Search NASA⌕ Search

SEARCH · Search NASA

Results for “hydrogen adsorption”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Hydrogen adsorption and diffusion, and subcritical-crack growth in high strength steels and nickel base alloys

Embrittlement, or the enhancement of crack growth by gaseous hydrogen in high strength alloys, is of primary interest in selecting alloys for various components in the space shuttle. Embrittlement is known to occur at hydrogen gas pressures ranging from fractions to several hundred atmospheres, and is most severe in the case of martensitic high strength steels. Kinetic information on subcritical crack growth in gaseous hydrogen is sparse at this time. Corroborative information on hydrogen adsorption and diffusion is inadequate to permit a clear determination of the rate controlling process and possible mechanism in hydrogen enhanced crack growth, and for estimating behavior over a range of temperatures and pressures. Therefore, coordinated studies of the kinetics of crack growth, and adsorption and diffusion of hydrogen, using identical materials, have been initiated. Comparable conditions of temperature and pressure will be used in the chemical and mechanical experiments. Inconel 718 alloy and 18Ni(200) maraging steel have been selected for these studies. Results from these studies are expected to provide not only a better understanding of the gaseous hydrogen embrittlement phenomenon itself, but also fundamental information on hydrogen adsorption and diffusion, and crack growth information that can be used directly for design.

Wei, R. P.↗

Hydrogen adsorption and diffusion, and subcritical-crack growth in high-strength steels and nickel base alloys

Coordinated studies of the kinetics of crack growth and of hydrogen adsorption and diffusion were initiated to develop information that is needed for a clearer determination of the rate controlling process and possible mechanism for hydrogen enhanced crack growth, and for estimating behavior over a range of temperatures and pressures. Inconel 718 alloy and 18Ni(200) maraging steel were selected for these studies. 18Ni(250) maraging steel, 316 stainless steel, and iron single crystal of (111) orientation were also included in the chemistry studies. Crack growth data on 18Ni(250) maraging steel from another program are included for comparison. No sustained-load crack growth was observed for the Inconel 718 alloy in gaseous hydrogen. Gaseous hydrogen assisted crack growth in the 18Ni maraging steels were characterized by K-independent (Stage 2) extension over a wide range of hydrogen pressures (86 to 2000 torr or 12 kN/m2 to 266 kN/m2) and test temperatures (-60 C to +100 C). The higher strength 18Ni(250) maraging steel was more susceptible than the lower strength 200 grade. A transition temperature was observed, above which crack growth rates became diminishingly small.

Wei, R. P.↗

Sticking probabilities for the adsorption of hydrogen on clean Ni/111/, Ni/100/, Ni sheet and evaporated Ni films

Determination of the sticking probability for hydrogen adsorption on clean Ni(111), Ni(100), polycrystalline nickel sheet, and polycrystalline evaporated nickel films, using a modification of the reflection detector technique of Horgan and King (1970) for metal films. The initial sticking probability for hydrogen adsorption on a nickel film at 300 K by the proposed method is found to be 0.25 in comparison to 0.35 for hydrogen adsorption on a nickel film using the reflection detector technique. Also, the sticking probabilities on smooth single-crystal (111) and (100) planes and polycrystalline sheets are found to be lower than those on the rougher polycrystalline nickel films.

Horgan, A. M.↗

Adsorption of hydrogen chloride on microcrystalline silica

The interaction of hydrogen chloride with quartz was studied to determine the extent to which silica can irreversibly remove hydrogen chloride from the atmosphere. Adsorption isotherms were measured at 30 C for hydrogen chloride on silica outgassed between 100 C and 400 C. Readsorption isotherms were also measured. The silica surface was characterized further by infrared spectroscopy, electron spectroscopy for chemical analysis, scanning electron microscopy, and immersional calorimetry. Ground debris samples obtained from the Kennedy Space Center, were likewise examined.

Kang, Y.↗

Preparation and evaluation of advanced electrocatalysts for phosphoric acid fuel cells

A number of electrocatalyst combinations were prepared and characterized. These electrocatalysts were formulated to contain platinum combined with transition metal carbide forming elements (W, Mo, V) for cathodes and platinum combined with palladium for anodes. High resolution electron microscopy was used to determine the crystallite size and dispersion of platinum-palladium alloy electrocatalysts in order to provide analytical support for the electrochemical determinations of the particle dispersions. An equation was derived which correlates palladium crystallite size with electrochemical hydrogen adsorption. Based on comparisons of electrocatalyst performances in the presence of pure hydrogen and hydrogen containing carbon monoxide, it was shown that the apparent poisoning of the electrocatalyst by carbon monoxide is influenced by the electrode structure.

Stonehart, P.↗

Hydrogen Desorption and Adsorption Measurements on Graphite Nanofibers

Graphite nanofibers were synthesized and their hydrogen desorption and adsorption properties are reported for 77 and 300 K. Catalysts were made by several different methods including chemical routes, mechanical alloying and gas condensation.

graphite nanofibers hydrogen desorption adsorption↗

Recent advances in the understanding of electrocatalysis and its relation to surface chemistry

It is pointed out that electrosorption plays a key role in electrocatalysis. Little information is available, however, concerning the chemical nature of the interactions of the adsorbed species with the electrode and even less about the adsorption sites. The role of adsorbed species and surface layers in electrocatalysis is reviewed for several electrode systems. In recent years, some general insights have been achieved into the relationship of hydrogen electrode kinetics to hydrogen adsorption. For a given mechanism the exchange current density is related to the standard free energy of adsorption of the particular type of adsorbed hydrogen upon which the kinetics depend. The oxygen electrode reactions are less well understood than the reactions for the hydrogen electrode. The pronounced irreversibility of the oxygen electrode reactions at moderate temperatures has severely complicated mechanistic studies.

Yeager, E.↗

Adsorption of carbon monoxide and hydrogen on graphite.

Adsorption of carbon monoxide and hydrogen was investigated on three graphites: a high-density pyrolytic graphite, a small-grain extruded graphite, and a processed pyrolytic graphite tape. The sticking probability of CO was found to decrease rapidly as the average surface coverage approached 0.01 monolayer. Lower sticking probabilities were observed on the highly oriented pyrolytic graphite which indicated that adsorption occurs principally on the edge atoms. There is negligible adsorption of molecular hydrogen on graphite that has been heated to 2400 K in vacuo.

Beitel, G. A.↗

Behavior of hydrogen on nickel

Hydrogen adsorption behavior on polycrystalline nickel surfaces, using electron impact desorption flash filament with gas phase and ion spectrometer and vapor deposition

Gilbreath, W. P.↗

Adhesion theory review

Bonding theories reviewed include physical adsorption, hydrogen bonding, chemisorption and surface energy; bond failure mechanisms include phase discontinuity, swelling and corrosion. Concept of bond failure by water desorption is introduced and discussed.

Delollis, N. J.↗