The effect of ink ball milling time on interparticle interactions and ink microstructure and their influence on crack formation in rod-coated catalyst layers

This work investigates the influence of ballmilling (sometimes also referred to as jar roller milling) time on cathode catalyst layer (CL) inks and electrode properties using formulations and coating methods relevant for industrial manufacturing. Four CL inks with the same composition were milled for 24, 48, 72, or 96 h. Rheological investigation of these inks showed a reduction of elastic moduli and steady-shear viscosity with continuous ink milling, which is correlated to a decrease in particle-particle interactions as well as formation of smaller agglomerates. Optical microscopy (OM) analysis of the fabricated electrodes revealed a trend in surface crack formation; formulations milled for 24 h contained the lowest average surface crack area percentages of 0.370% at heavy-duty loadings of ~0.300 mg Pt cm -2 , compared to 2.418% for the ink milled for 96 h. Further characterization of the CL through transmission electron microscopy (TEM) imaging showed a decrease in the mean agglomerate and pore size with milling time. Furthermore, these smaller electrode features were consistent with reduced fracture resistance and, hence, development of larger stresses during drying. Our results highlight the need to consider ink processing as an important component in defect-free CL manufacturing.

30 DIRECT ENERGY CONVERSION↗

Advanced electrode manufacturing to enable low cost PEM electrolysis

A critical challenge for the implementation of proton exchange membrane (PEM)-based water electrolyzers for the H2@Scale vision is the capital cost, which is largely driven by related factors of overdesign and highly manual legacy manufacturing methods. Typical electrolyzer cells have an order of magnitude higher membrane thickness and catalyst loading vs. fuel cells, in part because the manufacturing methods being used are not capable of producing uniform and reliable electrodes on thin membranes with low loading. Advanced electrode manufacturing is therefore the key enabler to reduce the cost of the electrolyzer stack, particularly roll-to-roll (R2R) manufacturing of catalyst coated layers (CCLs) and catalyst coated membranes (CCMs). The electrolyzer manufacturing process still relies on traditional sheet-to-sheet (S2S) processes, which requires intensive labor to make parts to meet the specification requirements. This project leverages fuel cell expertise (GM) with Proton’s knowledge of electrolyzer components to develop the electrocatalyst ink formulations and coating processes using slot die (ORNL) and gravure (NREL) coatings, with proof of concept at the pilot-scale (Kodak).

08 HYDROGEN↗

Influence of Coating Method on the Performance of Roll-to-Roll Coated PEM Fuel Cell Catalyst Layers

As production of fuel cell vehicles and power systems increases there is a need to understand the process science of fuel cell manufacturing. Industrial production of polymer electrolyte membrane fuel cell (PEMFC) electrodes will rely on continuous roll-to-roll (R2R) coating methods to meet the rates needed for mass production. There are a variety of coating methods that could be used to coat catalyst layers. The different physics of each method may result in different morphologies and performance. Here we present the results of a study comparing fuel cell catalyst layers coated using two R2R coating methods: slot-die and gravure. These two methods were selected because the physics of applying the liquid to the substrate is very different between the two cases. Pt/C catalysts layers were coated directly onto carbon-fiber gas diffusion media to create gas diffusion electrodes (GDEs), without the use of a decal transfer process. These GDEs were assembled into membrane electrode assemblies (MEAs) by hot pressing to Nafion membranes. In situ performance and other electrochemical diagnostics were used to determine the influence of coating method on catalyst layer electrochemical properties. Electron microscopy was utilized to understand the influence of coating method on electrode morphology and its influence on electrochemical properties. We also explored the influence of solvent ratio to understand the potential coupling between ink formulation and coating methodology.

DIRECT ENERGY CONVERSION,MATERIALS SCIENCE↗

Prediction of Performance Variation Caused by Manufacturing Tolerances and Defects in Gas Diffusion Electrodes of Phosphoric Acid (PA)–Doped Polybenzimidazole (PBI)-Based High-Temperature Proton Exchange Membrane Fuel Cells

The automated process of coating catalyst layers on gas diffusion electrodes (GDEs) for high-temperature proton exchange membrane fuel cells results inherently into a number of defects. These defects consist of agglomerates in which the platinum sites cannot be accessed by phosphoric acid and which are the consequence of an inconsistent coating, uncoated regions, scratches, knots, blemishes, folds, or attached fine particles—all ranging from μm to mm size. These electrochemically inactive spots cause a reduction of the effective catalyst area per unit volume (cm2/cm3) and determine a drop in fuel cell performance. A computational fluid dynamics (CFD) model is presented that predicts performance variation caused by manufacturing tolerances and defects of the GDE and which enables the creation of a six-sigma product specification for Advent phosphoric acid (PA)-doped polybenzimidazole (PBI)-based membrane electrode assemblies (MEAs). The model was used to predict the total volume of defects that would cause a 10% drop in performance. It was found that a 10% performance drop at the nominal operating regime would be caused by uniformly distributed defects totaling 39% of the catalyst layer volume (~0.5 defects/μm2). The study provides an upper bound for the estimation of the impact of the defect location on performance drop. It was found that the impact on the local current density is higher when the defect is located closer to the interface with the membrane. The local current density decays less than 2% in the presence of an isolated defect, regardless of its location along the active area of the catalyst layer.

Gurau, Vladimir (ORCID:0000000327429061)↗

Slot-die-coating operability windows for polymer electrolyte membrane fuel cell cathode catalyst layers

Roll-to-roll (R2R) slot-die coating of polymer electrolyte membrane fuel cell (PEMFC) catalyst layers represents a scalable deposition method for producing 10–20 m 2 ·min -1 of catalyst-coated gas diffusion layers (GDLs). This high-throughput production technique will help lower the cost of PEMFC catalyst layers. The uniformity of the wet layer applied by slot die deposition is affected by process parameters such as substrate speed, vacuum pressure applied at the upstream meniscus, gap between the slot die lips and substrate, ink rheology, and other ink and substrate properties. The set of conditions for producing a defect-free coating with a dilute ink typically requires little to no upstream vacuum pressure, so suitable operating conditions can be found easily through trial and error and operator intuition. However, the higher viscosity of more concentrated inks dramatically shifts the range of settings that result in a homogeneous coating to higher vacuum levels, which are harder to find through hit or miss. A predictive model showing the range of operable conditions decreases material wastage inherent in experimentally searching for suitable parameters. In this study, the defect-free coating parameter window is explored experimentally and theoretically for two concentrations of PEFC cathode inks. Both a full capillary hydrodynamic model and a computationally cheaper viscocapillary model successfully predict the experimentally determined coating window within the experimental and model uncertainty limits for inks with 5.3 wt% and 12.0 wt% solids ink while maintaining the 0.1 mg Pt ·cm -2 Pt areal loading target. Here, this paper demonstrates a viable pathway for meeting the $30/kW net ultimate cost target of the United States Department of Energy (U.S. DOE) Hydrogen Fuel Cells Technologies Office (HFTO). The concentrated ink lowers the thermal energy and capital expenditure (CapEx) budget of the coating process by decreasing the amount of time, energy, and floorspace required for drying the coating.

25 ENERGY STORAGE↗

Uniformity, performance, and durability of roll-to-roll-coated iridium oxide electrolyzer catalyst layers

This work investigates the use of roll-to-roll coating methods for the production of iridium oxide catalyst layers for proton exchange membrane water electrolyzers. Catalyst layers were produced using two coating methods: slot die and gravure. By varying the solids content of the catalyst ink and coating process variables loadings between 0.08 and 0.64 mg Ir cm −2 were prepared with relatively high spatial uniformity. However, at loadings below 0.2 mg Ir cm −2 microscopy reveals voids in the catalyst layer due to similar length scales of catalyst agglomerates and overall layer thickness. Electrochemical testing shows that these voids do not impact initial membrane electrode assembly performance but lead to increased performance losses after potential cycling compared to spray coated catalyst layers.

08 HYDROGEN↗

Impact of polymer additives on crack mitigation of rod-coated fuel cell cathode catalyst layers

Cracks in catalyst layers (CLs) are a potential source of long-term failure in a fuel cell membrane electrode assembly (MEA). While modifications to the CL ink formulation can affect the degree of cracking, these changes may lead to lower initial performance than their cracked analogues due to the established link between formulation and performance. In this work, we explored the use of polymeric additives to mitigate CL cracks. Small quantities of poly (acrylic acid), poly (ethylene oxide), poly (methyl methacrylate), or poly (vinyl alcohol) - 5 wt% relative to ionomer mass - were added to the ink prior to its final mixing. Poly (vinyl alcohol) resulted in crack-free CLs, whereas the other polymers resulted in CLs with similar crack percentages as the control CL. Through a combination of transmission electron microscopy, X-ray computed tomography, and infrared spectroscopy, we ascribed the crack-mitigating mechanism of poly (vinyl alcohol) to its ability to hydrogen-bond with Nafion, the ion conducting polymer binder in the catalyst ink. Initial performance of this non-cracked electrode exhibited nearly identical electrochemical behavior to its cracked counterpart, demonstrating that PVA additives successfully reduce cracks while maintaining cell initial performance.

30 DIRECT ENERGY CONVERSION↗

Towards improved conversion of wet waste to jet fuel with atomic layer deposition-coated hydrodeoxygenation catalysts

The conversion of wet waste-derived volatile fatty acids into jet fuel-range hydrocarbons is a promising route for increasing the production of sustainable aviation fuel; however, the cost and moderate alkane selectivity of Pt-based hydrodeoxygenation catalysts present challenges for commercialization. Here, to address this, we used atomic layer deposition to apply TiO 2 overcoats to Pt/Al 2 O 3 catalysts and create new interface sites that exhibited 8 times higher site time yield of the desirable n-alkane product than uncoated catalyst. Through TPR/TPD, XPS, CO DRIFTS, and DFT calculations, we found that the increased selectivity of the ALD-coated catalyst was due to the creation of O vacancies at the Pt-TiO 2 interface under reducing conditions, resulting in new Ti 3+ acid sites near the active metal. Maximum conversion and alkane selectivity during HDO was achieved with an ALD-coated 0.5% wt Pt catalyst, indicating that TiO 2 ALD can be used to maximize the utility of precious-metal catalysts.

09 BIOMASS FUELS↗

Fabrication of high-performance gas-diffusion-electrode based membrane-electrode assemblies

This paper demonstrates the fabrication and processing steps required to produce high performance fuel cell membrane electrode assemblies (MEAs) based on spray-coated gas-diffusion electrodes (GDEs). It is demonstrated that coating the catalyst layer with a thin layer of ionomer and then hot pressing the GDEs to the membrane is required to achieve comparable catalyst activity and air performance to catalyst-coated-membrane MEAs. We show that there is a critical amount of ionomer required to achieve maximized performance. Using electron microscopy, we show that the combination of the ionomer overlayer and hot-pressing bonds the catalyst layer to the membrane, increasing the interfacial contact area and quality of this interface. We also find that the ionomer overlayer smooths the surface of the GDE and provides increased contact area between the GDE and the membrane. Additionally, we demonstrate that much less ionomer is required for high-performance than has been previously reported. Through model fitting of electrochemical impedance spectroscopy, we show that this improvement in the catalyst layer - membrane interface reduces the effective catalyst layer resistance, which reduces Ohmic losses and increases catalyst utilization.

33 ADVANCED PROPULSION SYSTEMS↗

Roll-to-roll production of catalyst coated membranes for low-temperature electrolyzers

Here we demonstrate a roll-to-roll (R2R) process for direct coating of anode catalyst layers on a polymer electrolyte membrane for low-temperature water electrolysis. To develop this process, we studied catalyst ink formulation, ink-membrane interactions, and coating quality. The catalyst inks were a mixture of iridium oxide (IrO2) and Nafion in a water and alcohol dispersion medium. The type of alcohol (methanol, ethanol, propanols) and water-to-alcohol ratio were varied to determine their influence on membrane swelling, dispersion quality, and coatability. Interactions of the ink dispersion medium with the membrane were characterized using sessile-drop contact-angle measurements. These measurements show that the ratio of water to alcohol has a strong influence on how rapidly the dispersion media is absorbed by the membrane. Rheology of the catalyst inks was measured to understand the microstructure of the catalyst particles in the ink. This analysis found that 1-propanol leads to better dispersion of the IrO2 particles than ethanol. Small-scale coating samples were prepared to understand coating uniformity and formation of irregularities. Subsequently, two water/1-propanol ratios (90:10 and 75:25) were down-selected for large-scale R2R slot die coating. The R2R catalyst-coated membrane (CCM) coating process increased catalyst layer production throughput by over 500x compared to our standard lab-scale spray coating. The CCMs obtained from this process were tested as single-cell membrane electrode assemblies. They exhibited a cell voltage of 1.91 V at a current density of 2 A/cm2, which is comparable to spray-coated CCMs. In conclusion, the work presented here demonstrates a continuous, scalable manufacturing process that eliminates the need for the decal transfer step typically used in CCM production.

42 ENGINEERING↗

Improved Cathode Structure for a Direct Methanol Fuel Cell

An improved cathode structure on a membrane/electrode assembly has been developed for a direct methanol fuel cell, in a continuing effort to realize practical power systems containing such fuel cells. This cathode structure is intended particularly to afford better cell performance at a low airflow rate. A membrane/electrode assembly of the type for which the improved cathode structure was developed (see Figure 1) is fabricated in a process that includes brush painting and spray coating of catalyst layers onto a polymer-electrolyte membrane and onto gas-diffusion backings that also act as current collectors. The aforementioned layers are then dried and hot-pressed together. When completed, the membrane/electrode assembly contains (1) an anode containing a fine metal black of Pt/Ru alloy, (2) a membrane made of Nafion 117 or equivalent (a perfluorosulfonic acid-based hydrophilic, proton-conducting ion-exchange polymer), (3) a cathode structure (in the present case, the improved cathode structure described below), and (4) the electrically conductive gas-diffusion backing layers, which are made of Toray 060(TradeMark)(or equivalent) carbon paper containing between 5 and 6 weight percent of poly(tetrafluoroethylene). The need for an improved cathode structure arises for the following reasons: In the design and operation of a fuel-cell power system, the airflow rate is a critical parameter that determines the overall efficiency, cell voltage, and power density. It is desirable to operate at a low airflow rate in order to obtain thermal and water balance and to minimize the size and mass of the system. The performances of membrane/electrode assemblies of prior design are limited at low airflow rates. Methanol crossover increases the required airflow rate. Hence, one way to reduce the required airflow rate is to reduce the effect of methanol crossover. Improvement of the cathode structure - in particular, addition of hydrophobic particles to the cathode - has been demonstrated to mitigate the effects of crossover and decrease the airflow required.

Valdez, Thomas↗

Influence of Ink Formulation and Drying Conditions on Ionomer Distribution in High-Performance Roll-to-Roll-Coated Gas-Diffusion Electrodes

To enable mass production of fuel cell membrane electrode assemblies (MEAs) catalyst layers production will require continuous roll-to-roll (R2R) coating processes. Gas diffusion electrodes (GDEs) are advantageous for mass production because the catalyst layer can be directely coated on the microporous layer of the gas diffusion media without the need for a decal-transfer process. It is known that the water-to-alcohol ratio in the catalyst ink influences the interactions of the ionomer with the catalyst leading to different distributions of ionomer in spray-coated catalyst layers. It is also known that during drying of colloidal mixtures, like fuel cell inks, factors such as drying rate, particle size, and agglomeration influence how the materials distribute themselves throughout the thickness of the dired film. Thus far there have only been limited studies to understand how process conditions such as ink formulation and drying temperature influence the distribution of ionomer and catalyst coated using scalable methods. This understanding is especially important for GDEs since it is known that having a sufficient amount of ionomer at the catalyst layer-membrane interface is critical for high performance. In this study we have focused on determining how the ratio of water to 1-propanol in the catalyst ink ink and drying temperature influence the distribution of ionomer throughout the thickness of the catalyst layer. Using a combination of Kelvin probe and x-ray photoelectron spectroscopy we show that an ionomer-rich surface is promoted by a higher drying rate and a water-rich catalyst ink. In contrast, a 1-propanol catalyst ink leads to a lower concentration of ionomer on the top surface. Using x-ray computed tomography, we are able to characterize the ionomer distribution throughout the thickness of the layer. We find that, in addition to promoting an ionomer-rich top surface, water-rich inks lead to a more homogenous distribution of ionomer, whereas a 1-propanol-rich ink leads to a more irregular distribution. It is found that MEA performance is improved by selecting conditions and ink formulations that promote ionomer enrichment at the top surface to facilitate a good interface with the membrane. MEAs prepared with a 75 wt% water catalyst ink with a 0.9 I/C have equivalent performance to spray-coated GDEs. Critically, these R2R-coated GDEs do not need an additional ionomer overlayer like the spray-coated GDEs do, reducing the number of processing steps in a manufacturing setting. This work shows that with the appropriate selection of materials, ink formulation, and processing conditions gas-diffusion electrodes are a viable pathway for fuel cell manufacturing.

ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATION↗

Tuning Catalyst Activation and Utilization Via Controlled Electrode Patterning for Low-Loading and High-Efficiency Water Electrolyzers

An anode electrode concept of thin catalyst-coated liquid/gas diffusion layers (CCLGDLs), by integrating Ir catalysts with Ti thin tunable LGDLs with facile electroplating in proton exchange membrane electrolyzer cells (PEMECs), is proposed. The CCLGDL design with only 0.08 mg Ir cm -2 can achieve comparative cell performances to the conventional commercial electrode design, saving ~97% Ir catalyst and augmenting a catalyst utilization to ~24 times. CCLGDLs with regulated patterns enable insight into how pattern morphology impacts reaction kinetics and catalyst utilization in PEMECs. A specially designed two-sided transparent reaction-visible cell assists the in situ visualization of the PEM/electrode reaction interface for the first time. Oxygen gas is observed accumulating at the reaction interface, limiting the active area and increasing the cell impedances. In this work, it is demonstrated that mass transport in PEMECs can be modified by tuning CCLGDL patterns, thus improving the catalyst activation and utilization. The CCLGDL concept promises a future electrode design strategy with a simplified fabrication process and enhanced catalyst utilization. Furthermore, the CCLGDL concept also shows great potential in being a powerful tool for in situ reaction interface research in PEMECs and other energy conversion devices with solid polymer electrolytes.

08 HYDROGEN↗

Impact of Porous Transport Layer In-Plane Conduction on Spatially Resolved Current and EIS Measurements in a Proton Exchange Membrane Water Electrolyzer

An XY segmented cell was developed for low temperature PEM water electrolysis (PEMWE). The system can assess the local performance by enabling in situ measurements of spatial currents and impedances. In this work, we show through experiments, as well as through modelling work, that the porous transport layer (PTL) must be segmented to eliminate crosstalk. Accurate measurements are only possible when crosstalk is fully eliminated. The XY segmented cell is applied to a case study characterizing the impact of a PTL platinum coating void on spatial performance. The localized performance impact of the coating void is found to be orientation specific: coating voids facing the catalyst layer reduce performance significantly more than coating voids facing the flow field. The results suggest that the tolerances for PTL coating uniformity can be lower at the side facing the flow field. The work showcases the feasibility of the XY segmented cell for impact assessment studies. The presented XY segmented cell enables the characterization of spatial phenomena in PEMWE devices and is envisioned to support modeling efforts and the investigation of manufacturing related tolerances for mass produced PEMWE devices.

08 HYDROGEN↗

Catalyst layer formulations for slot-die coating of PEM fuel cell electrodes

The series of electrodes were fabricated by the scalable and manufacturable slot-die coating method for proton exchange membrane fuel cell (PEMFC) application. The inks with different amounts of solids were studied by rheological methods in order to establish a coating window with minimum manufacturing defects. The obtained electrodes were characterized by SEM, AFM, and optical microscopy, which showed that they were uniform and homogeneous with minimum defects. The electrochemical evaluation of the manufactured gas diffusion electrodes (GDE) showed that the main characteristics of the electrodes, like electrochemical surface area, proton resistivity, and double layer capacitance, were found to be close for all samples confirming the reproducibility of the slot-die process. Additionally, we studied the effects of membrane thickness on the performance of the GDE membrane electrode assemblies and determined that a decrease in membrane thickness favored the performance. Furthermore, the obtained results clearly demonstrated the applicability and feasibility of the approach for the Manufacturing of catalyst layers for the fuel cell application with potential for future mass production.