At least 19 records

Unraveling the convoluted and dynamic interphasial mechanisms on Li metal anode

Accurate understanding of the chemistry of solid-electrolyte interphase (SEI) is key to developing new electrolytes for high-energy batteries using lithium metal (Li-0) anodes(1). SEI is generally believed to be formed by the reactions between Li-0 and electrolyte(2,3). However, our new study shows this is not the whole story. Through synchrotron-based X-ray diffraction and pair distribution function analysis, we reveal a much more convoluted formation mechanism of SEI, which receives considerable contributions from electrolyte, cathode, moisture and native surface species on Li-0, with highly dynamic nature during cycling. Using isotope labelling, we traced the origin of LiH to electrolyte solvent, moisture and a new source: the native surface species (LiOH) on pristine Li-0. When lithium accessibility is very limited as in the case of anode-free cells, LiOH develops into plate-shaped large crystals during cycling. Alternatively, when the lithium source is abundant, as in the case of Li||NMC811 cells, LiOH reacts with Li-0 to form LiH and Li2O. While the desired anion-derived LiF-rich SEI is typically found in the concentrated electrolytes or their derivatives, we found it can also be formed in low-concentration electrolyte via the crosstalk effect, emphasizing the importance of formation cycle protocol and opening up opportunities for low-cost electrolyte development.

Polzin, Bryant J.↗

Mechanical and tribological properties of anodic Al coatings as a function of anodizing conditions

Enhanced wear and corrosion resistance properties are vital for numerous functional and decorative applications. Anodizing is a process frequently used to generate stable oxide coatings on metal surfaces, including aluminium (Al). In this work, we present an evaluation of process variables for optimized anodized coating properties using existing methods and as a baseline for novel coating development. A representative relatively pure Al alloy was chosen as a model system with a goal of finding conditions to achieve high wear coatings with retained ductility. AA5052 alloy coupons were anodized in two different electrolytes (sulfuric and phosphoric acid) to study the effects of anodizing conditions on the mechanical and tribological properties of the anodic coatings. Porosity was evaluated with microscopy, coating hardness was determined via nanoindentation, and tribological properties were characterized using a pin-on-disk tribometer. These measurements were correlated and a loading evaluation was performed to assess the optimum nanoindentation parameters for the use of representative coupons without the need for special processing prior to anodizing. The porosity and coating thickness were found to depend on the anodizing time and the type of electrolyte. Thicker and harder anodic coatings were generated in sulfuric acid compared to phosphoric acid. Porosity studies of the anodic coatings generated in phosphoric acid revealed that coating porosity decreased as the anodizing time increased. Both electrolytes generated anodic coatings with improved tribological properties (friction coefficient and dimensional wear rate), and an optimum processing time was identified for best wear properties.

36 MATERIALS SCIENCE↗

Understanding the Origin of the Nonpassivating Behavior of Si-Based Anodes during the Initial Cycles

In this contribution, we combined electrochemical cycling and X-ray photoelectron spectroscopy (XPS) to understand the nonpassivating behavior of the solid electrolyte interphase (SEI) on Si anodes during the first cycles. Based on galvanostatic measurements, we show that the irreversible capacity loss is reduced after the first cycle, and it stays almost constant from the second cycle onwards. XPS was used to determine the root causes of the Coulombic inefficiency, showing that the rate of decomposition of the organic solvents strongly decreased after the first cycle, whereas the rate of salt decomposition is almost unchanged between cycles. We determine that the inhibition of the decomposition reaction of the organic solvent is responsible for the lower Coulombic loss during the second electrochemical cycle in comparison to the first, whereas the nonpassivating behavior toward the salt decomposition is one of the main causes of capacity loss upon cycling. Here, we further revisit the role of cracking in contributing to capacity loss. Whereas high volumetric expansion remains an issue plaguing the performance of Si anodes, our chronoamperometry studies reveal that the SEI formed on Si anodes does not passivate even when the electrode is fully expanded, and no additional surface is exposed. Overall, our work establishes the need to address the chemical and electrochemical instability of the SEI on the Si anode in addition to the more notorious issue of cracking.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Anode power deposition in an applied-field segmented anode MPD thruster

Anode heat flux measurements of a water cooled segmented anode applied-field MPD thruster were made to investigate anode heat transfer phenomena. Pure argon and argon-hydrogen mixtures were used as propellants for a variety of thruster currents, propellant mass flow rates, and axial applied magnetic field strengths. The thruster was operated in two modes; with all four segments active, and with two of the segments floating. In addition, thrust and specific impulse were determined for each operating condition. The results show that the heat flux to the anode increases monotonically with axial magnetic field strength and thruster current. Between 50 and 75 percent of the anode heat flux is transported by the current carrying electrons. Convective and radiative heat transfer account for the remaining portion of the power deposited in the anode. The addition of hydrogen to the argon propellant results in the reduction of the fraction of anode power deposited by the anode fall to a level equivalent to that deposited by convection and radiation.

Myers, R. M.↗

Anode power deposition in a MPD thruster with a magnetically annulled Hall parameter anode

Results from previous studies indicate that the anode fall increases monotonically with the electron Hall parameter. In an attempt to reduce the anode fall by decreasing the local electron Hall parameter, a proof-of-concept test was performed in which an array of 36 permanent magnets were imbedded within the anode of a high power quasi-steady MPD thruster to decrease the local azimuthal component of the induced magnetic field. The modified thruster was operated at power levels between 150 kW and 4 MW with Ar and He propellants. Terminal voltage, triple probe, floating probe, and magnetic probe measurements were made to characterize the performance of the thruster with new anode. Incorporation of the modified anode resulted in a reduction of the anode fall by up to 15 V with Ar and 20 V with He, which corresponded to decreased anode power fractions of 40 and 45 percent with Ar and He, respectively.

Gallimore, Alec D.↗

Electroanalytical Exploration of Li Loss at the Solid Electrolyte-Anode Interface in Anode-Free Batteries with Polymer Electrolytes

Li loss during cycling at the solid electrolyte|anode interface strongly determines the cycle life of anode-free solid-state batteries (SSBs). Here, this loss is probed electroanalytically for polymer electrolyte (PE)-based SSBs in anode-free coin cells with practical pressures. A wide range of parameters expected to impact the measured average coulombic efficiency (CE) were explored to estimate the expected range of performance. These factors include PE type, cycling profiles, current collector type, and the presence of a thin Li seed layer. Further, low CE values in the ~50%–85% range are observed for all electrolytes and test conditions. Other than the electrolyte type, a strong dependence of the CE on the electrochemical cycling profile and the type of metallic current collector is observed. Compared to the anode-free setup, the presence of a thin (5 μ m) Li seed layer did not improve the average CE for two out of three PEs, suggesting its presence to be a weak contributor in minimizing the Li loss. This work provides baseline data on the Li losses in low-pressure anode-free configuration cells with PEs.

25 ENERGY STORAGE↗

Surprising Relationship between Silicon Anode Calendar Aging and Electrolyte Components in a Localized High-Concentration Electrolyte System

Although localized high-concentration electrolytes (LHCEs) have been shown to improve the calendar lifetime of silicon anodes, the roles of the electrolyte constituents in calendar aging are not well understood. Here, in this work, we utilize a voltage hold protocol and an LHCE with varying molar ratios of lithium bis(fluorosulfonyl)imide (LiFSI), tetramethylene sulfone (TMS), and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) to probe the component roles during aging. Interestingly, the estimated calendar lifetime and irreversible lithium losses from the V-hold experiments are independent of the electrolyte formulations. Contrarily, the solid electrolyte interphase (SEI) composition depends on the electrolyte formulation. X-ray photoelectron spectroscopy shows that TMS-coordinated species decompose to form insoluble alkanes and lithium hydroxide (LiOH), while lithium fluoride (LiF) originates from the anion-coordination complex. The SEI composition does not appear to play a significant role in the silicon anode passivity, as measured by parasitic current, suggesting that the SEI-electrolyte interactions dictate the calendar aging mechanisms.

Si anode↗

Thin-film sulfuric acid anodizing as a replacement for chromic acid anodizing

Chromic acid has long been used to produce a thin, corrosion resistant (Type I) coating on aluminum. Following anodizing, the hardware was sealed using a sodium dichromate solution. Sealing closes up pores inherent in the anodized coating, thus improving corrosion resistance. The thinness of the brittle coating is desirable from a fatigue standpoint, and chromium was absorbed by the coating during the sealing process, further improving corrosion resistance. Unfortunately, both chromic acid and sodium dichromate contain carcinogenic hexavalent chromium. Sulfuric acid is being considered as a replacement for chromic acid. Sulfuric acid of 10-20 percent concentration has traditionally been used to produce relatively thick (Types II and III) or abrasion resistant (Type III) coatings. A more dilute, that is five weight percent, sulfuric acid anodizing process, which produces a thinner coating than Type II or III, with nickel acetate as the sealant has been developed. The process was evaluated in regard to corrosion resistance, throwing power, fatigue life, and processing variable sensitivity, and shows promise as a replacement for the chromic acid process.

Kallenborn, K. J.↗

Solid‐State Prealkylation of Electrode Architectures (SPEAR): Direct Control of Prelithiation Levels in Silicon Anodes and Electrochemical Cycling

The Solid-state Prealkylation of Electrode ARchitectures (SPEAR) is different than traditional electrochemical prealkylation processes. Through SPEAR, alkylation is driven by solid-state diffusion without the simultaneous SEI formation concomitant with polarization. Here, we investigate the prelithiation of 80 wt. % Si-based anodes to varying amounts (up to Li 1.38 Si) to understand the trade-off between improved Li capacity and expansion-induced stress. Through dilatometry, we found that solid-state lithiation led to filling of the electrode pores through silicon expansion. This swelling changed the SEI formation process and accessibility of the silicon compared to an electrochemically lithiated electrode. Indeed, optimal prelithiation to Li 0.82 Si increases the initial C/3 cycling capacity post-SEI formation up to 43%, consistent with deeper Si activation through the electrode bulk. Prelithiation and cycling cells prelithiated beyond Li 0.82 Si results in a state of charge (SOC) close to 100% which facilitates parasitic degradation mechanisms and volume expansion of the Si electrode. The results demonstrate a pathway to modify silicon activation/SEI formation to enable high-energy electrodes.

Musgrove, Amanda L. [Oak Ridge National Laboratory↗

SEI formation mechanisms and Li + dissolution in lithium metal anodes: Impact of the electrolyte composition and the electrolyte-to-anode ratio

The lithium metal battery is one of today's most promising high-energy-density storage devices. Its full-scale implementation depends on solving operational and safety issues intrinsic to the Li metal high reactivity leading to uncontrolled electrolyte decomposition and uneven Li deposition. In this work, we study the spontaneous formation of the solid electrolyte interphase (SEI) upon contact of Li metal with the electrolyte and describe the heterogeneous SEI morphological features. Multiple electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethoxyethane (DME), dimethyl carbonate (DMC), 1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) and bis(2,2,2-trifluoroethyl) ether (BTFE) are used. Findings include the description of the SEI evolution from dispersed LiO, LiS, LiN, and LiF clusters to a continuous and compact inorganic phase in which the LiO and LiF content depend on the presence of fluorine diluents. Further, the role of the DME ether solvent helping the growth of a “wet-SEI” is compared to that of the highly unstable carbonate DMC, which decomposes into complex radical oligomers that might contribute to further electrolyte decomposition. The impact of the electrolyte-to-anode ratio on LiFSI decomposition is highlighted. Finally, we suggest the existence of a critical LiFSI concentration and electrolyte-to-anode ratio that could potentially balance the rate of electrolyte depletion and lithium consumption.

25 ENERGY STORAGE↗

Solvent-Free Melt-Processed Cathode Mitigates Li Anode Instability in Polymer-Based Solid-State Batteries

Solvent-free manufacturing of battery components is a promising alternative to traditional slurry processing for reducing the cost and environmental impact. In this work, we used twin-screw melt extrusion to fabricate a polymer-based high voltage composite cathode. The melt-processed cathode is dense (near zero porosity) and thick (65 μm) and has high active material loading (80 wt %). The active particles are distributed uniformly throughout the melt-processed cathode, unlike the traditional slurry-cast cathode, which exhibits inhomogeneous particle distribution. In the melt-processed cathode, polymer and carbon form separate phases, whereas in the slurry-cast cathode they blend into a single phase. Due to these structural differences, the melt-processed cathode shows smooth charge–discharge profiles, while the slurry-cast cathode shows noisy charging and soft-shorting behavior. In conclusion, this work highlights that twin-screw extrusion as a scalable, solvent-free manufacturing method is advantageous in producing uniform cathodes, which mitigates anode instability.

25 ENERGY STORAGE↗

Metallic Cu Surface Enables Reversible Na Metal Anodes and Stabilizes Anode-Free Sodium Metal Batteries

Anode free Na metal batteries are promising for future energy storage because they not only provide the highest energy densities but also eliminate the need of handling hazardous Na metals during battery manufacturing. However, they suffer from much faster degradation due to strong sensitivities even to trace levels of side reactions. In view of the crucial roles of surface chemistry on modulating electrochemical plating, this work systematically investigated a series of Cu surfaces for Na plating and stripping in the 1.0 M NaPF 6 diglyme electrolyte. Our results suggest that Na plating and stripping on pure Cu surface without Cu oxide species exhibits much better reversibility and smaller overpotentials across a wide range of current densities, especially for the first plating/stripping cycle. The high performance includes consistently higher than 99.8% Faradaic efficiencies, much more stable interfacial resistance, and negligible formation of mossy Na after 500 cycles. This improved performance can be explained based on the stronger Na-Cu affinity compared with the Na-CuO affinity. Anode-free Na metal batteries equipped with high-capacity sodium vanadium phosphate cathodes and pure Cu current collector exhibited at least 70% capacity retention for 100 cycles.

Electrochemistry↗

Mechanisms of anode power deposition in a low pressure free burning arc

Anode power deposition is a dominant power loss mechanism for arc jets and MPD thrusters. In this study, a free burning arc experiment was operated at pressures and current densities similar to those in arc jets and MPD thrusters in an attempt to identify the physics controlling this loss mechanism. Use of a free burning arc allowed for the isolation of independent variables controlling anode power deposition and provided a convenient and flexible way to cover a broad range of currents, anode surface pressures, and applied magnetic field strengths and orientations using an argon gas. Test results showed that anode power deposition decreased with increasing anode surface pressure up to 6.7 Pa (0.05 torr) and then became insensitive to pressure. Anode power increased with increasing arc current while the electron number density near the anode surface increased linearity. Anode power also increased with increasing applied magnetic field strength due to an increasing anode fall voltage. Applied magnetic field orientation had an effect only at high currents and low anode surface pressures, where anode power decreased when applied field lines intercepted the anode surface. The results demonstrated that anode power deposition was dominated by the current carrying electrons and that the anode fall voltage was the largest contributor. Furthermore, the results showed that anode power deposition can be reduced by operating at increased anode pressures, reduced arc currents, and applied magnetic field strengths and with magnetic field lines intercepting the anode.