Development of processing techniques for advanced thermal protection materials

The main purpose of this work has been in the development and characterization of materials for high temperature applications. Thermal Protection Systems (TPS) are constantly being tested, and evaluated for increased thermal shock resistance, high temperature dimensional stability, and tolerance to environmental effects. Materials development was carried out through the use of many different instruments and methods, ranging from extensive elemental analysis to physical attributes testing. The six main focus areas include: (1) protective coatings for carbon/carbon composites; (2) TPS material characterization; (3) improved waterproofing for TPS; (4) modified ceramic insulation for bone implants; (5) improved durability ceramic insulation blankets; and (6) ultra-high temperature ceramics. This report describes the progress made in these research areas during this contract period.

Selvaduray, Guna S.↗

Ion Beam Sputtered Coatings of Bioglass

The ion beam sputtering technique available at the NASA-Lewis was used to apply coatings of bioglass to ceramic, metallic, and polymeric substrates. Experiments in vivo and in vitro described investigate these coatings. Some degree of substrate masking was obtained in all samples although stability and reactivity equivalent to bulk bioglass was not observed in all coated samples. Some degree of stability was seen in all coated samples that were reacted in vitro. Both metallic and ceramic substrates coated in this manner failed to show significantly improved coatings over those obtained with existing techniques. Implantation of the coated ceramic substrate samples in bone gave no definite bonding as seen with bulk glass; however, partial and patchy bonding was seen. Polymeric substrates in these studies showed promise of success. The coatings applied were sufficient to mask the underlying reactive test surface and tissue adhesion of collagen to bioglass was seen. Hydrophilic, hydrophobic, charged, and uncharged polymeric surfaces were successfully coated.

Hench, Larry L.↗

Resources for a lunar base: Rocks, minerals, and soil of the Moon

The rocks and minerals of the Moon will be included among the raw materials used to construct a lunar base. The lunar regolith, the fragmental material present on the surface of the Moon, is composed mostly of disaggregated rocks and minerals, but also includes glassy fragments fused together by meteorite impacts. The finer fraction of the regolith (i.e., less than 1 cm) is informally referred to as soil. The soil is probably the most important portion of the regolith for use at a lunar base. For example, soil can be used as insulation against cosmic rays, for lunar ceramics and abodes, or for growing plants. The soil contains abundant solar-wind-implanted elements as well as various minerals, particularly oxide phases, that are of potential economic importance. For example, these components of the soil are sources of oxygen and hydrogen for rocket fuel, helium for nuclear energy, and metals such as Fe, Al, Si, and Ti.

Taylor, Lawrence A.↗

Status and directions of modified tribological surfaces by ion processes

An overview is presented of recent advances in modifying contacting surfaces in motion by the various ion assisted surface coating/modification processes to reduce and control tribological failures. The ion assisted coating processes and the surface modification processes offer the greatest potential to custom tailor and optimize the tribological performance. Hard, wear resistant and low shear coatings deposited by the ion assisted processes are discussed. Primarily the recent advances of sputtered MoS2 ion plated Au, Ag, Pb lubricating films and sputtered and ion plated hard, wear resistant TiN, HfN, TiC films are described in terms of structural property performance interrelationships which lead to improved adhesion, cohesion, nucleation, morphological growth, density, film thickness as determined by structural and chemical characterization and frictional and wear behavior. Also, the recent tribological advances using the surface modification processes such as ion implantation, ion beam mixing is discussed with emphasis on the development of lubricous high temperature ceramic surfaces.

Spalvins, Talivaldis↗

Reliability of scanning laser acoustic microscopy for detecting internal voids in structural ceramics

The reliability of 100 MHz scanning laser acoustic microscopy (SLAM) for detecting internal voids in sintered specimens of silicon nitride and silicon carbide was evaluated. The specimens contained artificially implanted voids and were positioned at depths ranging up to 2 mm below the specimen surface. Detection probability of 0.90 at a 0.95 confidence level was determined as a function of material, void diameter, and void depth. The statistical results presented for void detectability indicate some of the strengths and limitations of SLAM as a nondestructive evaluation technique for structural ceramics.

Roth, D. J.↗

Reliability of scanning laser acoustic microscopy for detecting internal voids in structural ceramics

The reliability of 100 MHz scanning laser acoustic microscopy (SLAM) for detecting internal voids in sintered specimens of silicon nitride and silicon carbide was evaluated. The specimens contained artificially implanted voids and were positioned at depths ranging up to 2 mm below the specimen surface. Detection probability of 0.90 at a 0.95 confidence level was determined as a function of material, void diameter, and void depth. The statistical results presented for void detectability indicate some of the strengths and limitations of SLAM as a nondestructive evaluation technique for structural ceramics.

Roth, D. J.↗

Physical and Tribological Characteristics of Ion-Implanted Diamond Films

Unidirectional sliding friction experiments were conducted with a natural, polished diamond pin in contact with both as-deposited and carbon-ion-implanted diamond films in ultrahigh vacuum. Diamond films were deposited on silicon, silicon carbide, and silicon nitride by microwave-plasma-assisted chemical vapor deposition. The as-deposited diamond films were impacted with carbon ions at an accelerating energy of 60 keV and a current density of 50 micron A/cm(exp 2) for approximately 6 min, resulting in a dose of 1.2 x 10(exp 17) carbon ions/cm(exp 2). The results indicate that the carbon ion implantation produced a thin surface layer of amorphous, nondiamond carbon. The nondiamond carbon greatly decreased both friction and wear of the diamond films. The coefficients of friction for the carbon-ion-implanted, fine-grain diamond films were less than 0.1, factors of 20 to 30 lower than those for the as-deposited, fine-grain diamond films. The coefficients of friction for the carbon-ion-implanted, coarse-grain diamond films were approximately 0.35, a factor of five lower than those for the as-deposited, coarse-grain diamond films. The wear rates for the carbon-ion-implanted, diamond films were on the order of 10(exp -6) mm(exp 3)/Nm, factors of 30 to 80 lower than that for the as-deposited diamond films, regardless of grain size. The friction of the carbon-ion-implanted diamond films was greatly reduced because the amorphous, nondiamond carbon, which had a low shear strength, was restricted to the surface layers (less than 0.1 micron thick) and because the underlying diamond materials retained their high hardness. In conclusion, the carbon-ion-implanted, fine-grain diamond films can be used effectively as wear resistant, self-lubricating coatings for ceramics, such as silicon nitride and silicon carbide, in ultrahigh vacuum.

Miyoshi, K.↗

Effect of surface texture by ion beam sputtering on implant biocompatibility and soft tissue attachment

The objectives in this report were to use the ion beam sputtering technique to produce surface textures on polymers, metals, and ceramics. The morphology of the texture was altered by varying both the width and depth of the square pits which were formed by ion beam erosion. The width of the ribs separating the pits were defined by the mask used to produce the texture. The area of the surface containing pits varies as the width was changed. The biological parameters used to evaluate the biological response to the texture were: (1) fibrous capsule and inflammatory response in subcutaneous soft tissue; (2) strength of the mechanical attachment of the textured surface by the soft tissue; and (3) morphology of the epidermal layer interfacing the textured surface of percutaneous connectors. Because the sputter yield on teflon ribs was approximately an order of magnitude larger than any other material the majority of the measurements presented in the report were obtained with teflon.

Gibbons, D. F.↗

Application of modern surface analytical tools in the investigation of surface deterioration processes

Surface profilometry and scanning electron microscopy were utilized to study changes in the surface of polymers when eroded. The X-ray photoelectron spectroscopy (XPS) and depth profile analysis indicate the corrosion of metal and ceramic surfaces and reveal the diffusion of certain species into the surface to produce a change in mechanical properties. Ion implantation, nitriding and plating and their effects on the surface are characterized. Auger spectroscopy analysis identified morphological properties of coatings applied to surfaces by sputter deposition.

Buckley, D. H.↗

Sliding seal materials for low heat rejection engines

Sliding friction coefficients and wear rates of promising piston seal materials were measured under temperature, environmental, velocity, and loading conditions that are representative of the low heat rejection (LHR) diesel engine environment. These materials included carbides, oxides, and nitrides. In addition, silicon nitride and partially stablized zirconia disks (cylinder liners) were ion-implanted with TiNi, Ni, Co, and Cr, and subsequently run against carbide pins (piston rings), with the objective of producing reduced friction via solid lubrication at elevated temperature. Friction and wear measurements were obtained using pin-on-disk laboratory experiments and a unique engine friction test rig. Unmodified ceramic sliding couples were characterized at all temperatures by friction coefficients of 0.24 and above during the pin-on-disk tests. The coefficient at 800 C in an oxidizing environment was reduced to below 0.1, for certain material combination, by the ion-implantation of TiNi or Co. This beneficial effect was found to derive from the lubricious Ti, Ni, and Co oxides. Similar results were demonstrated on the engine friction test rig at lower temperatures. The structural integrity and feasibility of engine application with the most promising material combination were demonstrated during a 30-hour single-cylinder, direct-injection diesel engine test.

Beaty, Kevin↗

Probability of detection of internal voids in structural ceramics using microfocus radiography

The reliability of microfocus x-radiography for detecting subsurface voids in structural ceramic test specimens was statistically evaluated. The microfocus system was operated in the projection mode using low X-ray photon energies (20 keV) and a 10 micro m focal spot. The statistics were developed for implanted subsurface voids in green and sintered silicon carbide and silicon nitride test specimens. These statistics were compared with previously-obtained statistics for implanted surface voids in similar specimens. Problems associated with void implantation are discussed. Statistical results are given as probability-of-detection curves at a 95 percent confidence level for voids ranging in size from 20 to 528 micro m in diameter.

Baaklini, G. Y.↗

Probability of detection of internal voids in structural ceramics using microfocus radiography

The reliability of microfocous X-radiography for detecting subsurface voids in structural ceramic test specimens was statistically evaluated. The microfocus system was operated in the projection mode using low X-ray photon energies (20 keV) and a 10 micro m focal spot. The statistics were developed for implanted subsurface voids in green and sintered silicon carbide and silicon nitride test specimens. These statistics were compared with previously-obtained statistics for implanted surface voids in similar specimens. Problems associated with void implantation are discussed. Statistical results are given as probability-of-detection curves at a 95 precent confidence level for voids ranging in size from 20 to 528 micro m in diameter.

Baaklini, G. Y.↗

Friction and wear behaviour of ion beam modified ceramics

In the present study, the sliding friction coefficients and wear rates of carbide, oxide, and nitride materials for potential use as sliding seals (ring/liner) were measured under temperature, environmental, velocity, and loading conditions representative of a diesel engine. In addition, silicon nitride and partially stabilized zirconia discs were modified by ion mixing with TiNi, nickel, cobalt and chromium, and subsequently run against carbide pins, with the objective of producing reduced friction via solid lubrication at elevated temperature. Unmodified ceramic sliding couples were characterized at all temperatures by friction coefficients of 0.24 and above. However, the coefficient at 800 C in an oxidizing environment was reduced to below 0.1, for certain material combinations, by the ion implantation of TiNi or cobalt. This beneficial effect was found to derive from lubricious titanium, nickel, and cobalt oxides.

Lankford, J.↗

Long-term measurement of bone strain in vivo: the rat tibia

Despite the importance of strain in regulating bone metabolism, knowledge of strains induced in bone in vivo during normal activities is limited to short-term studies. Biodegeneration of the bond between gauge and bone is the principle cause of this limitation. To overcome the problem of bond degeneration, a unique calcium phosphate ceramic (CPC) coating has been developed that permits long-term attachment of microminiature strain gauges to bone. Using this technique, we report the first long-term measurements of bone strain in the rat tibia. Gauges, mounted on the tibia, achieved peak or near peak bonding at 7 weeks. Measurements were made between 7-10 weeks. Using ambulation on a treadmill, the pattern and magnitude of strain measured in the tibia remained relatively constant between 7-10 weeks post implantation. That strain levels were similar at 7 and 10 weeks suggests that gauge bonding is stable. These data demonstrate that CPC-coated strain gauges can be used to accurately measure bone strain for extended periods, and provide an in vivo assessment of tibial strain levels during normal ambulation in the rat. Copyright 2001 John Wiley & Sons, Inc.

Non-programmatic↗

Interfaces in polymer, ceramic, and metal matrix composites; Proceedings of the Second International Conference on Composite Interfaces (ICCI-II), Cleveland, OH, June 13-17, 1988

The present conference on interfacial factors in advanced composite materials discusses such topics in their development status and properties as silane coupling, the electrochemical and plasma-surface treatment of carbon fibers, fiber surface-analytical techniques, polymer molecular scale characterization by atom-probe field-ion microscopy, the study of carbon fiber-epoxy resin interface interactions by means of labeling techniques, and the surface tailoring of SiC by ion implantation. Also discussed are developments in laser light-scattered photoelasticity, microstructural evolutions under heat treatment and radiation damage, TEM for composites, the interfaces of carbon fiber-reinforced Al composites, the influence of the interface on macroscopic composite properties, and the status of the theoretical understanding of composite interfaces.

Ishida, Hatsuo↗

Sliding Seal Materials for Adiabatic Engines, Phase 2

An essential task in the development of the heavy-duty adiabatic diesel engine is identification and improvements of reliable, low-friction piston seal materials. In the present study, the sliding friction coefficients and wear rates of promising carbide, oxide, and nitride materials were measured under temperature, environmental, velocity, and loading conditions that are representative of the adiabatic engine environment. In addition, silicon nitride and partially stabilized zirconia disks were ion implanted with TiNi, Ni, Co, and Cr, and subsequently run against carbide pins, with the objective of producing reduced friction via solid lubrication at elevated temperature. In order to provide guidance needed to improve materials for this application, the program stressed fundamental understanding of the mechanisms involved in friction and wear. Electron microscopy was used to elucidate the micromechanisms of wear following wear testing, and Auger electron spectroscopy was used to evaluate interface/environment interactions which seemed to be important in the friction and wear process. Unmodified ceramic sliding couples were characterized at all temperatures by friction coefficients of 0.24 and above. The coefficient at 800 C in an oxidizing environment was reduced to below 0.1, for certain material combinations, by the ion implanation of TiNi or Co. This beneficial effect was found to derive from lubricious Ti, Ni, and Co oxides.

Lankford, J.↗

NASA Tech Briefs, May 2008

Topics covered inclde: Deployable Wireless Camera Penetrators; Hand-Held Units for Short-Range Wireless Biotelemetry; Wearable Wireless Telemetry System for Implantable BioMEMS Sensors; Electronic Escape Trails for Firefighters; Architecture for a High-to-Medium-Voltage Power Converter; 24-Way Radial Power Combiner/Divider for 31 to 36 GHz; Three-Stage InP Submillimeter-Wave MMIC Amplifier; Fast Electromechanical Switches Based on Carbon Nanotubes; Solid-State High-Temperature Power Cells; Fast Offset Laser Phase-Locking System; Fabricating High-Resolution X-Ray Collimators; Embossed Teflon AF Laminate Membrane Microfluidic Diaphragm Valves; Flipperons for Improved Aerodynamic Performance; System Estimates Radius of Curvature of a Segmented Mirror; Refractory Ceramic Foams for Novel Applications; Self-Deploying Trusses Containing Shape-Memory Polymers; Fuel-Cell Electrolytes Based on Organosilica Hybrid Proton Conductors; Molecules for Fluorescence Detection of Specific Chemicals; Cell-Detection Technique for Automated Patch Clamping; Redesigned Human Metabolic Simulator; Compact, Highly Stable Ion Atomic Clock; LiGa(OTf)(sub 4) as an Electrolyte Salt for Li-Ion Cells; Compact Dielectric-Rod White-Light Delay Lines; Single-Mode WGM Resonators Fabricated by Diamond Turning; Mitigating Photon Jitter in Optical PPM Communication; MACOS Version 3.31; Fiber-Optic Determination of N2, O2, and Fuel Vapor in the Ullage of Liquid-Fuel Tanks; Spiking Neurons for Analysis of Patterns; Symmetric Phase-Only Filtering in Particle-Image Velocimetry; Efficient Coupler for a Bessel Beam Dispersive Element; and Attitude and Translation Control of a Solar Sail Vehicle.

Source record↗

A Two-Dimensional, Semiconducting Bolometer Array for HAWC

The Stratospheric Observatory For Infrared Astronomy's (SOFIA's) High resolution Airborne Wideband Camera (HAWC) will use an ion-implanted silicon bolometer array developed at NASA s Goddard Space Flight Center (GSFC). The GSFC Pop-Up Detectors (PUDs) use a unique folding technique to enable a 12 x 32 element closepacked array of bolometers with a filling factor greater than 95%. The HAWC detector uses a resistive metal film on silicon to provide frequency independent, approx. 50% absorption over the 40 - 300 micron band. The silicon bolometers are manufactured in 32-element rows within silicon frames using Micro Electro Mechanical Systems (MEMS) silicon etching techniques. The frames are then cut, "folded", and glued onto a metallized, ceramic, thermal bus "bar". Optical alignment using micrometer jigs ensures their uniformity and correct placement. The rows are then stacked side-by-side to create the final 12 x 32 element array. A kinematic Kevlar suspension system isolates the 200 mK bolometer cold stage from the rest of the 4K detector housing. GSFC - developed silicon bridge chips make electrical connection to the bolometers, while maintaining thermal isolation. The Junction Field Effect Transistor (JFET) preamplifiers for all the signal channels operate at 120 K, yet they are electrically connected and located in close proximity to the bolometers. The JFET module design provides sufficient thermal isolation and heat sinking for these, so that their heat is not detected by the bolometers. Preliminary engineering results from the flight detector dark test run are expected to be available in July 2004. This paper describes the array assembly and mechanical and thermal design of the HAWC detector and the JFET module.

Voellmer, George M.↗