At least 19 records

Sequential Infiltration Synthesis of Bilayer Porous Alumina Nanostructures for Broad-Angle, Broadband Antireflective Coatings

Antireflective coatings (ARCs) are thin films engineered to reduce light reflections. Delivering broadband, wide-angle performance is essential for photovoltaics, imaging, and sensing, yet truly omnidirectional antireflection remains difficult due to angle-dependent optical paths and a narrow palette of suitable refractive indices. Here, in this study, we systematically investigate an emerging class of multilayer inorganic ARCs based on conformally coated nanoporous alumina templated by intrinsically microporous polymers (PIMs) and block copolymers (BCPs). We establish a design framework that maps thickness reflectance relationships to identify thickness pairs minimizing reflection across wavelength and incidence angle. We show that deliberately separating the local reflectance minima of the top and bottom layers in bilayer nanostructures broadens the antireflective bandwidth and angular range. We show that 235-nm single-side bilayer porous alumina nanostructures achieves under 2 % reflectance from 380–750 nm for incidence angles up to 45° with less than 0.6% reflectance for incidence angles under 20°. The approach is readily extensible to additional layers or materials with refractive indices tuned via templated nanoporosity and composition, enabling practical, etch-free ARC fabrication without HF or fluorinated precursors and advancing straightforward design of broadband, wide-angle (quasi-omnidirectional) ARCs for next-generation optical systems.

antireflective coatings↗

Pulse-length dependence of the laser-induced damage behavior of a fused-silica antireflective metasurface

A broadband, antireflective metasurface optic on a silica substrate is subjected to laser-induced damage-threshold measurements to quantify its performance under exposure to high-intensity/fluence laser pulses in the near-infrared at four pulse durations, ranging from 20 fs to 1.4 ns. The performance of the metasurface is benchmarked against that obtained from an equivalent bare fused-silica substrate that did not receive reactive-ion-etching metasurface treatment. Results showed that the damage threshold of the antireflective metasurface was always lower than the input-surface damage threshold of the untreated substrate. The damage initiations with nanosecond and picosecond pulses resulted in localized modification and removal of the nanostructures, whereas the onset of laser-induced modification with 20-fs pulses in a vacuum environment manifested as changes in the optical and electronic properties without significant material removal. The broader goal of this work is to develop a preliminary understanding of the laser-induced failure mechanisms of silica-based metasurface optics.

antireflection↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting From Hot-Humid High-Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable legacy aluminum back surface field cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60 degrees C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission Technical Specification 62804-1; 70 degrees C/70% RH for 200 h; and 85 degrees C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage curve tracing. Final characterizations included: Suns-Voc, spatial mapping of external quantum efficiency, high-resolution photoluminescence, EL, and dark lock-in thermography imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy, and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500 V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline corrosion and delamination, and other concurrent degradation modes. SEM/EDS and SAM identified the conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Diagnosis of PV Cell Antireflective Coating Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on a photovoltaic cell ("ARc corrosion") has previously been observed in studies using hot-humid test conditions with external high-voltage (HV) bias. This study primarily focuses on known vulnerable, legacy aluminum back surface field (Al-BSF) cells in mini-modules (MiMos) put through comparative stepped stress tests. Each cell type had MiMos at +1500 V, -1500 V, or unbiased ("Voc") potential, which were sequentially subjected to test conditions of 60deg C/60% relative humidity (RH) for 96 h, as in International Electrotechnical Commission (IEC) Technical Specification 62804-1; 70 deg C/70% RH for 200 h; and 85 deg C/85% RH for 200 h. Characterizations at each step included visual camera and electroluminescence (EL) imaging, colorimetry, and current-voltage (I-V) curve tracing. Final characterizations included: Suns-Voc; spatial mapping of external quantum efficiency (EQE); high-resolution photoluminescence (PL), EL, and dark lock-in thermography (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray photoelectron spectroscopy (XPS), and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos from previous studies that underwent stepped HV aging and separate outdoor aged full-sized modules. ARc corrosion was specifically seen for the glass/encapsulant/cell side of the +1500V (HV+) stressed MiMos and modules. Appearance, color, and reflectance were the most distinguishing characteristics relative to glass corrosion, gridline-corrosion and -delamination as well as other concurrent degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to hydrated silica, hydrous silica, or hydrated amorphous silica, which preferentially occurred at the edges and tips of the pyramidal textured cell surface.

14 SOLAR ENERGY↗

Antireflective Multi‐Dielectric Metasurfaces Operating in the Visible

Abstract As increasingly more demanding photonics applications are brought on‐chip, more complex design solutions are employed to deliver enhanced performance: e.g., meta‐molecules, inverse‐designed freeform structures, and multilayer metasurfaces. Instead, this study introduces anti‐reflective metasurfaces fabricated in a single nanolithography step that follows deposition of multiple dielectrics onto a substrate. Anti‐reflective metasurfaces offer fundamentally better transmission efficiencies compared to conventional equivalents. Conventional and anti‐reflective metalenses, both fabricated in the Ta 2 O 5 /SiO 2 material platform for 461 nm operation, show an improvement in focusing efficiencies from ≈ 55% to ≈ 90% at low numerical apertures and from ≈ 35% to ≈ 65% at high numerical apertures. Simulations of ideal and imperfect metalenses indicate that anti‐reflective metasurfaces not only improve transmission at the design library level, but also reduce spurious diffraction and protect against higher‐order scattering.

Optics↗

Reducing module soiling with scalable and robust photocatalytic coatings

The air-glass interface at the front of a photovoltaic (PV) module reflects approximately 4% of incident light, decreasing the potential power output of the module by the same amount. Today’s modules reduce this loss by adding a low-refractive-index (1.25-1.30) SiO2 coating to the sunward side of the module glass; this antireflection coating recovers approximately 3% of the 4% light that would otherwise be lost. While such antireflection coatings work very well on clean, new modules, they do not inhibit soiling—the accumulation of soilants such as dust, pollen, soot, or other foreign material—on the module glass, and soilants reflect and scatter incident light. An improved coating would serve provide not only an antireflection effect, but also an anti-soiling effect. The goal of this project was to develop such a coating and provide a path for it to be manufactured in the U.S. The project successfully designed and fabricated coatings that provided >3% transmittance gain compared to bare glass (matching the performance of commercial antireflection coatings) and displayed anti-soiling behavior in standard laboratory soiling effects. This was achieved by using a Swift Coat proprietary coating deposition technique, aerosol impact-driven assembly (AIDA), to control the porosity and thus refractive index of coatings of photocatalytic materials—such as TiO2—that would otherwise increase (instead of decrease) reflection. These combined antireflection/anti-soiling coatings passed PV industry standard module reliability tests as well as coating-specific abrasion tests, showing that they have the durability needed for decades in the field. Swift Coat scaled the AIDA hardware and deposition process to make mini-modules that were monitored for nearly two years during field tests administered by a third party, as well as demonstrated scaling to the widths of full-sized modules. The fielded mini-modules outperformed reference modules (with commercial antireflection coatings) in two locations, providing a 1% absolute average performance boost and larger increases during periods of heavier soiling. Swift Coat’s cost analysis indicated a coating manufacturing cost below the sales price of today’s antireflection coatings. More than five module manufacturers sampled and assessed the coatings, and three provided letters of support. The coating developed in this project increases the energy output of PV modules, thereby decreasing the cost per kilowatt-hour of solar energy generated. Cheaper solar electricity benefits the public by accelerating the transition to a stable, affordable, carbon-free energy economy. In addition, for select applications in which PV modules are highly visible—such as on residential rooftops—the coating provides an aesthetic benefit because it stays cleaner than today’s modules. Finally, Swift Coat and its prospective customers are U.S. companies, and successful commercialization of this technology will provide U.S. jobs and a secure solar supply chain.

14 SOLAR ENERGY↗

Enhanced laser-induced damage performance of all-glass metasurfaces for energetic pulsed laser applications

To fabricate optical components with surface layers compatible with high power laser applications that may operate as antireflective coatings, polarization rotators, or harness physical anisotropy for other uses, metasurfaces are becoming an appealing candidate. In this study, a large-beam (1.05 cm diameter) 351-nm laser-induced damage testing was done on an all-glass metasurface structure composed of cone-like features with a subwavelength spacing of adjacent features. These structures were fabricated on untreated fused silica glass and damage tested, as were structures that were fabricated on fused silica glass that experienced a preliminary etching process to remove the surface Beilby layer that is characteristic of polished fused silica. The laser-induced damage onset for structures on untreated fused silica glass was 19.3 J∙cm -2 , while the sample that saw an initial pretreatment etch exhibited an improved damage onset of 20.4 J∙cm -2 , only 6% short of the reference pretreated glass damage onset of 21.7 J∙cm -2 . For perspective, the National Ignition Facility (NIF) operational average fluence at this wavelength and pulse length is about 10 J/cm2. At a fluence of 25.5 J∙cm -2 , the reference (pretreated) fused silica initiated 5.2 damage sites per mm 2 , while the antireflective metasurface sample with a preliminary etching process treatment initiated 9.8 damage sites per mm 2 . In conclusion, these findings demonstrate that substrate-engraved metasurfaces are compatible with high energy and power laser applications, further broadening their application space.

36 MATERIALS SCIENCE↗

A Comprehensive Comparative Study of Active Learning Schemes for Nanophotonics Design

We present a benchmarking study of active learning (AL) schemes for designing planar multilayer nanophotonic metamaterials, where the design tasks are formulated as binary optimization problems. Different surrogate models, including factorization machine (FM), Gaussian process regression (GPR), and convolutional neural network (CNN), combined with different optimization methods, including exhaustive enumeration, discrete particle swarm optimization (DPSO), quantum annealing (QA), hybrid QA, and simulated annealing are studied. The benchmark cases investigated range from small problems with short binary lengths (N = 25) to large problems with N up to 100, focusing on the design of two classes of photonic structures, including antireflective coatings for the long-wavelength infrared region and transparent radiative coolers. For small problems, CNN coupled with DPSO in AL achieves the best performance. As N increases, FM with QA outperforms GPR and CNN. For FM-based AL, hybrid QA yields the best optimization results, particularly in high-dimensional cases (N = 100). These results demonstrate that the optimization method can significantly affect in AL performance as N increases, and that QA-based optimization can provide practical routes for mitigating the optimization bottleneck in high-dimensional problems.

Jung, Serang [Kyung Hee University, Korea]↗

Electrochemical Modeling of PID Leakage Current of PV Modules: Steady-State Current, Transient Current, and RC-Equivalent Circuit

Potential-induced degradation (PID) remains a significant reliability concern for photovoltaic (PV) modules, arising when a voltage difference between the module frame and the solar cells drives unintended leakage current through the glass-encapsulant stack. Although PID ultimately manifests as PID-s, PID-p, or PID-c, the underlying behavior of the leakage current-its magnitude and time dependence-requires clearer electrochemical interpretation. Traditional explanations attribute the initial transient current to bulk capacitive elements of the glass, encapsulant, and antireflection coatings, and the steady-state current according to their effective ohmic resistance. More recent studies, however, indicate that electrochemical charge-transfer processes at the encapsulant-metallization interface can play a dominant role in defining the leakage-current path. This paper develops a unified electrochemical framework for modeling PID leakage current. First, an RC-equivalent circuit is formulated by combining conventional RC elements with a Randles-type interface to capture transient leakage current through double-layer capacitance and faradaic processes at ionic-electronic boundaries. Second, the steady-state current-voltage behavior is explained using a linearized Butler-Volmer relationship, showing that the measured ohmic response corresponds to the low-overpotential limit of charge-transfer kinetics. Analytical results demonstrate that, for typical module materials-3.2-mm soda-lime glass and 0.45-mm encapsulant-the dominant modulators to PID leakage current are the glass surface resistance (under dry-surface conditions), the glass bulk capacitance, and the encapsulant resistance (under wet-surface conditions), with soda lime glass surface and EVA/POE encapsulant resistances primarily governing steady-state current. The proposed electrochemical model is validated against measured leakage-current data, showing good agreement in both the magnitude and the time-dependent evolution of PID leakage current.

14 SOLAR ENERGY↗

Formation of tunable diamond micro- and nanopillars for field effect enhancement applications

Here, we developed a process for the fabrication of tunable single crystal diamond micro- and nanopillars, with tip widths ranging from 40 to 460 nm, densities ranging from 0.5 to 53.5 pillars/μm 2 , and heights greater than 4.5 μm. A self-assembled Au nanodot ensemble etch mask was formed from an annealed Au thin film. The nanodot diameter and density can be tuned using the initial film thickness. The pillars were etched from the nanodot mask using an RIE O 2 plasma, which has infinite selectivity for the diamond when applied at low RF powers (50 W). Finally, the pillars can be sharpened to ~40 nm tip widths by annealing in air at 650 °C. These pillars can be used for applications such as field effect enhancement of diamond photocathode devices, enhancement of optical emission from N-V centers, and antireflective coatings.

36 MATERIALS SCIENCE↗

Bio-inspired multiscale design for perovskite solar cells

Metal halide perovskite semiconductors have attractive light-harvesting and charge-carrier transport properties for photovoltaics. Perovskite solar cells (PSCs) and modules have demonstrated their commercial promise with high power conversion efficiencies, but still face stability challenges. In this Review, we explore how biomaterials offer design inspiration for the development of durable and efficient PSCs at three different scales. At the molecular level, bio-inspired molecular interactions are harnessed towards crystallization control and degradation prevention, which offers an enhancement in long-term maximum-power-point tracking stability. At the microstructural level, self-healing and strength-enhancing strategies, utilizing dynamic bonds and interfacial reinforcement, can help PSCs to recover from physical damage and maintain high performance. At the device level, macroscopic functionalities, such as moth-eye-inspired structures tailored to different layers, can collectively enable antireflection, radiative cooling and self-cleaning to optimize light management, heat dissipation and encapsulation in PSCs. Bio-inspired PSC research can combine improved efficiency and lifetime, with abundant, biocompatible alternatives to conventional stabilizers. Future efforts should focus on screening bioinspired molecules to optimize film crystallization and stability, developing self-healing mechanisms triggered by operational stress, designing cost-efficient biomicrostructures, and integrating multifunctional encapsulation to enhance the efficiency and lifespan of PSCs.

Duan, Tianwei↗

Evidence for ionization damage in mid-wave infrared nBn detectors

The effects of 63 MeV proton and 60Co gamma irradiation on the operation of 4.3 μm cutoff nBn photodetectors are demonstrated separately, and both are shown to yield a total ionizing dose (TID) effect. The effect is shown here in an InAsSbBi nBn detector and has been observed in other bulk alloy nBn detectors, and is unusual as it is notably absent in superlattice nBn detectors. The non-antireflection coated detectors exhibit a pre-radiation quantum efficiency of 17% at 3.3 μm wavelength and a dark current density of 50 μA/cm2, or roughly 300× the Rule 07 expectation, at their ideal operating voltage of −0.4 V bias at 150 K. Step-wise proton irradiation and in situ measurement indicate that the dark current increases to about 400× Rule 07 at the highest proton dose level of 150 krad(Si) (9.10 × 1011 p+/cm2), while the quantum efficiency is degraded at a relatively faster rate than the majority of analogous detectors characterized by our lab. Both the photocurrent and dark current are also shown to exhibit a turn-on voltage magnitude reduction of 100 mV following either gamma or proton irradiation, a trend which is attributable to negative trapped charge at the barrier interface (TID effect). This theory is further supported by an observed capacitance density magnitude reduction with dose and affirmed with Silvaco TCAD simulations. Following both proton exposure and subsequent anneal and gamma exposure and subsequent anneal; dark current, photocurrent, and CV all approach their pre-radiation baseline values.

Physics↗

Setting Priorities for Photovoltaic Reliability Research Using Criticality Analysis

A forward-looking research opportunity number (RON) is defined for photovoltaic reliability researchers. The RON enables researchers to prioritize their efforts toward the highest impact. For a given degradation mode, the RON is based on three factors: the effect on levelized cost of electricity, the susceptibility of future module products, and the maturity of accelerated tests that can detect and quantify the mode. Reporting bias is avoided because the RON does not rely on polls. The RON is derived for three example cases: light and elevated temperature degradation, backsheet cracking, and antireflective coating abrasion. Finally, these examples demonstrate that targeted research has reduced the risk for these modes over the last several years.

14 SOLAR ENERGY↗

In Situ MOVPE Smoothing of Acoustically Spalled GaAs for Substrate Reuse

High material costs, especially for substrates, have limited the widespread adoption of III-V photovoltaics. A potential to reduce this cost is to reuse the III-V substrate via acoustic spalling, however this technique can leave a rough surface, hindering subsequent device performance. This research investigates the potential of using metalorganic vapor-phase epitaxy growth as a buffer layer to smooth the surface of acoustically spalled germanium and gallium arsenide (GaAs) substrates for improved III-V photovoltaic cell yield and performance, while retaining the maximum number of reuses of a substrate. Three potential smoothing layers were explored: lightly doped C:GaAs, highly doped Se:GaInP, and lightly doped Se:GaInP. C:GaAs showed the most promise as a smoothing layer, while Se:GaInP tended to conform to the underlying morphology, potentially increasing roughness in some areas. Utilizing 5 ..mu..m of C:GaAs as a planarizing buffer increased the average efficiency (without an antireflection coating) from an as-spalled baseline from 2.1% to 4.9% and performing a 5-min 30 degrees C 8:1:1 H2SO4:H2O2:H2O etch prior to a 5 ..mu..m of C:GaAs as a planarizing buffer further increased efficiency to 11.1%.

14 SOLAR ENERGY↗

Diagnosis of PV Cell Passivation Degradation Resulting from Hot-Humid, High Voltage Potential Aging

Corrosion of the antireflective coating on the cell ("AR c corrosion") was previously observed in studies using hot-humid test conditions with external high voltage (HV) bias. Because AR c corrosion is not well understood, mini-modules (MiMos) were examined in a comparative experiment using PERC and PERT as well as legacy Al-BSF cells. For separate MiMos with the cell circuit electrical at +1500 V, -1500 V, or unbiased "V oc", test conditions in the comparative study included 60degrees C/60% RH for 96 h, as in IEC TS 62804-1; 70degrees C/70%RH for 200 h; and 85degrees C/85% RH for 200 h. Characterizations at each read point included: camera and electroluminescence (EL) imaging, colorimetry, and I-V curve tracing. Characterizations at the final read point included: SunsVoc; spatially mapping external quantum efficiency (EQE); high resolution: photoluminescence (PL), EL, and dark lock-in thermographic (DLIT) imaging. Forensics were performed on extracted cores, including scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS) and scanning Auger microscopy (SAM). Forensics were also conducted on MiMos (stepped HV aging) and full-sized modules (outdoor aging) from previous studies. AR c corrosion was specifically observed for the glass/encapsulant/cell side of +1500 V (HV+) stressed MiMos, where appearance, color, and reflectance were the characteristics most distinguished relative to simultaneously occurring degradation modes. SEM/EDS and SAM identified conversion of silicon nitride to silicon oxide or hydrous silica, preferentially occurring at the edges and tips of the pyramidal textured cell surface.

aging↗

Eye-Safe 1.5 and 2.0 Micron Laser Power Conversion Using Metamorphic InGaAs Photovoltaic Devices

Laser power transmission at 1.5 and 2.0 microns are considered eye-safe up to 0.1 W/cm2 irradiance. Further, the atmospheric bands at these two wavelengths may provide the highest optical transmission through the atmosphere in hazy conditions. By slowly changing the lattice-constant of InGaAs with a Compositionally Graded Buffer (CGB), we have fabricated InGaAs photovoltaic (PV) devices over a wide range of bandgaps useful for multijunction concentrating photovoltaic devices, thermophotovoltaic devices, and Laser Power Converters (LPC). Here, we have demonstrated monochromatic power conversion of 1.5-micron light with an eye-safe efficiency of 39.8% at 0.1 W/cm2 with InGaAs devices lattice-matched to InP with an Antireflection Coating (ARC). We have also demonstrated 30.2% and 24.5% eye-safe LPC efficiency of metamorphic InGaAs devices grown on GaAs substrates using GaInP and AlGaAsP CGBs, respectively. Finally, we have demonstrated metamorphic InGaAs devices grown on InP and GaAs substrates that are estimated to have eye-safe LPC efficiencies at 2.0 microns of 27.4% and 20.9% respectively. The efficiencies of all these LPC devices continues to increase up to about 30-70 times the eye-safe irradiance.

eye-safe↗

Low loss fiber-coupled volumetric interconnects fabricated via direct laser writing

Photonic integrated circuits (PICs) are vital for high-speed data transmission. However, optical routing is limited in PICs composed of only one or a few stacked planes. Further, coupling losses must be low in deployed systems. Previously, we developed the subsurface controllable refractive index via beam exposure (SCRIBE) technique to write accurate 3D gradient refractive index (GRIN) profiles within a mesoporous silica scaffold. Here, we apply SCRIBE to fabricate low loss, broadband, polarization insensitive, fiber-coupled, single-mode volumetric interconnects that include waveguides traversing arbitrary 3D paths. By seamlessly integrating mode-matching subsurface lenses and GRIN waveguide tapers, calibrating for positional writing errors, implementing multipass exposure, automating alignment, and switching to antireflection coated fibers, we reduced the insertion loss for a fiber-PIC-fiber interconnect from 50 to 2.14 dB, or 1.47 dB, excluding the fiber array’s loss. Further, we establish an upper bound of 0.45 dB loss per coupler. We report quality factors of 27,000 and 77,000 and bending losses of 6 and 3 dB/cm for 15 and 30 µm radii microrings, respectively. We also demonstrate Bézier escalators, polarization-rotating and polarization-splitting interconnects, and a seven-channel 25 µm pitch volumetric interconnect. The SCRIBE platform presents a clear path toward realizing 3D PICs with unique functionality.