At least 19 records

Porosity and biocompatibility study of ceramic implants based on ZrO{sub 2} and Al{sub 2}O{sub 3}

The work studies ZrO{sub 2}(Me{sub x}O{sub y})-based porous ceramics produced from the powders consisting of hollow spherical particles. It was shown that the structure is represented by a cellular framework with bimodal porosity consisting of sphere-like large pores and pores that were not filled with the powder particles during the compaction. For such ceramics, the increase of pore volume is accompanied by the increased strain in an elastic area. It was also shown that the porous ZrO{sub 2} ceramics had no acute or chronic cytotoxicity. At the same time, ceramics possess the following osteoconductive properties: adhesion support, spreading, proliferation and osteogenic differentiation of MSCs.

36 MATERIALS SCIENCE↗

Strain profiles in ion implanted ceramic polycrystals: An approach based on reciprocal-space crystal selection

The determination of the state of strain in implanted materials is a key issue in the study of their mechanical stability. Whereas this question is nowadays relatively easily solved in the case of single crystals, it remains a challenging task in the case of polycrystalline materials. In this paper, we take benefit of the intense and parallel beams provided by third generation synchrotron sources combined with a two-dimensional detection system to analyze individual grains in polycrystals, hence obtaining “single crystal-like” data. The feasibility of the approach is demonstrated with implanted UO{sub 2} polycrystals where the in-depth strain profile is extracted for individual grains using numerical simulations of the diffracted signal. The influence of the implantation dose is precisely analyzed for several diffracting planes and grains. This work suggests that, at low fluences, the development of strain is mainly due to ballistic effects with little effect from He ions, independently from the crystallographic orientation. At higher fluences, the evolution of the strain profiles suggests a partial and anisotropic plastic relaxation. With the present approach, robust and reliable structural information can be obtained, even from complex polycrystalline ceramic materials.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Material Science Smart Coatings

The contribution of electrostatic interactions to the free energy of binding between model protein and a ceramic implant surface in the aqueous solvent, considered in the framework of the nonlocal electrostatic model, is calculated as a function of the implant low-frequency dielectric constant. We show that the existence of a dynamically ordered (low-dielectric) interfacial solvent layer at the protein-solvent and ceramic-solvent interface markedly increases charging energy of the protein and ceramic implant, and consequently makes the electrostatic contribution to the protein-ceramic binding energy more favorable (attractive). Our analysis shows that the corresponding electrostatic energy between protein and oxide ceramics depends nonmonotonically on the dielectric constant of ceramic, ε C . Obtained results indicate that protein can attract electrostatically to the surface if ceramic material has a moderate ε C below or about 35 (in particularly ZrO 2 or Ta 2 O 5 ). This is in contrast to classical (local) consideration of the solvent, which demonstrates an unfavorable electrostatic interaction of protein with typical metal oxide ceramic materials (ε C >10). Thus, a solid implant coated by combining oxide ceramic with a reduced dielectric constant can be beneficial to strengthen the electrostatic binding of the protein-implant complex.

36 MATERIALS SCIENCE↗

Cobalt triggers necrotic cell death and atrophy in skeletal C2C12 myotubes

Severe poisoning has recently been diagnosed in humans having hip implants composed of cobalt–chrome alloys due to the release of particulate wear debris on polyethylene and ceramic implants which stimulates macrophagic infiltration and destroys bone and soft tissue, leading to neurological, sensorial and muscular impairments. Consistent with this premise, in this study, we focused on the mechanisms underlying the toxicity of Co(II) ions on skeletal muscle using mouse skeletal C2C12 myotubes as an in vitro model. As detected using propidium iodide incorporation, increasing CoCl{sub 2} doses (from 5 to 200 μM) affected the viability of C2C12 myotubes, mainly by cell necrosis, which was attenuated by necrostatin-1, an inhibitor of the necroptotic branch of the death domain receptor signaling pathway. On the other hand, apoptosis was hardly detectable as supported by the lack of caspase-3 and -8 activation, the latter resulting in only faint activation after exposure to higher CoCl{sub 2} doses for prolonged time points. Furthermore, CoCl{sub 2} treatment resulted in atrophy of the C2C12 myotubes which was characterized by the increased expression of HSP25 and GRP94 stress proteins and other typical 'pro-atrophic molecular hallmarks, such as early activation of the NF-kB pathway and down-regulation of AKT phosphorylation, followed by the activation of the proteasome and autophagy systems. Overall, these results suggested that cobalt may impact skeletal muscle homeostasis as an inducer of cell necrosis and myofiber atrophy. - Highlights: • The effects of cobalt on muscle myofibers in vitro were investigated. • Cobalt treatment mainly causes cell necrosis in skeletal C2C12 myotubes. • Cobalt impacts the PI3K/AKT and NFkB pathways and induces cell stress markers. • Cobalt induces atrophy of C2C12 myotubes through the activation of proteasome and autophagy systems. • Co treatment triggers NF-kB and PI3K/AKT pathways in C2C12 myotubes.

60 APPLIED LIFE SCIENCES↗

Structural properties of a bone-ceramic composite as a promising material in spinal surgery

The paper describes the results of in vitro tests of composite bone-ceramic implants and procedures for modifying implant surfaces to enhance osteogenesis. Analysis of CBCI ESs demonstrated that they have a porous structure with the mean longitudinal pore size of 70 µm and the mean transverse pore size of 46 µm; surface pores are open, while inner pores are closed. Elemental analysis of the CBCI surface demonstrates that CBCIs are composed of aluminum and zirconium oxides and contain HA inclusions. Profilometry of the CBCI ES surface revealed the following deviations: the maximum deviation of the profile in the sample center is 15 µm and 16 µm on the periphery, while the arithmetical mean and mean square deviations of the profile are 2.65 and 3.4 µm, respectively. In addition, CBCI biodegradation products were pre-examined; a 0.9% NaCl solution was used as a comparison group. Potentially toxic and tissue accumulated elements, such as cadmium, cobalt, mercury, and lead, are present only in trace amounts and have no statistically significant differences with the comparison group, which precludes their potential toxic effects on the macroorganism. Ceramic-based CBCI may be effective and useful in medicine for restoration of the anatomic integrity and functions of the bone tissue.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Histological response of soda-lime glass-ceramic bactericidal rods implanted in the jaws of beagle dogs

Bacterial and fungal infections remain a major clinical challenge. Implant infections very often require complicated revision procedures that are troublesome to patients and costly to the healthcare system. Innovative approaches to tackle infections are urgently needed. We investigated the histological response of novel free P 2 O 5 glass-ceramic rods implanted in the jaws of beagle dogs. Due to the particular percolated morphology of this glass-ceramic, the dissolution of the rods in the animal body environment and the immature bone formation during the fourth months of implantation maintained the integrity of the glass-ceramic rod. No clinical signs of inflammation took place in any of the beagle dogs during the four months of implantation. This new glass-ceramic biomaterial with inherent bactericidal and fungicidal properties can be considered as an appealing candidate for bone tissue engineering.

60 APPLIED LIFE SCIENCES↗

Implantable devices having ceramic coating applied via an atomic layer deposition method

Substrates coated with films of a ceramic material such as aluminum oxides and titanium oxides are biocompatible, and can be used in a variety of applications in which they are implanted in a living body. The substrate is preferably a porous polymer, and may be biodegradable. An important application for the ceramic-coated substrates is as a tissue engineering scaffold for forming artificial tissue.

47 OTHER INSTRUMENTATION↗

High-energy metal ion implantation for reduction of surface resistivity of alumina ceramic

In this work, the possibility to increase the surface conductivity of ceramic insulators through their treatment with accelerated metal ion beams produced by a MevvaV.Ru vacuum arc source is demonstrated. The increase in surface conductivity is made possible due to experimental conditions in which an insulated collector is charged by beam ions to a potential many times lower than the accelerating voltage, and hence, than the average beam ion energy. The observed effect of charge neutralization of the accelerated ion beam is presumably associated with electrons knocked out of the electrodes of the accelerating system of the source and of the walls of the vacuum chamber by the accelerated ions.

36 MATERIALS SCIENCE↗

A comparative study of TiN and TiC: Oxidation resistance and retention of xenon at high temperature and under degraded vacuum

Dense TiN and TiC samples were prepared by hot pressing using micrometric powders. Xenon species (simulating rare gas fission products) were then implanted into the ceramics. The samples were annealed for 1 h at 1500 deg. C under several degraded vacuums with P{sub O{sub 2}} varying from 10{sup -6} to 2x10{sup -4} mbars. The oxidation resistance of the samples and their retention properties with respect to preimplanted xenon species were analyzed using scanning electron microscopy, grazing incidence x-ray diffraction, Rutherford backscattering spectrometry, and nuclear backscattering spectrometry. Results indicate that TiC is resistant to oxidation and does not release xenon for P{sub O{sub 2{<=}}}6x10{sup -6} mbars. When P{sub O{sub 2}} increases, geometric oxide crystallites appear at the surface depending on the orientation and size of TiC grains. These oxide phases are Ti{sub 2}O{sub 3}, Ti{sub 3}O{sub 5}, and TiO{sub 2}. Apparition of oxide crystallites is associated with the beginning of xenon release. TiC surface is completely covered by the oxide phases at P{sub O{sub 2}}=2x10{sup -4} mbars up to a depth of 3 {mu}m and the xenon is then completely released. For TiN samples, the results show a progressive apparition of oxide crystallites (Ti{sub 3}O{sub 5} mainly) at the surface when P{sub O{sub 2}} increases. The presence of the oxide crystallites is also directly correlated with xenon release, the more oxide crystallites are growing the more xenon is released. TiN surface is completely covered by an oxide layer at P{sub O{sub 2}}=2x10{sup -4} mbars up to 1 {mu}m. A correlation between the initial fine microstructure of TiN and the properties of the growing layer is suggested.

36 MATERIALS SCIENCE↗

Effect of H and He Irradiation on Cavity Formation and Blistering in Ceramics

Single- or poly-crystalline specimens of SiC, Si{sub 3}N{sub 4}, MgO, Al{sub 2}O{sub 3} and MgAl{sub 2}O{sub 4} were implanted with 0.4-1 MeV H{sup +} or He{sup +} ion beams at room temperature and 650 C up to fluences of {approx}1 x 10{sup 22}/m{sup 2}. This produced peak implanted gas and displacement damage levels as high as {approx}50 at.% and 34 displacements per atom (dpa). The specimens were subsequently examined optically, and in cross-section using transmission electron microscopy. Subsurface blistering occurred for specimens irradiated to H or He fluences greater than about 3 x 10{sup 21}/m{sup 2} ({approx}15 at.% peak implanted gas concentration), and surface exfoliation occurred for fluences above {approx}1 x 10{sup 22}/m{sup 2} ({approx}40 at.% implanted gas). Both helium and hydrogen had comparable effectiveness for inducing blistering and exfoliation on an atomic basis. The threshold blistering and exfoliation fluences for both ions were weakly dependent on temperature between 25 and 650 C. Both H and He were found to be very effective in inducing matrix cavity formation, due to their low solubility in these ceramics. The implanted gas concentrations that resulted in visible cavity formation generally ranged from 1 to 5 at.%. Visible cavity formation was readily induced during room temperature irradiation despite the limited vacancy mobility in these ceramics at room temperature. Three general types of cavity morphologies were observed: isolated cavities, clusters of small cavities (typically associated with dislocation loops), and two-dimensional platelets. Cavity formation was observed to initiate at the periphery of dislocation loops in some cases. During elevated temperature irradiation, cavity formation was often observed to be preferentially associated with certain low-index habit planes, particularly if the habit plane was oriented nearly parallel to the irradiated surface: (0001) and {l_brace}1{bar 1}00{r_brace} for Al{sub 2}O{sub 3}, (0001) for a-SiC, {l_brace}001{r_brace} and {l_brace}110{r_brace} for MgO, and {l_brace}110{r_brace} and {l_brace}111{r_brace} for MgAl{sub 2}O{sub 4}. The bubble formation and blistering behavior of the ceramics was similar to that observed in other studies of metals irradiated at comparable homologous temperatures. Ionization-induced diffusion effects associated with dual-beam light ion irradiation appeared to exert only a weak effect on cavity and dislocation loop growth compared to the single ion irradiation conditions.

08 HYDROGEN↗

Analysis of the Structure of Heavy Ion Irradiated LaFeO 3 Using Grazing Angle X-ray Absorption Spectroscopy

Crystalline ceramics are candidate materials for the immobilization of radionuclides, particularly transuranics (such as U, Pu, and Am), arising from the nuclear fuel cycle. Due to the α-decay of transuranics and the associated recoil of the parent nucleus, crystalline materials may eventually be rendered amorphous through changes to the crystal lattice caused by these recoil events. Previous work has shown irradiation of titanate-based ceramics to change the local cation environment significantly, particularly in the case of Ti which was shown to change from 6- to 5-fold coordination. Here, this work expands the Ti-based study to investigate the behavior in Fe-based materials, using LaFeO 3 as an example material. Irradiation was simulated by heavy ion implantation of the bulk LaFeO 3 ceramic, with the resulting amorphous layer characterized with grazing angle X-ray absorption spectroscopy (GA-XAS). Insights into the Fe speciation changes exhibited by the amorphized surface layer were provided through quantitative analysis, including pre-edge analysis, and modeling of the extended X-ray absorption fine structure (EXAFS), of the GA-XAS data.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Processing and characterization of multi-cellular monolithic bioceramics for bone regenerative scaffolds

Multicellular monolithic ceramic body is a ceramic material which has many gas or liquid passages partitioned by thin walls throughout the bulk material. There are many currently known advanced industrial applications of multicellular ceramics structures i.e. as supports for various catalysts, electrode support structure for solid oxide fuel cells, refractories, electric/electronic materials, aerospace vehicle re-entry heat shields and biomaterials for dental as well as orthopaedic implants by naming only a few. Multicellular ceramic bodies are usually made of ceramic phases such as mullite, cordierite, aluminum titanate or pure oxides such as silica, zirconia and alumina. What make alumina ceramics is excellent for the above functions are the intrinsic properties of alumina which are hard, wear resistant, excellent dielectric properties, resists strong acid and alkali attacks at elevated temperatures, good thermal conductivities, high strength and stiffness as well as biocompatible. In this work the processing technology leading to truly multicellular monolithic alumina ceramic bodies and their characterization are reported. Ceramic slip with 66 wt.% solid loading was found to be optimum as impregnant to the polyurethane foam template. Mullitic ceramic composite of alumina-sodium alumino disilicate-Leucite-like phases with bulk and true densities of 0.852 and 1.241 g cm{sup −3} respectively, pore linear density of ±35 cm{sup −1}, linear and bulk volume shrinkages of 7-16% and 32 vol.% were obtained. The compressive strength and elastic modulus of the bioceramics are ≈0.5-1.0 and ≈20 MPa respectively.

36 MATERIALS SCIENCE↗

High energy X-ray diffraction study of a dental ceramics–titanium functional gradient material prepared by field assisted sintering technique

A functional gradient material with eleven layers composed of a dental ceramics and titanium was successfully consolidated using field assisted sintering technique in a two-step sintering process. High energy X-ray diffraction studies on the gradient were performed at High Energy Material Science beamline at Desy in Hamburg. Phase composition, crystal unit edges and lattice mismatch along the gradient were determined applying Rietveld refinement procedure. Phase analysis revealed that the main crystalline phase present in the gradient is α-Ti. Crystallinity increases stepwisely along the gradient with a decreasing increment between every next layer, following rather the weight fraction of titanium. The crystal unit edge a of titanium remains approximately constant with a value of 2.9686(1) Å, while c is reduced with increasing amount of titanium. In the layer with pure titanium the crystal unit edge c is constant with a value of 4.7174(2) Å. The lattice mismatch leading to an internal stress was calculated over the whole gradient. It was found that the maximal internal stress in titanium embedded in the studied gradient is significantly smaller than its yield strength, which implies that the structure of titanium along the whole gradient is mechanically stable. - Highlights: • High energy XRD studies of dental ceramics–Ti gradient material consolidated by FAST. • Phase composition, crystallinity and lattice parameters are determined. • Crystallinity increases stepwisely along the gradient following weight fraction of Ti. • Lattice mismatch leading to internal stress is calculated over the whole gradient. • Internal stress in α-Ti embedded in the gradient is smaller than its yield strength.

36 MATERIALS SCIENCE↗

Helium Irradiation and Implantation Effects on the Structure of Amorphous Silicon Oxycarbide

Despite recent interest in amorphous ceramics for a variety of nuclear applications, many details of their structure before and after irradiation/implantation remain unknown. Here we investigated the short-range order of amorphous silicon oxycarbide (SiOC) alloys by using the atomic pair-distribution function (PDF) obtained from electron diffraction. The PDF results show that the structure of SiOC alloys are nearly unchanged after both irradiation up to 30 dpa and He implantation up to 113 at%. TEM characterization shows no sign of crystallization, He bubble or void formation, or segregation in all irradiated samples. Irradiation results in a decreased number of Si-O bonds and an increased number of Si-C and C-O bonds. This study sheds light on the design of radiation-tolerant materials that do not experience helium swelling for advanced nuclear reactor applications.

36 MATERIALS SCIENCE↗

The Effect of Titanium Dioxide (TiO{sub 2}) Nanoparticles on Hydroxyapatite (HA)/TiO{sub 2} Composite Coating Fabricated by Electrophoretic Deposition (EPD)

Composite coatings of Hydroxyapatite (HA) with ceramics, polymers and metals are used to modify the surface structure of implants. In this research, HA/TiO{sub 2} composite coating was fabricated by electrophoretic deposition (EPD) on 316 stainless steel substrate. HA/TiO{sub 2} composite coatings with 5, 10 and 20 wt.% of TiO{sub 2}, deposited at 40 V and 90 s as an optimum condition. The samples coated at this condition led to an adherent, continuous and crack-free coating. The influence of TiO{sub 2} content was studied by performing different characterization methods such as scanning electron microscopy (SEM), energy dispersive x-ray spectroscopy (EDS), corrosion resistance in simulated body fluid (SBF), coating’s dissolution rate in physiological solution and bond strength to the substrate. The results showed that the higher amount of TiO{sub 2} in the composite coating led to increase in bond strength of coating to stainless steel substrate from 3 MPa for HA coating to 5.5 MPa for HA-20 wt.% TiO{sub 2} composite coating. In addition, it caused to reduction of corrosion current density of samples in the SBF solution from 18.92 μA/cm{sup 2} for HA coating to 6.35 μA/cm{sup 2} for HA-20 wt.% TiO{sub 2} composite coating.

36 MATERIALS SCIENCE↗

Nitrogen ion implantation into various materials using 28 GHz electron cyclotron resonance ion source

The installation of the 28 GHz electron cyclotron resonance ion source (ECRIS) ion implantation beamline was recently completed at the Korea Basic Science Institute. The apparatus contains a beam monitoring system and a sample holder for the ion implantation process. The new implantation system can function as a multipurpose tool since it can implant a variety of ions, ranging hydrogen to uranium, into different materials with precise control and with implantation areas as large as 1–10 mm{sup 2}. The implantation chamber was designed to measure the beam properties with a diagnostic system as well as to perform ion implantation with an in situ system including a mass spectrometer. This advanced implantation system can be employed in novel applications, including the production of a variety of new materials such as metals, polymers, and ceramics and the irradiation testing and fabrication of structural and functional materials to be used in future nuclear fusion reactors. In this investigation, the first nitrogen ion implantation experiments were conducted using the new system. The 28 GHz ECRIS implanted low-energy, multi-charged nitrogen ions into copper, zinc, and cobalt substrates, and the ion implantation depth profiles were obtained. SRIM 2013 code was used to calculate the profiles under identical conditions, and the experimental and simulation results are presented and compared in this report. The depths and ranges of the ion distributions in the experimental and simulation results agree closely and demonstrate that the new system will enable the treatment of various substrates for advanced materials research.

36 MATERIALS SCIENCE↗

Radiation damage of hollandite in multiphase ceramic waste forms

Radiation damage was simulated in multiphase titanate-based ceramic waste forms using an ion accelerator to generate high energy alpha particles (He + ) and an ion implanter to generate 7 MeV gold (Au 3+ ) particles. X-ray diffraction and transmission electron microscopy were used to characterize the damaged surfaces and nearby regions. Simulated multiphase ceramic waste forms were prepared using two processing methods: spark plasma sintering and melt-processing. Both processing methods produced ceramics with similar phase assemblages consisting of hollandite-, zirconolite/pyrochlore-, and perovskite- type phases. The measured heavy ion (Au 3+ ) penetration depth was less in spark plasma sintered samples than in melt-processed samples. Furthermore, structural breakdown of the hollandite phase occurred under He + irradiation indicated by the presence of x-ray diffraction peaks belonging to TiO 2 , BaTiO 5 , and other hollandite related phases (Ba 2 Ti 9 O 20 ). The composition of the constituent hollandite phase affected the extent of damage induced by Au 3+ ions.

36 MATERIALS SCIENCE↗