Search NASA⌕ Search

SEARCH · Search NASA

Results for “high voltage electrode conditioning”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Surface processing and discharge-conditioning of high voltage electrodes for the Ra EDM experiment

The Ra EDM experiment uses a pair of high voltage electrodes to search for the atomic electric dipole moment of 225 Ra. We use identical, plane–parallel electrodes with a primary high gradient surface of 200 mm 2 to generate reversible DC electric fields. Our statistical sensitivity is linearly proportional to the electric field strength in the electrode gap. We adapted surface decontamination and processing techniques from accelerator physics literature to chemical polish and clean a suite of newly fabricated large-grain niobium and grade-2 titanium electrodes. Three pairs of niobium electrodes and one pair of titanium electrodes were discharge-conditioned with a custom high voltage test station at electric field strengths as high as +52.5 kV/mm and –51.5 kV/mm over electrode gap sizes ranging from 0.4 mm to 2.5 mm. One pair of large-grain niobium electrodes was discharge-conditioned and validated to operate at ±20 kV/mm with steady-state leakage current ≤ 25 pA (1σ) and a polarity-averaged 98 ± 19 discharges per hour. These electrodes were installed in the Ra EDM experimental apparatus, replacing a copper electrode pair, and were revalidated to ±20 kV/mm. Here, the niobium electrodes perform at an electric field strength 3.1 times larger than the legacy copper electrodes and are ultimately limited by the maximum output of our 30 kV bipolar power supply.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Understanding the limits of Li-NMC811 half-cells

As we push the boundaries of state-of-the-art lithium-ion intercalation materials, such as nickel-rich chemistries, the ability to isolate and understand specific degradation and performance limitations is becoming increasingly important. Half-cells, wherein lithium metal is employed as a dual counter and reference electrode, are commonly used in industry and academia for this purpose. However, the high reactivity of lithium metal drives premature electrolyte degradation and limits cell lifetime, bringing into question the reliability and validity of this cell configuration. Here we explore the limitations of half-cell studies of LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) electrodes with commercially relevant loading. We identify the failure mechanism of this cell configuration through a combination of electrochemical, chemical, and spectroscopic techniques and show that the Li has a direct detrimental impact on the NMC811 chemistry. Our measurements show that vinylene carbonate is critical for these half-cell studies and underpins the cycle limits. Furthermore, we demonstrate the use of Li 4 Ti 5 O 12 (LTO) as an alternative counter electrode for understanding the performance of NMC positive electrode materials, due to its high coulombic efficiency and low reactivity with the organic carbonates routinely employed in lithium-ion battery cell chemistries. These data confirm that NMC811 electrodes can tolerate high voltages (stressed) conditions and that cell failure is mainly a result of crossover effects.

25 ENERGY STORAGE↗

Breakdown characteristics and conditioning of carbon and refractory metal electrodes

High voltage carbon and refractory metal electrodes employed in devices used in space, such as ion thrusters and traveling wave tubes, can be easily damaged by electrical breakdown and arcing events. Modification of the electrode surfaces due to these events can impact the voltage hold off capability of the surfaces, which could lead to additional arcing, further damage, and the potential for device failure. On the cathode-potential surface, the arc energy is deposited by all of the processes at the surface ultimately responsible for net electron emission, such as melting, vapor and particulate formation, sputtering, ion bombardment, etc. On the anode-potential surface, the energy is deposited from the plasma or electron stream that crosses the gap, which causes surface damage by local heating. In spite of this energy dependence on the damage, many systems that use arc discharges characterize the amount of material removed from the surfaces and the lifetime of the device for voltage hold-off by the amount of current that passes through the arc, or the 'Coulomb-rating'. The results of a series of tests that were preformed on the boltage hold off capability and damage to carbon-carbon composite surfaces and molybdenum surfaces due to induced arcing will be presented and discussed. Damage to the surfaces was characterized by the field emission performance after the arc initiation and SEM photographs for the different energy and coulomb-transfer arc conditions. Both conditioning and damage to the surfaces were observed, and will be related to the characteristics of the electrical breakdown.

high voltage breakdown↗

Long Life Nickel Electrodes for Nickel-Hydrogen Cells: Fiber Substrates Nickel Electrodes

Samples of nickel fiber mat electrodes were investigated over a wide range of fiber diameters, electrode thickness, porosity and active material loading levels. Thickness' were 0.040, 0.060 and 0.080 inches for the plaque: fiber diameters were primarily 2, 4, and 8 micron and porosity was 85, 90, and 95%. Capacities of 3.5 in. diameter electrodes were determined in the flooded condition with both 26 and 31% potassium hydroxide solution. These capacity tests indicated that the highest capacities per unit weight were obtained at the 90% porosity level with a 4 micron diameter fiber plaque. It appeared that the thinner electrodes had somewhat better performance, consistent with sintered electrode history. Limited testing with two-positive-electrode boiler plate cells was also carried out. Considerable difficulty with constructing the cells was encountered with short circuits the major problem. Nevertheless, four cells were tested. The cell with 95% porosity electrodes failed during conditioning cycling due to high voltage during charge. Discharge showed that this cell had lost nearly all of its capacity. The other three cells after 20 conditioning cycles showed capacities consistent with the flooded capacities of the electrodes. Positive electrodes made from fiber substrates may well show a weight advantage of standard sintered electrodes, but need considerably more work to prove this statement. A major problem to be investigated is the lower strength of the substrate compared to standard sintered electrodes. Problems with welding of leads were significant and implications that the electrodes would expand more than sintered electrodes need to be investigated. Loading levels were lower than had been expected based on sintered electrode experiences and the lower loading led to lower capacity values. However, lower loading causes less expansion and contraction during cycling so that stress on the substrate is reduced.

Rogers, Howard H.↗

Voltage cycling as a dynamic operation mode for high temperature electrolysis solid oxide cells

Solid Oxide Electrolysis Cells (SOECs) have emerged as a promising technology for the efficient production of H2 via high-temperature electrolysis. However, power input from dynamic energy sources remains a significant challenge for their long-term stability. It is important to analyze the tolerance of cells under dynamic operation conditions. This study focuses on evaluating the impact of voltage cycling on the performance and durability of electrode-supported SOECs. We explore the operational limits and degradation mechanisms of SOECs subjected to various voltage conditions and find that the cells have high tolerance for dynamic voltage. Voltage cycling between 1.3 V and 1.5 V for 9000 cycles does not damage the cell. Conversely, cycling to higher voltages (≥1.7 V) results in accelerated degradation. Advanced characterization is used to screen for various degradation modes post operation. Within the oxygen electrode, XRD and STEM EDS find compositional and phase evolution in all voltage cycled samples including increased decomposition of the air electrode resulting in cation migration. Microstructural analysis of the fuel electrode from nano-CT data shows minimal change throughout the sample set and no evidence of Ni migration, indicating the fuel electrode is stable and not impacted by cycling to higher voltages within the timeframe studied.

Zhu, Zhikuan↗

Experimental study of atmospheric pressure single-pulse nanosecond discharge in pin-to-pin configuration

We present an experimental study of nanosecond high-voltage discharges in a pin-to-pin electrode configuration at atmospheric conditions operating in single-pulse mode (no memory effects). Discharge parameters were measured using microwave Rayleigh scattering, laser Rayleigh scattering, optical emission spectroscopy enhanced with a nanosecond probing pulse, and fast photography. Spark and corona discharge regimes were studied for electrode gap sizes 2-10 mm and discharge pulse duration of 90 ns. The spark regime was observed for gaps < 6 mm using discharge pulse energies of 0.6-1 mJ per mm of the gap length. Higher electron number densities, total electron number per gap length, discharge currents, and gas temperatures were observed for smaller electrode gaps and larger pulse energies, reaching maximal values of about 7.5 x 10 15 cm -3 , 3.5 x 10 11 electrons per mm, 22 A, and 4,000 K (at 10 microseconds after the discharge), respectively, for a 2 mm gap and 1 mJ/mm discharge pulse energy. Initial breakdown was followed by a secondary breakdown occurring about 30-70 ns later and was associated with ignition of a cathode spot and transition to cathodic arc. Here, a majority of the discharge pulse energy was deposited into the gas before the secondary breakdown (85-89%). The electron number density after the ns-discharge pulse decayed with a characteristic time scale of 150 ns governed by dissociative recombination and electron attachment to oxygen mechanisms. For the corona regime, substantially lower pulse energies (~0.1 mJ/mm), peak conduction current (1-2 A), and electron numbers (3-5 x 10 10 electrons per mm), and gas temperatures (360 K) were observed.

42 ENGINEERING↗

Enabling high areal capacity for Co-free high voltage spinel materials in next-generation Li-ion batteries

The rapidly growing technological demand for lithium-ion batteries has prompted the development of novel cathode materials with high energy density, low cost, and improved safety. High voltage spinel, LiNi 0.5 Mn 1.5 O 4 (LNMO), is one of the most promising candidates yet to be commercialized. The two primary obstacles for this material are the inferior electronic conductivity and fast capacity degradation in full cells due to the high operating voltage. By systematically addressing these limitations, we successfully develop a thick LNMO electrode with areal capacity loadings up to 3 mAh·cm –2 . The optimized thick electrode is paired with a commercial graphite anode at both the coin cell and pouch cell level, achieving a full cell capacity retention as high as 72% and 78%, respectively, after 300 cycles. We attribute this superior cycling stability to careful optimizations of cell components and testing conditions, with a specific focus improving electronic conductivity and high voltage compatibility. These results suggest precise control of materials quality, electrode architecture and electrolyte optimization can soon support the development of a cobalt-free battery system based on a thick LNMO cathode (>4 mAh·cm 2 ), which will eventually meet the needs of next-generation Li-ion batteries with reduced cost, improved safety, and assured sustainability.

25 ENERGY STORAGE↗

Pressed boride cathodes

Results of experimental studies of emission cathodes made from lanthanum, yttrium, and gadolinium hexaborides are presented. Maximum thermal emission was obtained from lanthanum hexaboride electrodes. The hexaboride cathodes operated stably under conditions of large current density power draw, at high voltages and poor vacuum. A microtron electron gun with a lanthanum hexaboride cathode is described.

Wolski, W.↗

Effects of the space environment on space-based radar phased-array antenna; status and preliminary observations (LDEF Experiment A0133)

The overall objective of the experiment was to evaluate the effect of the space environment on components considered for a Space-Based Radar (SBR) Phased-Array Antenna. Of primary interest was a study of the degradation of the polyimide film Kapton (DuPont trademark), the material considered for use in the antenna plane. The most striking result of the experiment was the overall good condition of the Kapton antenna planes and Kapton tensile specimens, despite nearly six years of exposure to the space environment. This was largely attributable to the orientation of the Kapton (parallel and flush on the space end) and the stability of the Long Duration Exposure Facility (LDEF) in orbit. However, weathering of exposed Kapton surfaces was not insignificant. Results on elongation and mechanical properties of the plain and the fiberglass-reinforced Kapton are presented. Reduction in strain to failure of flight-exposed Kapton is attributed to surface defects of these specimens. Physical property testing of the materials to date reveals no significant difference between flight-exposed and control material. The second objective was to investigate the interaction between high-voltage electrodes and typical spacecraft contaminants in simulation of discharge triggering across differentially charged dielectric surfaces (spacecraft charging conditions). Electronic data acquisition and memory systems appeared to operate correctly, but very few discharges were recorded. Induced radioactivity, contamination, impacts, and orientation features of atomic oxygen erosion were observed.

J B Whiteside↗

Electrode Erosion and Prefire Studies Towards Fusion Scale Pulsed Power

This study presents a comprehensive investigation of electrode erosion and discharge behavior in spark gap switches over long switching cycle lifetimes. Brass, copper–tungsten (CuW), and stainless steel electrodes are tested under controlled conditions to quantify material degradation, debris accumulation, and changes in breakdown voltage. High-resolution imaging and statistical analysis of spark channel locations and gap breakdown voltages reveal how surface evolution influences long-term performance and reliability. These results provide essential data for lifetime modeling and inform design strategies for pulsed power systems in emerging applications such as private sector fusion energy and large-scale facilities like Sandia’s Z Machine and proposed ZX upgrades, where high repetition reliability and predictable behavior are critical.

electrical breakdown↗

AMPPED LDRD: Advanced Models of the Physics & Phenomena of Electrical Discharge.

This Laboratory Directed Research and Development (LDRD) project aimed at addressing an unmet need for physics-based models that enable prediction of electrical breakdown in the presence of high voltage gradients and real-world environments. This project focused on understanding coupled plasma-surface feedback phenomena critical to electrical discharge processes and design of breakdown voltages, breakdown times, and breakdown paths. New secondary electron emission and coupled plasma-surface measurement methods and models were developed. Highly reproducible discharge experiments were developed to provide current-voltage data as a function of time, and methods were developed to condition electrodes for predictable discharge. To assess plasma-surface feedback mechanisms, new surface physics capabilities, including measurement systems for local and global photoemission yield and ion-induced secondary electron emission yield were developed. Discharge models were developed to incorporate these yields for predicting discharge behavior to understand influence of surface physics on discharge current and time evolution, and methods to accelerate these simulations were demonstrated. A key finding was that the initiation process of a non-vacuum discharge appears highly dependent on photoemission at the cathode. Advanced diagnostics were developed, including spatial electrical field imaging, spectroscopy of plasmas, and high-speed imaging of discharge event s in metal and dielectric environments. These diagnostics and improved electrical models are a step toward enabling quantitative design margins, assurance of safety architectures, and implementation of novel materials and technologies for wide ranging energy and electronics applications.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Battery state-of-health diagnostics during fast cycling using physics-informed deep-learning

Rapid, in-situ Li-ion battery state-of-health (SOH) quantification is challenging. Li-ion battery aging can vary significantly with chemistry, operating conditions, cycling demands, electrode design, and operation history. As a cell ages, optimal and safe operating conditions need to be adapted to account for battery degradation by tracking critical aging modes such as loss-of-lithium-inventory (LLI), loss-of-active-material (LAM) in either electrode, and/or impedance rise. This manuscript describes a framework for identifying battery aging modes in-operando using fast-rate voltage charge/discharge responses. The framework uses a physically based Li-ion battery model to produce synthetic high-rate responses at aged states. The aging model is calibrated against experimental data from cells with different electrode loadings and cycled under a variety of fast-charging conditions (1 h, 15 min, 10 min, and 7 min charging). The synthetically generated high-rate responses at aged states are then used to train a deep-learning model to identify real cell state-of-health from fast charge/discharge battery voltage responses. The synthetically trained deep-learning model performance is validated by comparing to standard incremental capacity analysis and half-cell measurements. Finally, the framework demonstrates the benefits of using high-rate physics-based models to generate synthetic data for training deep-learning models.

25 ENERGY STORAGE↗

Design and Modelling of a Microfluidic Electro-Lysis Device with Controlling Plates

Many Lab-on-Chip applications require sample pre-treatment systems. Using electric fields to perform cell-lysis in bio-MEMS systems has provided a powerful tool which can be integrated into Lab-on-a-Chip platforms. The major design considerations for electro-lysis devices include optimal geometry and placement of micro-electrodes, cell concentration, flow rates, optimal electric field (e.g. pulsed DC vs. AC), etc. To avoid electrolysis of the flowing solution at the exposed electrode surfaces, magnitudes and the applied voltages and duration of the DC pulse, or the AC frequency of the AC, have to be optimized for a given configuration. Using simulation tools for calculation of electric fields has proved very useful, for exploring alternative configurations and operating conditions for achieving electro cell-lysis. To alleviate the problem associated with low electric fields within the microfluidics channel and the high voltage demand on the contact electrode strips, two "control plates" are added to the microfluidics configuration. The principle of placing the two controlling plate-electrodes is based on the electric fields generated by a combined insulator/dielectric (gladwater) media. Surface charges are established at the insulator/dielectric interface. This paper discusses the effects of this interface charge on the modification of the electric field of the flowing liquid/cell solution.

Jenkins, A.↗

An experimental investigation of electric flashover across solid insulators in vacuum

The insulation of high voltage conductors often employs solid insulators for many applications. In such applications, an unexpected electric flashover may occur along the insulator surface. Under conditions of high vacuum, the flashover voltage across the insulator is observed to be lower compared with that of the same electrode separation without an insulator. The reason for such an extreme reduction of flashover voltage is not well understood. Several models based on the secondary electron emission, were proposed to explain the onset of the surface flashover. The starting point and the developing velocity of the surface flashover were determined. An intensified image converter camera was used to observe the initial stage of electrical flashover along the insulator surface parallel to the electric field. Several different insulator materials were used as test pieces to determine the effect of the dielectric constant on the flashover voltage characteristics.

Vonbaeyer, H. C.↗

Wear Trends of the HERMeS Thruster as a Function of Throttle Point

A series of short-duration (200 hour) wear tests were conducted with two Hall Effect Rocket with Magnetic Shielding (HERMeS) technology demonstration units (TDU). Front pole covers, cathode keeper, and discharge channel wear were characterized as a function of discharge voltage, magnetic field strength, and chamber pressure. No discharge channel erosion was observed. Inner pole cover erosion was shown to be a weak function of discharge voltage with most erosion occurring at the lowest value, 300 volts. The TDU-3 keeper electrode eroded with each operating condition, with high magnetic field yielding the greatest erosion rate. The TDU-1 keeper electrode exhibited net deposition suggesting its configuration is more consistent with meeting overall HERMeS service life requirements. Ratios of molybdenum to graphite erosion rates suggests, with high uncertainty, that the sputtering ions are originating downstream of the thruster exit plane, striking the surface with small angles of incidence.

life (durability)↗

High-Voltage Droplet Dispenser

An apparatus that is extremely effective in dispensing a wide range of droplets has been developed. This droplet dispenser is unique in that it utilizes a droplet bias voltage, as well as an ionization pulse, to release a droplet. Apparatuses that deploy individual droplets have been used in many applications, including, notably, study of combustion of liquid fuels. Experiments on isolated droplets are useful in that they enable the study of droplet phenomena under well-controlled and simplified conditions. In this apparatus, a syringe dispenses a known value of liquid, which emerges from, and hangs onto, the outer end of a flat-tipped, stainless steel needle. Somewhat below the needle tip and droplet is a ring electrode. A bias high voltage, followed by a high-voltage pulse, is applied so as to attract the droplet sufficiently to pull it off the needle. The voltages are such that the droplet and needle are negatively charged and the ring electrode is positively charged.

Eichenberg, Dennis J.↗

Early calendar life and health prediction of silicon batteries via machine learning with uncertainty quantification

Lithium-ion batteries with silicon anodes promise high energy density but are limited by calendar lifetime. Reducing the long iteration time to obtain experimental results requires predicting calendar lifetime early in a cell's life. In this study, we demonstrate that lightweight machine learning models with feature engineering can provide calendar lifetime estimates from early electrochemical signals. After 1 month of electrochemical aging, the best models achieve 10% error in calendar-life prediction and can separate "bad" from "good" lifetime cells with a mean F1 score of 0.857. As battery systems exhibit inherent variability, four methods for uncertainty quantification are compared, and confidence intervals are demonstrated with an uncertainty of +-3.6 months in lifetime prediction. A feature importance analysis indicates that early patterns in voltage decay are the strongest indicators of calendar lifetime. Finally, this modeling approach has high error when generalizing to new electrode chemistries or testing conditions but with appropriately low confidence.

25 ENERGY STORAGE↗

High voltage solar array experiments

The interaction between the components of a high voltage solar array and a simulated space plasma is studied to obtain data for the design of a high voltage solar array capable of 15kW at 2 to 16kV. Testing was conducted in a vacuum chamber 1.5-m long by 1.5-m diameter having a plasma source which simulated the plasma conditions existing in earth orbit between 400 nautical miles and synchronous altitude. Test samples included solar array segments pinholes in insulation covering high voltage electrodes, and plain dielectric samples. Quantitative data are presented in the areas of plasma power losses, plasma and high voltage induced damage, and dielectric properties. Limitations of the investigation are described.

Kennerud, K. L.↗