Results for “capacity loss”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

A new strategy to mitigate the initial capacity loss of lithium ion batteries

Hard carbon (non-graphitizable) and related materials, like tin, tin oxide, silicon, and silicon oxide, have a high theoretical lithium delivery capacity (>550 mAh/g depending on their structural and chemical properties) but unfortunately they also exhibit a large initial capacity loss (ICL) that overrides the true reversible capacity in a full cell. Overcoming the large ICL of hard carbon in a full-cell lithium-ion battery (LIB) necessitates a new strategy wherein a sacrificial lithium source additive, such as, Li5FeO4 (LFO), is inserted on the cathode side. Full batteries using hard carbon coupled with LFO-LiCoO2 (LCO) are currently under development at our laboratory. We find that the reversible capacity of a cathode containing LFO can be increased by 14%. Furthermore, the cycle performance of full cells with LFO additive is improved from <90% to >95%. We show that the LFO additive not only can address the irreversible capacity loss of the anode, but can also provide the additional lithium ion source required to mitigate the lithium loss caused by side reactions. In addition, we have explored the possibility to achieve higher capacity with hard carbon, whereby the energy density of full cells can be increased from ca. 300 Wh/kg to >400 Wh/kg.

hard carbon↗

Unravelling the origin of irreversible capacity loss in NaNiO 2 for high voltage sodium ion batteries

Layered transition metal compounds have attracted much attention due to their high theoretical capacity and energy density for sodium ion batteries. However, this kind of material suffers from serious irreversible capacity decay during the charge and discharge process. Here, using synchrotron-based operando transmission X-ray microscopy and high-energy X-ray diffraction combined with electrochemical measurements, the visualization of the dissymmetric phase transformation and structure evolution mechanism of layered NaNiO2 material during initial charge and discharge cycles are clarified. Phase transformation and deformation of NaNiO2 during the voltage range of below 3.0 V and over 4.0 V are responsible for the irreversible capacity loss during the first cycling, which is also confirmed by the evolution of reaction kinetics behavior obtained by the galvanostatic intermittent titration technique. These findings reveal the origin of the irreversibility of NaNiO2 and offer valuable insight into the phase transformation mechanism, which will provide underlying guidance for further development of high-performance sodium ion batteries.

high voltage↗

Capacity loss on storage and possible capacity recovery for HST nickel-hydrogen cells

Negatively precharged nickel hydrogen cells will experience a useable capacity loss during extended open circuit storage periods. Some of the lost capacity can be recovered through cycling. Capacity recovery through cycling can be enhanced by cycling at high depths of discharge (DOD). The most timely procedure for recovering the faded capacity is to charge the cell fully and allow the cell to sit open-circuit at room temperature. This procedure seems to be effective in part because of the enlarged structure of the active materials. The compounds that formed during storage at the low electrode potentials can more easily dissolve and redistribute. All of the original capacity cannot be recovered because the lattice structure of the active material is irreversibly altered during storage. The recommendation is to use positively precharged cells activated with 26 percent KOH if possible. In aerospace applications, the benefits of negative precharge are offset by the possibility of delays and storage periods.

Lowery, John E.↗

Nickel-hydrogen capacity loss on storage

A controlled experiment evaluating the capacity loss experienced by nickel electrodes stored under various conditions of temperature, hydrogen pressure, and electrolyte concentration was conducted using nickel electrodes from four different manufacturers. It was found that capacity loss varied with respect to hydrogen pressure, and storage temperature as well as with respect to electrode manufacturing processes. Impedance characteristics were monitored and found to be indicative of electrode manufacturing processes and capacity loss. Cell testing to evaluate state-of-charge effects on capacity loss were inconclusive as no loss was sustained by the cells tested in this experiment.

Manzo, Michelle A.↗

Nickel-hydrogen capacity loss on storage

A controlled experiment evaluating the capacity loss experienced by nickel electrodes stored under various conditions of temperature, hydrogen pressure, and electrolyte concentration was conducted using nickel electrodes from four different manufacturers. It was found that capacity loss varied with regard to hydrogen pressure and storage temperature, as well as with regard to electrode manufacturing processes. Impedance characteristics were monitored and found to be indicative of electrode manufacturing processes and capacity loss. Cell testing to evaluate state-of-charge effects on capacity loss were inconclusive as no loss was sustained by the cells tested in this experiment.

Manzo, Michelle A.↗

Investigation on capacity loss mechanisms of lithium-ion pouch cells under mechanical indentation conditions

Capacity loss was observed in Li-ion cells after mechanical deformation approaching the onset of internal short circuit (ISCr). In this paper, a series of indentation tests were carried out on commercial Li-ion cells of three capacities (500, 1500 and 2000 mAh). Both in-situ and ex-situ methods were used to investigate the mechanisms of indentation-induced capacity loss. We note after indentation test, the cell capacity reduced by 0.5%–6% of its original value. The incremental capacity (IC) analysis results showed that IC curves generally shifted to lower voltage region, indicating the increase in cell internal resistance. In addition, the fitting results of electrochemical impedance spectroscopy (EIS) indicated that mechanical indentation can result in a reduction in ohmic resistance and the increase in polarization resistance. Scanning electron microscopy (SEM) and X-ray computed tomography (XCT) results showed crushing of graphite, mud cracking of copper current collectors and enlarged pores in separator, which is proposed to be the main reasons for the increase in polarization resistance and permanent capacity loss. The rapid capacity loss due to mechanical abuse was compared with the long-term capacity fading.

25 ENERGY STORAGE↗

Nickel-hydrogen capacity loss on storage

Nickel-hydrogen batteries are rapidly becoming accepted for use in low-earth-orbit and geosynchronous orbit applications. With their increased use it has become evident that the storage procedures commonly used for nickel-cadmium cells are not adequate for the nickel-hydrogen system. The capacity loss exhibited by nickel electrodes from various manufacturers when exposed to different storage conditions was determined. A comprehensive test matrix was developed to evaluate capacity loss in nickel electrodes from four different manufacturers. Two types of tests were run; individual electrode tests, which involved flooded capacity and impedance measurements before and after storage under varied conditions of temperature, hydrogen pressure, and electrolyte concentration; and cell tests which primarily evaluated the effects of state-of-charge on storage. The cell tests evaluated capacity loss on cells stored open circuit, shorted and trickle charged at C/100 following a full charge. The results indicate that capacity loss varies with the specific electrode manufacturing process, storage temperature and hydrogen pressure. In general, electrodes stored at low temperatures or low hydrogen pressures exhibited a smaller loss in capacity over the twenty-eight day storage period than those stored at high pressure and high temperature. The capacity loss appears to correlate with the level of cobalt in the nickel electrode, with the most significant loss of capacity occurring in electrodes with higher cobalt levels. Impedance measurements appear to correlate well with the capacity loss observed for a given type of electrode but do not correlate well with the capacity loss between electrodes fabricated by different manufacturers. There was a definite correlation between the electrode potential measured immediately following storage and the measured capacity loss.

Manzo, Michelle A.↗

Revealing the Mechanism Behind Sudden Capacity Loss in Lithium Metal Batteries

Rechargeable Li-metal batteries (LMBs) are attractive energy storage candidates for electric vehicles (EVs) because they offer higher energy density than batteries built with intercalation electrodes. However, one of the main barriers to the commercial deployment of LMBs has been their relatively short cycle life. Re-designing the electrolyte system shows promise in achieving acceptable cycle life, but even so, the resulting cells display a challenging end-of-life (EOL) behavior: a sudden capacity loss. Herein, we report a new method for analyzing voltage profiles during cycling to distinguish between the capacity loss originating from the loss of cathode capacity vs growth in cell resistance. Further, this analysis reveals that sudden capacity loss was preceded by acceleration in the rate of growth of cell resistance, and cycling of multiple cells showed that this phenomenon is sensitive to the initial quantity of electrolyte in the cells. In contrast, the cathode capacity degraded at a constant rate independent of the electrolyte quantity. Combining this evidence with post-analysis of harvested electrolyte and electrodes, we conclude that neither the loss of active lithium nor the loss of active cathode material was the primary source of sudden capacity loss; instead, consumption and decomposition of electrolyte causes the drastic capacity loss at EOL.

25 ENERGY STORAGE↗

Revisiting the initial irreversible capacity loss of LiNi 0.6 Co 0.2 Mn 0.2 O 2 cathode material batteries

Layered LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622) attracts widespread attention primarily due to its potential for high energy density and moderate thermal stability. However, the low initial coulombic efficiency (ICE) of the material limits the maximum utilization of their capacity. The capacity loss in the first cycle occurs under 4.0V and keep almost constant are considered as common characteristics for NCM-based materials. A clear cognition on the initial capacity loss may light the way to improve the practical reversible capacity of NCM622 at 4.0V. Conducting operando X-ray diffraction during galvanostatic charge/discharge cycling at different temperature (25 degrees C, 45 degrees C and 60 degrees C) and different current (0.1C, 0.01C, 1C=120 mA g -1 ) in the voltage range of 2.7-4.0V, we find that only 8% of the measured initial irreversible capacity loss is associated with parasitic reactions that form cathode/electrolyte interface, and that the dominant contributors include the slow Li + diffusion kinetics (similar to 46% contribution) and irreversible O3/H1-3 phase transition (similar to 46% contribution). Finally, this semi-quantitative study provides new insight on initial capacity loss, guiding further targeted modification and fully utilization of NCM622.

25 ENERGY STORAGE↗

Decoupling first-cycle capacity loss mechanisms in sulfide solid-state batteries

Solid-state batteries (SSBs) promise more energy-dense storage than liquid electrolyte lithium-ion batteries (LIBs). However, first-cycle capacity loss is higher in SSBs than in LIBs due to interfacial reactions. The chemical evolution of key interfaces in SSBs has been extensively characterized. Electrochemically, however, we lack a versatile strategy for quantifying the reversibility of solid electrolyte (SE) redox for established and next-generation SSB electrolytes. In this work, we perform tailored electrochemical tests and operando X-ray diffraction to disentangle reversible and irreversible sources of capacity loss in positive electrodes composed of Li 6 PS 5 Cl SE, Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 (NMC), and carbon conductive additives. We leverage an atypically low voltage cutoff (2.0 V vs. Li/Li + ) to quantify the reversibility of SE redox. Using slow (5.5 mA g NMC −1 ) cycling paired with >100 h low-voltage holds, our cells achieve a surprising 96.2% first-cycle coulombic efficiency, which is higher than previously reported (mean: 72%, maximum: 91.6% across surveyed literature). We clarify that sluggish NMC relithiation kinetics have been historically mistaken for permanently irreversible capacity loss. In conclusion, through systematic decoupling of loss mechanisms, we uncover the unexpected reversibility of SE redox and isolate the major contributors to capacity loss, outlining a strategy for accurate assessment of next-generation SE materials and interface modifications.

54 ENVIRONMENTAL SCIENCES↗

Mathematical Model for Li-S Cell with Shuttling-Induced Capacity Loss Approximation

Lithium sulfur (Li-S) batteries have the potential to outperform the current lithium ion batteries and transform the technology of the future. However, dissolution, diffusion, and shuttling of the dissolved polysulfides result in parasitic reactions and substantial capacity loss. To provide a better understanding of the shuttling process, a 1D porous electrode mathematical model has been developed in this paper. An approximation method is used to account for the shuttling-induced capacity loss by adding an extra source/sink term in the material balance equations for the species involved in the parasitic reactions. Shuttling constants used in the source terms can be determined by fitting the model predictions to the experimental measurements. Here, the results showed that by including the approximation method, the model was able to predict the active material loss and the continuous decrease of volume fractions of Li 2 S on the cathode surface. The model sheds light on the capacity loss mechanism occurring inside the cell as a result of the shuttling of polysulfides.

25 ENERGY STORAGE↗

Connecting the irreversible capacity loss in Li-ion batteries with the electronic insulating properties of solid electrolyte interphase (SEI) components.

The formation and continuous growth of a solid electrolyte interphase (SEI) layer are responsible for the irreversible capacity loss of batteries in the initial and subsequent cycles, respectively. In this article, the electron tunneling barriers from Li metal through three insulating SEI components, namely Li 2 CO 3 , LiF and Li 3 PO 4 , are computed by density function theory (DFT) approaches. Based on electron tunneling theory, it is estimated that sufficient to block electron tunneling. It is also found that the band gap decreases under tension while the work function remains the same, and thus the tunneling barrier decreases under tension and increases under compression. A new parameter, η, characterizing the average distances between anions, is proposed to unify the variation of band gap with strain under different loading conditions into a single linear function of η. An analytical model based on the tunneling results is developed to connect the irreversible capacity loss, due to the Li ions consumed in forming these SEI component layers on the surface of negative electrodes. As a result, the agreement between the model predictions and experimental results suggests that only the initial irreversible capacity loss is due to the self-limiting electron tunneling property of the SEI.

25 ENERGY STORAGE↗

Mitigating the initial capacity loss and improving the cycling stability of silicon monoxide using Li 5 FeO 4

Silicon monoxide (SiO) is a promising next-generation anode material for lithium-ion batteries due to the high capacity it offers. However, such material also exhibits a large initial capacity loss which results in significant loss of Li inventory to irreversible reactions in a full cell. To mitigate the Li inventory loss due to the initial capacity loss of the SiO anode, a prelithiation reagent, Li 5 FeO 4 , is added to the LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523) cathode, which is then paired with a SiO anode for electrochemical evaluation. The addition of Li 5 FeO 4 leads to a significant 22% improvement in lithium utilization in NCM523. Furthermore, the capacity retention of the full cell increased from 90.94% to 98.92% for 50 cycles. We then further studied the impact of Li 5 FeO 4 addition on the energy density of the cell via modeling. In order to maximize the energy density improvement, thicker electrodes need to be utilized.

25 ENERGY STORAGE↗

Nickel hydrogen capacity loss

The results of tests to assess capacity loss in nickel hydrogen cells are presented in outline form. The effects of long storage (greater than 1 month), high hydrogen pressure storage, high cobalt content, and recovery actions are addressed.

Goualard, Jacques↗