A statistical analysis of elevated temperature gravimetric cyclic oxidation data of 36 Ni- and Co-base superalloys based on an oxidation attack parameter

A large body of high temperature cyclic oxidation data generated from tests at NASA Lewis Research Center involving gravimetric/time values for 36 Ni- and Co-base superalloys was reduced to a single attack parameter, K(sub a), for each run. This K(sub a) value was used to rank the cyclic oxidation resistance of each alloy at 1000, 1100, and 1150 C. These K(sub a) values were also used to derive an estimating equation using multiple linear regression involving log(sub 10)K(sub a) as a function of alloy chemistry and test temperature. This estimating equation has a high degree of fit and could be used to predict cyclic oxidation behavior for similar alloys and to design an optimum high strength Ni-base superalloy with maximum high temperature cyclic oxidation resistance. The critical alloy elements found to be beneficial were Al, Cr, and Ta.

Barrett, Charles A.↗

Enabling Multi-Material Structures of Co-Based Superalloy Using Laser Directed Energy Deposition Additive Manufacturing

Cobalt superalloys such as Tribaloys are widely used in environments that involve high temperatures, corrosion, and wear degradation. Additive manufacturing (AM) processes have been investigated for fabricating Co-based alloys due to design flexibility and efficient materials usage. AM processes are suitable for reducing the manufacturing steps and subsequently reducing manufacturing costs by incorporating multi-materials. Laser directed energy deposition (laser DED) is a suitable AM process for fabricating Co-based alloys. T800 is one of the commercially available Tribaloys that is strengthened through Laves phases and of interest to diverse engineering fields. However, the high content of the Laves phase makes the alloy prone to brittle fracture. In this study, a Ni-20%Cr alloy was used to improve the fabricability of the T800 alloy via laser DED. Different mixture compositions (20%, 30%, 40% NiCr by weight) were investigated. The multi-material T800 + NiCr alloys were heat treated at two different temperatures. These alloy chemistries were characterized for their microstructural, phase, and mechanical properties in the as-fabricated and heat-treated conditions. SEM and XRD characterization indicated the stabilization of ductile phases and homogenization of the Laves phases after laser DED fabrication and heat treatment. In conclusion, the NiCr addition improved the fabricability and structural integrity of the T800 alloy.

36 MATERIALS SCIENCE↗

Co-Based superalloy morphology evolution: A phase field study based on experimental thermodynamic and kinetic data

Cobalt-based superalloys with two phase $\gamma$/$\gamma '$ microstructures offer great promise as candidates for next-generation high-temperature alloys for applications, such as turbine blades. It is essential to understand the thermodynamic and kinetic factors that influence the microstructural evolution of these alloys in order to optimize the alloy compositions and processing steps with a goal to improve their coarsening, creep and rafting behavior. We are using a continuum phase field approach to study the diffusion process and to predict the equilibrium shapes of Co-Al-W $\gamma '$ precipitates. In order to obtain quantitatively predictive capabilities, we extract chemical free energies for the $\gamma$/$\gamma '$ phases based on CALculation of PHAse Diagrams (CALPHAD) thermodynamic data and diffusion mobilities for Co alloys based on CALPHAD kinetic data. We also use experimental or first-principles data for other quantities, such as misfit strain and interface information, for the parameterization of our model. A particular focus of our study is to understand how different energy balances, misfit strain and kinetics affect the coarsening and rafting behavior of $\gamma '$ precipitates, and the sensitivity of the final precipitate shape to materials parameters. Here, we find that the equilibrium shape of the precipitate results from a delicate competition between chemical, interfacial, and elastic energies, and it is very sensitive to changes in model parameters. Here, we examine how modeling input parameters affect the equilibrium shape of precipitates and relate these parameters to experimentally available values.

36 MATERIALS SCIENCE↗

High-temperature mechanical properties of a γ′-strengthened Co-based superalloy designed for additive manufacturing

GammaPrint®-700 is a recently developed high γ′ (∼70% volume fraction) CoNi-based superalloy designed to combine high-temperature mechanical performance with laser powder bed fusion processability. Room-temperature yield strength ranged from 610 to 658 MPa and increased to 661 MPa (longitudinal) and 730 MPa (transverse) at 760 °C. The creep behavior compared favorably to high-γ′ Ni-based superalloys manufactured via laser powder bed fusion such as Incoloy® 939 and Inconel® 738LC. In-situ neutron diffraction data measured during creep revealed that plastic deformation was largely localized to the γ phase at 760 °C, allowing the γ’ phase to elastically compensate and maintain creep strain resistance. Furthermore, at 900 °C, this load sharing behavior was weakened, contributing to accelerated creep rate and rupture.

Creep↗

Designing Ni- and Co-Base Superalloys To Resist Oxidation

Analysis of experimental cyclic-oxidation data yields quantitative design criterion. Equation characterizing abilities of superalloys to resist oxidation at high temperatures proves useful for designing new alloy compositions to resist oxidation. Rates tendency to become oxidized in terms of single attack parameter, K(a), as function of composition and temperature: decrease in K(a) signifies increase in resistance to oxidation.

Barrett, Charles A.↗

Enhancement of γ/γ’ Microstructured Cobalt Superalloys Produced from Atomized Powder by Creating a Harmonic Structure

A material’s properties must be continuously improved to meet the demands of extreme conditions in high-temperature applications. It is demonstrated that γ-γ’ Co-based superalloys could surpass the yield stress of Ni-based superalloys at high temperature due to the γ-γ’ structure. The powders were subjected to a harmonic modification in order to refine the grain structure on the surface and to activate the sintering process. This study examines how harmonic structure affects microstructure and mechanical properties at high temperatures. Spark Plasma Sintering (SPS) was used for consolidation to maintain the ultrafine grain size microstructure of the powder. Compression tests were conducted from room temperature (RT) to 750 °C to assess the mechanical properties of the material. Yield stress values obtained from harmonic structures are four times higher than those obtained from cast alloys.

36 MATERIALS SCIENCE↗

Extreme hardness at high temperature with a lightweight additively manufactured multi-principal element superalloy

Materials are needed that can tolerate increasingly harsh environments, especially ones that retain high strength at extreme temperatures. Higher melting temperature alloys, like those consisting primarily of refractory elements, can greatly increase the efficiency of turbomachinery used in grid electricity production worldwide. Existing alloys, including Ni- and Co-based superalloys, used in components like turbine blades, bearings, and seals, remain a performance limiting factor due to their propensity, despite extensive optimization efforts, for softening and diffusion-driven elongation at temperatures often well above half their melting point. To address this critical materials challenge, we present results from integrating additive manufacturing and alloy design to guide significant improvements in performance via traditionally difficult-to-manufacture refractory alloys. We present an example of a multi-principal element alloy (MPEA), consisting of five refractory elements and aluminum, that exhibited high hardness and specific strength surpassing other known alloys, including superalloys. The alloy shows negligible softening up to 800°C and consists of four compositionally distinct phases, in distinction to previous work on MPEAs. Density functional theory calculations reveal a thermodynamic explanation for the observed temperature-independent hardness and favorability for the formation of this multiplicity of phases.

36 MATERIALS SCIENCE↗

Advancing Development and Application of Superalloys

This JOM topic is sponsored by the High Temperature Alloys Committee of TMS and addresses advances in the development and application of superalloys. Each year, the High Temperature Alloys Committee organizes symposia at the TMS and Materials Science and Technology annual meetings. In 2020, two symposia were organized for the TMS annual meeting on February 23–27 in San Diego, CA: Materials Design Approaches & Experiences V, co-sponsored by the Integrated Computational Materials Engineering Committee and Advancing Current and State-of-the-Art Applications of Ni- and Co-base Superalloys, co-sponsored by the Corrosion and Environmental Effects Committee. Later this year, the 14th International Symposium on Superalloys will be held on September 13-17 in Seven Springs, PA. The conference, held every 4 years, convenes members of the superalloy community to discuss recent challenges and discoveries affecting future performance and use of superalloys. The TMS High Temperature Alloys Committee meets at both the TMS Annual Meeting & Exhibition and the annual Materials Science and Technology conference. The meetings are open to anyone interested in high-temperature alloys. This special topic on Advancing Development and Application of Superalloys includes a range of sub-topics including mechanical performance, corrosion resistance, processing and advanced manufacturing techniques, which were submitted by research groups from industry, national laboratories and universities.

36 MATERIALS SCIENCE↗

Stress-dependent χ phase transformation in a Ni-based superalloy

The ongoing push to elevate operating temperatures in aerospace gas turbine engines – driven by goals of enhanced fuel efficiency and reduced CO 2 emissions – mandates advancements in the creep resistance of Ni- and Co-based superalloys, which are integral for critical engine components. This study elucidates the role of stress assisted localized phase transformations in the creep properties of these alloys. By leveraging chemo-mechanical coupling, self-healing γ′ precipitates are designed to immobilize planar defects, thereby increasing creep resistance. Employing advanced characterization techniques such as high-resolution Scanning Transmission Electron Microscopy (HR-STEM), in conjunction with atomistic simulations and thermodynamic calculations, novel deformation pathways facilitated by χ local phase transformation (LPT) strengthening have been uncovered; notably, the formation of χ nano-laths through microtwinning and superlattice intrinsic stacking fault (SISF) shearing. This study highlights critical insights into the compositional boundaries necessary for optimizing LPT strengthening while avoiding deleterious bulk formation of η/χ phases. These advancements will guide the design of new alloys maximizing high-temperature creep strength for advanced aerospace applications.

Egan, Ashton J. [Friedrich-Alexander University Er↗

The Influence of C and Si on the Flow Behavior of NiAl Single Crystals

Alloys based on the intermetallic compound NiAl are considered potential replacements for Ni and Co-based superalloys in high temperature structural applications due to their excellent oxidation resistance, low densities, high thermal conductivities, and increased melting points. Unfortunately, NiAl exhibits low tensile ductility at room temperature and low strengths at elevated temperatures which have combined to hinder its development. Recent efforts, have revealed that NiAl in the presence of sufficient solute levels, is subject to the phenomenon of strain aging which manifests itself as: sharp yield points, abnormally low strain rate sensitivities (SRS), plateaus or peaks in yield stress and work hardening rate as a function of temperature, flow stress transients upon an upward change in strain rate, reduced tensile elongations at elevated temperatures, and serrated stress-strain curves. Though recent efforts via either alloying or the removal of interstitial impurities, have resulted in consistent room-temperature tensile elongations exceeding 5% and the elimination of serrated flow, the effects of particular substitutional and interstitial elements and the mechanisms by which they might enhance or hinder the mechanical properties remain unknown. Consequently, the purpose of the present paper is to provide a preliminary assessment of the influence of common substitutional and interstitial impurities on the deformation behavior of NiAl. To accomplish this goal a series of NiAl single crystal alloys containing various interstitial solutes were prepared and their mechanical properties were evaluated between 77 and 1100 K. Because Si is a common impurity in conventional purity single crystals grown by the Bridgman method, Si concentrations were also varied in order to determine the influence of this element.

Weaver, M. L.↗

NiAl-Based Approach For Rocket Combustion Chambers

A multi-layered component, such as a rocket engine combustion chamber, includes NiAl or NiAl-based alloy as a structural layer on the hot side of the component. A second structural layer is formed of material selected form Ni-based superalloys, Co-based alloys, Fe-based alloys, Cu, and Cu-based alloys. The second material is more ductile than the NiAl and imparts increased toughness to the component. The second material is selected to enhance one or more predetermined physical properties of the component. Additional structural layers may be included with the additional material(s) being selected for their impact on physical properties of the component.

Michael V Nathal↗

NiAl-based approach for rocket combustion chambers

A multi-layered component, such as a rocket engine combustion chamber, includes NiAl or NiAl-based alloy as a structural layer on the hot side of the component. A second structural layer is formed of material selected from Ni-based superalloys, Co-based alloys, Fe-based alloys, Cu, and Cu-based alloys. The second material is more ductile than the NiAl and imparts increased toughness to the component. The second material is selected to enhance one or more predetermined physical properties of the component. Additional structural layers may be included with the additional material(s) being selected for their impact on physical properties of the component.

Nathal, Michael V.↗

Improving Structural Integrity of Direct Laser-Deposited Ni – Co – Cr – Al – Y Superalloys by Alloy Modification

Abstract Ni- and Co-based M–Cr–Al–Y (M = Ni and/or Co), dual phase β and γ/γ′, β—Ni–Al, γ—Ni(Co, Cr), and γ′—Ni3–Al superalloys exhibit several beneficial high-temperature (>1000 °C) (2012 °F) strength and corrosion resistance properties. Our study investigates the feasibility of fabricating a commercially available Ni–Co–Cr–AlY alloy (tradename “Amdry 386”) using laser directed energy deposition (laser-DED). A significant challenge for laser fabrication of bulk Amdry 386 (A386) structures stems from the presence of relatively higher amounts of the β phase than γ/γ′ phases. While prior studies report laser fabrication of these materials in coating and cladding configurations, bulk structures have not been realized. To investigate these challenges, this study was developed to systematically evaluate the effects of modifying the A386 alloy by adding 10, 20, and 30% by weight of a Ni–20%Cr (Ni–Cr) alloy (mainly γ/γ′). Laser-DED-fabricated A386 coupons exhibited a metastable, rapidly solidified β-rich microstructure typical to laser processes. The A386 + Ni–Cr mixtures were processed using laser-DED, and small coupons from each composition were evaluated using SEM, XRD, and microhardness to characterize the as-processed microstructure. Thermodynamic modeling was performed to determine the phase evolution as a function of the alloy composition. The dominating phase switches from β to γ/γ’ between the A386 and A386 + 10% Ni–Cr mixtures, but the increase in structural integrity is not observed until the Ni–Cr additions reach a minimum of 20%. Our results show that the alloy chemistry can be successfully modified to improve the structural integrity of laser-processed structures.

Engineering↗

Effect of Long-Term 1093 K Exposure to Air or Vacuum on the Structure of Several Wrought Superalloys

Long-term 1093 K heat treatments of three commercial superalloy sheet materials were undertaken in air -IAI and vacuum. With either exposure, significant precipitation of second phases occurred in the Co-base Haynes(R) Alloy 188 (HA 188) and the Ni-base Haynes(R) Alloy 230 (HA 230); however, much less precipitation was found in the exposed Ni-base alloy Inconel(R) 617 (IN 617). Although some grain growth occurred in HA 198, no changes in the grain size of either HA 230 or IN 617 were observed after 22,500 h at temperature. Oxidation during air heat treatments led to weight gain due to the formation of chromia + spinel scales and surface-connected grain boundary pits/oxides in all three superalloys. Both the weight gain and depth of intergranular attack were dependent on the square root of time, which is indicative of diffusion-controlled phenomena. Because many alloy samples had neighbors in close proximity, most vacuum heat treated specimens did not suffer significant loss of volatile elements. However, some exposed samples were subjected to unrestricted vacuum heat treatments, allowing estimates of volatilization to be made. Based on the data for HA 188, the weight loss during 1093 K vacuum exposure was diffusion controlled once the inhibiting effects of surface films on the as-received alloys were broken down.

J.D. Whittenberger↗

Eutectic superalloys by edge-defined, film-fed growth

The feasibility of producing directionally solidified eutectic alloy composites by edge-defined, film-fed growth (EFG) was carried out. The three eutectic alloys which were investigated were gamma + delta, gamma/gamma prime + delta, and a Co-base TaC alloy containing Cr and Ni. Investigations into the compatibility and wettability of these metals with various carbides, borides, nitrides, and oxides disclosed that compounds with the largest (negative) heats of formation were most stable but poorest wetting. Nitrides and carbides had suitable stability and low contact angles but capillary rise was observed only with carbides. Oxides would not give capillary rise but would probably fulfill the other wetting requirements of EFG. Tantalum carbide was selected for most of the experimental portion of the program based on its exhibiting spontaneous capillary rise and satisfactory slow rate of degradation in the liquid metals. Samples of all three alloys were grown by EFG with the major experimental effort restricted to gamma + delta and gamma/gamma prime + delta alloys. In the standard, uncooled EFG apparatus, the thermal gradient was inferred from the growth speed and was 150 to 200 C/cm. This value may be compared to typical gradients of less than 100 C/cm normally achieved in a standard Bridgman-type apparatus. When a stream of helium was directed against the side of the bar during growth, the gradient was found to improve to about 250 C/cm. In comparison, a theoretical gradient of 700 C/cm should be possible under ideal conditions, without the use of chills. Methods for optimizing the gradient in EFG are discussed, and should allow attainment of close to the theoretical for a particular configuration.

Hurley, G. F.↗

Superior Ballistic Impact Resistance Achieved by the Co-Base Alloy Haynes 25

The fan case in a jet engine is required to contain a fan blade in the rare event of a blade loss during operation. Because of its function, the fan case is the largest structural component in high-bypass-ratio turbofan engines used in commercial aircraft. Therefore, the use of lighter and stronger materials would be advantageous in most engines and is practically a necessity in the latest generation of high-bypass engines. Small panels, 7 in. wide by 7 in. long, of a number of metallic alloys were impact tested at room temperature with a 0.50-caliber blunt-nose titanium alloy projectile at the NASA Glenn Research Center (ref. 1). These metallic systems included several high-strength aluminum (Al) alloys, Al-based laminates, aluminum metal matrix composites (Al-MMCs), nickel-base superalloys (Inconel 718 and 625), several titanium (Ti) alloys in different heat treated conditions, 304L stainless steel, a stainless-steel-based laminate, and a high strength steel (Nitronic 60). It was determined that a simple Co-base alloy (Haynes 25) had the best impact resistance on an areal weight basis. Haynes 25 was at least 10 percent better than IMI 550, the best titanium alloy tested to date, and it was far superior to other metals, especially at higher impact velocities (greater than 1100 ft/sec). Because this material could be ideal for fan containment applications in supersonic aircraft as a replacement for titanium, impact tests were also conducted at 371 oC and compared with results from alloys tested at elevated temperature under previous programs (i.e., Inconel 718, Ti-6242, M-152, Timetal 21S, and Aeromet 100). Although cobalt-base alloys are used in some high-temperature engine applications, to our knowledge they are not used in any containment systems. Advantages of cobalt over titanium include lower cost, easier processing, better high-temperature strength, and no fire hazard if tip rub occurs. Future plans include testing of lightweight sandwich panels with Haynes 25 as a core material in the form of a foam or lattice block structure and scaling up the current tests by using blade-simulating projectiles impacting large plates and half rings.

Hebsur, Mohan G.↗

Tensile properties of HA 230 and HA 188 after 400 and 2500 hour exposures to LiF-22CaF2 and vacuum at 1093 K

The solid-to-liquid phase transformation of the nominal LiF-20CaF2 eutectic at 1043 K is considered to be an ideal candidate thermal energy storage mechanism for a space based low temperature Brayton cycle solar dynamic system. Although Co, Fe, and Ni superalloys are thought to be suitable containment materials for LiF based salts, long term containment is of concern because molten fluorides are usually corrosive and Cr can be lost into space through evaporation. Two examples of commercially available superalloys in sheet form, the Ni-base material HA 230 and the Co-base material Ha 88, have been exposed to molten LiF-22CaF2, its vapor, and vacuum, at 1093 K, for 400 and 2500 hr. Triplicate tensile testing of specimens subjected to all three environments have been undertaken between 77 to 1200 K. Comparison of the weight gain data, microstructure, and tensile properties indicate that little, if any, difference in behavior can be ascribed to the exposure environment.

Whittenberger, J. Daniel↗