At least 19 records

Degradation Mechanisms of High Capacity 18650 Cells Containing Si-Graphite Anode and Nickel-Rich NMC Cathode

Application of advanced anode and cathode materials in commercial lithium-ion batteries is attracting attention due to their high capacity. Silicon (Si)/graphite anodes and nickel (Ni)-rich lithium nickel manganese cobalt oxide with layered structures have been paired in commercial 18650 high energy density cells (~270 Wh/kg). It is crucial to investigate the cell performance and the aging behavior of this commercial cell. In this study, we present commercial cell degradation mechanisms by comparing fresh and aged electrodes, including changes of crystal structure, morphology, elemental composition, and electrochemical properties. The quantitative analysis was done based on dV/dQ incremental capacity analysis of 18650 cells. To determine the amount of cyclable lithium ions (Li + ) and active material loss, the lithiation and delithiation capacity were compared for fresh and aged electrodes in half coin cells. Results showed that even with 5% (by mass) of Si added in the anode, cracks occurred across the anode leading to contact loss and thickening of the solid electrolyte interphase (SEI) layer. Additionally, the average fluorine (F) ratio of the aged anodes was higher compared to that of the fresh anodes. More severely, the F content on the Si aggregations on aged anodes increased to as high as 5 times that of the fresh anode, indicating SEI growth, especially on Si particles. Solid 7 Li nuclear magnetic resonance results showed no detectable Li metal deposition on the aged anode. On the cathode side, cracks on the primary particle interfaces contributed to cathode material loss, contact loss, and impedance rise. Furthermore, Li + loss into the thickened SEI layer, particle cracking, and impedance rise are the main reasons behind cell degradation.

25 ENERGY STORAGE↗

Electrochemical modeling of lithium-ion positive electrodes during hybrid pulse power characterization tests.

An electrochemical model was developed to examine hybrid pulsed power characterization (HPPC) tests on the positive electrode of lithium-ion cells. By utilizing the same fundamental equations as in previous electrochemical impedance spectroscopy studies, this investigation serves as an extension of the earlier work and a comparison of the two techniques. The electrochemical model was used to examine performance characteristics and limitations for the positive electrode during HPPC tests. Parametric studies using the electrochemical model and focusing on the positive electrode thickness were employed to examine methods of slowing electrode aging and improving performance.

25 ENERGY STORAGE↗

Survey on aging on electrodes and electrocatalysts in phosphoric acid fuel cells

The processes which contribute to the decay in performance of electrodes used in phosphoric acid fuel cell systems are discussed. Loss of catalytic surface area, corrosion of the carbon support, electrode structure degradation, electrolyte degradation, and impurities in the reactant streams are identified as the major areas for concern.

Stonehart, P.↗

Oxygen electrode bifunctional electrocatalyst NiCo2O4 spinel

A significant increase in energy density may be possible if a two-unit alkaline regenerative H2-O2 fuel cell is replaced with a single-unit system that uses passive means for H2O transfer and thermal control. For this single-unit system, new electrocatalysts for the O2 electrode will be required which are not only bifunctionally active but also chemically and electrochemically stable between the voltage range of about 0.7 and 1.5 V. NiCo2O4 spinel is reported to have certain characteristics that make it useful for a study of electrode fabrication techniques. High surface area NiCo2O4 powder was fabricated into unsupported, bifunctional, PTFE-bonded, porous gas fuel cell electrodes by commercial sources using varying PTFE contents and sintering temperatures. The object of this study is to measure the bifunctional activities of these electrodes and to observe what performance differences might result from different commercial electrode fabricators. O2 evolution and O2 reduction data were obtained at 80 C (31 percent KOH). An irreversible reaction (i.e., aging) occurred during O2 evolution at potentials greater than about 1.5 V. Anodic Tafel slopes of 0.06 and 0.12 V/decade were obtained for the aged electrodes. Within the range of 15 to 25 percent, the PTFE content was not a critical parameter for optimizing the electrode for O2 evolution activity. Sintering temperatures between 300 and 340 C may be adequate but heating at 275 C may not be sufficient to properly sinter the PTFE-NiCo2O4 mixture. Electrode disintegration was observed during O2 reduction. Transport of O2 to the NiCo2O4 surface became prohibitive at greater than about -0.02 A/sq cm. Cathodic Tafel slopes of -0.6 and -0.12 V/decade were assumed for the O2 reduction process. A PTFE content of 25 percent (or greater) appears to be preferable for sintering the PTFE-NiCo2O4 mixture.

Fielder, William L.↗

Auger Electrons as Probes for Composite Micro- and Nano- structured Materials: Application to Solid Electrolyte Interphases in Graphite and Silicon-Graphite Electrodes

In this study, Auger electron spectroscopy (AES) combined with ion sputtering profilometry, Xray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) have been used in a complementary fashion to examine chemical and microstructural changes in graphite (Gr) and silicon/graphite (Si/Gr) blends contained in the negative electrodes of lithium-ion cells. We demonstrate how AES can be used to characterize morphology of the solid-electrolyte interphase (SEI) deposits in such heterogeneous media, complementing well-established methods, such as XPS and SEM. In this way we demonstrate that the SEI does not consist of uniformly thick layers on the graphite and silicon; the thickness of the SEI layers in cycle-life aged electrodes follows an exponential distribution with a mean of ca. 13 nm for the graphite and ca. 20-25 nm for the silicon nanoparticles (with a crystalline core of 50-70 nm in diameter). Furthermore, a “sticky-sphere” model, in which Si nanoparticles are covered with a layer of polymer binder (that is replaced by the SEI during cycling) of variable thickness is introduced to account for the features observed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cycling Performance and Structure Evolution of Co-Free Lithium- and Manganese-Rich Layered Oxides in Lithium-Ion Batteries

Lithium- and manganese-rich (LMR) layered oxides are high-capacity cathode materials that are being considered for electric vehicle (EV) lithium-ion batteries (LIBs). Here, we investigate the electrochemical cycling behavior of cells containing a cobalt-free LMR oxide, 0.3Li 2 MnO 3 ·0.7LiMn 0.5 Ni 0.5 O 2 , paired with either Li or graphite anodes. Two- and three-electrode cells are cycled under varying conditions to examine the effects of oxide activation, upper cutoff voltage, separator type, and electrolyte composition. Post-cycling characterization of harvested electrodes, with electrochemical, X-ray absorption spectroscopy, and solid-state 6 Li nuclear magnetic resonance spectroscopy techniques, are used to correlate cell performance changes with redox state evolution in the oxide and Li inventory shifts in the cell. Our results show that capacity fade and impedance rise primarily originate at the graphite anode and LMR cathode, respectively. Notably, while Ni undergoes reversible redox, Mn shows no evidence of bulk redox activity even in highly-aged electrodes: only relithiated LMR electrodes show some reduction of Mn. Graphite electrodes degrade due to particle isolation and SEI growth, exacerbated by Mn dissolution and deposition on graphite anodes. These findings highlight the coupled structural and electrochemical degradation mechanisms in LMR/graphite cells and underscore lithium inventory retention and electrode interfacial stability as critical factors for enhancing long-term performance.

Badami, Pavan P. [Argonne National Laboratory (ANL↗

Extreme fast charge aging: Correlation between electrode scale and heterogeneous degradation in Ni-rich layered cathodes

Extreme fast charging (XFC) is a key requirement for the adoption of battery-based electric vehicles by the transportation sector. However, XFC has been shown to accelerate degradation, causing the capacity, life, and safety of batteries to deteriorate. There are no systematic studies in the open literature regarding aging modes in Ni-rich Li y Ni 0.a Mn 0.b Co 0.c O 2 (NMCabc) cathodes caused by fast charging. Herein, we report the effects of cathode composition and electrode loading in pouch cells containing NMC532, 622 and 811 paired with graphite and cycled under XFC conditions. The relative anisotropic volume change in the unit cell increases with Ni content in low-loading cells, while it levels up for all three NMC cathodes in high-loading cells because of substantial Li plating. The amounts of lithium plating and heterogeneity on the anode, determined by crystallographic phase quantification, were found to be correlated with electrode loading and cathode heterogeneity. The concentrations of the transition metals deposited on the anodes depend on NMCabc composition in a complex way. More particle cracking and surface degradation was found in NMC811. Here, the findings in this work provide a new understanding of the failure mechanisms and their practical implications for compositional tuning of future high-Ni NMCabc cathode materials during fast charging.

25 ENERGY STORAGE↗

Extreme fast charge aging: Effect of electrode loading and NMC composition on inhomogeneous degradation in graphite bulk and electrode/electrolyte interface

Empowering extreme fast charging (XFC) requires a comprehensive understanding of its application with advanced anode and cathode materials in lithium-ion batteries. No report exists for the full extent of limitations for the anode with crosstalk effect from paired cathode as well as Li plating due to electrode loading under XFC. In this study, a combination of cell testing and multiple length characterization is used to investigate XFC aging mechanism in cells with a low loading of 1.5 mAh cm -2 and high loading of 2.5 mAh cm -2 for graphite (Gr)/Ni-rich LiNi x Mn y Co 1-x-y O 2 (NMCs). Operando XRD mappings show 1.5 mAh cm -2 loadings result in higher strain in graphite for all three cathode types. Among the three NMC cathodes, the graphite from NMC532 and NMC811 cells show comparable strain. Scanning electron microscopy (SEM) images show distinct differences between 6-C-charged anodes in two loadings. Significantly increased electrode thickness can be seen due to more damage in the graphite bulk and accumulation of the electrolyte decomposition products in electrode pores. X-ray photoelectron spectroscopy (XPS) reveals both cathode chemistry and Li plating influence the non-uniform SEI composition on graphite surface. We report higher Ni content in NMC811 promotes the higher levels of salt decomposition on the SEI and formation of higher mass of electrolyte aging products.

25 ENERGY STORAGE↗

Examination of the mechanism for the reversible aging behavior at open circuit when changing the operating temperature of (La 0.8 Sr 0.2 ) 0.95 MnO 3 electrodes

The aging behavior of symmetrical cells, consisting of either (La 0.8 Sr 0.2 ) 0.95 MnO 3 (LSM) or La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 (LSCF) electrodes screen printed on either 8 mol% yttria-stabilized zirconia (YSZ) or Ce 0.8 Gd 0.2 O 2 (GDC) electrolyte substrates, is reported as the symmetrical cell is thermally cycled between 700 °C and 800 °C. For LSM, between 700 °C and 850 °C, the polarization resistance exhibits slow increases or decreases with time (on the order of days) after a quick change in temperature. When increasing the temperature, the polarization resistance decreases with time, and when decreasing the temperature, the polarization resistance slowly increases with time. In a previous work, the authors had explained these results with LSM by connecting the testing conditions to literature reports of surface analysis of LSM thin films which demonstrated a change in the amount of surface cation segregation as a function of temperature. In this work, TEM/EDS/XPS analysis of dense LSM pellets thermally cycled under the same conditions as the symmetrical cells does not indicate any significant reversible change in the surface composition of the LSM pellet between 700 °C and 800 °C. An alternative hypothesis is proposed to explain the relationship between polarization resistance and the LSM cation/anion vacancy concentrations controlled by the Schottky reaction. The timescale of aging behavior is related to the time necessary for the cations to move to or from the LSM surface to adjust to the new equilibrium at each temperature. Furthermore, the relevance in understanding the mechanism behind the aging behavior is emphasized with respect to fuel cell sample/stack modeling as well as to proper testing procedures for reaching reliable conclusions when comparing different electrode samples.

42 ENGINEERING↗

Composition and Impedance Heterogeneity in Oxide Electrode Cross-Sections Detected by Raman Spectroscopy

Lithium-bearing layered transition metal oxides are the materials of choice for positive electrodes in high energy lithium-ion cells being developed for electric vehicle applications. During electrochemical cycling, the loss of mobile lithium-ions due to undesirable side reactions and an increase in cell resistance leads to a decline in the energy and power performance of the cells. This performance loss is often non-uniform across multiple cells, especially for those cycled at high voltages and at high C-rates. This non-uniformity results from inhomogeneous behavior in the battery electrodes, which can lead to localized areas that deteriorate faster than the neighboring regions. Raman spectroscopy is among the many advanced techniques that have been used to probe inhomogeneity in electrode behavior. Typically, Raman spectroscopy of lithium-ion cell electrodes are conducted in the top-down mode, and at-best provide an incomplete, surface biased account of electrode behavior. In contrast, micro-Raman measurements conducted on ion-milled electrode cross-sections provide information from regions that span the full thickness of the electrode. Here, spectroscopy data from pristine, aged, and relithiated/aged positive electrodes are reported. In conclusion, the spectral differences between oxide particles near the top-surface and particles deeper into the aged electrodes highlight a clearly defined non-uniform behavior during cell aging.

36 MATERIALS SCIENCE↗

Reversible aging behavior of La0.8Sr0.2MnO3 electrodes at open circuit

La0.8Sr0.2MnO3 (LSM) electrodes on yttria-stabilized zirconia (YSZ) electrolytes were characterized at open circuit by impedance spectroscopy. An initial irreversible change in the polarization resistance is observed for cells aged with no prior current activation. After the initial break-in, the polarization resistance rises with time at 700 C and decays at 800 C, reversibly, over repeated temperature cycles. The initial irreversible break-in and subsequent reversible cycling behavior suggests multiple processes happening within the time and temperatures measured. The authors propose that these processes are (1) changes in the wetting behavior of the LSM on the YSZ and (2) the reversible segregation/desegregation of cations within LSM. Between 700 C and 800 C, there is a transition temperature at which the segregation behavior of cations to the cathode surface changes. These measurable changes in the impedance behavior of LSM indicate that cation segregation, while considered by some to be part of the cathode activation process, may be dictated by thermodynamic factors, and thus not strictly dependent on the passage of current through the cathode.

99 GENERAL AND MISCELLANEOUS↗

Real time lithium metal calendar aging in common battery electrolytes

Li metal anodes are highly sought after for high energy density applications in both primary commercial batteries and next-generation rechargeable batteries. In this research, Li metal electrodes are aged in coin cells for a year with electrolytes relevant to both types of batteries. The aging response is monitored via electrochemical impedance spectroscopy, and Li electrodes are characterized post-mortem. It was found that the carbonate-based electrolytes exhibit the most severe aging effects, despite the use of LiBF 4 -based carbonate electrolytes in Li/CF x Li primary batteries. Highly concentrated LiFSI electrolytes exhibit the most minimal aging effects, with only a small impedance increase with time. This is likely due to the concentrated nature of the electrolyte causing fewer solvent molecules available to react with the electrode surface. LiI-based electrolytes also show improved aging behavior both on their own and as an additive, with a similar impedance response with time as the concentrated LiFSI electrolytes. Since I − is in its most reduced state, it likely prevents further reaction and may help protect the Li electrode surface with a primarily organic solid electrolyte interphase.

25 ENERGY STORAGE↗

Intracranial electrode implantation produces regional neuroinflammation and memory deficits in rats

Deep brain stimulation (DBS) is an established treatment for advanced Parkinson's disease (PD). The procedure entails intracranial implantation of an electrode in a specific brain structure followed by chronic stimulation. Although the beneficial effects of DBS on motor symptoms in PD are well known, it is often accompanied by cognitive impairments, the origin of which is not fully understood. To explore the possible contribution of the surgical procedure itself, we studied the effect of electrode implantation in the subthalamic nucleus (STN) on regional neuroinflammation and memory function in rats implanted bilaterally with stainless steel electrodes. Age-matched sham and intact rats were used as controls. Brains were removed 1 or 8 weeks post-implantation and processed for in vitro autoradiography with [(3)H]PK11195, an established marker of microglial activation. Memory function was assessed by the novel object recognition test (ORT) before surgery and 2 and 8 weeks after surgery. Electrode implantation produced region-dependent changes in ligand binding density in the implanted brains at 1 as well as 8 weeks post-implantation. Cortical regions showed more intense and widespread neuroinflammation than striatal or thalamic structures. Furthermore, implanted animals showed deficits in ORT performance 2 and 8 weeks post-implantation. Thus, electrode implantation resulted in a widespread and persistent neuroinflammation and sustained memory impairment. These results suggest that the insertion and continued presence of electrodes in the brain, even without stimulation, may lead to inflammation-mediated cognitive deficits in susceptible individuals, as observed in patients treated with DBS.

36 MATERIALS SCIENCE↗

High accuracy in-situ direct gas analysis of Li-ion batteries

Cycling of lithium-ion batteries containing Ni-rich NMC cathodes at high voltage involves intense gas generation. From the safety standpoint, it is critical to understand how different gas species respond to changes of upper cut-off voltages. In this manuscript, we introduce a novel experimental set up for real-time analysis of gas generation in prismatic pouch cells. In a typical experiment, a lithium-ion pouch cell is directly connected to a quadruple mass spectrometer by glass capillary. Pressure difference helps move the generated gases to the mass spectrometer column for full analysis. The gaseous species are probed during both formation cycle and aging cycles in Li-ion pouch cells comprising NMC811 cathode and graphite anode. The gases are generated upon the creation of the solid electrolyte interphase on graphite during the first formation charge. Besides ethylene gas, C 2 H 4 , whose occurrence is related to the decomposition of ethylene carbonate, a minor solvent decomposition happened at a lower voltage is demonstrated to be associated with residue water on the electrode. For aging cycles, three upper cut-off voltages have been selected to investigate the gas evolution behavior upon charging to 4.2, 4.4 and 4.6 V. Higher upper cut-off voltages do not affect the amount of O 2 measured as a part of the generated oxygen could have reacted with electrolytes. Quite similar and low amounts of O 2 remain in the cells upon charging to the selected cut-off voltages. On the other hand, the generation of CO 2 has been found to be very sensitive to upper cut-off voltage. During similar aging cycles, 6167 nmol $g_{NMC}^{-1}$ of CO 2 is generated at 4.6 V, versus 1650 nmol $g_{NMC}^{-1}$ of CO 2 at 4.4 V, versus 91 nmol $g_{NMC}^{-1}$ of CO 2 at 4.2 V.

25 ENERGY STORAGE↗

Process design tools and techno-economic analysis for capacitive deionization

Capacitive deionization (CDI) devices use cyclical electrosorption on porous electrode surfaces to achieve water desalination. Process modeling and design of CDI systems requires accurate treatment of the coupling among input electrical forcing, input flow rates, and system responses including salt removal dynamics, water recovery, energy storage, and dissipation. Techno-economic analyses of CDI further require a method to calculate and compare between a produced commodity (e.g. desalted water) versus capital and operational costs of the system. In this work, we demonstrate a new modeling and analysis tool for CDI developed as an installable Matlab program that allows direct numerical simulation of CDI dynamics and calculation of key performance and cost parameters. The program is provided for free and is used to run open-source Simulink models. The Simulink environment sends information to the program and allows for a drag and drop design space where users can connect CDI cells to relevant periphery blocks such as grid energy, battery, solar panel, waste disposal, and maintenance/labor cost streams. The program allows for simulation of arbitrary current forcing and arbitrary flow rate forcing of one or more CDI cells. We employ validated well-mixed reactor formulations together with a non-linear circuit model formulation that can accommodate a variety of electric double layer sub-models (e.g. for charge efficiency). The program includes a graphical user interface (GUI) to specify CDI plant parameters, specify operating conditions, run individual tests or parameter batch-mode simulations, and plot relevant results. The techno-economic models convert among dimensional streams of species (e.g. feed, desalted water, and brine), energy, and cost and enable a variety of economic estimates including levelized water costs.

42 ENGINEERING↗

Fluoro‐Ethylene‐Carbonate Plays a Double‐Edged Role on the Stability of Si Anode‐Based Rechargeable Batteries During Cycling and Calendar Aging

Abstract The energy storage density of Li‐ion batteries can be improved by replacing graphite anodes with high‐capacity Si‐based materials, though instabilities have limited their implementation. Performance degradation mechanisms that occur in Si anodes can be divided into cycling stability (capacity retention after repeated battery cycles) and calendar aging (shelf life). While cycling instabilities and improvement strategies have been researched intensively, there is little known about the underlying mechanisms that cause calendar aging. In this work, multiple electron microscope techniques are used to explore the mechanism that governs calendar aging from the sub‐nanometer‐to‐electrode scale. Plasma focused ion beam tomography is used to create 3D reconstructions of calendar aged electrodes and revealed the growth of a LiF‐rich layer at the interface between the copper current collector and the silicon material, which can lead to delamination and increased interfacial impendence. The LiF layer appeared to derive from the fluoro‐ethylene‐carbonate electrolyte additive, which is commonly used to improve cycling stability in Si‐based systems. The results reveal that additives necessary to improve cycling stability can cause performance degradation over the long‐term during calendar aging. The results show that high performing, stable systems require careful design to simultaneously mitigate both cycling and calendar aging instabilities.

25 ENERGY STORAGE↗

CRADA: Synthesis and Evaluation of NMC Cathode Materials

Ni-rich NMCs, technologically important cathode materials for lithium-ion batteries were synthesized and studied for this project. Electrodes were also harvested from cycled and/or aged commercial Li-ion cells and examined using high-throughput, ensemble average synchrotron soft x-ray absorption techniques developed at LBNL to observe surface reconstruction in NMC materials (see F. Lin et al. Nature Commun. 5:3529, (2014)). A goal was to observe which cycling and storage conditions lead to degradation of cathode materials, a process that has been implicated in premature failure of the devices in some cases. VW provided pristine electrodes to use as baselines. Cells containing electrodes synthesized at LBNL were cycled or subjected to various storage conditions at LBNL, and VW also provided cycled or aged electrodes from commercial cells with histories of interest.

25 ENERGY STORAGE↗