At least 19 records

Nb₃Sn Coating of a 2.6 GHz SRF Cavity by Sputter Deposition Technique

Nb₃Sn is of interest as a coating for SRF cavities due to its higher transition temperature Tc ~18.3 K and superheating field Hsh ~400 mT, both are twice that of Nb. Nb₃Sn coated cavities can achieve high-quality factors at 4 K and can replace the bulk Nb cavities operated at 2 K. A cylindrical magnetron sputtering system was built, commissioned, and used to deposit Nb₃Sn on the inner surface of a 2.6 GHz single-cell Nb cavity. With two identical cylindrical magnetrons, this system can coat a cavity with high symmetry and uniform thickness. Using Nb-Sn multilayer sequential sputtering followed by annealing at 950°C for 3 hours, polycrystalline Nb₃Sn films were first deposited at the equivalent positions of the cavity’s beam tubes and equator. The film’s composition, crystal structure, and morphology were characterized by energy dispersive spectroscopy, X-ray diffraction, and atomic force microscopy. The Tc of the films was measured by the four-point probe method and was 17.61 to 17.76 K. Based on these studies, ~1.2 micron thick Nb₃Sn was deposited inside a 2.6 GHz Nb cavity. We will discuss first results from samples and cavity coatings, and the status of the coating system.

43 PARTICLE ACCELERATORS↗

Differential Deposition Technique for Figure Corrections in Grazing Incidence X-ray Optics

A differential deposition technique is being developed to correct the low- and mid-spatial-frequency deviations in the axial figure profile of Wolter type grazing incidence X-ray optics. These deviations arise due to various factors in the fabrication process and they degrade the performance of the optics by limiting the achievable angular resolution. In the differential deposition technique, material of varying thickness is selectively deposited along the length of the optic to minimize these deviations, thereby improving the overall figure. High resolution focusing optics being developed at MSFC for small animal radionuclide imaging are being coated to test the differential deposition technique. The required spatial resolution for these optics is 100 m. This base resolution is achievable with the regular electroform-nickel-replication fabrication technique used at MSFC. However, by improving the figure quality of the optics through differential deposition, we aim at significantly improving the resolution beyond this value.

Kilaru, Kiranmayee↗

Application and Development of Atomic Layer Deposition Techniques to Improve Thermo-Optical Coatings for Spacecraft Thermal Control and Advanced Optical Instruments

A key technology development driver in environmental control systems and next generation optics are discussed utilizing thin film development borrowed from the semiconductor industry. The optical and physical properties of spacecraft radiator coatings are dictated by orbital environmental conditions. For example, coatings must adequately dissipate charge buildup when orbital conditions, such as polar, geostationary or gravity neutral, result in surface charging. Current dissipation techniques include depositing a layer of ITO (indium tin oxide) on the radiator surface in a high temperature process. The application of these enhanced coatings must be such that the properties in question are tailored to mission-specific requirements. The multi-billion-dollar semiconductor industry has adopted Atomic Layer Deposition (ALD) for self-assembly and atomic-scale placement. ALD is a cost-effective nanoadditive-manufacturing technique that allows for the conformal coating of substrates with atomic control in a benign temperature and pressure environment. By using ALD, modification of these coatings can be accomplished during coating application preprocessing. The preprocessing is rendered directly on the coating dry pigment before binding. Through the introduction of paired precursor gases, thin films can be deposited on a myriad of substrates ranging from glass, polymers, aerogels, metals, powders, and other high aspect-ratio micro- and nano- structures. By providing atomic-level control, where single layers of atoms can be deposited, the fabrication of metal transparent films, precise nano-laminates, and coatings of nano-channels and pores is achievable. A method has been demonstrated for the ALD of In2O3 and films on a variety of substrates from Si(100) wafers, glass slides, and on Z93P pigments resulting in a direct spaceflight application. Results will be presented that verify the chemical composition of ALD pigments and charge dissipation properties when the pigment goes through its binding and coating process and we present early results of ALD for carbon nanotube formation and encapsulation.

Dwivedi, Vivek H.↗

High T(sub c) superconductors fabricated by plasma aerosol mist deposition technique

We report new results on high T(sub c) superconductors fabricated by a plasma aerosol mist deposition technique, in atmospheric environment. Materials fabricated are YBaCuO, BiPbSrCaCuO, BaCaCuO precursor films for TlBaCaCuO, and other buffers such as YSZ. Depending on processing conditions, sizes of crystallites and/or particles are between dozens of nano-meters and several micrometers. Superconductive properties and other material characteristics can also be tailored.

Wang, X. W.↗

Colloidal Quantum Dot Solar Cells: Progressive Deposition Techniques and Future Prospects on Large-area Fabrication

Colloidally grown nanosized semiconductors yield extremely high-quality optoelectronic materials. Many examples have pointed to near perfect photoluminescence quantum yields, meaning non-radiative optical processes (losses) can be completely suppressed allowing for technology-leading materials as high purity color centers in display technology and emitters in LEDs. Furthermore, because of high chemical yield, and improved understanding of the surfaces, these materials, particularly colloidal quantum dots (QDs) can also be ideal candidates for other optoelectronic applications. Given the strong drive toward carbon neutrality and limiting climate change, electricity from solar photovoltaics will play a large role in the power generation sector. QDs have been developed and shown dramatic improvements over the past 15 years as photoactive materials in photovoltaics and have unique potential with various innovative deposition properties which could lead to exceptionally low-cost and high-performance devices. Once the key issues related to charge transport in optically thick arrays are addressed, QD-based photovoltaic technology could become a better candidate for practical application. In this article, w e show how the possibilities of different deposition techniques could bring QD-based solar cells to the industrial level and discuss the challenges for perovskite QD solar cells in particular, to achieve large-area fabrication for further advancing technology to solve pivotal energy and environmental issues.

14 SOLAR ENERGY↗

High-efficiency CdTe thin-film solar cells using metalorganic chemical vapor deposition techniques

Energy conversion efficiency of metalorganic chemical vapor deposited CdTe as an intrinsic active layer in n-i-p solar cell structures is reported. Small-area devices with efficiencies over 9 percent have been demonstrated. I-V characteristics, photospectral response, and the results of Auger profiling of structural composition for typical devices will be presented. Also presented are preliminary results on similar photovoltaic devices having Cd(0.85)Mn(0.15)Te in place of CdTe as an i layer.

Nouhi, A.↗

A Novel Catalyst Deposition Technique for the Growth of Carbon Nanotubes

This viewgraph presentation provides information on the development of a technique at NASA's Ames Research Center by which carbon nanotubes (NT) can be grown. The project had several goals which included: 1) scaleability, 2) ability to control single wall nanotube (SWNT) and multiwall nanotube (MWNT) formation, 3) ability to control the density of nanotubes as they grow, 4) ability to apply standard masking techniques for NT patterning. Information regarding the growth technique includes its use of a catalyst deposition process. SWNTs of varying thicknesses can be grown by changing the catalyst composition. Demonstrations are given of various methods of masking including the use of transmission electron microscopic (TEM) grids.

Delzeit, Lance↗

Lunar Simulant Deposition Technique for Dust Tolerance Studies

A renewed interest in lunar exploration has spawned an array of development efforts for lunar surface assets. These systems depend on the reliable operation of mechanisms and components that may be susceptible to performance degradations or failure due to dust. The Uniform Dust Deposition System was developed at the NASA Glenn Research Center to provide repeatable, uniform, and automated deposition of simulants on surfaces of interest for dust mitigation testing. The system is capable of depositing simulants on test articles up to 60 cm in diameter and 15 cm high in a dry air environment with less than 1 percent relative humidity while keeping users safe from aerosolized dust. The automation of the system allows for high testing throughput while not sacrificing test quality and allows the user to reduce data in parallel. The additional development of a simulant preparation technique complements the repeatability of the deposition physics during testing. The system includes an imaging subsystem that leverages the power of machine learning to count simulant particles and measure their size, thereby allowing for accurate predictions of surface deposition densities (coefficient of determination R^(2) = 0.93) from images alone. The coverage of dust on a surface was shown to be uniform (coefficient of variation CV < 0.11), allowing developers to accurately evaluate the performance of their technology with a prescribed amount of lunar simulant, information that can be used to develop and refine models. The accuracy of the system is currently less than desired for a single deposition run, with a standard deviation (SD) ranging from 18 to 24 mg, or 0.839 to 1.184 mg/sq. cm , for a 5-cm-diameter area. However, the accuracy can be improved by performing multiple deposition runs to build dust to a desired level. Testing has shown that a SD of 0.2 to 0.6 mg, or 0.076 to 0.227 mg/sq. cm, can be achieved for a 5-cm-diameter area using this technique.

Stephen Gerdts↗

Controlling the Morphology of PEDOT:PSS Blend Films with Pre-Deposition Solution Composition and Deposition Technique

Understanding the relationships between morphology, fabrication processes, and thermoelectric performance in conducting polymers is essential to the development of high- efficiency organic thermoelectrics as an alternative to commonly used rare metals. Altering the film fabrication process of poly(3,4-ethylenedioxythiophene):poly(styrene sulfonate) (PEDOT:PSS) with the addition of high boiling solvents to the precast solution improves the electrical conductivity and significantly increases its Seebeck value. Neutron scattering monitors the changes in the atomic, nanoscale, and mesoscale morphologies of PEDOT:PSS thin films with the addition of dimethyl sulfoxide (DMSO) to the aqueous solution prior to film formation and with varying fabrication procedures. The neutron scattering results show a decrease in the deuterated PSS domain size along with systematic variations in PEDOT fibril assemblies in the final blend film with the addition of DMSO to the pre-deposition solution. These structural modifications indicate that the increase in conductivity of PEDOT:PSS blends with addition of DMSO reported in the literature can be ascribed to the disruption of solvated PEDOT assemblies by the DMSO, forming smaller PSS domains in the pre-deposition solution and allowing smoother film formation. These improvements are observed significantly with the addition of just 1% DMSO but continue to modestly improve with the addition of up to 5% DMSO to the PEDOT:PSS blend pre-deposition solution. The fact that the variations in the measured morphology are independent of whether the films were deposited by spin or ultrasonic spray casting methods emphasizes the crucial importance of the structure of the blend in the pre-deposition solution in determining the final thin film blend morphology.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Bringing high-efficiency silicon solar cells with heterojunction contacts to market with a new, versatile deposition technique

Silicon heterojunction (SHJ) and tunnel-oxide-passivated-contacts (TOPCon) solar cells are the future for silicon technology after passivated-emitter-and-rear-contact (PERC) cells. However, the tool costs (CapEx) for SHJ (TOPCon) make the cell lines more than 2 (1.5) times of the cost of the PERC, which hinders the wide adoption these new technologies despite higher efficiencies. A common challenge for both cell types is that the passivation layers are sensitive to sputter damage. Furthermore, for TOPCon cells, it is desirable to have an inline (instead of batch) process for tunnel oxide and polysilicon to maximize the throughput and thus reduce the operation cost.

14 SOLAR ENERGY↗

Development of Repair Techniques for Cast Iron Engine Blocks by Additive Manufacturing

ORNL partnered with Cummins Inc to demonstrate the feasibility of using additive manufacturing techniques to deposit large volume of new material on cast iron in the context of remanufacturing. Remanufacturing at Cummins Inc is carried out to repair any field damage and, in some cases, provide additional value by adding new features. Large volume deposition on difficult to weld materials is a challenging problem due to involved metallurgy. Phase-1 of this work evaluated the feasibility of using laser directed energy deposition technique to deposit new material layer by layer on cast iron engine blocks. During phase-1 deposits were made using Inconel-718, Nickel, Nr-Cr-B braze filler. Leveraging the knowledge gained during Phase-1, Phase-2 focused on developing a low- cost crack resistant ferrous alloy to repair cast iron via volume deposition techniques without preheating. Three different alloy chemistries were identified, and trials were performed on cast iron substrates to identify the optimal chemistry that provided adequate resistance to cracking in both, the deposits as well as the cast iron substrate.