Toward ultrafast, ultra-stable imaging arrays: Superlattice doping to enhance the performance of backside-illuminated 3D-hybridized silicon photodetectors

In this paper, the authors report the latest results on their development of superlattice-doped, thinned, backside-illuminated (BSI), 3D-integrated photodiode detectors—a step toward their ultimate goal of demonstrating ultrafast, ultrastable CMOS imaging arrays. As with most silicon-based photodetectors, backside-illumination and backside surface passivation are keys to achieve the highest performance capability. The two-dimensional (2D) doping technique developed at the Jet Propulsion Laboratory (JPL) has proved to result in a highly efficient, highly stable detector response when combined with a variety of detectors. Here, JPL's 2D-doping has been combined with Sandia's BSI photodetectors hybridized with custom fanout wafer via copper Direct Bond Interconnect (DBI®), a technology that is rapidly becoming industry standard for BSI CMOS imaging arrays. The prototype detectors were packaged and evaluated with respect to their response to low energy electrons. The authors find that the responsivity of 2D-doped BSI detectors is higher than devices prepared using other surface passivation techniques (i.e., ion implantation). The success of the work described herein verifies that the 2D-doping processes previously developed for Sandia's frontside-illuminated photodetectors are generally applicable to BSI detectors and demonstrates for the first time that JPL's 2D-doping process is compatible with the Cu-DBI® technology.

Jewell, April D.↗

Soft X-ray quantum efficiency of a commercial CMOS imaging sensor

The demonstrated performance and cost-effectiveness of complementary metal-oxide-semiconductor (CMOS) sensors make them a potentially attractive option for low-cost space-based X-ray observatories. We have previously reported on the performance of a commercially available backside-illuminated Sony IMX290LLR-C CMOS sensor and found it to offer X-ray spectral resolutions comparable to the charged coupled devices (CCDs) aboard Suzaku and Chandra and to have a sufficient radiation hardness for use in low Earth orbit. Here, in this work, we report on the quantum efficiency (QE) of this sensor, an essential metric for modeling the sensitivity of an instrument as an X-ray detector. Using the Advanced Photon Source at Argonne National Laboratory, we measure the soft X-ray QE of this CMOS sensor to be 0.28 ± 0.02 at a photon energy of 490.5 eV. This energy was chosen for its proximity to the astrophysically important O VII triplet emission lines (~574 eV) studied by the HaloSat mission. Although not surpassing that of the back-illuminated CCDs aboard Suzaku and Chandra, this QE compares favorably to that of the front-illuminated CCDs aboard the same observatories and is competitive with that of the silicon drift detectors used aboard HaloSat, making it a strong candidate for use on future X-ray small satellite (SmallSat) missions.

47 OTHER INSTRUMENTATION↗

Method of fabricating photosensitive devices with reduced process-temperature budget

A method is provided for fabricating a backside-illuminated photodetector in which a device wafer is joined to a readout wafer in an IC hybridization step. Before the IC hybridization step, the device layer is defined in the device wafer, and an LPCVD layer is formed over the device layer. The LPCVD layer may be a passivation layer, an antireflection coating, or both. The side of the device wafer having the LPCVD layer is bonded to a handle wafer, the IC is hybridized by mating the device wafer to the readout wafer, and the handle wafer is then removed, exposing the LPCVD layer. Because the LPCVD layer is formed before the active devices are fabricated, it can be made by high-temperature techniques for deposition and processing. Accordingly, a layer of high quality can be fabricated without any hazard to the active devices.

Kay, Randolph R.↗