Search NASA⌕ Search

SEARCH · Search NASA

Results for “insulation polymers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Evaluation of Oxygen Consumption as a Sensitive Measure of Electrical Cable Polymer Insulation Degradation

Polymers used as dielectric materials in nuclear grade electrical cables, such as cross-linked polyethylene (XLPE) and ethylene-propylene rubber (EPR), are long-lived and durable. Estimating the decades-long useful service life of polymers experimentally in a feasible timeframe of weeks or months requires greatly accelerated aging in the laboratory at elevated temperatures and/or gamma dose rates. Many limitations of accelerated aging, such as due to artefacts of the process including diffusion limited oxidation and dose rate effects, have been identified that can make accurate lifetime prediction at service conditions challenging. This can be due to differences in degradation mechanisms between rapid and extended aging or to the presence of induction periods during which early aging is undetectable using common metrics of polymer insulation characterization such as tensile elongation at break. Conceptually, an ideal measure of aging would track clearly and predictably with material changes throughout the lifecycle of the evolving material state from early aging through end of useful life. With such a metric accelerated aging could be performed at much milder conditions, conditions closer to those found in long term service, and end of life calculated from the early data. Oxygen consumption has previously been proposed as a sensitive measure of insulation polymer oxidation that might meet such desirable characteristics. In this work, nuclear cable insulation samples of the two most common types, XLPE and EPR, from two of the most sourced manufacturers, RSCC and The Okonite Company, were subjected to gamma irradiation at dose rates of 100, 200, and 300 Gy/hr for up to 42 days at 26°C. The aged samples were used to evaluate oxygen consumption as a sensitive measure of aging for these materials and these conditions. For comparison and validation, the aged samples were also characterized using the more conventional tests of mass change, density, carbonyl index, and yellowness index. For both materials, oxygen consumption during irradiation was found to track consistently with applied dose—oxygen consumption rate was linear with time. Mass change and carbonyl index were also clearly proportional to exposure dose. Yellowness index, a surface sensitive measure, was observed to increase linearly with dose at low exposure levels before plateauing. Sample density was not observed to change under the conditions explored. Oxygen consumption was found to be a particularly sensitive metric to measure the degradation of polymeric cable insulation exposed to radiation. Oxygen consumption was compared to Arrhenius and time-temperature-superposition methods for activation energy calculation using literature date and found to be a useful and viable alternative for lifetime prediction. The techniques developed in this work are anticipated to be valuable in the estimation of insulation aging rates under mild conditions approaching service conditions. Direction comparison of useful life prediction by oxygen consumption with prediction via Arrhenius methodology for thermal aging and existing methods for radiation and combined thermal/radiation aging would serve to further validate this promising approach and refine our understanding of material-specific aging rates.

36 MATERIALS SCIENCE↗

Mitigation of Galvanic Corrosion in Bolted Joint of AZ31B and Carbon Fiber-Reinforced Composite Using Polymer Insulation

The use of polymer insulation to mitigate galvanic corrosion was examined for bolted joints of AZ31B Mg alloy and carbon fiber-reinforced composite. To assess the corrosion behaviors of bolted joints with and without polymer insulation, solution immersion and salt spray exposure (ASTM B117) tests were conducted, and the corrosion depths and volumes were determined for the joint specimens after the tests. The polymer-insulated bolted joints exhibited much lower corrosion depths and volumes, highlighting the effective mitigation of galvanic corrosion. The reductions of joint strength in the post-corrosion joint specimens were relatively small (up to ~10%) in the polymer-insulated group but greater (up to 90%) in the group with no insulation. Cross-sectional characterization of post-corrosion joints with polymer insulation revealed local pits developed on AZ31B under galvanic influence, indicating that limited galvanic attack (that did not decrease the joining integrity significantly) could still occur during a long salt spray exposure (~1264 h) owing to the permeation of an aqueous corrosive medium.

36 MATERIALS SCIENCE↗

Evaluation of Copper Catalytic Effects in Cable Insulation Polymers

This paper summarizes work performed to evaluate a phenomenon that occurs in electrical cable insulation polymers subjected to accelerated aging while in contact with copper metal. This effect, commonly known as the copper catalytic effect, is a result of chemical reactions that occur when copper ions diffuse into insulation polymers. This diffusion process is observed in various types of polymeric materials exposed to elevated temperatures and happens at the interface between the insulation and metallic components (e.g., conductor, shielding, etc.) in a cable. This polymer-metal interaction has only been observed in cables constructed with copper components (i.e., no interactions observed in cables with aluminum or other metal conductor/shielding) and results in a significant catalytic effect that increases the oxidation rate (e.g., aging) of the material. Under this research, the copper catalytic effects observed in cross-linked polyethylene, cross-linked polyolefin and ethylene propylene rubber insulated cables subjected to thermal accelerated aging were evaluated. These evaluations involved applying infrared spectroscopy, microscopy, and energy dispersive X-ray spectroscopy cross-sectional depth profiling to obtain an in-depth understanding of the aging characteristics of the materials under accelerated conditions. Based on the results of these assessments, the copper catalytic effect can have a significant impact on the mechanical, thermal, chemical, and electrical properties of cable insulation polymers. Here, the results acquired from this research provided the information needed to characterize the copper catalytic effects observed in these polymers, analyze how this phenomenon affected the polymer degradation process, and compare and understand the differences in the properties of the materials.

42 ENGINEERING↗

Stress-Dependent Voltage Offsets From Polymer Insulators Used in Rock Mechanics and Material Testing

Dielectric insulators are used in a variety of laboratory settings when performing experiments in rock mechanics, petrology, and electromagnetic studies of rocks in the fields of geophysics,material science, and civil engineering. These components may be used to electrically isolate geological samples from the experimental equipment, to perform a mechanical compliance function between brittle samples and the loading equipment, to match ultrasonic transducers, or perform other functions. In manyexperimental configurations the insulators bear the full brunt of force applied to the sample but do not need to withstand high voltages, therefore the insulators are often thin sheets of mechanically tough polymers. From an instrument perspective, transduction from various types of mechanical perturbation has beenqualitatively compared for a number of polymers [1, 2] and these error sources are readily apparent duringhigh-impedance measurements if not mitigated. However even when following best practices, a force dependent voltage signal still remains and its behavior is explored in this presentation. In this experimenttwo thin sheets (0.25 mm) of high-density polyethylene (HDPE) were set up in a stack, held alternatelybetween three aluminum bars; this stack was placed on the platen of a 60T capacity hydraulic testingmachine. The surface area, A, over which the force is applied to the PE sheets in this sandwich is roughly 40 square cm, each sheet forming a parallel-plate capacitor having roughly 320 pF [3], assuming therelative dielectric permittivity of PE is approximately 2.3. The outer two aluminum bars were connected to the LO input ofthe electrometer and the central aluminum bar was connected to the HI input of a Keithley model 617 electrometer. Once the stack is mechanically well-seated with no air gaps, the voltage offset is observed tobe a linear function of the baseline voltage for a given change in applied force. For a periodically appliedforce of 66.7 kN the voltage offsets were measured as a function of initial voltage, and these data were fitwith a linear function that was constrained to pass through the origin. The best fit solution had a correlation coefficient of R=0.85 and a slope of approximately -0.0228 volts/volt. The voltage offset when normalizedis demonstrated to be constant -2.28% for both positive and negative polarities over nearly 3 orders ofbaseline voltage magnitude. From this, the voltage-force coefficient is derived to be -0.34 ppm/N. Thiscorrelates well to a first-order parallel plate capacitor model that assumes constant area, and smalldeformation such that the polymer may be mechanically modeled by a spring that obeys Hookes law. Thissimple model predicts that the coefficient of proportionality is a function of Youngs modulus E= 0.8 GPaand surface area of the insulator, theoretically -1EA= -0.31 ppm/N. The outcome of this work is animproved insulator made from ultra-high molecular weight (UHMW) polyethylene and other approachestoward the minimization of and compensation for these experimental artifacts.

Electromagnetic Studies of Rocks↗

Long-term photothermal/humidity testing of photovoltaic module polymer insulations and cover films

The life expectancies of Tedlar and other polymer films considered for use as cover materials in terrestrial photovoltaic (PV) modules were investigated by exposing them for more than 13,000 h on an outdoor test stand and for up to 10,000 h in several accelerated multistress environments. Visual observations and diagnostic analyses of weight and mechanical strength losses were periodically conducted to assess the nature and rate of degradation of mechanical properties and to assess the effects of film thickness and UV stabilizer content. Spectroscopic analyses of pristine and degraded materials linked weight and mechanical property losses to the underlying photothermal/photooxidation chemistry. It is shown that heavy doses of UV stabilizers prolong, while elevated temperatures shorten, the useful life of these materials; humidity plays only a minor role. The most heavily UV-stabilized films are expected to operate usefully in a PV module front-cover application for only five to ten years. The performance of none of the tested films appears consistent with the 20-30 year life goals of the PV industry.

Mon, G.↗

A thin polymer insulator for Josephson tunneling applications

The progress made towards forming thin organic layers on superconductors and how these layers effect the transition temperature is discussed. The work was primarily directed towards 1) synthesis of the organics, 2) deposition of organics, and 3) setting up to make transition temperature measurements. The greatest effort was placed on synthesis, and most of the synthesis procedures are now perfected.

Wilmsen, C. W.↗

A thin polymer insulator for Josephson tunneling applications

The use of an organic monolayer formed from a vapor as an insulating barrier for thin film Josephson junctions is considered, and the effect of an organic monolayer on the transition temperature of a thin film superconductor is investigated. Also analyzed are the geometric factors which influence Josephson junctions and Josephson junction interferometers.

Wilmsen, C. M.↗

Organometallic Polymeric Conductors

For aerospace applications, the use of polymers can result in tremendous weight savings over metals. Suitable polymeric materials for some applications like EMI shielding, spacecraft grounding, and charge dissipation must combine high electrical conductivity with long-term environmental stability, good processability, and good mechanical properties. Recently, other investigators have reported hybrid films made from an electrically conductive polymer combined with insulating polymers. In all of these instances, the films were prepared by infiltrating an insulating polymer with a precursor for a conductive polymer (either polypyrrole or polythiophene), and oxidatively polymerizing the precursor in situ. The resulting composite films have good electrical conductivity, while overcoming the brittleness inherent in most conductive polymers. The highest conductivities reported (approximately 4/Scm) were achieved with polythiophene in a polystyrene host polymer. The best films using a polyamide as base polymer were four orders of magnitude less conductive than the polystyrene films. The authors suggested that this was because polyimides were unable to swell sufficiently for infiltration of monomer as in the polystyrene. It was not clear, however, if the different conductivities obtained were merely the result of differing oxidation conditions. Oxidation time, temperature and oxidant concentration varied widely among the studies.

Source record↗

Organometallic Polymeric Conductors

For aerospace applications, the use of polymers can result in tremendous weight savings over metals. Suitable polymeric materials for some applications like EMI shielding, spacecraft grounding, and charge dissipation must combine high electrical conductivity with long-term environmental stability, good processability, and good mechanical properties. Recently, other investigators have reported hybrid films made from an electrically conductive polymer combined with insulating polymers. In all of these instances, the films were prepared by infiltrating an insulating polymer with a precursor for a conductive polymer (either polypyrrole or polythiophene), and oxidatively polymerizing the precursor in situ. The resulting composite films have good electrical conductivity, while overcoming the brittleness inherent in most conductive polymers. Many aerospace applications require a combination of properties. Thus, hybrid films made from polyimides or other engineering resins are of primary interest, but only if conductivities on the same order as those obtained with a polystyrene base could be obtained. Hence, a series of experiments was performed to optimize the conductivity of polyimide-based composite films. The polyimide base chosen for this study was Kapton. 3-MethylThiophene (3MT) was used for the conductive phase. Three processing variables were identified for producing these composite films, namely time, temperature, and oxidant concentration for the in situ oxidation. Statistically designed experiments were used to examine the effects of these variables and synergistic/interactive effects among variables on the electrical conductivity and mechanical strength of the films. Multiple linear regression analysis of the tensile data revealed that temperature and time have the greatest effect on maximum stress. The response surface of maximum stress vs. temperature and time (for oxidant concentration at 1.2 M) is shown. Conductivity of the composite films was measured for over 150 days in air at ambient temperature. The conductivity of the films dropped only half an order of magnitude in that time. Films aged under vacuum at ambient temperature diminished slightly in conductivity in the first day, but did not change thereafter. An experimental design approach will be applied to maximize the efficiency of the laboratory effort. The material properties (initial and long term) will also be monitored and assessed. The experimental results will add to the existing database for electrically conductive polymer materials. Attachments: 1) Synthesis Crystal Structure, and Polymerization of 1,2:5,6:9,10-Tribenzo-3,7,11,13-tetradehydro(14) annulene. 2) Reinvestigation of the Photocyclization of 1,4-Phenylene Bis(phenylmaleic anhydride): Preparation and Structure of (5)Helicene 5,6:9,10-Dianhydride. 3) Preparation and Structure Charecterization of a Platinum Catecholate Complex Containing Two 3-Ethynyltheophone Groups. and 4) Rigid-Rod Polymers Based on Noncoplanar 4,4'-Biphenyldiamines: A Review of Polymer Properties vs Configuration of Diamines.

Youngs, Wiley J.↗

High temperature polymer dielectric film insulation

PFPI polymers were invented in the late 1970's. Assessment of emerging requirements has dictated that 300 C performance is the goal for next generation wire insulation. TRW PFPI as superior 300 C polymer candidates is presented. Included is a comparison of promising PFPI film properties with Kapton. Also included are the promising bulk polymer or coating properties.

Jones, Robert J.↗

Carboxylating Elastomer via Thiol‐Ene Click Reaction to Improve Miscibility with Conjugated Polymers for Mechanically Robust Organic Solar Cells with Efficiency of 19%

Abstract Incorporating flexible insulating polymers is a straightforward strategy to enhance the mechanical properties of rigid conjugated polymers, enabling their use in flexible electronic devices. However, maintaining electronic characteristics simultaneously is challenging due to the poor miscibility between insulating polymers and conjugated polymers. This study introduces the carboxylation of insulating polymers as an effective strategy to enhance miscibility with conjugated polymers via surface energy modulation and hydrogen bonding. The carboxylated elastomer, synthesized via a thiol‐ene click reaction, closely matches the surface energy of the conjugated polymer. This significantly improves the mechanical properties, achieving a high crack‐onset strain of 21.48%, surpassing that (5.93%) of the unmodified elastomer:conjugated polymer blend. Upon incorporating the carboxylated elastomer into PM6:L8‐BO‐based organic solar cells, an impressive power conversion efficiency of 19.04% is attained, which top‐performs among insulating polymer‐incorporated devices and outperforms devices with unmodified elastomer or neat PM6:L8‐BO. The superior efficiency is attributed to the optimized microstructures and enhanced crystallinity for efficient and balanced charge transport, and suppressed charge recombination. Furthermore, flexible devices with 5% carboxylated elastomer exhibit superior mechanical stability, retaining ≈88.9% of the initial efficiency after 40 000 bending cycles at a 1 mm radius, surpassing ≈83.5% for devices with 5% unmodified elastomer.

Chemistry↗

Advanced Polymer For Multilayer Insulating Blankets

Polymer resisting degradation by monatomic oxygen undergoing commercial development under trade name "Aorimide" ("atomic-oxygen-resistant imidazole"). Intended for use in thermal blankets for spacecraft in low orbit, useful on Earth in outdoor applications in which sunlight and ozone degrades other plastics. Also used, for example, to make threads and to make films coated with metals for reflectivity.

Haghighat, R. Ross↗

Application of Cable Condition Monitoring Technologies to Assess Age-Related Degradation of Industrial Cables Installed in Harsh Environments

The aging of electrical cables has been the subject of substantial research and development (R&D) projects performed by national and international laboratories, universities, and private organizations for many years. This R&D was conducted to develop guidance, equipment, and techniques to support aging management of in-service cables in industrial facilities such as nuclear power plants, research reactors, waste facilities, and fuel fabrication plants. Through these research efforts, condition monitoring technologies have been developed that can determine the severity of age-related degradation that occurs in industrial cables and insulation polymers during service. This paper summarizes the results of aging assessments that were performed for cables installed in two U.S. nuclear power plants, one a pressurized water reactor and one a boiling water reactor. These cables had been in service for over 40 years and during plant operation were exposed to harsh environmental conditions including elevated temperatures and radiation. For these assessments, a comprehensive series of measurements was performed to assess the aged condition of the cables. These cables came from different manufacturers, were manufactured in different years, and were constructed with a variety of jacket and insulation polymers including chloro-sulfonated polyethylene (CSPE), cross-linked polyethylene (XLPE)/cross-linked polyolefin (XLPO), neoprene, and ethylene propylene rubber (EPR). The goal of these assessments was to determine the current aged condition of the cable polymers and provide an estimate of how long the cable insulation materials could remain exposed to their in-service environmental conditions before reaching their end-of-life condition. Both nuclear power plants have received license renewals to extend their operation from 40 to 60 years, and the utilities need objective evidence to show that critical components such as cables will be able to function safely and reliably during the extended operating period. Furthermore, the results of these assessments showed that the cables exhibited different aged conditions depending on the type of polymers they were constructed with and the environment they were exposed to during service. Some of the cables and insulation polymers showed signs of significant age-related degradation and were estimated to have approximately 5 years of remaining service life. Other cables exhibited no signs of significant age-related degradation and were estimated to have 50 years or more of remaining service life. Using the results of these cable aging assessments, plant personnel were able to (1) determine the overall aged condition of cables and insulation polymers using objective test results, (2) identify aged or degraded cables before they caused operability issues, and (3) avoid unnecessary and costly replacement of cables that can continue to operate safely and reliably.