Microstructure and texture evolution of friction stir lap welded dissimilar multi-aluminum stack

Here this work investigates the microstructural evolution of a dissimilar multiple-aluminum alloy stack (AA7055, AA7055, AA6022) produced by friction stir lap welding (FSLW). A through-thickness analyses of grain orientation map, grain size and distribution, strain distribution, and texture evolution by electron backscattered diffraction-based characterization technique were performed. Two different welding parameters (combination of tool rotation and traverse speed) were used to study the effects of the welding parameters on these microstructural characteristics. The study shows that higher welding speed and higher rotation speed of the FSLW tool yield finer grains. FSLW resulted in shear texture formation in the weld regions due to high welding speeds. This texture development in the nugget zone is consistent with shear deformation, and (111) pole figures show ideal shear texture components. The Stir Zone (SZ) exhibits shear texture (A/A ̅ and B/B ̅ components), consistent with other shear-assisted processes. Recrystallization mechanisms observed are CDRX in SZ and DDRX in TMAZ (Thermo-Mechanically Affected Zone). Interface analysis reveals the presence of oxide layers between different aluminum sheets, affecting joint mechanical performance. The mechanical property of the lap welded joints was presented in terms of microhardness distribution across the weld cross section. Slightly higher hardness in higher speed welding setup was observed throughout the SZ and AA6022 layer, indicating greater grain refinement and uniform grain structure distribution.

36 MATERIALS SCIENCE↗

THE ROLE OF FRACTURE PROPERTIES ON LAP JOINT STRENGTH OF FRICTION STIR WELDED AA7055-T6 SHEETS

Friction stir lap welded (FSLW) joints have weight-saving potential in aluminum-intensive automotive assembly. However, FSLW also modifies the material microstructure close to the joint. Optimizing the FSLW process requires understanding the relationship between the strength and the joint's microstructure. In previous studies, efforts have been dedicated to determining the effects of local softening, the shape of the oxide line, and porosity. However, the impact of changes to the fracture properties on the joint's strength has not been studied. In this work, strength testing, and simulations, aided by material characterization, were used to determine the role of fracture properties on the shear strength of a 3-sheet (aluminum alloys 7055-7055-6022) lap joint. Characterization involved testing for fracture properties in the weld region. This data was then implemented into finite element simulations. As a result, the joint strength was predicted with a deviation of less than 6% from the experimental value. Comparison with strength prediction using only the base metal properties indicates that fracture property in the nugget region determines the strength of AA7055 FSLW.

Finite element analysis, Friction stir welding, ma↗

Numerical Simulation and Experimental Validation of Joint Performance in Aluminum-Steel Lap Welds Formed by Friction Stir Dovetailing

Friction stir dovetailing (FSD) is a new dissimilar material joining process that simultaneously forms a mechanical interlock and metallurgical bond at the dissimilar material interface. This work presents development of a modeling and simulation approach to predict mechanical performance of FSD thick section aluminum to steel joints. A finite element analysis (FEA) was carried out in order to predict the load-carrying capacity and failure location for aluminum thicknesses between 12.7 mm and 50.8 mm with different numbers of dovetails. The numerical results and corresponding experimental investigation are in agreement and suggest that the developed methods can be used effectively for design and analysis of FSD joints using standard FEA tools.

Friction stir dovetailing, Friction stir welding, ↗

Stress characterization for friction-stir-welded electric vehicle battery trays with application of neutron diffraction

The battery tray is an essential component that protects and controls battery-cell temperatures in electric and plug-in hybrid vehicles. The functional stress limit of the battery tray heavily depends on the residual stress acquired from the manufacturing process. Consequently, exceeding the stress limit of the battery tray during operation could compromise the battery-cell banks and may risk the vehicle's safety. Hence, understanding residual stress formation is vital for design and safety concerns. Here, in the current study, AA 6061-plates were friction stir welded to an A365 high-pressure die-cast battery tray to create sealed coolant channels in the battery tray. However, this multi-material lap friction stir weld introduces residual stress into the battery tray, resulting in distortion. This distortion was mitigated using burnishing or coining operations, though straightening the battery tray had initially unknown effects on the residual stress. Therefore, neutron diffraction was utilized to characterize residual stresses after straightening. The results indicate that the friction stir welding (FSW) operation generated residual stresses exceeding the yield strength of the material, consequently deforming the battery tray by ±3 mm from the pre-weld geometry. The burnishing operation reduced the residual stresses below the material's yield strength while restoring the tray to within ±0.75 mm of the pre-weld geometry. Similarly, the coining operation restored the battery tray to within ±0.75 mm of the pre-weld geometry, however, increasing the number of locations where the residual stress exceeds the yield strength of the material.

36 MATERIALS SCIENCE↗

Friction Stir Dovetailing of AA7099 to Steel with AA6061 Interlayer for Reduced Zn Embrittlement at Dissimilar Interface

Joining of high strength Al alloy (AA7099) to steel (rolled homogeneous armor) with and without AA6061 interlayer was achieved using a friction stir dovetailing (FSD) method. Detailed investigations were conducted to establish correlations between mechanical performance and microstructural evolution of FSD joints. Lap shear tensile testing revealed that incorporation of the AA6061 interlayer combined with tailored processing methodology significantly improved both mechanical interlocking and load transmission across the dovetail interface. Following incorporation of the interlayer, the maximum load carrying capacity and peak extension (of the AA7099/AA6061/steel joint) are 60% and 210% higher, respectively, than results obtained from an AA7099/steel joint without an interlayer. Without an AA6061 interlayer, formation of zinc rich intermetallic compounds led to brittle interfacial failure of the AA7099-steel FSD joint. Incorporation of novel tool and joint configuration eliminated asymmetric joint performance as a function of loading direction, which is generally observed in friction stir lap welding. The efficacy of the use of an AA6061 interlayer in joining AA7099 to steel was demonstrated through mechanical testing as well as high resolution analytical electron microscopy characterization.

Dissimilar metal joining, Friction stir dovetailin↗

Three Sheet Al alloy assembly for automotive application

An update on joint characterization of three sheet friction stir lap welds (FSLW) in three aluminum alloys (7xxx, 5xxx, and 6xxx) for automotive assembly application is presented. Welding speed of 0.3-2.9m/min was used with pin length >5mm with the aim to reduce upturn hooking on the retreating side and avoid wormhole defect on the advancing side. Joints were also made in to enable T peel and U peel testing. Stitch welds were used to understand effects of weld length and ramp length on T peel performance. Hat sections were joined for 3-point bending and axial crush testing and tested with promising results. Several key issues that require further investigations are identified including flash management near the trim edge, weld quality with limited clamping, tool failures at speeds greater than 0.5m/min, and propensity of incipient melting for 7xxx stack-up.

Upadhyay, Piyush↗

A review of technologies for welding magnesium alloys to steels

Here we review various state-of-the-art methods for welding magnesium alloys and steels using different joint configurations. Microstructural characterizations indicate that four microstructures may form at the Mg/steel interface after welding: unwelded gap, metal oxides, solid solutions, or intermetallic compounds. Reaction products at the Mg/steel interface vary with different welding methods, alloying elements in base materials, interlayers or coatings applied, and preparations of base material before welding. Regarding mechanical property characterization, (a) lap tensile shear testing for lap-welded and spot-welded joints, (b) tensile testing for butt-welded joints and (c) fatigue properties of lap-welded and spot-welded joints are summarized and compared, separately. Reaction products at the Mg/steel interface are correlated with mechanical properties. Finally, ways to enhance Mg/steel joint strength, such as introducing interlocking features during friction stir lap and butt welding, are discussed.

Wang, Tianhao↗

Characterization of microstructure and residual stress following the friction stir welding of dissimilar aluminum alloys

Friction-stir-welding (FSW) has gained importance as an effective way to join dissimilar materials due to its solid-state nature. However, FSW produces substantial residual stresses in aluminum welding, often deteriorating the component's structural performance and reliability. In the current study, the d-spacing (inter-atomic distance) of several locations on a battery tray and stress-free reference samples are measured with neutron diffraction to calculate the residual stresses in a lap 6061 to A365 dissimilar friction-stir-weld. Furthermore, the present study connects the measured residual stress to microstructure properties through electron backscatter diffraction (EBSD) and optical microscopy analyses. The EBSD results indicate that the FSW operation affects the grains’ orientation, thereby producing location-specific directionally varying elasticity across the weldment. Further, this varied elasticity creates unique d-spacing profiles even in the stress-free material. Additionally, the resulting stressed and stress-free d-spacing profiles show dependencies on the FSW tool geometry, traverse direction, and rotational direction. Lastly, this study suggests that the final component residual stress can be influenced by the sequence of multi-pass welds contributing to a rise in temperature in the presence of a completed weld relaxing its residual stress.

36 MATERIALS SCIENCE↗

Microstructural, Corrosion, and Mechanical Characterization of Friction Stir Welded Al 6022-to-ZEK100 Mg Joints

Friction stir welded (FSW) aluminum–magnesium lightweight vehicle joints have gained significant interest due to their high strength-to-weight ratio. In this work, the corrosion resistance of this material is analyzed through electrochemical tests, which include open circuit potential (OCP) inspection and potentiodynamic polarization (PD) scanning. Weight loss measurements tested the corrosion rate of the FSW weld through cyclic corrosion testing (CCT) according to the standard SAEJ 2334. Mechanical properties were also investigated, including lap-shear strength, micro- and nano-hardness mapping, and true stress–strain curves as a function of local processing history. The electrochemical results indicate that the center weld zone’s corrosion property stays between the two base alloys. Indentation-based testing demonstrated that the weld zone behaves differently from base alloys. Lap shear strength surprisingly did not drop much even after eight weeks of cyclic corrosion tests, indicating that the joint did not allow any ingress of the electrolyte.

36 MATERIALS SCIENCE↗

Friction-Stir Welding and Mathematical Modeling

The friction-stir welding process is a remarkable way for making butt and lap joints in aluminum alloys. This process operates by passing a rotating tool between two closely butted plates. Through this process it generates a lot of heat and heated material is stirred from both sides of the plates in which the outcome will one high quality weld. My research has been done to study the FSW through mathematical modeling, and using modeling to better understand what take place during the friction-stir weld.

Rostant, Victor D.↗

Friction Stir Welding of Curved Plates

Friction stir welding (FSW) is a remarkable technology for making butt and lap joints in aluminum alloys. The process operates by passing a rotating tool between two closely butted plates. This process generates heat and the heated material is stirred from both sides of the plates to generate a high quality weld. Application of this technique has a very broad field for NASA. In particular, NASA is interested in using this welding process to manufacture tanks and curved elements. Therefore, this research has been oriented to the study the FSW of curved plates. The study has covered a number of topics that are important in the model development and to uncover the physical process involve in the welding itself. The materials used for the experimental welds were as close to each other as we could possibly find, aluminum 5454-0 and 5456-0 with properties listed at http://matweb.com. The application of FSW to curved plates needs to consider the behavior that we observed in this study. There is going to be larger force in the normal direction (Fz) as the curvature of the plate increases. A particular model needs to be derived for each material and thickness. A more complete study should also include parameters such as spin rate, tool velocity, and power used. The force in the direction of motion (Fx) needs to be reconsidered to make sure of its variability with respect to other parameters such as velocity, thickness, etc. It seems like the curvature does not play a role in this case. Variations in temperature were found with respect to the curvature. However, these changes seem to be smaller than the effect on Fz. The temperatures were all below the melting point. We understand now that the process of FSW produces a three dimensional flow of material that takes place during the weld. This flow needs to be study in a more detailed way to see in which directions the flow of material is stronger. It could be possible to model the flow using a 2-dimensional model in the particular directions where the flow moves faster. More experimental information is required to enrich the knowledge about FSW, and from this point, derive useful mathematical formulas to optimize the process and the design of the machines that will perform it. More experiments and experimental equipment are required to uncover the mathematics of the process.

Sanchez, Nestor↗

Galvanic corrosion of AZ31B joined to dual-phase steel with and without Zn layer by ultrasonic and friction stir welding

Galvanic corrosion of AZ31B joined with bare or Zn-coated DP590 steel by ultrasonic spot welding or linear friction stir welding was quantitatively studied by pre-defining anode and cathode in the lap joint samples. Corrosion volume and depth from Mg anode surfaces exposed to 0.1 M sodium chloride solution was analyzed as functions of cathode surface type and welding method. Characterization of as-welded joints was performed to identify any microstructural feature of the bonding zone that could impact galvanic corrosion behavior. COMSOL modeling with modified user subroutine was conducted to simulate the progression of Mg corrosion in the same joint and electrode configurations used for the corrosion experiments. The experimental results indicated that Zn-coated cathode surface can reduce Mg galvanic corrosion significantly as galvanic polarization and cathodic current on Zn-coated surface remained relatively low for Mg in the weld joints. COMSOL modeling described the growth of Mg galvanic corrosion in a reasonable manner but showed limitation by underestimating the corrosion volume as it did not capture self-corrosion.

36 MATERIALS SCIENCE↗

Joining of Thermoset Carbon Fiber Reinforced Polymer and AZ31 Magnesium Alloy Sheet Via Friction Stir Interlocking

A new technique called friction stir interlocking (FSI) was applied for lap-joining of AZ31 magnesium sheet and thermoset carbon fiber reinforced polymer (TS-CFRP) sheet. Instead of directly joining AZ31 and TS-CFRP, a series of magnesium interlocks were used to friction stir weld with AZ31 sheet to enable joining with TS-CFRP. Microstructural characterization of joint cross sections showed that a tool rotation rate of 800 rpm produced incomplete mixing of magnesium interlocks and the top AZ31 sheet, while 1200 rpm achieved sufficient material mixing to avoid unwelded regions. Mechanical property characterization showed that AZ31/TS-CFRP dissimilar joints failed through the magnesium interlock shanks during lap shear tensile testing, with a maximum normalized joint strength reaching ~100 MPa.

Wang, Tianhao↗

Joining AA7099 to Ni-Cr-Mo Steel Using Single Pass Friction Stir Dovetailing and AA6061 Butter Layer

A novel single pass friction stir dovetailing (FSD) was developed to join thick plate AA7099 to Ni-Cr-Mo steel in a lap configuration through the use of an AA6061 butter layer. The butter layer approach can be shown to significantly reduce interfacial failures by inhibiting the formation of brittle Fe–Al intermetallic compounds (IMCs) which are typically formed during conventional friction stir welding (FSW) of AA7099 directly to steel. This study evaluates the strength and microstructural evolution of the aluminum/steel joint interface between single pass FSD of AA7099/AA6061(butter)/steel fabricated using three different FSD tool configurations. The butter layer was achieved by placement of a free-floating strip of AA6061 within the dovetail groove that was pre-machined in the steel substrate. Friction stir welding was then used to simultaneously join the thick plate AA7099, the AA6061 strip and the AA7099 in a single weld pass. To optimize the joining process, three different pin geometries (full thread, half smooth/half thread, no thread) were evaluated; it was demonstrated that the half smooth/half thread tool produced the strongest weld joint due to the absence of a Zn rich layer at the Al/steel interface. The efficacy of this unique processing technique was tested using lap shear tensile testing as well as high resolution transmission electron microscopy (TEM). A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.

Olszta, Matthew J.↗

Three Dimensional Numerical Simulation and Characterization of Crack Growth in the Weld Region of a Friction Stir Welded Structure

Friction stir welding (FSW) fabrication technology is being adopted in aerospace applications. The use of this technology can reduce production cost, lead-times, reduce structural weight and need for fasteners and lap joints, which are typically the primary locations of crack initiation and multi-site fatigue damage in aerospace structures. FSW is a solid state welding process that is well-suited for joining aluminum alloy components; however, the process introduces residual stresses (both tensile and compressive) in joined components. The propagation of fatigue cracks in a residual stress field and the resulting redistribution of the residual stress field and its effect on crack closure have to be estimated. To insure the safe insertion of complex integral structures, an accurate understanding of the fatigue crack growth behavior and the complex crack path process must be understood. A life prediction methodology for fatigue crack growth through the weld under the influence of residual stresses in aluminum alloy structures fabricated using FSW will be detailed. The effects and significance of the magnitude of residual stress at a crack tip on the estimated crack tip driving force are highlighted. The location of the crack tip relative to the FSW and the effect of microstructure on fatigue crack growth are considered. A damage tolerant life prediction methodology accounting for microstructural variation in the weld zone and residual stress field will lead to the design of lighter and more reliable aerospace structures

Seshadri, Banavara R.↗

Process Robustness of Friction Stir Dovetailing of AA7099 to Steel with In Situ AA6061 Interlayer Linking

Rolled homogeneous armor (RHA) steel was joined to aluminum alloy AA7099-T7451 with an interlayer of AA6061-T651 by single-pass friction stir dovetailing (FSD). The evolution of the AA7099/AA6061 and AA6061/steel interfacial microstructures and mechanical properties of the joints were examined. The AA6061 interlayer prevented Zn migration from the AA7099 to the steel during FSD and inhibited formation of brittle, Zn-rich, Fe-Al intermetallic compounds within the joint. The flow of the dissimilar aluminum alloys at the interface was controlled with a partially threaded friction stir welding pin and a dovetail geometric configuration optimized in previous work. The process robustness was explored to establish parameter windows by elucidating parametric effects on the relationship between process conditions and the joint’s microstructure and mechanical properties. Ranges of process forge force (50–70 kN) and interface temperature (475°C–515°C) consistently yielded joints with adequate performance. The load-carrying capacity in lap shear tensile tests was 2025 ? 100 N/mm.

Friction Stir Dovetailing, FSW, AA7099, AA6061, Ro↗

Stationary Shoulder Friction Stir Assisted Scribe Technique for Dissimilar Joining

We report on implementation of a stationary shoulder in dissimilar joints of Al-steel and Al-carbon fiber reinforced polymer (CFRP) using friction stir assisted scribe technology (FaST ). Viable joint strength similar to that with the conventional FAST process was demonstrated in Al-steel. A significant improvement in as-welded surface roughness for both Al-steel and Al-CFRP cases was achieved by using stationary shoulder. Interrupted lap shear tests performed on Al-steel joints and a corresponding computational model indicate the joint failure typically occurs in Al sheet via a crack tip that originates at the steel hook tip on the loading side. A similar fracture path was observed in an Al-CFRP joint.

Das, Hrishikesh↗

Microstructural, Corrosion and Mechanical Characterization of Friction-Stir Welded Joints Between Aluminum and Magnesium Alloys

Friction Stir Welding (FSW) of Aluminum-Magnesium (Al-Mg) alloys has garnered increasing attention due to its wide-ranging applications in the automotive and aerospace industries. The microstructural, corrosion, and mechanical properties of FSW Al-Mg welds under selected conditions are critical factors that must be well-investigated to ensure their durability and performance. In this study, electrochemical tests, including Open Circuit Potential (OCP), Linear Polarization Resistance (LPR), Potentiodynamic Polarization Scan (PD), and Electrochemical Impedance Spectroscopy (EIS), have been used to analyze the corrosion resistance of these welds, along with weight loss measurements through cyclic corrosion testing (CCT) and surface evolution via SEM over an 8-week period. Mechanical properties are evaluated through microindentation, nanoindentation, fatigue, and lap-shear tests. The results of the electrochemical tests reveal that the corrosion properties of the center weld zone differ from those of the two base alloys. Indentation tests indicate that the weld zone behaves differently from the base alloys. Surprisingly, the lap shear strength did not decrease significantly even after 8 weeks of cyclic corrosion testing, indicating that the joint prevented any ingress of the electrolyte. Fatigue testing showed that applying an adhesive between the Al and Mg joint improved the fatigue life to some extent, although the corrosion resistance reduced due to the discontinuous bonding of the adhesive layer. Overall, these findings highlight the importance of investigating the corrosion and mechanical properties of FSW Al-Mg welds and provide valuable insights for future modeling works.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗