Search NASA⌕ Search

SEARCH · Search NASA

Results for “fracture initiation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Dynamic Fracture Initiation Toughness at Elevated Temperatures With Application to the New Generation of Titanium Aluminide Alloys

Recently, a new generation of titanium aluminide alloy, named Gamma-Met PX, has been developed with better rolling and post-rolling characteristics. I'revious work on this alloy has shown the material to have higher strengths at room and elevated temperatures when compared with other gamma titanium aluminides. In particular, this new alloy has shown increased ductility at elevated temperatures under both quasi-static and high strain rate uniaxial compressive loading. However, its high strain rate tensile ductility at room and elevated temperatures is limited to approx. 1%. In the present chapter, results of a study to investigate the effects of loading rate and test temperature on the dynamic fracture initiation toughness in Gamma-Met PX are presented. Modified split Hopkinson pressure bar was used along with high-speed photography to determine the crack initiation time. Three-point bend dynamic fracture experiments were conducted at impact speeds of approx. 1 m/s and tests temperatures of up-to 1200 C. The results show that thc dynamic fracture initiation toughness decreases with increasing test temperatures beyond 600 C. Furthermore, thc effect of long time high temperature air exposure on the fracture toughness was investigated. The dynamic fracture initiation toughness was found to decrease with increasing exposure time. The reasons behind this drop are analyzed and discussed.

Shazly, Mostafa↗

Impact of position and density of nanoscale voids on fracture initiation in iron from phase field fracture simulation

Understanding the impact of these bubbles on crack propagation, like that of helium bubble-induced cracking in irradiated materials is incredibly complex. A useful first study towards understanding bubble effects on fracture is to examine how voids impact fracture first. In this work, we used phase-field fracture simulations to examine the influence of voids and their distribution on Mode I fracture in Fe. Assuming brittle fracture, two simulation configurations were considered: (1) nanoscale systems with one or two voids, and (2) nanoscale systems with an experimentally relevant distribution of voids, with up to 20% void area. Results from simulations with one and two voids showed that voids within 10 nm of a crack tip reduce the stress required for crack growth, with the magnitude of reduction depending on void-to-crack orientation. Comparisons with linear elastic fracture mechanics and evaluation of one versus two void systems revealed deviations from linear superposition, implying complex interactions between void and crack tip stress fields. In multi-void simulations, as void sizes increase, the nearest void to the crack tip exerts a greater influence on fracture stress than the overall porosity. Furthermore this study provides valuable insights into the relationship between void size and concentration, and the stress necessary for crack growth, marking a step forward towards understanding He bubble-induced fracture in ferrous materials.

36 MATERIALS SCIENCE↗

The Relationship Between Constraint and Ductile Fracture Initiation as Defined by Micromechanical Analyses

The use of small laboratory specimens to predict the integrity of large, complex structures relies on the validity of single parameter fracture mechanics. Unfortunately, the constraint loss associated with large scale yielding, whether in a laboratory specimen because of its small size or in a structure because it contains shallow flaws loaded in tension, can cause the breakdown of classical fracture mechanics and the loss of transferability of critical, global fracture parameters. Although the issue of constraint loss can be eliminated by testing actual structural configurations, such an approach can be prohibitively costly. Hence, a methodology that can correct global fracture parameters for constraint effects is desirable. This research uses micromechanical analyses to define the relationship between global, ductile fracture initiation parameters and constraint in two specimen geometries (SECT and SECB with varying a/w ratios) and one structural geometry (circumferentially cracked pipe). Two local fracture criteria corresponding to ductile fracture micromechanisms are evaluated: a constraint-modified, critical strain criterion for void coalescence proposed by Hancock and Cowling and a critical void ratio criterion for void growth based on the Rice and Tracey model. Crack initiation is assumed to occur when the critical value in each case is reached over some critical length. The primary material of interest is A516-70, a high-hardening pressure vessel steel sensitive to constraint; however, a low-hardening structural steel that is less sensitive to constraint is also being studied. Critical values of local fracture parameters are obtained by numerical analysis and experimental testing of circumferentially notched tensile specimens of varying constraint (e.g., notch radius). These parameters are then used in conjunction with large strain, large deformation, two- and three-dimensional finite element analyses of the geometries listed above to predict crack initiation loads and to calculate the associated (critical) global fracture parameters. The loads are verified experimentally, and microscopy is used to measure pre-crack length, crack tip opening displacement (CTOD), and the amount of stable crack growth. Results for A516-70 steel indicate that the constraint-modified, critical strain criterion with a critical length approximately equal to the grain size (0.0025 inch) provides accurate predictions of crack initiation. The critical void growth criterion is shown to considerably underpredict crack initiation loads with the same critical length. The relationship between the critical value of the J-integral for ductile crack initiation and crack depth for SECT and SECB specimens has been determined using the constraint-modified, critical strain criterion, demonstrating that this micromechanical model can be used to correct in-plane constraint effects due to crack depth and bending vs. tension loading. Finally, the relationship developed for the SECT specimens is used to predict the behavior of circumferentially cracked pipe specimens.

Panontin, Tina L.↗

Fracture initiation and propagation in a cylindrical shell containing an initial surface flaw

An attempt is made to provide the necessary analytical tools for the application of two different types of fracture criteria to shell structures. Of particular interest is the problem of fracture propagation and arrest in a cylindrical pressure vessel containing an initial surface flaw. It is assumed that the flaw has the most unfavorable geometry and orientation, namely, it is a crack lying on a meridional plane. Stress intensity factor for a part-through crack, and a surface or internal crack with a fully yielded net ligament are considered. Attention is given to constant delta curves for depressurization studies and to depressurization and crack arrest in pressure vessels.

Erdogan, F.↗

Interface Finite Elements for the Analysis of Fracture Initiation and Progression

Progressive failure analyses (PFA) are important for the prediction of residual strength and damage tolerance of vehicle structures, and to predict the energy absorbing capability of vehicle structures under crash-type loads. Typically continuum damage mechanics (CDM) and fracture mechanics (FM) are the methods used for PFA. The method of interfacial damage mechanics (IDM) is used for PFA in this research. IDM has capabilities intermediate between CDM and FM, and is used to numerically model the initiation, growth, and arrest of cracks. IDM smooths the stress singularity at the crack tip, and is easily adaptable with other nonlinearties such as plasticity and material damage. IDM is implemented by user-defined interface elements in the ABAQUS/ Standard structural analysis software package. The structural components selected to demonstrate the effectiveness PFA using interface elements are, for the most part, those with published test data. These structural components were subjected to quasi-static loading in the tests. Thus, the ABAQUS analyses are used to predict geometrically and materially nonlinear equilibrium states. Impact loading, dynamic fracture, reflected stress waves, inertia, and time dependent material behavior are not considered.

Ambur, Damodar R.↗

DECOVALEX-2023: Task A Final Report

Task A, also known as HGFrac, examines the fracturing processes that may occur in the Callovo-Oxfordian claystone (COx) in the context of the high-level (HLW) and intermediate-level long-lived (ILW-LL) radioactive waste repository in France. Understanding these processes and improving numerical models to reproduce them will aid in the design, optimization, and safety of the repository. Heat and gas fracturing are studied in two independent subtasks following a stepwise approach: laboratory tests/benchmark exercises, in-situ experiment, and finally, an application case. The in-situ heater experiment aimed to thermally induce a hydraulic fracture; temperature and pore pressure were monitored to detect any evidence of fracturing. The in-situ gas injection experiment aimed to study the effect of the stress orientation and gas injection kinetics on the gas fracturing process. The occurrence of fracturing was monitored by gas pressure measured in the injection interval. In both experiments, the excavation-induced fracture network around the heater/injection boreholes played an important role in the reduction of the compressive stress state, leading to both a tensile and shear failure response of the COx. During the first two years of the project, the research teams working on each task developed and/or proposed numerical approaches for reproducing the occurrence of fracturing in the in-situ experiments. The failure criteria were defined by reproducing the measurements from laboratory extension tests for the heat fracturing subtask. In the gas fracturing subtask, their approaches were used for simulating several benchmark exercises, and an inter-comparison between models was carried out. In both tasks, the developed approaches were compared with a simplified approach considering poro-elasticity for the mechanical behaviour of the COx. Most of the developed approaches are based on a continuous medium that takes into account variations in hydraulic properties due to mechanical degradation, such as plastic deformation or damage. Other approaches implicitly modelled weak planes or embedded discontinuities to reproduce fracture propagation. The potential for fracture initiation was also studied through of a discrete approach. In the second half of the project, the research teams mainly focused on interpretative modelling of two in-situ experiments and a blind prediction exercise to test their respective approaches. The models developed by the research teams were also applied at the repository scale to evaluate fracture initiation in a case study under vi unfavourable conditions, particularly in terms of spacing between High-Level Waste cells. The results showed that the poro-elasticity approach could be an efficient tool for understanding the main processes occurring in the COx. One example is the explicit representation of the excavation-induced fracture network around the boreholes, which yielded acceptable results compared to the measurement data. However, advanced approaches were needed to evaluate the potential increase of the excavation-induced fracture network extend and better understand fracture initiation. The stress analyses carried out by the teams revealed that hydraulic boundary conditions had a strong impact on fracture initiation in the heater experiment. Furthermore, in most cases, the results required higher pore pressure increments to reach fracturing than those measured in the experiment. This implies that the measurements may have been biased by the packer’s capacity to fully isolate the piezometric chambers, leading to lower pressures. On the contrary, there was no agreement on the fracturing mode, as some reported either shear or tensile fracturing, while others reported a combination of the two modes. In the case of gas fracturing, the research teams were limited to the comparison of a single point, which complicated their task. Nonetheless, the numerical results were able to reproduce the measurements and capture processes such as longitudinal gas flow through the excavation-induced fracture network, as suggested by some evidence in the observation piezometric chambers. The numerical models also agreed with the measurements in the sense of higher probability of developing along the injection borehole than radially towards the sound rock. The approaches developed by the research teams showed that they are capable of analysing and reproducing fracture initiation in the COx. However, areas of future work should focus on the fracture propagation and fracture aperture, which were out of the scope of this task. To this end, additional data must be gathered for the parameter characterisation and validation of the numerical models. Nonetheless, various approaches showed promising results as they were able to reproduce fracture development under certain conditions.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Plastic intensity factors for cracked plates subjected to biaxial loading

An elastic-plastic analysis is performed for an infinite plate under plane stress conditions which contains a finite line crack and is subjected to biaxial loading. In the large scale yielding range, the amplitude of the dominant singularity at the crack tip, the plastic stress (or strain) intensity factor, is found to depend on the magnitude of loading parallel to the crack direction. The predicted value for the fracture initiation stress which is based on a plastic intensity factor fracture criterion, increases under lateral, tensile loading. Compressive loading parallel to the crack has the opposite effect on the fracture initiation stress.

Hilton, P. D.↗

Failure mechanics of fiber composite notched charpy specimens

A finite element stress analysis was performed to determine the stress variation in the vicinity of the notch and far field of fiber composites Charpy specimens (ASTM Standard). NASTRAN was used for the finite element analysis assuming linear behavior and equivalent static load. The unidirectional composites investigated ranged from Thornel 75 Epoxy to S-Glass/Epoxy with the fiber direction parallel to the long dimension of the specimen. The results indicate a biaxial stress state exists in (1) the notch vicinity which is dominated by transverse tensile and interlaminar shear and (2) near the load application point which is dominated by transverse compression and interlaminar shear. The results also lead to the postulation of hypotheses for the predominant failure modes, the fracture initiation, and the fracture process. Finally, the results indicate that the notched Charpy test specimen is not suitable for assessing the impact resistance of nonmetallic fiber composites directly.

Chamis, C. C.↗

Static and dynamic strain energy release rates in toughened thermosetting composite laminates

In this work, the static and dynamic fracture properties of several thermosetting resin based composite laminates are presented. Two classes of materials are explored. These are homogeneous, thermosetting resins and toughened, multi-phase, thermosetting resin systems. Multi-phase resin materials have shown enhancement over homogenous materials with respect to damage resistance. The development of new dynamic tests are presented for composite laminates based on Width Tapered Double Cantilevered Beam (WTDCB) for Mode 1 fracture and the End Notched Flexure (ENF) specimen. The WTDCB sample was loaded via a low inertia, pneumatic cylinder to produce rapid cross-head displacements. A high rate, piezo-electric load cell and an accelerometer were mounted on the specimen. A digital oscilloscope was used for data acquisition. Typical static and dynamic load versus displacement plots are presented. The ENF specimen was impacted in three point bending with an instrumented impact tower. Fracture initiation and propagation energies under static and dynamic conditions were determined analytically and experimentally. The test results for Mode 1 fracture are relatively insensitive to strain rate effects for the laminates tested in this study. The test results from Mode 2 fracture indicate that the toughened systems provide superior fracture initiation and higher resistance to propagation under dynamic conditions. While the static fracture properties of the homogeneous systems may be relatively high, the apparent Mode 2 dynamic critical strain energy release rate drops significantly. The results indicate that static Mode 2 fracture testing is inadequate for determining the fracture performance of composite structures subjected to conditions such as low velocity impact. A good correlation between the basic Mode 2 dynamic fracture properties and the performance is a combined material/structural Compression After Impact (CAI) test is found. These results underscore the importance of examining rate-dependent behavior for determining the longevity of structures manufactured from composite materials.

Cairns, Douglas S.↗

Friction and wear of ceramics

The adhesion, friction, wear and lubricated behaviors of both oxide and non-oxide ceramics are reviewed. Ceramics are examined in contact with themselves, other harder materials and metals. Elastic, plastic and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Grit size effects in two- and three-body abrasive wear are observed for ceramics. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing.

Buckley, D. H.↗

Friction and wear of ceramics

The adhesion, friction, wear, and lubricated behaviors of both oxide and non-oxide ceramics are reviewed. Ceramics are examined in contact with themselves, other harder materials, and metals. Elastic, plastic, and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Grit size effects in two and three body abrasive wear are observed for ceramics. Both the free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing.

Buckley, Donald H.↗

Tribological properties of structural ceramics

The tribological and lubricated behavior of both oxide and nonoxide ceramics are reviewed in this chapter. Ceramics are examined in contact with themselves, other harder materials and metals. Elastic, plastic and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as has been observed with metals. Grit size effects in two and three body abrasive wear are observed for ceramics. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing. Ceramics compositions both as coatings and in composites are described for the high temperature lubrication of both alloys and ceramics.

Buckley, D. H.↗

Tribological properties of structural ceramics

The tribological and lubricated behavior of both oxide and nonoxide ceramics are reviewed in this chapter. Ceramics are examined in contact with themselves, other harder materials and metals. Elastic, plastic and fracture behavior of ceramics in solid state contact is discussed. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as has been observed with metals. Grit size effects in two and three body abrasive wear are observed for ceramics. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Surface contaminants affect friction and adhesive wear. For example, carbon on silicon carbide and chlorine on aluminum oxide reduce friction while oxygen on metal surfaces in contact with ceramics increases friction. Lubrication increases the critical load necessary to initiate fracture of ceramics both in indentation and with sliding or rubbing. Ceramics compositions both as coatings and in composites are described for the high temperature lubrication of both alloys and ceramics.

Buckley, Donald H.↗

Effects of loading rate and temperature on dynamic fracture of ceramic matrix composites

A hybrid experimental-numerical procedure was used to determine the dynamic fracture initiation toughnesses and the dynamic stress intensity factors of alumina, TiB2-particulate/SiC-matrix, and SiC(w)/Al2O3-matrix composites at room and elevated temperatures under static and impact loadings. The dynamic fracture initiation toughnesses at room and elevated temperatures were greater than the corresponding static fracture toughness. The crack velocity versus the dynamic stress intensity factor relations showed minor differences due to temperature changes but significant differences due to the change in loading rates.

Yang, K. H.↗

Fundamental tribological properties of ceramics

When a ceramic is brought into contact with itself, another ceramic, or a metal, strong bond forces can develop between the materials. Adhesion between a ceramic and itself or another solid are discussed from a theoretical consideration of the nature of the surfaces and experimentally by relating bond forces to the interface resulting from solid state contact. Elastic, plastic, and fracture behavior of ceramics in solid-state contact are discussed as they relate to friction and wear. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Lubrication is found to increase the critical load necessary to initiate fracture of ceramics with sliding or rubbing contact.

Buckley, D. H.↗

Fundamental tribological properties of ceramics

When a ceramic is brought into contact with itself, another ceramic, or a metal, strong bond forces can develop between the materials. Adhesion between a ceramic and itself or another solid are discussed from a theoretical consideration of the nature of the surfaces and experimentally by relating bond forces to the interface resulting from solid state contact. Elastic, plastic, and fracture behavior of ceramics in solid-state contact are discussed as they relate to friction and wear. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Lubrication is found to increase the critical load necessary to initiate fracture of ceramics with sliding or rubbing contact.

Buckley, D. H.↗