Metallurgical and Thermal Properties of 57Ni-40Ti-3Hf (wt%)

Selected properties of 57Ni-40Ti-3Hf (wt%) were measured to further develop this material for use in aerospace rolling-element bearings. The average grain size and microindentation hardness of the material at room temperature were 90 μm and 549 HV, respectively. From room temperature to 500 °C, electrical resistivity increased from 8.9×10–7 to 11.3×10–7 Ω⋅m, thermal expansion coefficients varied from 1.1×10–5 to 1.2×10–5 mm/mm⋅°C, specific heat increased from 0.44 to 0.53 W⋅sec/g⋅K, thermal diffusivity rose from approximately 0.003 to 0.005 cm2/sec and thermal conductivity increased from approximately 0.09 to 0.19 W/cm⋅K. The behavior of the material can be explained by well-known metallurgical theory. These results are expected to provide a basis for design and modeling of future aerospace components.

rule of mixtures

Evaluation of high-temperature properties of binary, eutectic Ni-X alloys (X = B, Ca, Ce, La, Y, Zr)

We investigated the high-temperature behavior of binary eutectic nickel-base alloys with low-solubility elements, towards developing alloys with new combinations of structural and functional (e.g. thermal or corrosion) properties. Based on thermodynamic screening, we cast binary near-eutectic Ni-B, Ni-Ca, Ni-Ce, Ni-La, Ni-Y, and Ni-Zr alloys and characterized their microstructure and high-temperature properties. All alloys (except Ni-Ca) contain a fine eutectic microstructure, containing submicron alternating lamellae of γ-Ni and continuous intermetallic phases. The eutectic microstructure did not significantly coarsen at 700°C (except for Ni-B), but measurably coarsened in all alloys at 900°C, most quickly in Ni-B, followed by Ni-Ce, Ni-La, Ni-Y, and Ni-Zr. Coarsening in these alloys occurs by fault migration; diffusion within the intermetallic, and its interfacial energy, likely influence coarsening kinetics. At room-temperature, all alloys possess negligible ductility due to the continuous, brittle intermetallic. At 700 and 900°C, the Ni-Zr alloy showed the best combination of strength and ductility. Oxidation experiments at 900°C on Ni-Zr and Ni-Ce revealed heavy internal oxidation of the continuous intermetallic phase. Overall, the Ni-Zr alloy showed good high-temperature coarsening resistance and strength, though ductility and oxidation resistance require improvement for use in structural applications. Possible routes for improving alloy properties via additive manufacturing are discussed.

Ekaputra, Clement [ORNL] (ORCID:0000000307166479)

Up-and-Coming IMCs

While the good oxidation and environmental resistance, high melting points, and comparatively low densities of such ordered intermetallics as Ti 3 Al, NiAl, FeAl, and NbAl 3 render them good candidates for advanced aerospace structures, their poor toughness at low temperatures and low strength at elevated temperatures have prompted the development of fiber-reinforced intermetallic-matrix composites (IMCs) with more balanced characteristics. Fabrication methods for continuous-fiber IMCs under development include the P/M 'powder cloth' method, the foil/fiber method, and thermal spraying. The ultimate success of IMCs depends on fibers truly compatible with the matrix materials.

Randy Bowman

Reliability Analysis of Single Crystal NiAl Turbine Blades

As part of a co-operative agreement with General Electric Aircraft Engines (GEAE), NASA LeRC is modifying and validating the Ceramic Analysis and Reliability Evaluation of Structures algorithm for use in design of components made of high strength NiAl based intermetallic materials. NiAl single crystal alloys are being actively investigated by GEAE as a replacement for Ni-based single crystal superalloys for use in high pressure turbine blades and vanes. The driving force for this research lies in the numerous property advantages offered by NiAl alloys over their superalloy counterparts. These include a reduction of density by as much as a third without significantly sacrificing strength, higher melting point, greater thermal conductivity, better oxidation resistance, and a better response to thermal barrier coatings. The current drawback to high strength NiAl single crystals is their limited ductility. Consequently, significant efforts including the work agreement with GEAE are underway to develop testing and design methodologies for these materials. The approach to validation and component analysis involves the following steps: determination of the statistical nature and source of fracture in a high strength, NiAl single crystal turbine blade material; measurement of the failure strength envelope of the material; coding of statistically based reliability models; verification of the code and model; and modeling of turbine blades and vanes for rig testing.

Joseph Palko

Characterization of Ternary NiTiPt High-Temperature Shape Memory Alloys

Pt additions substituted for Ni in NiTi alloys are known to increase the transformation temperature of the alloy but only at fairly high Pt levels. However, until now only ternary compositions with a very specific stoichiometry, Ni 50-x Pt x Ti 50 , have been investigated and then only to very limited extent. In order to learn more about this potential high-temperature shape memory alloy system, a series of over twenty alloys along and on either side of a line of constant stoichiometry between NiTi and TiPt were arc melted, homogenized, and characterized in terms of their microstructure, transformation temperatures, and hardness. The resulting microstructures were examined by scanning electron microscopy and the phase compositions quantified by energy dispersive spectroscopy. "Stoichiometric" compositions along a line of constant stoichiometry between NiTi to TiPt were essentially single phase but any deviations from a stoichiometry of (Ni,Pt) 50 Ti 50 resulted in the presence of at least two different intermetallic phases, depending on the overall composition of the alloy. Essentially all alloys, whether single or two-phase, still under went a martensitic transformation. It was found that the transformation temperatures were depressed with initial Pt additions but at levels greater than 10 at.% the transformation temperature increased linearly with Pt content. Also, the transformation temperatures were relatively insensitive to alloy stoichiometry within the range of alloys examined. Finally, the dependence of hardness on Pt content for a series of Ni 50-x Pt x Ti 50 alloys showed solution softening at low Pt levels, while hardening was observed in ternary alloys containing more than about 10 at.% Pt. On either side of these "stoichiometric" compositions, hardness was also found to increase significantly.

Transformation Temperatures

Atomic faulting drives exceptional toughness in low thermal expansion chromium alloys

Endowing functional properties with mechanical responses in traditional metals has been a frontier topic, akin to transforming base metal into gold. Chromium and its alloys, with their functional deficiencies and limited ductility, serve as typical examples. Herein, we report a Cr96Fe4Ge1.3B1 alloy that unifies low thermal expansion (LTE, αl = 1.79 × 10-6 K-1, 200 − 315 K) with exceptional toughness (240.2 J·cm-3). The enhancement in mechanical responses is primarily attributed to layered Cr2B intermetallic precipitates, which ameliorate interfacial cohesion and simultaneously refine the grain structure. The weakened interlayer interactions within the Cr-B layers facilitate the nucleation and movement of numerous tiny stacking faults in precipitates, efficiently alleviating strain energy and resulting in marked work-hardening ability. Additionally, antiferromagnetic fluctuations in the BCC matrix contribute to the unique LTE behavior. This paves the way for the design of high-performance alloys featuring layered-symmetry precipitates.

Yu, Chengyi [University of Science and Technology

Compatibility of Type 304H Stainless Steel in Static Molten FLiBe for Inertial Confinement Fusion Reactors: Role of Impurities and Redox Control

Molten fluoride salts, such as FLiBe (LiF-BeF2), are promising candidates for tritium breeding and heat transfer in fusion reactors, but corrosion of structural materials remains a major challenge. This study investigates the corrosion behavior of austenitic stainless steel 304H in purified and NiF2-containing FLiBe at 500°C and 600°C, focusing on the effects of impurities and redox control. Exposure to purified FLiBe resulted in the concurrent depletion of Cr, Mn, and Fe, with corrosion at 500 °C dominated by the combined oxide formation and elemental dissolution, while at 600°C elemental depletion was predominant. The addition of a controlled NiF2 impurity significantly accelerated corrosion at both temperatures, demonstrating the sensitivity of 304H to the salt redox state. Beryllium additions were effective in mitigating corrosion for both baseline and NiF2-containing FLiBe; minimal depletion of Cr, Mn, and Fe occurred with Be additions as low as 2.5 mg (147 wppm), and no NiBe intermetallics formed at 5 mg (294 wppm), indicating that small Be inventories can provide substantial protection without deleterious phase formation. Thermodynamic equilibrium and coupled thermodynamic-kinetic analyses at the salt-alloy interface suggested low corrosion rates in systems with limited hydrogen fluoride (HF) generation, highlighting the importance of salt redox control. Estimates for a Be addition rate were calculated for the HYLIFE-II fusion reactor that can mitigate corrosion-induced degradation, assuming complete conversion of tritium to tritium fluoride (TF). Overall, 304H shows reasonable compatibility with FLiBe under optimized redox conditions. These results provide quantitative guidance for material selection and salt management in fusion blanket and heat exchanger systems and motivate validation under flowing, nonisothermal, and irradiated conditions.

Pillai, Rishi [ORNL] (ORCID:0000000243688197)