt chemistry, providing pathways to improve reversible lithium metal anodes while reducing reliance on LiTFSI.

anion chemistry↗

A low-cost, fluorine-free electrolyte for improved sodium batteries

Sodium batteries are an attractive alternative to lithium-ion technologies due to sodium’s lower cost and natural abundance—over 1,000 times greater than lithium, comprising approximately 2.4% of the Earth’s crust. However, most current electrolytes rely on fluorine-containing components, which raise economic and environmental concerns. This study explores fluorine-free, borate-based electrolytes that offer improved cycling stability and significant cost and sustainability benefits. We demonstrate stable sodium metal stripping and plating on aluminum foil, enabling anode-free cell configurations with over 50% capacity retention after 700 cycles. Spectroscopic and electrochemical analyses reveal the effects of solvents and salt composition on solvation, ionic conductivity, and oxidative stability. In full-cell configurations, the fluorine-free electrolyte maintains more than 98% capacity retention after 400 cycles. Furthermore, these findings represent a critical step toward the development of cost-effective, environmentally friendly, and high-performance sodium battery systems suitable for future electrification.

anode-free sodium batteries↗

Hydride-Based Interlayer for Solid-State Anode-Free Battery

Solid-state batteries (SSBs) are considered a promising approach to realizing an anode-free concept with high energy densities. However, the initial Coulombic efficiency (ICE) has remained insufficient for anode-free batteries using sulfide-based solid electrolytes (SEs). Herein, we incorporated a hydride-based interlayer, 3LiBH 4 -LiI (LBHI), between a typical sulfide SE, Li 6 PS 5 Cl, and the Cu current collector. Further, by investigating the Li plating and stripping behaviors and the (electro)chemical stability between SEs and plated Li, we demonstrated that LBHI can effectively improve interfacial stability, leading to an ICE exceeding 94% in anode-free half cells. This interlayer also improves Coulombic efficiencies and specific capacities in anode-free full cells. Furthermore, the utilization of LBHI enables one to study Li plating behaviors without interference from interfacial (electro)chemical instabilities. The analysis of stack pressure evolution during electrochemical cycling reveals that soft shorting in SSBs arises from both dendrite formation and deformation, offering insights into further optimizing solid-state anode-free batteries.

25 ENERGY STORAGE↗

Solid-state polymer-particle hybrid electrolytes: Structure and electrochemical properties

Solid-state electrolytes (SSEs) are challenged by complex interfacial chemistry and poor ion transport through the interfaces they form with battery electrodes. Here, we investigate a class of SSE composed of micrometer-sized lithium oxide (Li 2 O) particles dispersed in a polymerizable 1,3-dioxolane (DOL) liquid. Ring-opening polymerization (ROP) of the DOL by Lewis acid salts inside a battery cell produces polymer-inorganic hybrid electrolytes with gradient properties on both the particle and battery cell length scales. These electrolytes sustain stable charge-discharge behavior in Li||NCM811 and anode-free Cu||NCM811 electrochemical cells. On the particle length scale, Li 2 O retards ROP, facilitating efficient ion transport in a fluid-like region near the particle surface. On battery cell length scales, gravity-assisted settling creates physical and electrochemical gradients in the hybrid electrolytes. By means of electrochemical and spectroscopic analyses, we find that Li 2 O particles participate in a reversible redox reaction that increases the effective CE in anode-free cells to values approaching 100%, enhancing battery cycle life.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Time-Evolved Hetero-Alkali Interphases Enable Long-Life Sulfide-Based Anode-Free Solid-State Batteries

Sulfide-based anode-free solid-state batteries (AFSSBs) offer compelling advantages in terms of energy density and safety, yet their practical implementation is severely hindered by undesirable interfacial reactions between sulfide solid electrolytes (SEs) and freshly plated lithium (Li), as well as non-uniform Li plating/stripping behavior. Herein, an effective interfacial stabilization strategy by incorporating sodium bis(fluorosulfonyl)imide (NaFSI) additive into the Li5.4PS4.4Cl1.6 (LPSC) is investigated. Unlike conventional Li-based additives that form static passivation layers, NaFSI introduces a transient hetero-alkali chemistry that kinetically governs interphase evolution during fresh Li plating. NaFSI induces a timesequenced interphase evolution: an initial NaF/LiF-rich layer that suppresses early sulfide reduction, followed by a LiF/Li3N-rich layer that optimizes Li⁺ transport during repeated anode-free cycling. This evolved robust and fast ion conducting layer mitigates interfacial impedance growth, enhances Li + transport kinetics, and suppresses localized Li growth and filamentary shorting. As a result, the anode-free full cell with NaFSI modified LPSC as the interlayer exhibits an excellent cycling stability over 500 cycles at 0.2 C with a capacity retention of 77.6%, whereas the cell with bare LPSC suffers from rapid capacity decay after 100 cycles, retaining only 32.1% of its initial capacity. This work establishes dynamic heteroalkali additive chemistry as a general strategy to kinetically program solid-solid interphases, guiding the interface design in anode-free solid-state batteries.

25 ENERGY STORAGE↗

Non-fluorinated electrolyte for high-voltage anode-free sodium metal battery

Abundant sodium (Na) batteries are a sustainable alternative to resource-constrained lithium-ion batteries, offering huge cost advantages. However, developing high-voltage anode-free sodium metal batteries (SMBs) to narrow the energy density gap with lithium-ion batteries is hindered by a critical challenge: existing electrolytes cannot simultaneously achieve ultra-high Na coulombic efficiency and anodic stability. Here, in this study, we present a rationally designed non-fluorinated electrolyte (1.0 M NaPF 6 in 1,2-diethoxyethane/1,2-di-tert-butoxyethane) to address this key limitation, achieving Na coulombic efficiency of >99.95% and anodic stability of >4.8 V. For coin cells (2.0 mAh cm −2 , N/P = 1.7), our electrolyte design enables 4.0 V Na | |Na 3 V 2 (PO 4 ) 3 (NVP) at 5 C and 4.3 V Na | |NaNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) at 0.3 C for 5,000 and 500 cycles with a capacity retention >80%. Remarkably, the 50 mAh anode-free pouch cells 4.0 V Al | |NVP and 4.3 V Al | |NMC622 also achieve 500 and 300 cycles (retention >75%) with a specific energy of >360 Wh kg (electrode) −1 . This work focuses on electrolyte optimization and conceptual advances, whereas critical aspects such as safety, large-scale manufacturability and practical feasibility of SMBs require further investigation. The electrolyte design using non-fluorinated solvents enhances the anodic stability without sacrificing Na efficiency, laying groundwork for advancing low-cost, high-energy SMBs and supporting the transition to sustainable battery technologies.

25 ENERGY STORAGE↗

Jumpstart Opportunities to Unleash Leadership in Energy Storage (JOULES)

Current-generation Li-ion batteries with cobalt- and nickel-containing cathodes and graphite anodes are approaching performance and cost limits. In this program, 24M Technologies, Inc. (24M) is teaming with the Massachusetts Institute of Technology (MIT) and University of Michigan (UM) to develop low cost and fast charging sodium metal batteries with good low-temperature performance and high energy density, building upon previous work performed under ARPA-E programs. Key achievements include optimization of solid electrolyte and anode current collector, optimized cathode active materials, development of high-performance electrolyte formulations, and integration of these components into full cells. The cell design incorporates (1) an ultra-thick cathode (>9 mAh/cm 2 ) comprising advanced cobalt-free, sodium cathode active material, (2) advanced fast-charging electrolyte (up to 12 mS/cm) developed using machine learning and automated high-throughput screening technology by UM, and (3) ceramic modified separator that enable smooth Na transport and deposition, developed at MIT, enabling a high-energy density anode-free configuration and maximizing the energy density of sodium batteries. The team has successfully combined these approaches to sodium chemistry and paved the way to meeting the fast-charging, high-energy density, and low-cost requirements of next-generation drone, electric vertical take-off and -landing, and electric vehicle batteries. Performance for anode-free sodium cells developed under this program is more powerful than the commercial Li-ion batteries. The final deliverable cell design has achieved over 300 Wh/kg and volumetric energy density above 800 Wh/L (Table 1). Additionally, the team has achieved over (1) a lifetime of 340 cycles, (2) 80% capacity retention at -20 °C (compared 25 °C), and (3) the ability to fast charge to 80% SOC in 20 minutes.

25 ENERGY STORAGE↗

Asymmetric ether solvents for high-rate lithium metal batteries

Recent electrolyte solvent design based on weakening lithium-ion solvation have shown promise in enhancing cycling performance of Li-metal batteries. However, they often face slow redox kinetics and poor cycling reversibility at high rate. Here we report using asymmetric solvent molecules substantially accelerates Li redox kinetics. Asymmetric ethers (1-ethoxy-2-methoxyethane, 1-methoxy-2-propoxyethane) showed higher exchange current densities and enhanced high-rate Li 0 plating/stripping reversibility compared to symmetric ethers. Adjusting fluorination levels further improved oxidative stability and Li 0 reversibility. The asymmetric 1-(2,2,2-trifluoro)-ethoxy-2-methoxyethane, with 2 M lithium bis(fluorosulfonyl)imide, exhibited high exchange current density, oxidative stability, compact solid–electrolyte interphase (~10 nm). This electrolyte exhibited superior performance among state-of-the-art electrolytes, enabling over 220 cycles in high-rate Li (50 μm)||LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811, 4.9 mAh cm −2 ) cells and for the first time over 600 cycles in anode-free Cu | |Ni95 pouch cells (200 mAh) under electric vertical take-off and landing cycling protocols. Our findings on asymmetric molecular design strategy points to a new pathway towards achieving fast redox kinetics for high-power Li-metal batteries.

batteries↗

In Situ Li Seed Formation Enables Uniform Plating in Anode-Free Solid-State Batteries

Anode-free solid-state batteries (AFSSBs) are a promising route toward achieving high energy density. In these cells, the anode contains no pre-stored lithium (Li). Instead, all Li inventory originates from the cathode and is freshly deposited onto a bare current collector during charging. However, achieving uniform and defect-free Li plating on this bare current collector remains a major challenging, often resulting in low Li plating/stripping efficiency and rapid capacity decay. Here, for the first time, operando neutron imaging is employed to visualize Li plating/stripping behavior in an anode-free full cell with LiNi 0.82 Mn 0.07 Co 0.11 O 2 (NMC) as the cathode. Operando measurements reveal that complete stripping of Li leaves isolated Li residues on the current collector, which degrades interfacial contact between the current collector and solid-state electrolyte. To mitigate this interfacial issue and promote more uniform Li deposition, we implement a discharge cutoff voltage strategy that intentionally retains a thin residual Li layer after stripping. This thin Li layer, serving as an in situ–formed seed layer, not only enables more homogeneous subsequent Li plating but also improves interfacial contact. As a result, the anode-free cell with a controlled discharge voltage of 3.5 V exhibits excellent long-term cycling stability, maintaining a discharge capacity of 116 mAh g -1 with a retention rate of 83.4% and an average Coulombic efficiency of approximately 99.9% after 430 cycles at 0.25 C. In contrast, the cell with a conventional discharge cutoff voltage of 2.8 V exhibits rapid capacity decay, retaining only 59.7 mAh g -1 after 50 cycles with a capacity retention of 40.7%. This work offers a practical strategy to unlock the long-term viability of anode-free solid-state batteries.

25 ENERGY STORAGE↗

Controlled lithium stripping enables a stable interface for long-cycling anode-free solid-state batteries

Anode-free solid-state batteries (AFSSBs) are a promising route toward achieving high energy density. In these cells, the anode contains no pre-stored lithium (Li). Instead, the entire Li inventory originates from the cathode and is freshly deposited onto a bare current collector during charging. However, achieving uniform and defect-free Li plating on this bare current collector remains a major challenge, often resulting in low Li plating/stripping efficiency and rapid capacity decay. Here, for the first time, operando neutron imaging is employed to visualize Li plating/stripping behavior in an anode-free full cell with LiNi0.82Mn0.07Co0.11O2 (NMC) as the cathode. Operando measurements reveal that complete stripping of Li leaves isolated Li residues on the current collector, which degrades the interfacial contact between the current collector and the solid-state electrolyte. To mitigate this interfacial issue and promote more uniform Li deposition, we implement a discharge-cutoff-voltage strategy that intentionally retains a thin residual Li layer after stripping. This preserved Li-containing interfacial reservoir not only improves interfacial contact but also serves as an in situ formed seed layer that enables more homogeneous subsequent Li plating. As a result, the optimized anode-free cell with limited stripping depth exhibits excellent long-term cycling stability, maintaining a discharge capacity of 112.1 mAh g−1 with a capacity retention of 80.6% and an average coulombic efficiency of approximately 99.9% after 500 cycles at 0.25 C. In contrast, the cell with a conventional discharge cutoff voltage of 2.8 V exhibits rapid capacity decay, retaining only 59.7 mAh g−1 after 50 cycles with a capacity retention of 40.7%. This work demonstrates that limiting deep stripping to preserve a thin Li-containing interfacial layer can effectively improve the cycling stability of sulfide-based AFSSBs.

Wang, Jiwei [Northeastern University, Boston]↗

Hyperconjugation-controlled molecular conformation weakens lithium-ion solvation and stabilizes lithium metal anodes

Tuning the solvation structure of lithium ions via electrolyte engineering has proven effective for lithium metal (Li) anodes. Further advancement that bypasses the trial-and-error practice relies on the establishment of molecular design principles. Expanding the scope of our previous work on solvent fluorination, we report here an alternative design principle for non-fluorinated solvents, which potentially have reduced cost, environmental impact, and toxicity. By studying non-fluorinated ethers systematically, we found that the short-chain acetals favor the [gauche, gauche] molecular conformation due to hyperconjugation, which leads to weakened monodentate coordination with Li + . The dimethoxymethane electrolyte showed fast activation to >99% coulombic efficiency (CE) and high ionic conductivity of 8.03 mS cm -1 . The electrolyte performance was demonstrated in anode-free Cu$∥$LFP pouch cells at current densities up to 4 mA cm -2 (70 to 100 cycles) and thin-Li$∥$high-loading-LFP coin cells (200–300 cycles). Overall, we demonstrated and rationalized the improvement in Li metal cyclability by the acetal structure compared to ethylene glycol ethers. We expect further improvement in performance by tuning the acetal structure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Monofluorinated acetal electrolyte for high-performance lithium metal batteries

High degree of fluorination for ether electrolytes has resulted in improved cycling stability of lithium metal batteries due to stable solid electrolyte interphase (SEI) formation and good oxidative stability. However, the sluggish ion transport and environmental concerns of high fluorination degree drive the need to develop less fluorinated structures. Here, we depart from the traditional ether backbone and introduce bis(2-fluoroethoxy)methane (F2DEM), featuring monofluorination of the acetal backbone. High coulombic efficiency and stable long-term cycling in Li||Cu half cells can be achieved with F2DEM even under fast Li metal plating conditions. The performance of F2DEM is further compared with diethoxymethane (DEM) and 2-[2-(2,2-difluoroethoxy)ethoxy]-1,1,1-trifluoroethane (F5DEE). A significantly lower overpotential is observed with F2DEM, which improves energy efficiency and enables its application in high-rate conditions. Comparative studies of F2DEM with DEM and F5DEE in anode-free lithium iron phosphate (LiFePO4) LFP pouch cells and high-loading LFP coin cells further show improved capacity retention of F2DEM electrolyte, demonstrating its practical applicability. More importantly, we also extensively investigate the underlying mechanism for the superior performance of F2DEM through various techniques, including X-ray photoelectron spectroscopy, scanning electron microscopy, cryogenic electron microscopy, focused ion beam, electrochemical impedance spectroscopy, and titration gas chromatography. Overall, F2DEM facilitates improved Li deposition morphology with reduced amount of dead Li. This enables F2DEM to show superior performance, especially under higher charging and slower discharging rate conditions.

25 ENERGY STORAGE↗

Visualizing diverse lithium growth and stripping behaviors in anode-free solid-state batteries with operando X-ray tomography

Anode-free solid-state batteries (SSBs), which eliminate the need for lithium metal use during cell assembly, have the potential to enable high energy densities and simplified manufacturing. However, the factors that control lithium growth/stripping at the anode current collector are not well understood. Here, we use operando X-ray microcomputed tomography to comprehensively image and quantify lithium deposition and stripping under various conditions in three different Li|Li 6 PS 5 Cl|current collector cells, revealing diverse behavior that depends on interface morphology, cell resistance, and solid-state electrolyte (SSE) microstructure. A cell with high resistance exhibits extensive lithium filament growth across the entire current collector interface, with filaments that grow around pre-existing pores in the SSE rather than lithium filling these pores. Lithium filament formation is partially reversible, with the cracks shrinking as lithium metal is stripped. Uniform lithium deposition is achievable at low current densities in low-resistance cells, whereas higher current densities in these cells cause an increase in interfacial roughness, which is correlated with subsequent filamentary growth at the edges of the cell. These results provide insight into filamentary vs. planar lithium growth and highlight that the evolution of lithium is sensitively dependent on SSE microstructure and electrochemical processes.

25 ENERGY STORAGE↗

Understanding the Role of Borohydride Doping in Electrochemical Stability of Argyrodite Li 6 PS 5 Cl Solid‐State Electrolyte

This work elucidates the mechanism by which lithium borohydride (LiBH 4 ) doping into argyrodite-type Li 6 PS 5 Cl (LBH-LPSCl) solid-state electrolyte (SSE) enhances electrochemical stability. State-of-the-art electrochemical performance is achieved with 5 wt% borohydride. Symmetric cells achieve critical current density (CCD) of 7.3 mA cm −2 , versus 2.6 mA cm −2 for baseline-LPSCl. All solid-state batteries (ASSBs) employing lithium metal and NMC811 cathode are stable over 400 cycles at 0.5C, with capacity retention of 83%. An anode-free ASSB (AF-ASSB) is stable over 600 cycles, with capacity loss of 0.04% per cycle. 5LBH-LPSCl allows for enhanced low temperature operation, down to −14 °C. Yet the difference in electrolytes’ bulk microstructures and hardnesses are minimal, while ionic conductivity is incrementally improved (≈50%). Theoretical modeling indicates limited effect of substitution on thermodynamic stability of PS 4 3- units, which decompose when contacting Li. Instead, enhanced electrochemical stability is site-specific kinetic effect: In situ electrodeposition experiments using X-ray photoelectron spectroscopy (XPS) and time-of-flight secondary ion mass spectrometry (TOF-SIMS) reveal tri-layer SEI based predominately on Li 3 P/LiBH 4 /Li 2 S that blocks electrons while facilitating ion transport. This SEI manifests reduced interface resistance and accelerated nucleation and growth of metallic Li. With baseline-LPSCl the SEI based on Li 3 P/Li 2 S is substantially thicker, generating localized stresses that promote interfacial cracking while cycling.

argyrodite↗

A Reductively Stable Electrolyte Realizes Deep Cycling Behavior in Anode‐free Sodium Batteries

For anode‐free sodium batteries to achieve practical consideration, highly reversible chemistries require exceptional ≥99.95% coulombic efficiencies that maintain over prolonged cycling periods. To do so, consumption of this severely limited sodium inventory must be restricted while metal nucleation processes that comprise the in situ formed metal anode are improved. Herein, we describe a fluorine‐free carborane electrolyte that satisfies these criteria by emphasizing reductive stability and weakly coordinating anion behavior as design principles. We find this approach promotes the development of a thin, robust SEI chemistry rich in both organic speciation and boron. The electrolyte described herein exhibits ideal metal nucleation behavior on one‐micron thin carbonaceous current collector surfaces and achieves a metal deposition/stripping efficiency near parity for 400 cycles. This novel anode chemistry is introduced to anode‐free full cell configurations where 87% of the initial discharge capacity is retained after 1000 cycles at 2.0 C. In conclusion, post‐test characterization of deep‐cycled anode‐free cells reveals suppressed capacity fade in these systems is attributed to the chemical stability of the carborane anion.

anode-free↗