Corrosion of Molds in Injection Molding Machines
The high corrosion rates of molds in injection molding machines are analyzed. The causes of such corrosion are considered.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
The high corrosion rates of molds in injection molding machines are analyzed. The causes of such corrosion are considered.
The control of mold surface temperature is an important factor that determines surface morphology and its dimension in thickness direction. It can also affect the frozen molecular orientation and the mold surface replicability in injection molded products. In this work, thin thermally active films were used to quickly control the mold surface temperature. In particular, an active high electrical conductivity carbon black loaded polyimide composites sandwiched between two insulating thin polymeric layers was used to condition the mold surface. By controlling the heating time, it was possible to control precisely the temporal variation of the mold temperature surface during the entire cycle. The surface heating rate was about 40°C/s and upon contact with the polymer the surface temperature decreased back to 40°C within about 5 s; the overall cycle time increased only slightly. The effect on cross section sample morphology of samples of iPP were analyzed and discussed on the basis of the recorded temperature evolution.
Serial femtosecond crystallography (SFX) using X-ray Free-Electron Lasers (XFELs) allows for room temperature protein structure determination without evidence of conventional radiation damage. In this method, a liquid suspension of protein microcrystals can be delivered to the X-ray beam in vacuum as a micro-jet, which replenishes the crystals at a rate that exceeds the current XFEL pulse repetition rate. Gas dynamic virtual nozzles produce the required micrometer-sized streams by the focusing action of a coaxial sheath gas and have been shown to be effective for SFX experiments. Here, we describe the design and characterization of such nozzles assembled from ceramic micro-injection molded outer gas-focusing capillaries. Trends of the emitted jet diameter and jet length as a function of supplied liquid and gas flow rates are measured by a fast imaging system. The observed trends are explained by derived relationships considering choked gas flow and liquid flow conservation. Finally, the performance of these nozzles in a SFX experiment is presented, including an analysis of the observed background.
ORNL collaborated with Radio Systems Corporation to investigate additive manufacturing (AM) of mold plates for plastic injection molding by direct metal deposition. The team s modelling effort identified a 100% improvement in heat transfer through use of conformal cooling lines that could be built into the mold using a revolutionary design enabled by additive manufacturing. Using the newly installed laser deposition system at the ORNL Manufacturing Demonstration Facility (MDF) a stainless steel mold core was printed.
Additive manufacturing (AM) presents a promising approach for rapid tooling, offering significant reductions in production costs and lead times compared to that of conventional moldmaking processes. This work examines the fabrication of molds for injection molding through vat photopolymerization (VPP) AM, using a commercially available photopolymer resin intended for high temperature applications (High Temp V2 resin). The photorheological behavior of the resin is examined to evaluate its curing kinetics and mechanical development during polymerization, ensuring suitability for mold fabrication. The thermal and mechanical properties of the printed photopolymer resin are characterized, alongside assessments of dimensional accuracy and surface finish, which are critical factors influencing the performance and quality of injection molded parts. Additionally, specimens produced using VPP-fabricated molds are evaluated and benchmarked against those molded with traditional metal molds.
Fiber orientations in metal matrix composites have significant effect on improving tensile properties. Control of fiber orientations in metal injection molded metal composites is a difficult task. In this study, two mold cavities of dimensions 6x6x90 mm and 10x20x180 mm were used for comparison of fiber orientation in injection molded metal composites test parts. In both mold cavities, convergent and divergent flows were developed by modifying the sprue dimensions. Scanning electron microscope (SEM) was used to examine the fiber orientations within the test samples. The results showed highly aligned fiber in injection molded test bars developed from the convergent melt flow. Random orientation of fibers was noted in the composites test bars produced from divergent melt flow.
The cooling of injection molded plastic is targeted. Coolant flows into a porous medium disposed within an injection molding component via a porous medium inlet. The porous medium is thermally coupled to a mold cavity configured to receive injected liquid plastic. The porous medium beneficially allows for an increased rate of heat transfer from the injected liquid plastic to the coolant and provides additional structural support over a hollow cooling well. When the temperature of the injected liquid plastic falls below a solidifying temperature threshold, the molded component is ejected and collected.
Permanent magnets are expected to play a crucial role in the realization of the clean economy. In particular, the neodymium-iron-boron (Nd2Fe14B or NdFeB) magnets, which have the highest energy density among rare earth permanent magnets, are needed for building more efficient windmill generators, electric vehicle motors, etc. Currently, near-net shape magnets can be either made through sintering and compression molding with extensive post machining or directly through injection molding. However, injection molding has a loading volume fraction limitation of 0.65 for nylon binders. A novel method of manufacturing bonded permanent magnets with loading fraction greater than 0.65 has been demonstrated using Big Area Additive Manufacturing (BAAM) printers. As energy density is directly proportional to the square of the magnet loading fraction, magnets produced using BAAM printers require less volume and magnetic material compared to that of injection molded magnets on average. A comparative LCA shows that this difference in magnetic powder consumption nearly constitutes the difference in the environmental impact categories. Even after assuming recycled magnetic input, the BAAM magnets perform better environmentally than injection molded magnets, especially in the ozone depletion category. Since BAAM printers can accommodate even higher loading fractions, at scale, BAAM printers possibly can bring about a significant decrease in rare earth mineral consumption and environmental emissions. So furthermore, single screw extrusion enables BAAM printers to have high print speeds and allow them to be economically competitive against injection molding. Therefore, BAAM printed magnets show promise in transitioning towards the clean economy.
Abstract Manufacturing plastic parts with secondary feedstocks has risen to the forefront of importance in recent years. However, the variation in molecular weight and rheology of secondary feedstock can lead to inconsistent part quality. This work evaluates the effectiveness of a novel closed‐loop adaptive process control system that adjusts nozzle pressure in response to in‐mold pressure data. Five different recycled polypropylene blends, with a broad distribution of flow properties, were evaluated to determine the effectiveness of the control system at reducing processing variation. The experimental results show that the process control strategy reduced the variation within the mold, as seen by in‐mold pressure curves and calculated in‐mold viscosity values. Additionally, the parameters that control the automated process adjustments were investigated, showing the importance of optimization. The analysis of the correlation between in‐mold rheology and mechanical properties showed a slight variation in the mechanical properties and parts weight with a coefficient of variation of under 5%. Overall, the results demonstrate the ability of pressure‐controlled molding and automated viscosity adjustment to reduce the variability when molding a secondary feedstock. Highlights Pressure‐controlled injection molding of recycled polypropylene. Automated closed‐loop adaptive process control methodology. Methodology resulted in a reduction in pressure variation during molding. Changes in mechanical properties and in‐mold viscosity were investigated. Results show the potential of pressure‐controlled molding at reducing variation.
The injection molding behavior of a concentrated suspension of Si powder in wax was studied. It was found that the injection molding behavior was a function of the processing techniques used to generate the powder. Dry ball-milled powders had the best molding behavior, while air classified and impact-milled powders demonstrated poorer injection moldability. The relative viscosity of these molding batches was studied as a function of powder properties: distribution shape, surface area, packing density, and particle morphology. The experimental behavior, in all cases, followed existing theories. The relative viscosity of an injection molding composition composed of dry ball-milled powders could be expressed using Farris' relation.
Injection-molded semicrystalline polymer parts generally exhibited a so-called skin-core structure basically as a result of the large gradients of temperature, shear rate, stress, and pressure fields created by the boundary conditions of injection molding. Suppression of the skin-core structure is a long-term practical challenge. In the current work, the skin-core structure of the conventional injection-molded isotactic polypropylene (iPP) was largely relieved by the cooperative effects of an in situ microfibrillar network and interfacial compatibilizer. The in situ poly(ethylene terephthalate) microfibrils of 1-8 {micro}m in diameter and large aspect ratios of above 40 tended to entangle with each other to generate a microfibrillar network in the iPP melt. During injection molding, the iPP molecules experienced confined flow in the microchannels or pores formed by the microfibrillar network, which could redistribute and homogenize the flow field of polymer melt. Addition of the compatibilizer, glycidyl methacrylate-grafted iPP, restrained the molecular orientation but facilitated preservation of oriented molecules due to the chemical bonds at the interface between PET microfibrils and iPP. The cooperative effects of in situ microfibrillar network and interfacial compatibilizer led to almost the same molecular orientation across the whole thickness of the injection-molded parts. Additionally, the content of {beta} crystals in different layers of injection-molded iPP parts depended on the combined effects of the molecular orientation, the amount of oriented crystals, and the crystallization time between 105 and 140 C. The presence of the interfacial compatibilizer facilitated formation of the {beta} crystals because of preservation of the oriented molecules.
Room-temperature injection molding is proposed as a novel, low-cost and more energy efficient manufacturing process capable of forming complex-shaped zirconium diboride (ZrB2) parts. This innovative processing method utilized aqueous suspensions with high powder loading and a minimal amount (5 vol.) of water-soluble polyvinylpyrrolidone (PVP), which was used as a viscosity modifier. Rheological characterization was performed to evaluate the room-temperature flow properties of ZrB2-PVP suspensions. ZrB2 specimens were fabricated with high green body strength and were machinable prior to binder removal despite their low polymer content. After binder burnout and pressureless sintering, the bulk density and microstructure of specimens were characterized using Archimedes technique and scanning electron microscopy. X-Ray Diffraction was used to determine the phase compositions present in sintered specimens. Ultimate strength of sintered specimens will be determined using ASTM C1323-10 compressive C-ring test.
The purpose of the proposed project between Cummins and ORNL is to significantly reduce the cost of the tooling (machining and materials) required to create injection molds to make plastic components. Presently, the high cost of this tooling forces the design decision to make cast aluminum parts because Cummins typical production volumes are too low to allow injection molded plastic parts to be cost effective with the amortized cost of the injection molding tooling. In addition to reducing the weight of components, polymer injection molding allows the opportunity for the alternative cooling methods, via nitrogen gas. Nitrogen gas cooling offers an environmentally and economically attractive cooling option, if the mold can be manufactured economically. In this project, a current injection molding design was optimized for cooling using nitrogen gas. The various components of the injection mold tooling were fabricated using the Renishaw powder bed laser additive manufacturing technology. Subsequent machining was performed on the as deposited components to form a working assembly. The injection mold is scheduled to be tested in a projection setting at a commercial vendor selected by Cummins.
The chemorheological behavior of the PRM-15 molding compounds were characterized, the range of suitable processing parameters for injection molding in a reciprocating screw injection molding machine was determined, and the effects of the injection molding processing parameters on the mechanical properties of molded PMR-15 parts were studied. The apparatus and procedures for measuring viscosity and for determining the physical response of the material during heating are described. Results show that capillary rheometry can be effectively used with thermosets if the equipment is designed to overcome some of the inherent problems of these materials. A uniform temperature was provided in the barrel by using a circulating hot oil system. Standard capillary rheometry methods can provide the dependence of thermoset apparent viscosity on shear rate, temperature, and time. Process conditions resulting in complete imidization should be carefully defined. Specification of controlled oven temperature is inadequate and can result in incomplete imidization. For completely imidized PMR-15 heat at 15 C/min melt flow without gas evolution occurs in the temperature range of 325 C to 400 C.
An improved method for obtaining high fiber volume fraction, long fiber injection molded articles is provided. According to one embodiment, the method includes forming an injection molding feedstock by cutting pre-impregnated fiber-reinforced tape into platelets. The platelets can be coated with a thin layer of polymer to allow sliding of the platelets with respect to each other at the early stages of plastication, rather than forcing relative motion of fibers with respect to each other. The method can further include the dispersion of material only in the final stages of the injection molding screw to promote gentle motion of the feedstock at the earlier stages of the plastication process. The method allows improvement of mechanical properties of articles manufactured with equipment and techniques that are prevalent in high volume automotive and consumer industries.
Injection molded parts are driven down in size and weight especially for electronic applications. In this work, an investigation was carried out on the process of injection molding of thin iPP samples and on the morphology of these parts. Melt flow in the mold cavity was analyzed and described with a mathematical model. Influence of mold temperature and injection pressure was analyzed. Samples orientation was studied using optical microscopy.
Numerical prediction of the fiber orientation in the short-glass fiber (GF) reinforced polyamide 6 (PA6) composites with the fiber weight concentration of 30%, 50%, and 70% manufactured by the injection molding process is presented. And the fiber orientation was also directly observed and measured through X-ray computed tomography. During the injection molding process of the short-fiber/thermoplastic composite, the fiber orientation is produced by the flow states and the fiber-fiber interaction. Folgar and Tucker equation is the well known for modeling the fiber orientation in a concentrated suspension. They included into Jeffrey’s equation a diffusive type of term by introducing a phenomenological coefficient to account for the fiber-fiber interaction. Our developed model for the fiber-fiber interaction was proposed by modifying the rotary diffusion term of the Folgar-Tucker equation. This model was presented in a conference paper of the 29{sup th} International Conference of the Polymer Processing Society published by AIP conference proceeding. For modeling fiber interaction, the fiber dynamic simulation was introduced in order to obtain a global fiber interaction coefficient, which is sum function of the fiber concentration, aspect ratio, and angular velocity. The fiber orientation is predicted by using the proposed fiber interaction model incorporated into a computer aided engineering simulation package C-Mold. An experimental program has been carried out in which the fiber orientation distribution has been measured in 100 x 100 x 2 mm injection-molded plate and 100 x 80 x 2 mm injection-molded weld by analyzed with a high resolution 3D X-ray computed tomography system XVA-160α, and calculated by X-ray computed tomography imaging. The numerical prediction shows a good agreement with experimental validation. And the complex fiber orientation in the injection-molded weld was investigated.