At least 19 records

Effect of Solute Elements on Boron Segregation in Boron-Containing Steels

The addition of boron to steel alloys results in an increase in both hardenability and casting defects. The casting difficulties are predicted to stem from a metatectic reaction, δ + γ → L + γ, where a fully solidified material begins to locally remelt as the temperature decreases. Another possible source of casting defects is a boride-rich phase that is predicted to remain liquid at low temperatures. To experimentally determine which reaction is the likely source of the casting defects, the predicted reactions and the effect of solute elements on those reactions are investigated. Levitation zone melting is used to control segregation in a ternary Fe–C–B alloy and a commercial 22MnB5 alloy. Carbon segregation and a peritectic reaction result in a peritectic jump during directional solidification where the first directionally solidified (DS) zone undergoes δ-bcc solidification followed by a peritectic jump to steady state planar solidification of γ-fcc in the second DS zone. The presence of other solute elements in the zone melted 22MnB5 alloy lead to a breakdown in the planar solidification front before steady state solidification could be achieved in the second DS zone. With a cellular solid/liquid interface, boron-rich intercellular liquid formed low melting iron boro-carbide particles. The controlled solidification conditions in a levitation zone melter were unable to prevent ~0.003 wt% boron from segregating to high enough levels to form boride particles. Therefore, it is likely that during commercial casting, the formation of the low melting boride phase from interdendritic segregation is a key source of the casting issues.

36 MATERIALS SCIENCE↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Grain boundary engineering for efficient and durable electrocatalysis

Grain boundaries in noble metal catalysts have been identified as critical sites for enhancing catalytic activity in electrochemical reactions such as the oxygen reduction reaction. However, conventional methods to modify grain boundary density often alter particle size, shape, and morphology, obscuring the specific role of grain boundaries in catalytic performance. This study addresses these challenges by employing gold nanoparticle assemblies to control grain boundary density through the manipulation of nanoparticle collision frequency during synthesis. We demonstrate a direct correlation between increased grain boundary density and enhanced two-electron oxygen reduction reaction activity, achieving a significant improvement in both specific and mass activity. Additionally, the gold nanoparticle assemblies with high grain boundary density exhibit remarkable electrochemical stability, attributed to boron segregation at the grain boundaries, which prevents structural degradation. This work provides a promising strategy for optimizing the activity, selectivity, and stability of noble metal catalysts through precise grain boundary engineering.

36 MATERIALS SCIENCE↗

Friction and wear of some ferrous-base metallic glasses

Sliding friction experiments, X-ray photoelectron spectroscopy (XPS) analysis, and electron microscopy and diffraction studies were conducted with ferrous base metallic glasses (amorphous alloys) in contact with aluminum oxide at temperatures to 750 C in a vacuum. Sliding friction experiments were also conducted in argon and air atmospheres. The results of the investigation indicate that the coefficient of friction increases with increasing temperature to 350 C in vacuum. The increase in friction is due to an increase in adhesion resulting from surface segregation of boric oxide and/or silicon oxide to the surface of the foil. Above 500 C the coefficient of friction decreased rapidly. The decrease correlates with the segregation of boron nitride to the surface. Contaminants can come from the bulk of the material to the surface upon heating and impart boric oxide and/or silicon oxide at 350 C and boron nitride above 500 C. The segregation of contaminants is responsible for the friction behavior. The amorphous alloys have superior wear resistance to crystalline 304 stainless steel. The relative concentrations of the various constituents at the surfaces of the amorphous alloys are very different from the nominal bulk compositions.

Miyoshi, K.↗

Friction and wear of some ferrous-base metallic glasses

Sliding friction experiments, X-ray photoelectron spectroscopy (XPS) analysis, and electron microscopy and diffraction studies were conducted with ferrous base metallic glasses (amorphous alloys) in contact with aluminium oxide at temperatures to 750 C in a vacuum. Sliding friction experiments were also conducted in argon and air atmospheres. The results of the investigation indicate that the coefficient of friction increases with increasing temperature to 350 C in vacuum. The increase in friction is due to an increase in adhesion resulting from surface segregation of boric oxide and/or silicon oxide to the surface of the foil. Above 500 C the coefficient of friction decreased rapidly. The decrease correlates with the segregation of boron nitride to the surface. Contaminants can come from the bulk of the material to the surface upon heating and impart boric oxide and/or silicon oxide at 350 C and boron nitride above 500 C. The segregation of contaminants is responsible for the friction behavior. The amorphous alloys have superior wear resistance to crystalline 304 stainless steel. The relative concentrations of the various constituents at the surfaces of the amorphous alloys are very different from the nominal bulk compositions.

Miyoshi, K.↗

Effects Of B On Intergranular Hot Cracking In Ni Alloys

Report describes experiments on role of boron on solidification of 718-type nickel/chromium/iron superalloys containing niobium and relative intergranular segregations of boron, sulfur, and phosphorus in alloys. Ten alloys studied by use of light and scanning electron microscopy (SEM), energy-dispersive x-ray analysis, transmission electron microscopy (TEM) with energy-dispersive analysis of thin-film specimens, mechanical tests for susceptibility to microfissuring, differential thermal analysis (DTA), scanning Auger microscopy, and Gleeble thermal analysis.

Thompson, Raymond G.↗

Effect of boron on intergranular hot cracking in Ni-Cr-Fe superalloys containing niobium

Solidification mechanisms had a dominant influence on microfissuring behavior of the test group. Carbon modified the Laves formation significantly and showed that one approach to alloy design would be balancing carbide formers against Laves formers. Boron's strong effect on microfissuring can be traced to its potency as a Laves former. Boron's segregation to grain boundaries plays at best a secondary role in microfissuring.

Thompson, R. G.↗

Development of dispersion-strengthened XD (trademark) Cu alloys for high heat-flux applications

In a previous effort sponsored by NASA LeRC, the XD(trademark) process was used to produce ZrB2 particulate reinforcements in Cu and the resulting extruded material was microstructurally characterized and evaluated in tension over a range of temperatures. A problem that was encountered in that study was microstructural inhomogeneity resulting from the frequent presence of 'ZrB2 agglomerates' that were several microns in size. The presence of these agglomerates was attributed to improper mixing of powders in the green compact used in the XD process for elemental boron powder segregation. In this program, several milling parameters were examined in an effort to optimize this processing step; two levels of ZrB2 reinforcements were considered (7 vol. percent and 15 vol. percent). Microstructures of the reacted powder mass were examined to verify the absence of these agglomerates. Larger bathes of powder were then mixed, reacted, machined to size, canned, and extruded. The microstructure and tensile properties of these extrusions were examined, and the measured properties were correlated with the observed microstructure. Large unreacted or partially reacted Zr particles were present. These particles affected the mechanical properties deleteriously, and their presence is attributed to insufficient heat of reaction during XD synthesis. Alternate processing routes are recommended.

Kumar, K. Sharvan↗

Effect of boron on tensile properties of B2 BeAl

Small additions of boron were shown to improve the room temperature ductility of the intermetallic compound Ni3Al. Boron is believed to segregate to the gain boundaries and strengthen them, allowing the inheret ductility of the grains to be achieved. The present study was undertaken to see if boron has a similar effect on the low temperature tensile properties of the equiatomic intermetallic compound FeAl. A binary alloy without boron is compared with an alloy containing 0.78 at % B (0.2 wt %) B, by tensile testing over the temperature range of 300 K to 640 K. Both alloys were processed by powder metallurgy. Results showed that 0.78 at % B addition to FeAl does indeed change the room temperature fracture mode from intergranular to transgranular, suggesting a strengthening of grain boundaries. The alloy containing boron is, however, still brittle at room temperature. A slight decrease in the ductile to brittle transition temperature is, nevertheless, observed. In addition a significant increase in strength of the alloy is observed with boron addition.

Crimp, M.↗

Mechanical contact induced transformation from the amorphous to the crystalline state in metallic glass

Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.

Miyoshi, K.↗

Mechanical-contact-induced transformation from the amorphous to the partially crystalline state in metallic glass

Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.

Miyoshi, K.↗

Mechanical-contact-induced transformation from the amorphous to the partially crystalline state in metallic glass

Friction and wear tests were conducted with 3.2- and 6.4-millimeter-diameter aluminum oxide spheres sliding, in reciprocating motion, on a Fe67Co18B14Si1 metallic foil. Crystallites with a size range of 10 to 150 nanometers were produced on the wear surface of the amorphous alloy. A strong interaction between transition metals and metalloids such as silicon and boron results in strong segregation during repeated sliding, provides preferential transition metal-metalloid clustering in the amorphous alloy, and subsequently produces the diffused honeycomb structure formed by dark grey bands and primary crystals, that is, alpha-Fe in the matrix. Large plastic flow occurs on an amorphous alloy surface with sliding and the flow film of the alloy transfers to the aluminum oxide pin surface. Multiple slip bands due to shear deformation are observed on the side of the wear track. Two distinct types of wear debris were observed as a result of sliding: an alloy wear debris, and/or powdery-whiskery oxide debris.

Miyoshi, K.↗

Applications of analytical electron microscopy to guide the design of boron carbide

Compositional analysis of boron carbide on nanometer length scales to examine or interpret atomic mechanisms, for example, solid-state amorphization or grain-boundary segregation, is challenging. This work reviews advancements in high-resolution microanalysis to characterize multiple generations of boron carbide. First, ζ-factor microanalysis will be introduced as a powerful (scanning) transmission electron microscopy ((S)TEM) analytical framework to accurately characterize boron carbide. Three case studies involving the application of ζ-factor microanalysis will then be presented: (1) accurate stoichiometry determination of B-doped boron carbide using ζ-factor microanalysis and electron energy loss spectroscopy, (2) normalized quantification of silicon grain-boundary segregation in Si-doped boron carbide, and (3) calibration of a scanning electron microscope X-ray energy-dispersive spectroscopy (XEDS) system to measure compositional homogeneity differences of B/Si-doped arc-melted boron carbides in the as-melted and annealed conditions. Overall, the improvement and application of advanced analytical tools have helped better understand processing–microstructure–property relationships and successfully manufacture high-performance ceramics.

36 MATERIALS SCIENCE↗

Segregation of Impurities in Directionally Solidified Silicon

Hall measurements and four-point probe resistivity measurements are used to determine the concentration profile of boron and iron in doped semi-conductor silicon ingots grown by the Bridgman technique. The concentration profiles are fitted to the normal segregation equation and the effective segregation coefficient, K sub eff, is calculated. The average value of K sub eff, is 0.803 for boron. For iron, K sub eff, is concentration dependent and is in the range 0.00008 to 0.00012.

Ravishankar, P. S.↗

Effect of heat transfer of melt/solid interface shape and solute segregation in Edge-Defined Film-Fed growth - Finite element analysis

The effects of the heat transfer environment in Edge-Defined Film-Fed Growth on melt-solid interface shape and lateral dopant segregation are studied by finite-element analysis of two-dimensional models for heat and mass transfer. Heat transfer configurations are studied that correspond to the uniform surroundings assumed in previous models and to lowand high-speed growth systems. The maximum growth rate for a silicon sheet is calculated and the range of validity of one-dimensional heat transfer models is established. The lateral segregation that results from curvature of the solidification interface is calculated for two solutes, boron and aluminum. In this way, heat transfer is linked directly to the uniformity of the product crystal.

Ettouney, H. M.↗

Interstitials in f.c.c. High Entropy Alloys

The effects of interstitials on the mechanical properties of single-phase f.c.c. high entropy alloys (HEAs) have been assessed based on a review of the literature. It is found that in nearly all studies, carbon increases the yield strength, in some cases by more than in traditional alloys. This suggests that carbon can be an excellent way to strengthen HEAs. This strength increase is related to the lattice expansion from the carbon. The effects on other mechanical behavior is mixed. Most studies show a slight reduction in ductility due to carbon, but a few show increases in ductility accompanying the yield strength increase. Similarly, some studies show little or modest increases in work-hardening rate (WHR) due to carbon, whereas a few show a substantial increase. These latter effects are due to changes in deformation mode. For both undoped and carbon doped CoCrFeMnNi, the room temperature ductility decreases slightly with decreasing grain size until ~2–5 µm, below which the ductility appears to decrease rapidly. The room temperature WHR also appears to decrease with decreasing grain size in both undoped and carbon-doped CoCrFeMnNi and in nitrogen-doped medium entropy alloy NiCoCr, and, at least for the undoped HEA, shows a sharp decrease at grain sizes <2 µm. Interestingly, carbon has been shown to almost double the Hall–Petch strengthening in CoCrFeMnNi, suggesting the segregation of carbon to the grain boundaries. There have been few studies on the effects of other interstitials such as boron, nitrogen and hydrogen. It is clear that more research is needed on interstitials both to understand their effects on mechanical properties and to optimize their use.

36 MATERIALS SCIENCE↗

Multi-microscopy characterization of threading dislocations in CVD-grown diamond films

We present site-coincident imaging of a high dislocation density boron-doped chemical vapor deposition-grown homoepitaxial (001) diamond film using electron channeling contrast imaging (ECCI), cathodoluminescence, transmission electron microscopy (TEM), and scanning secondary ion mass spectroscopy (SIMS). With growing interest in large area heteroepitaxial substrates, we show that ECCI is a promising technique to accurately evaluate dislocations in diamond films. We find the electron backscatter yield is sufficient to distinguish individual threading dislocations in ECCI despite the low atomic number of carbon, and we have generally good agreement between dislocations observed in ECCI and TEM of the same region. Importantly, relying on luminescence in the 430 nm dislocation-related A-band alone results in an underestimation of the defect density as we find only 20%–40% of the threading dislocations luminesce. Here, we further show that dislocations do not perturb the spatial uniformity of boron doping measured by SIMS, even when the dislocations are clustered with high density, and we can tentatively rule out strong segregation effects at the dislocations. Our results establish the complementary use of microscopy and microanalysis methods to rapidly characterize and understand the impact of dislocations in diamond thin films.

36 MATERIALS SCIENCE↗