Search NASA⌕ Search

SEARCH · Search NASA

Results for “controlled spalling”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Adherent Al2O3 scales formed on undoped NiCrAl alloys

Changes in the spalling behavior of Al2O3 scales formed on an undoped NiCrAl alloy are described. Two samples of Ni-15Cr-13Al (wt pct), one a control and the other sanded, were subjected to 25 oxidation cycles. It is observed that adherent scales formed on the sanded sample; however, the control sample had speckled, spalled scales. The data reveal that the adherent scales are caused by repeated removal of surface layers after each oxidation cycle. It is determined that interfacial segregation of sulfur influences spallation and sulfur removal increases bonding. The effect of moisture on scale adhesions is investigated.

Smialek, James L.↗

The effect of 0.1 atomic percent zirconium on the cyclic oxidation behavior of beta-NiAl for 300 hours at 1200 C

The long time effect of 0.1 at percent Zr (0.2 wt percent Zr) on the cyclic oxidation behavior of hipped beta-NiAl was studied. Oxidation testing was performed in static air at 1200 C for up to 3000 one-hour exposure cycles. Specific weight change versus time data was modeled with the COSP computer program to analyze cyclic oxidation behavior. The Zr-free stoichiometric alloy oxidized and spalled randomly to bare metal between cycles at a rate high enough to deplete Al to a low enough level that oxidation breakaway took place as nonprotective NiO replaced the alpha-Al2O3/NiAl2O4 scale as the controlling oxide. The Zr minimized this severe type of spalling maintaining the protective alpha-Al2O3 scale even out to 3000 hours for the stoichiometric alloy with no significant Al depletion. A third beta-NiAl alloy containing 0.1 at percent Zr but with 10 percent less Al than the stoichiometric alloy was also tested and showed some depletion of Al, but the protective Al2O3/NiAl2O4 was still maintained to close to 2700 hours.

Barrett, C. A.↗

The effect of 0.1 atomic percent zirconium on the cyclic oxidation behavior of beta-NiAl for 3000 hours at 1200 C

The long time effect of 0.1 at percent Zr (0.2 wt percent Zr) on the cyclic oxidation behavior of hipped beta-NiAl was studied. Oxidation testing was performed in static air at 1200 C for up to 3000 one-hour exposure cycles. Specific weight change versus time data was modeled with the COSP computer program to analyze cyclic oxidation behavior. The Zr-free stoichiometric alloy oxidized and spalled randomly to bare metal between cycles at a rate high enough to deplete Al to a low enough level that oxidation breakaway took place as nonprotective NiO replaced the alpha-Al203/NiAl204 scale as the controlling oxide. The Zr minimized this severe type of spalling maintaining the protective alpha-Al203 scale even out to 3000 hours for the stoichiometric alloy with no significant Al depletion. A third beta-NiAl alloy containing 0.1 at percent Zr but with 10 percent less Al than the stoichiometric alloy was also tested and showed some depletion of Al, but the protective Al203/NiAl204 was still maintained to close to 2700 hours.

Barrett, C. A.↗

Impact and collisional processes in the solar system

The mechanical and thermodynamic aspects of shock impact cratering and accretionary processes on solid planets and satellites are being investigated experimentally. The recently proposed model of Melosh, describing the physics controlling the size and velocity of only lightly shocked spalled ejecta surrounding the crushed rock region of an impact crater, was studied at the Ames gun facility. Spall velocity measurements using lead and aluminum bullets were conducted. In addition, shock temperatures of silicates and volatile-bearing minerals were measured using radiative techniques. Finally impact devolatilization of minerals and accretion of planetary atmospheres were examined. Measurements of the release isentropes of CaCO3 were carried out. The effect on the water budgets of planets of reactions which occur when metallic iron (which would be present in chondritic material) is introduced into a simple accretion model is under investigation.

Ahrens, T. J.↗

Effects of chromium and aluminum on mechanical and oxidation properties of iron-nickel-base superalloys based on CG-27

The effects of chromium and aluminum on the mechanical and oxidation properties of a series of gamma-prime-strengthened alloys based on CG-27 were studied. Gamma-prime dispersion and solid-solution strengthening were the principal modes of alloy strengthening. The oxidation attack parameter K sub a decreased with increasing Cr and Al contents for each alloy group based on Al content. As a group, alloys with 3 wt % Al had the lowest attack parameters. Therefore, 3 wt % is the optimum level of Al for parabolic oxidation behavior. Spalling, due to diffusion-induced grain growth, was controlled by the overall Cr and Al levels. The alloy with 4 wt % Cr and 3 wt % Al had stress-rupture properties superior to those of the base alloy, CG-27, and maintained parabolic oxidation behavior while the Cr content was reduced by two-thirds of its value in cast CG-27.

Schuon, S. R.↗

Impact and Collisional Processes in the Solar System

The mechanical and thermodynamic aspects of shock impact cratering and accretionary processes on solid planets and satellites are being investigated experimentally. The recently proposed model of Melosh, describing the physics controlling the size and velocity of only lightly shocked spalled ejecta surrounding the crushed rock region of an impact crater, was studied at the Ames gun facility. Spall velocity measurements using lead and aluminum bullets were conducted. In addition, shock temperatures of silicates and volatile bearing minerals were measured using radiative techniques. Finally impact devolatilization of minerals and accretion of planetary atmospheres were examined. Measurements of the release isentropes of CaCO3 were carried out. The effect on the water budgets of planets of reactions which occur when metallic iron (which would be present in chondritic material) is introduced into a simple accretion model is under investigation.

Ahrens, T. J.↗

Preliminary results of the mission profile life test of a 30 cm Hg bombardment thruster

Long term tests were performed on a 30 cm Hg bombardment thruster and a power processing unit to determine lifetime characteristics. The thruster performance data and other operational characteristics taken at various times during the test segment are presented and evaluated with the life limiting mechanisms: discharge chamber erosion, deposition and spalling, external erosion, cathode degradation, and propellant isolator leakage. The control algorithms for thruster start up, steady state operation, throttle, detection and correction of off normal conditions, and shutdown are discussed.

Bechtel, R. T.↗

Solutions for discharge chamber sputtering and anode deposit spalling in small mercury ion thrusters

Small electron bombardment mercury ion thrusters are considered for attitude-control and station-keeping operations in the case of earth synchronous satellites. The required operational lifetimes of the order of 20,000 hours could present problems because of the occurrence of sputter erosion of thruster discharge chamber components. The investigation reported is concerned with a study of these problems and the development of approaches for overcoming them.

Power, J. L.↗

Health and safety evaluation of a modified tunnel borer design for application to single entry coal mine development

A health and safety analysis of a single entry coal tunnel borer system is given. The results of the health analysis indicated that while the tunnel borer design offered improvements in dust control through the use of water sprays, a higher face ventilation rule, and the application of spalling rather than the conventional grinding process, it interjected an additional mutagen and toxic compound into the environment through the use of shotcrete. The tunnel borer system easily conformed with the prescribed fatality limit, but exceeded the required limits for disabling and overall injuries. It also exhibited projected disabling and overall injury rates considerably higher than existing continuous mining injury rates. Consequently, the tunnel borer system was not considered an advanced system.

Zimmerman, W. F.↗

Recent developments in high temperature coatings for gas turbine airfoils

The importance of coatings for hot section airfoils has increased with the drive for more cost-effective use of fuel in a wide variety of gas turbine engines. Minor additions of silicon have been found to appreciably increase the oxidation resistance of plasma-sprayed NiCoCrAlY coatings on a single crystal nickel-base superalloy. Increasing the chromium content of MCrAlY coatings substantially increases the resistance to acidic (Na2SO4-SO3) hot corrosion at temperatures of about 1300 F (704 C) but gives no significant improvement beyond contemporary coatings in the range of 1600 F (871 C). Surface enrichment of MCrAlY coatings with silicon also gives large increases in resistance to acidic hot corrosion in the 1300 F region. The resistance to the thermal stress-induced spalling of zirconia-based thermal barrier coatings has been improved by lowering coating stresses with segmented structures and by controlling the substrate temperature during coating fabrication.

Goward, G. W.↗

Discontinuous Inter-Granular Separations (DIGS) in the Gas Nitride Layer of ISS Race Rings

The starboard solar alpha rotary joint (SARJ) race ring on the International space station (ISS) failed due to severe spalling of the outer diameter, 45 degree (outer canted) nitrided surface. Subsequent analysis at NASA-KSC revealed that almost all of the debris generated due to the failure was nitrided 15-5 stainless steel. Subsequent analysis of the nitride control coupons (NCC) at NASA-JSC revealed the presence of discontinuous inter-granular separations (DIGS) in the gas nitride layer. These DIGS were present in the inter-granular networking located in the top 2 mils of the nitride layer. The manufacturer's specification requires the maximum white structure to be 0.0003 inches and intergranular networking below the allowable white structure depth to be cause for rejection; a requirement that the NCCs did not meet. Subsequent testing and analysis revealed that lower DIGS content significantly lowered the probability of nitride spalling in simulated, dry condition runs. One batch of nitride samples with DIGS content similar to the port SARJ (did not fail on orbit) which exhibited almost no nitride spalling after being run on one test rig. Another batch of nitride samples with DIGS content levels similar to the starboard SARJ exhibited significant nitride spalling on the same test rig with the same load under dry conditions. Although DIGS were not the root cause of starboard race ring failure, testing indicates that increased DIGS reduced the robustness of the gas nitride layer under dry operating conditions.

Figert, John↗

Thermal fracture mechanisms in ceramic thermal barrier coatings

Ceramic thermal barrier coatings represent an attractive method of increasing the high temperature limits for systems such as diesel engines, gas turbines and aircraft engines. However, the dissimilarities between ceramics and metal, as well as the severe temperature gradients applied in such systems, cause thermal stresses which can lead to cracking and ultimately spalling of the coating. This paper reviews the research which considers initiation of surface cracks, interfacial edge cracks and the effect of a transient thermal load on interface cracks. The results of controlled experiments together with analytical models are presented. The implications of these findings to the differences between diesel engines and gas turbines are discussed. The importance of such work for determining the proper design criteria for thermal barrier coatings is underlined.

Kokini, K.↗

Thermal fracture mechanisms in ceramic thermal barrier coatings

Ceramic thermal barrier coatings represent an attractive method of increasing the high temperature limits for systems such as diesel engines, gas turbines and aircraft engines. However, the dissimilarities between ceramics and metal, as well as the severe temperature gradients applied in such systems cause thermal stresses which can lead to cracking and ultimately spalling of the coating. This paper reviews the research which considers initiation of surface cracks, interfacial edge cracks and the effect of a transient thermal load on interface cracks. The results of controlled experiments together with analytical models are presented. The implications of these findings to the differences between diesel engines and gas turbines are discussed. The importance of such work for determining the proper design criteria for thermal barrier coatings is underlined.

Kokini, Klod↗

Thermal barrier coatings for thermal insulation and corrosion resistance in industrial gas turbine engines

Four thermal barrier coatings were subjected to a 500-hour gas turbine engine test. The coatings were two yttria stabilized zirconias, calcium ortho silicate and calcium meta titanate. The calcium silicate coating exhibited significant spalling. Yttria stabilized zirconia and calcium titanate coatings showed little degradation except in blade leading edge areas. Post-test examination showed variations in the coating due to manual application techniques. Improved process control is required if engineering quality coatings are to be developed. The results indicate that some leading edge loss of the coating can be expected near the tip.

Vogan, J. W.↗

Design and fabrication of prototype system for early warning of impending bearing failure

A test program was conducted with the objective of developing a method and equipment for on-line monitoring of installed ball bearings to detect deterioration or impending failure of the bearings. The program was directed at the spin-axis bearings of a control moment gyro. The bearings were tested at speeds of 6000 and 8000 rpm, thrust loads from 50 to 1000 pounds, with a wide range of lubrication conditions, with and without a simulated fatigue spall implanted in the inner race ball track. It was concluded that a bearing monitor system based on detection and analysis of modulations of a fault indicating bearing resonance frequency can provide a low threshold of sensitivity.

Meacher, J.↗

Structural Damage Prediction and Analysis for Hypervelocity Impacts: Handbook

This handbook reviews the analysis of structural damage on spacecraft due to hypervelocity impacts by meteoroid and space debris. These impacts can potentially cause structural damage to a Space Station module wall. This damage ranges from craters, bulges, minor penetrations, and spall to critical damage associated with a large hole, or even rupture. The analysis of damage depends on a variety of assumptions and the area of most concern is at a velocity beyond well controlled laboratory capability. In the analysis of critical damage, one of the key questions is how much momentum can actually be transfered to the pressure vessel wall. When penetration occurs without maximum bulging at high velocity and obliquities (if less momentum is deposited in the rear wall), then large tears and rupture may be avoided. In analysis of rupture effects of cylindrical geometry, biaxial loading, bending of the crack, a central hole strain rate and R-curve effects are discussed.

Elfer, N. C.↗

The effect of yttrium and thorium on the oxidation behavior of Ni-Cr-Al alloys

The effect of quaternary additions of 0.5% Y, 0.5 and 1.0% Th to a base alloy of Ni-10CR-5Al on the oxidation behavior and mechanism was studied during oxidation in air over the range of 1000 to 1200 C. The presence of yttrium decreased the oxidation kinetics slightly, whereas, the addition of thorium caused a slight increase. Oxide scale adherence was markedly improved by the addition of the quaternary elements. Although a number of oxides formed on yttrium containing alloys, quantitative X-ray diffraction clearly showed that the rate-controlling step was the diffusion of aluminum through short circuit paths in a thin layer of alumina that formed parabolically with time. Although the scale adherence of the yttrium containing alloy was considerably better than the base alloys, spalling did occur that was attributed to the formation of the voluminous YAG particles which grew in a mushroom-like manner, lifting the protective scale off the subrate locally. The YAG particles formed primarily at grain boundaries in the substrate in which the yttrium originally existed as YNi9.

Kumar, A.↗

Moisture-Induced Delayed Alumina Scale Spallation on a Ni(Pt)Al Coating

Delayed interfacial scale failure takes place after cooling for samples of a Ni(Pt)Al-coated CMSX4 single crystal superalloy, cycled at 1150 C for up to 2000 hr. One sample exhibited premature coating grain boundary wrinkling, alumina scale spallation to bare metal, and a final weight loss of 3.3 mg/cm2 . Spallation under ambient conditions was monitored with time after cooldown and was found to continue for 24 hr. This produced up to 0.05 mg/cm2 additional loss for each hold, accumulating 0.7 mg/cm 2 (20 percent of the total) over the course of the test. After test termination, water immersion produced an additional 0.15 mg/cm2 loss. (A duplicate sample produced much less wrinkling and time dependent spalling, maintaining a net weight gain.) The results are consistent with the general phenomena of moisture-induced delayed spallation (MIDS) of mature, distressed alumina scales formed on oxidation resistant M-Al alloys. Relative ambient humidity is discussed as the factor controlling adsorbed moisture, reaction with the substrate, and hydrogen effects on interface strength.

Smialek, James L.↗