Unexpected Voltage Fade in LMR-NMC Oxides Cycled below the “Activation” Plateau

A common feature of lithium-excess layered oxides, nominally of composition xLi 2 MnO 3 •(1-x)LiMO 2 (M = transition metal) is a high-voltage plateau (~4.5 V vs. Li/Li + ) in their capacity-voltage profile during the first delithiation cycle. This plateau is believed to result from activation of the Li 2 MnO 3 component, which makes additional lithium available for electrochemical cycling. However, oxides cycled beyond this activation plateau are known to display voltage fade which is a continuous reduction in their equilibrium potential. In this article we show that these oxides display gradual voltage fade even on electrochemical cycling in voltage ranges well below the activation plateau. The average fade is ~0.08 mV-cycle-1 for Li 1.2 Ni 0.15 Mn 0.55 Co 0.1 O 2 vs. Li cells after 20 cycles in the 2–4.1 V range at 55°C; a ~54 mV voltage hysteresis, expressed as the difference in average cell voltage between charge and discharge cycles, is also observed. The voltage fade results from a gradual accumulation of local spinel environments in the crystal structure. Some of these spinel sites result from lithium deficiencies during oxide synthesis and are likely to be at the particle surfaces; other sites result from the migration of transition metal atoms in the partially-delithiated LiMO 2 component into the lithium planes during electrochemical cycling. The observed rate of voltage fade depends on a combination of factors that includes the phase equilibrium between the layered and spinel components and the kinetics of transition metal migration.

Li, Yan↗

Effect of Composition on the Voltage Fade Phenomenon in Lithium-, Manganese-Rich xLiMnO 3 •(1-x)LiNi a Mn b Co c O 2 : A Combinatorial Synthesis Approach

The effect of composition on the voltage fade phenomenon was probed using combinatorial synthesis methods. In compositions that have the general formula, (Li 2 MnO 3 ) a (LiNiO 2 ) b (LiMnO 2 ) c (LiCoO 2 ) d , where 0 ≤ a≤0.83, 0.15 ≤ b ≤ 0.42, 0 ≤ c ≤ 0.85, and 0 ≤ d ≤ 0.30 (a + b + c + d = 1), the dependence of features in the x-ray diffraction pattern and of voltage fade on composition were identified and mapped. The observed values of voltage fade indicated that it displayed some sensitivity to composition, but that the sensitivity was not large. The values of voltage fade were found to be amenable to statistical modeling. The model indicated that it may be possible to lower the value of voltage fade below 0.01% by adjusting the composition of the system; however, the composition is not expected to have the layered–layered structure.

combinatorial synthesis↗

Capacity Fade and Its Mitigation in Li-Ion Cells with Silicon-Graphite Electrodes

In this study we scrutinize the causes for capacity fade in lithium-ion cells containing silicongraphite (Si-Gr) blends in the negative electrode and examine approaches for minimizing this fade. The causal mechanisms are inferred from data obtained by electrochemistry, microscopy, spectroscopy and thermogravimetry techniques. The presence of SiOxFy signals in the Si-Gr electrode, LixPOyFz compounds in the electrolyte, and SiO2 species on the NCM523 positive electrode, highlight the crucial role of hydrolytically generated HF, which accelerates the degradation of Si particles. The hydrolysis could result from residual moisture in the current electrode fabrication process, which uses aqueous binders. Water can also be released when silanol groups on the Si nanoparticles react with HF to form Si-F compounds. We note that the primary cause of capacity fade in the full cells is the loss of solid electrolyte interphase (SEI) integrity resulting from volume changes in Si particles during electrochemical cycling. Adding fluoroethylene carbonate (FEC) to the conventional electrolyte slows capacity fade through the formation of a cross linked polymer with elastomeric properties. Further gains in cell longevity are possible by excluding water during electrode fabrication, using hydrolytically stable lithium salts, and adopting electrolyte systems that provide more elasticity to the SEI layers.

fluoroethylene carbonate↗

In-situ X-ray absorption spectroscopy analysis of capacity fade in nanoscale-LiCoO{sub 2}

The local structure of nanoscale (∼10–40 nm) LiCoO{sub 2} is monitored during electrochemical cycling utilizing in-situ X-ray absorption spectroscopy (XAS). The high surface area of the LiCoO{sub 2} nanoparticles not only enhances capacity fade, but also provides a large signal from the particle surface relative to the bulk. Changes in the nanoscale LiCoO{sub 2} metal-oxide bond lengths, structural disorder, and chemical state are tracked during cycling by adapting the delta mu (Δμ) technique in complement with comprehensive extended X-ray absorption fine structure (EXAFS) modeling. For the first time, we use a Δμ EXAFS method, and by comparison of the difference EXAFS spectra, extrapolate significant coordination changes and reduction of cobalt species with cycling. This combined approach suggests Li–Co site exchange at the surface of the nanoscale LiCoO{sub 2} as a likely factor in the capacity fade and irreversible losses in practical, microscale LiCoO{sub 2}. - Graphical abstract: Electrochemical cycling of Li-ion batteries has strong impact on the structure and integrity of the cathode active material particularly near the surface/electrolyte interface. In developing a new method, we have used in-situ X-ray absorption spectroscopy during electrochemical cycling of nanoscale LiCoO{sub 2} to track changes during charge and discharge and between subsequent cycles. Using difference spectra, several small changes in Co-O bond length, Co-O and Co-Co coordination, and site exchange between Co and Li sites can be tracked. These methods show promise as a new technique to better understand processes which lead to capacity fade and loss in Li-ion batteries. - Highlights: • A new method is developed to understand capacity fade in Li-ion battery cathodes. • Structural changes are tracked during Li intercalation/deintercalation of LiCoO{sub 2}. • Surface structural changes are emphasized using nanoscale-LiCoO{sub 2} and difference spectra. • Full multiple scattering calculations are used to support Δμ analysis.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of cycling temperatures on the voltage fade phenomenon in 0.5Li 2 MnO 3 ·0.5LiNi 0.375 Mn 0.375 Co 0.25 O 2 cathodes

The rate of voltage fade in 0.5Li2MnO3•0.5LiNi0.375Mn0.375Co0.25O2 cathodes was measured in half-cells in a temperature range of 25 to 55°C. On the basis of the dependence of the values of the open-circuit potential with cycle count and temperature, the voltage fade phenomenon seems to consist of two chemical processes: one that can be described using a parabolic rate law and another that uses a linear-with-time law. As the cycling temperature increased, the relative contributions of the two processes changed. On the basis of the overall rate versus temperature data, we believe the two processes may be in competition with one another.

kinetics↗

Structural integrity--Searching the key factor to suppress the voltage fade of Li-rich layered cathode materials through 3D X-ray imaging and spectroscopy techniques

Li-rich layered materials are important cathode compounds used in commercial lithium ion batteries, which, however, suffers from some drawbacks including the so-called voltage fade upon electrochemical cycling. Here, our study employs novel transmission X-ray microscopy to investigate the electrochemical reaction induced morphological and chemical changes in the Li-rich Li 2 Ru 0.5 Mn 0.5 O 3 cathode particles at the meso to nano scale. We performed combined X-ray spectroscopy, diffraction and microscopy experiments to systematically study this cathode material's evolution upon cycling as well as to establish a comprehensive understanding of the structural origin of capacity fade through 2D and 3D fine length scale morphology and heterogeneity change of this material. This work suggests that atomic manipulation (e.g. doping, substitution etc.) or nano engineering (e.g. nano-sizing, heterogeneous structure) are important strategies to mitigate the internal strain and defects induced by extensive lithium insertion/extraction. It also shows that maintaining the structural integrity is the key in designing and synthesizing lithium-rich layered materials with better cycle stability.

25 ENERGY STORAGE↗

Fading study of Harshaw LiF:Mg,Ti thermoluminescence dosimeters exposed to neutron doses

Sensitivity and signal fading were tested in Harshaw LiF:Mg,Ti thermoluminescence dosimeters (TLDs) exposed to neutron and beta/photons doses. A significant difference in the signal fading rate was observed for TLDs exposed to neutrons compared with TLDs exposed to betas. This difference may have been related to differences in glow curves for dosimeters exposed to different beams and to differences in glow curve evolution after exposure. A fading-correction algorithm was developed to correct the cumulative sensitivity + signal fading of TL doses for the fading time t using the formulae: y = 0.147∗exp(-t/4.36) + 0.308∗exp(-t/34.1) + 0.73 for neutrons, and: y = 0.132∗exp(-t/10.72) + 0.174∗exp(-t/31.5) + 0.8 for betas/photons. The formula was validated using the dose recovery test, where the average deviation of fading-corrected doses from delivery doses was within 1%. In conclusion, the proposed fading-correction approaches may significantly improve the accuracy of Harshaw TL dosimetry with LiF:Mg,Ti cards for both neutron and beta/gamma irradiation.

61 RADIATION PROTECTION AND DOSIMETRY↗

The FADE mass-stat: A technique for inserting or deleting particles in molecular dynamics simulations

The emergence of new applications of molecular dynamics (MD) simulation calls for the development of mass-statting procedures that insert or delete particles on-the-fly. In this paper we present a new mass-stat which we term FADE, because it gradually “fades-in” (inserts) or “fades-out” (deletes) molecules over a short relaxation period within a MD simulation. FADE applies a time-weighted relaxation to the intermolecular pair forces between the inserting/deleting molecule and any neighbouring molecules. The weighting function we propose in this paper is a piece-wise polynomial that can be described entirely by two parameters: the relaxation time scale and the order of the polynomial. FADE inherently conserves overall system momentum independent of the form of the weighting function. We demonstrate various simulations of insertions of atomic argon, polyatomic TIP4P water, polymer strands, and C{sub 60} Buckminsterfullerene molecules. We propose FADE parameters and a maximum density variation per insertion-instance that restricts spurious potential energy changes entering the system within desired tolerances. We also demonstrate in this paper that FADE compares very well to an existing insertion algorithm called USHER, in terms of accuracy, insertion rate (in dense fluids), and computational efficiency. The USHER algorithm is applicable to monatomic and water molecules only, but we demonstrate that FADE can be generally applied to various forms and sizes of molecules, such as polymeric molecules of long aspect ratio, and spherical carbon fullerenes with hollow interiors.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

SU-E-T-222: Investigation of Pre and Post Irradiation Fading of the TLD100 Thermoluminescence Dosimetry for Photon Beams

Purpose: The pre-irradiation and post-irradiation fading of the Thermoluminescense dosimeter signals were investigated in this study. Methods: Two groups of TLD chips with pre-determined ECC values were used in this study. The two groups were divided into 6 series, each composing of 5 TLD chips.The first group was used for pre-irradiation fading. 5 TLDs were exposed to a known amount of radiation from Cs-137 source, and were read out the next day. After seven days, the other 5 TLDs were exposed to the same amount of radiation and were read out after a day. The other series of 5 TLDs were also exposed after 7,19,28, 59, and 90 days, and were read out a day after irradiation. The loss in TLD signal were obtained for all the above cases. The second group, was used for postirradiation fading. All the TLDs of this group were exposed to a known amount of radiation from Cs-137 source. The 6 series composed of 5 TLDs were read out after 1,7,19,28,59, and 90 days. The above-mentioned procedures for obtaining pre-irradiation, and post-irradiation fading were performed for three storage temperatures (25°C, 4°C, and −18°C). Results: According to the results obtained in this study, in case of pre-irradiation fading study, the signal losses after 90 days are 12%, 24%, and 17% for 25°C, 4°C, and −18°C respectively. In case of post-irradiation fading study, the sensitivity losses after 90 days are 25%, 216%, and 20% for 25°C, 4°C, and −18°C respectively. Conclusion: The results indicate that the optimized time between exposing and reading out, and also the optimized time between annealing and exposing is 1 day.The reduction of Storage temperature will reduce the post-irradiation fading, While temperature reduction does not have any effect on pre-irradiation fading.

60 APPLIED LIFE SCIENCES↗

Hierarchical Fractional Advection-Dispersion Equation (FADE) to Quantify Anomalous Transport in River Corridor over a Broad Spectrum of Scales: Theory and Applications

Fractional calculus-based differential equations were found by previous studies to be promising tools in simulating local-scale anomalous diffusion for pollutants transport in natural geological media (geomedia), but efficient models are still needed for simulating anomalous transport over a broad spectrum of scales. This study proposed a hierarchical framework of fractional advection-dispersion equations (FADEs) for modeling pollutants moving in the river corridor at a full spectrum of scales. Applications showed that the fixed-index FADE could model bed sediment and manganese transport in streams at the geomorphologic unit scale, whereas the variable-index FADE well fitted bedload snapshots at the reach scale with spatially varying indices. Further analyses revealed that the selection of the FADEs depended on the scale, type of the geomedium (i.e., riverbed, aquifer, or soil), and the type of available observation dataset (i.e., the tracer snapshot or breakthrough curve (BTC)). When the pollutant BTC was used, a single-index FADE with scale-dependent parameters could fit the data by upscaling anomalous transport without mapping the sub-grid, intermediate multi-index anomalous diffusion. Pollutant transport in geomedia, therefore, may exhibit complex anomalous scaling in space (and/or time), and the identification of the FADE’s index for the reach-scale anomalous transport, which links the geomorphologic unit and watershed scales, is the core for reliable applications of fractional calculus in hydrology.

97 MATHEMATICS AND COMPUTING↗

Probing Sources of Capacity Fade in LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622): An Operando XRD Study of Li/NMC622 Batteries during Extended Cycling

LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) is one of the most promising Li-ion battery cathodes as it delivers high capacity at high potentials. However high potentials also lead to decreases in capacity retention where the disintegration of the secondary particles has been implicated as a major driving force of this capacity fade. This has been attributed to anisotropic lattice changes and increased microstrain during cycling. To probe how these factors affect capacity fade, Li/NMC622 batteries were cycled from 3-4.3 or 4.7 V and probed with operando X-ray diffraction over the 1st, 2nd, and 101st cycles. Further characterization with scanning electron microscopy, and inductively coupled plasmaoptical emission spectroscopy was also performed. The use of operando XRD over many cycles allowed for the collection of detailed structural information in real time over a time frame in which fading can be observed. During the first two cycles, the cells charged to 4.7 V exhibit increased anisotropic lattice changes as compared to the cells charged to 4.3 V. Upon the 101st cycle, when significant fade has been observed, the cells charged to 4.3 and 4.7 V show identical lattice changes to one another, while the 4.7 V charge limit induces more microstrain. This shows that elevated microstrain at high charge limits is a major driver for particle disintegration in NMC622 cathodes. This study provides important insights into the mechanisms of particle disintegration and capacity fade in NMC/Li-ion batteries, which will enable the design of NMC electrodes that deliver both higher capacities and exhibit better capacity retention.

25 ENERGY STORAGE↗

Predicting Li-Ion Battery Capacity Fade Using Early-Life Data and a Hybrid Data-Driven Gaussian Process-Bayesian Regression Approach

Accurately predicting Li-ion battery capacity trajectories using early-life data can dramatically improve battery-life understandings and be used to rapidly evaluate design/cost/performance trade-offs when developing new battery materials. Accurate early-life predictions enable researchers to quickly iterate over cell designs and material precursor properties without consistently cycling cells to failure. To this end, we present a toolbox that uses a combined Gaussian Process and Bayesian regression approach that capitalizes on signals other than just capacity (e.g., dQ/dV, voltage drops) to rapidly predict capacity-fade trajectories. The prediction tool uses Bayesian regression to fit functional forms, e.g., power law, sigmoids, etc., to predict capacity-fade dynamics. By fitting functional forms, the capacity fade can be interrogated at any point in the future, allowing for early cell-failure prediction. Additionally, Bayesian regression allows for accurate uncertainty estimates that account for cell-to-cell variability (aleatoric uncertainty) and the lack of observation data (epistemic uncertainty). By only using early cycle data to predict the capacity fade trajectory, uncertainty bounds at end-of-life can be extremely large. The large uncertainty bounds are further exacerbated because there is no systematic way to define the prior distribution of the functional forms' parameters. We improve our the predicted trajectory confidence interval of our predicted trajectory using two methods. First, we shows that a small amount of held-out cycling data is sufficientuse some train cells, that have been cycled to failure to derive information regarding the appropriate prior distributions for the functional forms' parameters of the functional form, effectively leading to data-driven priors.. We propose constructing the data-driven priors by first running a Bayesian regression starting with uninformed priors to generate intermediate cell-specific posterior parameter distributions. These posterior distributions are combined using a Ggaussian mixture model for each parameter to create the data-driven priors. These mixture models serve as the data-driven prior distributions for the parameters for. Second, we derive multiple features, e.g., C_dchg 0.5 DoD 0.5, log (|mean(dQ/dV_(w_3-w_0 ) (V)|), etc., from the train cellsheld-out cycling data, identify which the features are that best predicting capacity at early/mid-life cycles, and then create Ggaussian process regression models that are used for predicting capacity at early/mid-life cycles for the test cells (see blue dots with error bars in Fig 1b). Finally, these predicted data-points are used in addition to the actual early cycle data capacity fade to construct the Bayesian regression trajectory for the test cell s. Notably. We note that these two methods are complementary and can be combined with each other. We evaluate the performance of our proposed method on an testing open-source dataset from Iowa State University and Iowa Lakes Community College (ISU-ILCC). This dataset comprises of 251 nickel-manganese-cobalt/graphite Lithium-ion cells that are cycled under 63 different conditions. We compute the mean average percentage error (MAPE) and negative log predictive density (NLPD) to quantify the efficacy of our method. Our initial findings suggest that, when only few observations are available, for test cells, when using only Bayesian regression with uninformed priors, a power law functional provides the most accurate predictions. with very few data points. However, asHowever, a the number of data points increases, a twin sigmoidal function becomes more accurate as the number of observations further increases. We also find that using as little as 10% of the data set towards generating data-driven priors can lead to significant improvement in prediction accuracy when using early cycle data. Lastly, we found that augmenting early-cycle data with Gaussian process-predicted capacity data for Bayesian regression greatly improves the prediction accuracy. We will present a comprehensive comparison of our methods to other methods available in the literature and apply this method to additional battery datasets.

42 ENGINEERING↗

Fading AGN Candidates: AGN Histories and Outflow Signatures

We consider the energy budgets and radiative history of eight fading active galactic nuclei (AGNs), identified from an energy shortfall between the requirements to ionize very extended (radius > 10 kpc) ionized clouds and the luminosity of the nucleus as we view it directly. All show evidence of significant fading on timescales of ≈50,000 yr. We explore the use of minimum ionizing luminosity Q {sub ion} derived from photoionization balance in the brightest pixels in H α at each projected radius. Tests using presumably constant Palomar–Green QSOs, and one of our targets with detailed photoionization modeling, suggest that we can derive useful histories of individual AGNs, with the caveat that the minimum ionizing luminosity is always an underestimate and subject to uncertainties about fine structure in the ionized material. These consistency tests suggest that the degree of underestimation from the upper envelope of reconstructed Q {sub ion} values is roughly constant for a given object and therefore does not prevent such derivation. The AGNs in our sample show a range of behaviors, with rapid drops and standstills; the common feature is a rapid drop in the last ≈2×10{sup 4} yr before the direct view of the nucleus. The e -folding timescales for ionizing luminosity are mostly in the thousands of years, with a few episodes as short as 400 yr. In the limit of largely obscured AGNs, we find additional evidence for fading from the shortfall between even the lower limits from recombination balance and the maximum luminosities derived from far-infrared fluxes. We compare these long-term light curves, and the occurrence of these fading objects among all optically identified AGNs, to simulations of AGN accretion; the strongest variations over these timespans are seen in models with strong and local (parsec-scale) feedback. We present Gemini integral-field optical spectroscopy, which shows a very limited role for outflows in these ionized structures. While rings and loops of emission, morphologically suggestive of outflow, are common, their kinematic structure shows some to be in regular rotation. UGC 7342 exhibits local signatures of outflows <300 km s{sup −1}, largely associated with very diffuse emission, and possibly entraining gas in one of the clouds seen in Hubble Space Telescope images. Only in the Teacup AGN do we see outflow signatures of the order of 1000 km s{sup −1}. In contrast to the extended emission regions around many radio-loud AGNs, the clouds around these fading AGNs consist largely of tidal debris being externally illuminated but not displaced by AGN outflows.

79 ASTRONOMY AND ASTROPHYSICS↗