Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Low-temperature sintering and compatibility with silver electrode of Ba{sub 4}MgTi{sub 11}O{sub 27} microwave dielectric ceramic

Ba{sub 4}MgTi{sub 11}O{sub 27} microwave dielectric ceramic was investigated using X-ray diffraction, scanning electron microscopy and dielectric measurement. The pure Ba{sub 4}MgTi{sub 11}O{sub 27} ceramic shows a high sintering temperature ({approx}1275 {sup o}C) and good microwave dielectric properties as Q x f of 19,630 GHz, {epsilon}{sub r} of 36.1, {tau}{sub f} of 14.6 ppm/{sup o}C. It was found that the addition of BaCu(B{sub 2}O{sub 5}) (BCB) can effectively lower the sintering temperature from 1275 to 925 {sup o}C, and does not induce much degradation of the microwave dielectric properties. The BCB-doped Ba{sub 4}MgTi{sub 11}O{sub 27} ceramics can be compatible with Ag electrode, which makes it a promising ceramic for LTCC technology application.

36 MATERIALS SCIENCE↗

SrV2O6: An ultralow-firing microwave dielectric ceramic for LTCC applications

Highlights: • α-SrV{sub 2}O{sub 6} and β-SrV2O{sub 6} phase were coexisted below 500 °C, and stable α-SrV{sub 2}O{sub 6} phase at 630 °C. • Optimum microwave dielectric properties: ε{sub r} ∼9.66, Q × f ∼23,200 GHz, and τ{sub f} ∼ −205 ppm/°C were obtained. • CaTiO{sub 3} successfully adjusted τ{sub f} value toward to near-zero with −2.7 ppm/°C. • Their chemical compatibility with the aluminum electrodes were evaluated. - Abstract: A novel ultralow-firing microwave dielectric ceramic SrV{sub 2}O{sub 6} was prepared at 630 °C through the solid-state method. Phase evolution and crystal structure were analyzed by XRD and Raman spectroscopy. Results show that α-SrV{sub 2}O{sub 6} and β-SrV{sub 2}O{sub 6} phase coexisted when fired at lower temperatures (α-SrV{sub 2}O{sub 6} phase was obtained at 550 °C and remained stable up to 660 °C. Optimum microwave dielectric properties with a quality factor ∼23,200 GHz, a low dielectric constant ∼9.66, and a temperature coefficient of resonant frequency ∼−205 ppm/°C was obtained. SrV{sub 2}O{sub 6} ceramic possessed chemical compatibility with aluminum electrodes when cofired at 630 °C. The temperature stability of SrV{sub 2}O{sub 6} was adjusted by forming composite ceramics with CaTiO{sub 3} and a near-zero τ{sub f} ∼−2.7 ppm/°C was achieved in the 0.75SrV{sub 2}O{sub 6}-0.25CaTiO{sub 3} ceramic. All the results show that the SrV{sub 2}O{sub 6} ceramic might be a promising candidate as substrates in ultra-low temperature cofired (ULTCC) ceramics.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Low loss Sr{sub 1-x}Ca{sub x}La{sub 4}Ti{sub 5}O{sub 17} microwave dielectric ceramics

Highlights: {yields} New single phase highly dense (95%) microwave dielectric Sr{sub 1-x}Ca{sub x}La{sub 4}Ti{sub 5}O{sub 17} (0 {<=} x {<=} 1) ceramics were designed and processed. {yields} Theoretical density and molar volume decreased due to the substitution of small Ca{sup 2+} for large Sr{sup 2+}. {yields} As required for microwave dielectric applications, optimum properties (i.e. {epsilon}{sub r} {approx} 53.7, Qf{sub o} {approx} 11,532 GHz and {tau}{sub f} {approx} -1.4 ppm/{sup o}C) were achieved for Sr{sub 0.4}Ca{sub 0.6}La{sub 4}Ti{sub 5}O{sub 17} (x = 0.6). -- Abstract: Microwave dielectric ceramics in the Sr{sub 1-x}Ca{sub x}La{sub 4}Ti{sub 5}O{sub 17} (0 {<=} x {<=} 1) composition series were prepared through a solid state mixed oxide route. All the compositions formed single phase ceramics within the detection limit of in-house X-ray diffraction when sintered in the temperature range 1450-1580 {sup o}C. Theoretical density and molar volume decreased due to the substitution of Ca{sup 2+} for Sr{sup 2+} which was associated with a decrease in the dielectric constant ({epsilon}{sub r}) and temperature coefficient of resonant frequency ({tau}{sub f}) but an increase in quality factor, Qf{sub o}. Optimum properties were achieved for Sr{sub 0.4}Ca{sub 0.6}La{sub 4}Ti{sub 5}O{sub 17} which exhibited, {epsilon}{sub r} {approx} 53.7, Qf{sub o} {approx} 11,532 GHz and {tau}{sub f} {approx} -1.4 ppm/{sup o}C.

36 MATERIALS SCIENCE↗

Method for fabrication of ceramic dielectric films on copper foils

The present invention provides a method for fabricating a ceramic film on a copper foil. The method comprises applying a layer of a sol-gel composition onto a copper foil. The sol-gel composition comprises a precursor of a ceramic material suspended in 2-methoxyethanol. The layer of sol-gel is then dried at a temperature up to about 250.degree. C. The dried layer is then pyrolyzed at a temperature in the range of about 300 to about 450.degree. C. to form a ceramic film from the ceramic precursor. The ceramic film is then crystallized at a temperature in the range of about 600 to about 750.degree. C. The drying, pyrolyzing and crystallizing are performed under a flowing stream of an inert gas. In some embodiments an additional layer of the sol-gel composition is applied onto the ceramic film and the drying, pyrolyzing and crystallizing steps are repeated for the additional layer to build up a thicker ceramic layer on the copper foil. The process can be repeated one or more times if desired.

36 MATERIALS SCIENCE↗

Dielectric Ceramics in Nanosheet Form. Final report

This is the final project report detailing the preparation and chemistry of dielectric nanosheets. The major aim of this project was to develop two-dimensional dielectric materials in parallel with efforts to develop two-dimensional semiconductors. Dielectrics are insulating materials that can be polarized, leading to outstanding ferroelectric, ferromagnetic, piezoelectric, pyroelectric, electrostrictive, and electro-optical properties. Dielectric materials are arguably equally important as metallic and semiconducting materials in device engineering, and thus dielectric nanosheets would be valuable building blocks in multitudinous downscaled applications. The specific goals of this project encompassed the development of innovative chemical synthesis methodologies for preparing dielectric materials in freestanding, two-dimensional <10 nm thickness (nanosheet) form; characterization of the fundamental properties of the resulting nanosheets;

36 MATERIALS SCIENCE↗

Method for fabrication of ceramic dielectric films on copper foils

The present invention provides copper substrate coated with a lead-lanthanum-zirconium-titanium (PLZT) ceramic film, which is prepared by a method comprising applying a layer of a sol-gel composition onto a copper foil. The sol-gel composition comprises a precursor of a ceramic material suspended in 2-methoxyethanol. The layer of sol-gel is then dried at a temperature up to about 250.degree. C. The dried layer is then pyrolyzed at a temperature in the range of about 300 to about 450.degree. C. to form a ceramic film from the ceramic precursor. The ceramic film is then crystallized at a temperature in the range of about 600 to about 750.degree. C. The drying, pyrolyzing and crystallizing are performed under a flowing stream of an inert gas.

36 MATERIALS SCIENCE↗

First-principle calculation and assignment for vibrational spectra of Ba(Mg{sub 1/3}Nb{sub 2/3})O{sub 3} microwave dielectric ceramic

1:2 B-site cation ordered Ba(Mg{sub 1/3}Nb{sub 2/3})O{sub 3} ceramic was synthesized using conventional solid-state reaction at 1600 °C for 12 h. The structure parameters were obtained through Rietveld refinement of X-ray diffraction data. The Raman peak frequencies were obtained by Lorenz fitting on Raman spectrum. Four-parameter semiquantum model was used to fit the infrared (IR) reflectivity spectrum, and the fitted parameters were used to calculate the dielectric permittivity ε and dielectric loss tanδ. A total of 9 active Raman and 16 active IR modes were obtained using first-principle calculations based on density functional theory with local density approximation. All of the vibrational modes were assigned and represented by linear combinations of the symmetry coordinates deduced using group theory analysis. The Raman mode with the highest frequency A{sub 1g}{sup (4)} (789 cm{sup −1}) can be described as the breathing vibration of NbO{sub 6}. The IR modes E{sub u}{sup (1)} (149 cm{sup −1}) and A{sub 2u}{sup (2)} (212 cm{sup −1}), which can be described as the twisting vibrations of Ba–MgO{sub 6}/Ba–NbO{sub 6} on the a–b plane and the stretching vibrations of Ba–MgO{sub 6}/Ba–NbO{sub 6} along the c direction, respectively, are the dominant contributing modes to ε and tanδ. The dielectric property parameters obtained using IR spectrum fittings, first-principal calculations, and microwave measurements were compared.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Low-temperature sintering of temperature-stable LaNbO{sub 4} microwave dielectric ceramics

We demonstrate the correlation between sintering behavior and microstructural observations in low-temperature sintered, LaNbO{sub 4} microwave ceramics. Small CuO additions to LaNbO{sub 4} significantly lowered the sintering temperature from 1250 to 950 {sup o}C. To elucidate the sintering mechanism, the internal microstructure of the sample manipulated by a focused ion beam (FIB) was investigated using transmission electron microscopy (TEM) and energy-dispersive spectroscopy (EDS). LaNbO{sub 4} with 3 wt% CuO sintered at 950 {sup o}C for 2 h possessed the following excellent microwave dielectric properties: a quality factor (Qxf) of 49,000 GHz, relative dielectric constant ({epsilon}{sub r}) of 19.5, and temperature coefficient of resonant frequency ({tau}{sub f}) of 1 ppm/{sup o}C. The ferroelastic phase transformation was also investigated using in situ X-ray diffraction (XRD) to explain the variation of {tau}{sub f} in low-temperature sintered LaNbO{sub 4} as a function of CuO content.

36 MATERIALS SCIENCE↗

Long range B-site cation ordering and Briet–Wigner–Fano line shape of A{sub 1g}-like Raman mode in Nd{sub 1−x}Sm{sub x}(Mg{sub 0.5}Ti{sub 0.5})O{sub 3} microwave dielectric ceramics

Graphical abstract: Display Omitted Highlights: ► Q × f of Nd{sub 1–x}Sm{sub x}(Mg{sub 0.5}Ti{sub 0.5})O{sub 3} are correlated with B-site cation ordering (LRO). ► Correlation between LRO and Γ of A{sub 1g}-like mode in Raman spectrum is observed. ► Reason for asymmetry in A{sub 1g}-like Raman mode in these materials is revealed. ► Briet–Wigner–Fano resonance is confirmed with temperature variation in Raman spectra. -- Abstract: Nd{sub 1−x}Sm{sub x}(Mg{sub 0.5}Ti{sub 0.5})O{sub 3} (x = 0.0–1.0) samples were prepared by solid-state reaction method. Rietveld refinement of X-ray diffraction data was done using P2{sub 1}/n space group with monoclinic symmetry, which supports 1:1 B-site cation ordering. Long range ordering (LRO) parameter decreased up to x = 0.5 and then found to increase with further increase in Sm concentration. The A{sub 1g}-like mode in Raman spectra was observed to possess Briet–Wigner–Fano line shape. The variation in obtained line width of the A{sub 1g}-like mode supported LRO. Microwave dielectric characteristics such as dielectric constant (ε{sub r}), quality factor (Q) and temperature coefficient of resonant frequency (τ{sub f}) were measured in the range of 7–9 GHz. ε{sub r} decreased from 26.5 to 24.9 and τ{sub f} become less negative from −58 ppm/°C to −36 ppm/°C with increase in Sm concentration. Q × f decreased from 47,500 GHz (for x = 0) to 39,800 GHz (for x = 0.5) and then increased to 44,600 GHz (for x = 1).

36 MATERIALS SCIENCE↗

Method for fabrication of crack-free ceramic dielectric films

The invention provides a process for forming crack-free dielectric films on a substrate. The process comprise the application of a dielectric precursor layer of a thickness from about 0.3 .mu.m to about 1.0 .mu.m to a substrate. The deposition is followed by low temperature heat pretreatment, prepyrolysis, pyrolysis and crystallization step for each layer. The deposition, heat pretreatment, prepyrolysis, pyrolysis and crystallization are repeated until the dielectric film forms an overall thickness of from about 1.5 .mu.m to about 20.0 .mu.m and providing a final crystallization treatment to form a thick dielectric film. Also provided was a thick crack-free dielectric film on a substrate, the dielectric forming a dense thick crack-free dielectric having an overall dielectric thickness of from about 1.5 .mu.m to about 20.0 .mu.m.

36 MATERIALS SCIENCE↗

Method for fabrication of crack-free ceramic dielectric films

The invention provides a process for forming crack-free dielectric films on a substrate. The process comprises the application of a dielectric precursor layer of a thickness from about 0.3 .mu.m to about 1.0 .mu.m to a substrate. The deposition is followed by low temperature heat pretreatment, prepyrolysis, pyrolysis and crystallization step for each layer. The deposition, heat pretreatment, prepyrolysis, pyrolysis and crystallization are repeated until the dielectric film forms an overall thickness of from about 1.5 .mu.m to about 20.0 .mu.m and providing a final crystallization treatment to form a thick dielectric film. The process provides a thick crack-free dielectric film on a substrate, the dielectric forming a dense thick crack-free dielectric having an overall dielectric thickness of from about 1.5 .mu.m to about 20.0 .mu.m.

36 MATERIALS SCIENCE↗

Method for fabrication of crack-free ceramic dielectric films

The invention provides a process for forming crack-free dielectric films on a substrate. The process comprises the application of a dielectric precursor layer of a thickness from about 0.3 .mu.m to about 1.0 .mu.m to a substrate. The deposition is followed by low temperature heat pretreatment, prepyrolysis, pyrolysis and crystallization step for each layer. The deposition, heat pretreatment, prepyrolysis, pyrolysis and crystallization are repeated until the dielectric film forms an overall thickness of from about 1.5 .mu.m to about 20.0 .mu.m and providing a final crystallization treatment to form a thick dielectric film. The process provides a thick crack-free dielectric film on a substrate, the dielectric forming a dense thick crack-free dielectric having an overall dielectric thickness of from about 1.5 .mu.m to about 20.0 .mu.m.

36 MATERIALS SCIENCE↗