At least 19 records

Effects of Imide–Orthoborate Dual-Salt Mixtures in Organic Carbonate Electrolytes on the Stability of Lithium Metal Batteries

The effects of lithium imide and lithium orthoborate dual-salt electrolytes of different salt chemistries in carbonate solvents on the cycling stability of Li metal batteries were systematically and comparatively investigated. Two imide salts (LiTFSI and LiFSI) and two orthoborate salts (LiBOB and LiDFOB) were chosen for this study and compared with the conventional LiPF6 salt. The cycling stability of the Li metal cells with the electrolytes follows the order from good to poor as LiTFSI-LiBOB > LiTFSI-LiDFOB > LiPF6 > LiFSI-LiBOB > LiFSI-LiDFOB, indicating that LiTFSI behaves better than LiFSI and LiBOB over LiDFOB in these four dual-salt mixtures. The LiTFSI-LiBOB can effectively protect the Al substrate and form a more robust surface film on Li metal anode, while the LiFSI-LiBOB results in serious corrosion to the stainless steel cell case and a thicker and looser surface film on Li anode. Computational calculations indicate that the chemical and electrochemical stabilities also follow the order of LiTFSI-LiBOB > LiTFSI-LiDFOB > LiFSI-LiBOB > LiFSI-LiDFOB. The key findings of this work emphasize that the salt chemistry is critically important for enhancing the interfacial stability of Li metal anode and should be carefully manipulated in the development of high performance Li metal batteries.

Li metal batteries, dual-salt electrolyte, solid e↗

A Superior Carbonate Electrolyte for Stable Cycling Li Metal Batteries Using High Ni Cathode

Li metal batteries pairing Li metal anode with high-nickel layer structured oxide cathode are a promising energy storage technology to achieve high energy density. To obtain long cycling life for Li metal batteries, the electrolyte plays a pivotal role in stabilizing both the Li metal anode and the high-nickel cathode upon electrochemical cycling. Herein, we report a carbonate electrolyte that enables a Li||LiNi 0.8 Mn 0.1 Co 0.1 O 2 pouch cell to achieve a high gravimetric energy density of 366 Wh/kg and unprecedented cycling stability with 80% capacity retention after 335 cycles. Here, the 19 F quantitative nuclear magnetic resonance spectroscopy and interface characterization demonstrate that FEC and LiDFOB can reduce the consumption rate of each other and the electrolyte, form a robust LiF-rich SEI on Li metal anode, and improve the microstructure integrity of the high-nickel cathode.

25 ENERGY STORAGE↗

Anion Solvation in Carbonate-Based Electrolytes

The correlation between Li + solvation and interphasial chemistry on anodes firmly established in Li-ion batteries, the effect of cation–solvent interaction has gone beyond bulk thermodynamic and transport properties and become an essential element that determines the reversibility of electrochemistry and kinetics of Li-ion intercalation chemistries. Now, most studies are dedicated to the solvation of Li + , and the solvation of anions in carbonate-based electrolytes and its possible effect on the electrochemical stability of such electrolytes remains little understood. Moreover, as a mirror effort to prior Li + solvation studies, this work focuses on the interactions between carbonate-based solvents and two anions (hexafluorophosphate, PF 6– , and tetrafluoroborate, BF 4– ) that are most frequently used in Li-ion batteries. The possible correlation between such interaction and the interphasial chemistry on cathode surface is also explored.

25 ENERGY STORAGE↗

An Inorganic-Rich Solid Electrolyte Interphase for Advanced Lithium-Metal Batteries in Carbonate Electrolytes

In carbonate electrolytes, the organic-inorganic solid electrolyte interphase (SEI) formed on the lithium (Li) metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here we report, an inorganic-rich SEI is designed on a Li metal surface to reduce its bonding energy with Li metal by dissolving 4 M concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene carbonate (FEC) based electrolyte. Due to the aggregate structure of NO 3 - ions and its participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 - ions. The inorganic-rich SEI’s weak bonding (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping CE of 99.55% (1 mA cm -2 , 1.0 mAh cm -2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm -2 ) to retain 75%of its initial capacity after 200 cycles with an outstanding CE of 99.83%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

An Inorganic‐Rich Solid Electrolyte Interphase for Advanced Lithium‐Metal Batteries in Carbonate Electrolytes

Abstract In carbonate electrolytes, the organic–inorganic solid electrolyte interphase (SEI) formed on the Li‐metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here, an inorganic‐rich SEI is designed on a Li‐metal surface to reduce its bonding energy with Li metal by dissolving 4 m concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene‐carbonate (FEC)‐based electrolyte. Due to the aggregate structure of NO 3 − ions and their participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 − ions. The weak bonding of the SEI (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping Coulombic efficiency of 99.55 % (1 mA cm −2 , 1.0 mAh cm −2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm −2 ) to retain 75 % of its initial capacity after 200 cycles with an outstanding CE of 99.83 %.

Liu, Sufu↗

Lithium-ion hopping weakens thermal stability of LiPF 6 carbonate electrolytes

Lithium hexafluorophosphate (LiPF 6 )-based carbonate electrolytes are widely used in commercial lithium-ion batteries (LIBs), but their thermal instability limits the cycle life and safety of LIBs at elevated temperatures. Few studies have yielded insight into the initial PF 6 — decomposition reaction that promotes thermal instability of LiPF6-based electrolytes. Here, we find that lithium-ion hopping assisted by the overall reorientational motion of propylene carbonate molecules facilitates PF 6 — decomposition at elevated temperatures in 1 M LiPF 6 /propylene carbonate electrolyte. Further, we demonstrate that urea additives, by preventing lithium-ion hopping, suppress the initial LiPF 6 decomposition reaction and enhance the thermal stability of the electrolyte. LIB cell tests with LiNi 0.6 Mn 0.2 Co 0.2 O 2 ||Li 4 Ti 5 O 12 show improved LIB performance at elevated temperatures with the thermally stabilized electrolyte. This study provides key insights into the design of thermally stable LiPF 6 -based carbonate electrolytes for improving the cycle life, calendar life, and safety of LIBs in elevated-temperature applications.

25 ENERGY STORAGE↗

Enabling Non-Carbonate Electrolytes for Silicon Anode Batteries Using Fluoroethylene Carbonate

Silicon is considered as one of the most promising anodes for next generation lithium-ion batteries, due to its high theoretical capacity and energy density. However, many technical barriers remain to its implementation, due to its high chemical/electrochemical reactivities with standard electrolytes and incomplete passivation. In this work, we take the most effective passivating additive of fluoroethylene carbonate (FEC) and study its impact on non-carbonate electrolytes. Our results indicate that esters and ureas-based electrolytes are similarly stabilized by FEC, and have very similar capacity retentions and Coulombic efficiencies to the state-of-the-art carbonate electrolyte. This study indicates the discovery of more efficient additives other than FEC is vital in developing an electrolyte that can successfully enable a silicon-anode battery.

25 ENERGY STORAGE↗

Salt‐in‐Salt Reinforced Carbonate Electrolyte for Li Metal Batteries

Abstract The instability of carbonate electrolyte with metallic Li greatly limits its application in high‐voltage Li metal batteries. Here, a “salt‐in‐salt” strategy is applied to boost the LiNO 3 solubility in the carbonate electrolyte with Mg(TFSI) 2 carrier, which enables the inorganic‐rich solid electrolyte interphase (SEI) for excellent Li metal anode performance and also maintains the cathode stability. In the designed electrolyte, both NO 3 − and PF 6 − anions participate in the Li + ‐solvent complexes, thus promoting the formation of inorganic‐rich SEI. Our designed electrolyte has achieved a superior Li CE of 99.7 %, enabling the high‐loading NCM811||Li (4.5 mAh cm −2 ) full cell with N/P ratio of 1.92 to achieve 84.6 % capacity retention after 200 cycles. The enhancement of LiNO 3 solubility by divalent salts is universal, which will also inspire the electrolyte design for other metal batteries.

Liu, Sufu↗

Salt‐in‐Salt Reinforced Carbonate Electrolyte for Li Metal Batteries

Abstract The instability of carbonate electrolyte with metallic Li greatly limits its application in high‐voltage Li metal batteries. Here, a “salt‐in‐salt” strategy is applied to boost the LiNO 3 solubility in the carbonate electrolyte with Mg(TFSI) 2 carrier, which enables the inorganic‐rich solid electrolyte interphase (SEI) for excellent Li metal anode performance and also maintains the cathode stability. In the designed electrolyte, both NO 3 − and PF 6 − anions participate in the Li + ‐solvent complexes, thus promoting the formation of inorganic‐rich SEI. Our designed electrolyte has achieved a superior Li CE of 99.7 %, enabling the high‐loading NCM811||Li (4.5 mAh cm −2 ) full cell with N/P ratio of 1.92 to achieve 84.6 % capacity retention after 200 cycles. The enhancement of LiNO 3 solubility by divalent salts is universal, which will also inspire the electrolyte design for other metal batteries.

25 ENERGY STORAGE↗

Allotropic control: How certain fluorinated carbonate electrolytes protect aluminum current collectors by promoting the formation of insoluble coordination polymers

Here, there is a strong incentive for increasing the operation voltage of Li-ion cells above 4.5 V in order to increase the density of stored energy. Aluminum is an inexpensive, lightweight metal that is commonly used as a positive electrode current collector in these cells. Imide LiX salts, such as lithium bis(trifluoromethylsulfonyl)imide (X = TFSI), and lithium bis(fluorosulfonyl)imide (X = FSI), are chemically stable on the energized lithiated transition metal oxide electrodes, but their presence in the electrolyte causes rapid anodic dissolution and pitting of Al current collectors at potentials exceeding 4.0 V versus Li/Li + . For LiBF 4 and LiPF 6 , the release of HF near the energized surfaces passivates the exposed Al metal, inhibiting this pitting corrosion, but it also causes the gradual degradation of the cathode active material, negating this important advantage. Here we report that in certain electrolytes containing fluorinated carbonate solvents and LiX salts, the threshold voltage for safe operation of Al current collectors can be increased to 5.5 V versus Li/Li + . Interestingly, the most efficient solvent also facilitates the formation of an insoluble gel when AlX 3 is introduced into this solvent. We suggest that this solvent promotes the aggregation of coordination polymers of AlX 3 at the exposed Al surface that isolate this surface from the electrolyte, thereby preventing further Al dissolution and corrosion. Other examples of Al collector protection may also involve this mechanism. Our study suggests that such “allotropic control” could be a way of widening the operation window of Li-ion cells without electrode deterioration, Al current collector corrosion, and electrolyte breakdown.

36 MATERIALS SCIENCE↗

Electrochemical Reactivity and Passivation of Silicon Thin-Film Electrodes in Organic Carbonate Electrolytes

This work focuses on the mechanisms of interfacial processes at the surface of amorphous silicon thin-film electrodes in organic carbonate electrolytes to unveil the origins of the inherent nonpassivating behavior of silicon anodes in Li-ion batteries. Attenuated total reflection Fourier-transform infrared spectroscopy, X-ray absorption spectroscopy, and infrared near-field scanning optical microscopy were used to investigate the formation, evolution, and chemical composition of the surface layer formed on Si upon cycling. Herein, we found that the chemical composition and thickness of the solid/electrolyte interphase (SEI) layer continuously change during the charging/discharging cycles. This SEI layer “breathing” effect is directly related to the formation of lithium ethylene dicarbonate (LiEDC) and LiPF6 salt decomposition products during silicon lithiation and their subsequent disappearance upon delithiation. Furthermore, the detected appearance and disappearance of LiEDC and LiPF6 decomposition compounds in the SEI layer are directly linked with the observed interfacial instability and poor passivating behavior of the silicon anode.

25 ENERGY STORAGE↗

Nonflammable Lithium Metal Full Cells with Ultra-high Energy Density Based on Coordinated Carbonate Electrolytes

Coupling thin Li metal anodes with high-capacity/high-voltage cathodes such as LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NCM811) is a promising way to increase lithium battery energy density. Yet, the realization of high-performance full cells remains a formidable challenge. Here, we demonstrate a new class of highly coordinated, nonflammable carbonate electrolytes based on lithium bis(fluorosulfonyl)imide (LiFSI) in propylene carbonate/fluoroethylene carbonate mixtures. Utilizing an optimal salt concentration (4 M LiFSI) of the electrolyte results in a unique coordination structure of Li + -FSI - -solvent cluster, which is critical for enabling the formation of stable interfaces on both the thin Li metal anode and high-voltage NCM811 cathode. Under highly demanding cell configuration and operating conditions (Li metal anode = 35 μm, areal capacity/charge voltage of NCM811 cathode = 4.8 mAh cm -2 /4.6 V, and anode excess capacity [relative to the cathode] = 0.83), the Li metal-based full cell provides exceptional electrochemical performance (energy densities = 679 Wh kg cell -1 /1,024 Wh L cell -1 ) coupled with nonflammability.

25 ENERGY STORAGE↗

Performance Leap of Lithium Metal Batteries in LiPF 6 Carbonate Electrolyte by a Phosphorus Pentoxide Acid Scavenger

Phosphorus pentoxide (P 2 O 5 ) is investigated as an acid scavenger to remove the acidic impurities in a commercial lithium hexafluorophosphate (LiPF 6 ) carbonate electrolyte to improve the electrochemical properties of Li metal batteries. Nuclear magnetic resonance (NMR) measurements reveal the detailed reaction mechanisms of P 2 O 5 with the LiPF 6 electrolyte and its impurities, which removes hydrogen fluoride (HF) and difluor-ophosphoric acid (HPO 2 F 2 ) and produces phosphorus oxyfluoride (POF 3 ), OF 2 P-O-PF 5 - anions, and ethyl difluorophosphate (C 2 H 5 OPOF 2 ) as new electrolyte species. The P 2 O 5 -modified LiPF 6 electrolyte is chemically compatible with a Li metal anode and LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) cathode, generating a PO x F y -rich solid electrolyte interphase (SEI) that leads to highly reversible Li electrodeposition, while eliminating transition metal dissolution and cathode particle cracking. The excellent electrochemical properties of the P 2 O 5 -modified LiPF6 electrolytes are demonstrated on Li||NMC622 pouch cells with 0.4 Ah capacity, 50 mu m Li anode, 3 mAh cm -2 NMC622 cathode, and 3 g Ah -1 electrolyte/capacity ratio. The pouch cells can be galvanostatically cycled at C/3 for 230 cycles with 87.7% retention.

25 ENERGY STORAGE↗

Solubility-mediated sustained release enabling nitrate additive in carbonate electrolytes for stable lithium metal anode

Here, the physiochemical properties of the solid-electrolyte interphase, primarily governed by electrolyte composition, have a profound impact on the electrochemical cycling of metallic lithium. Herein, we discover that the effect of nitrate anions on regulating lithium deposition previously known in ether-based electrolytes can be extended to carbonate-based systems, which dramatically alters the nuclei from dendritic to spherical, albeit extremely limited solubility. This is attributed to the preferential reduction of nitrate during solid-electrolyte interphase formation, and the mechanisms behind which are investigated based on the structure, ion-transport properties, and charge transfer kinetics of the modified interfacial environment. To overcome the solubility barrier, a solubility-mediated sustained-release methodology is introduced, in which nitrate nanoparticles are encapsulated in porous polymer gel and can be steadily dissolved during battery operation to maintain a high concentration at the electroplating front. As such, effective dendrite suppression and remarkably enhanced cycling stability are achieved in corrosive carbonate electrolytes.

25 ENERGY STORAGE↗

Dendrite–Free Potassium Metal Anodes in a Carbonate Electrolyte

Potassium (K) metal anodes suffer from a challenging problem of dendrite growth. In this study, it is demonstrated that a tailored current collector will stabilize the metal plating–stripping behavior even with a conventional KPF 6 –carbonate electrolyte. A 3D copper current collector is functionalized with partially reduced graphene oxide to create a potassiophilic surface, the electrode being denoted as rGO@3D–Cu. Potassiophilic versus potassiophobic experiments demonstrate that molten K fully wets rGO@3D–Cu after 6 s, but does not wet unfunctionalized 3D–Cu. Electrochemically, a unique synergy is achieved that is driven by interfacial tension and geometry: the adherent rGO underlayer promotes 2D layer–by–layer (Frank–van der Merwe) metal film growth at early stages of plating, while the tortuous 3D–Cu electrode reduces the current density and geometrically frustrates dendrites. The rGO@3D–Cu symmetric cells and half–cells achieve state–of–the–art plating and stripping performance. Here, the symmetric rGO@3D–Cu cells exhibit stable cycling at 0.1–2 mA cm –2 , while baseline Cu prematurely fails when the current reaches 0.5 mA cm –2 . The half–cells cells of rGO@3D–Cu (no K reservoir) are stable at 0.5 mA cm –2 for 10 000 min (100 cycles), and at 1 mA cm –2 for 5000 min. The baseline 3D–Cu, planar rGO@Cu, and planar Cu foil fails after 5110, 3012, and 1410 min, respectively.

25 ENERGY STORAGE↗

The Effect of the SEI Layer Mechanical Deformation on the Passivity of a Si Anode in Organic Carbonate Electrolytes

The solid electrolyte interphase (SEI) on a Si negative electrode in carbonate-based organic electrolytes shows intrinsically poor passivating behavior, giving rise to unsatisfactory calendar life of Li-ion batteries. Moreover, mechanical strains induced in the SEI due to large volume changes of Si during charge-discharge cycling could contribute to its mechanical instability and poor passivating behavior. This study elucidates the influence that static mechanical deformation of the SEI has on the rate of unwanted parasitic reactions at the Si/electrolyte interface as a function of electrode potential. Further, the experimental approach involves the utilization of Si thin-film electrodes on substrates with disparate elastic moduli, which either permit or suppress the SEI deformation in response to Si volume changes upon charging-discharging. We find that static mechanical stretching and deformation of the SEI results in an increased parasitic electrolyte reduction current on Si. Furthermore, attenuated total reflection and near-field Fourier-transform infrared nanospectroscopy reveal that the static mechanical stretching and deformation of the SEI fosters a selective transport of linear carbonate solvent through, and nanoconfinement within, the SEI. These, in turn, promote selective solvent reduction and continuous electrolyte decomposition on Si electrodes, reducing the calendar life of Si anode-based Li-ion batteries. Finally, possible correlations between the structure and chemical composition of the SEI layer and its mechanical and chemical resilience under prolonged mechanical deformation are discussed in detail.