Search NASA⌕ Search

SEARCH · Search NASA

Results for “internal short circuit”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Transport Processes in a Li-ion Cell during an Internal Short-Circuit

Internal short-circuit in a lithium-ion cell causes an abrupt increase in cell temperature and triggers subsequent thermal runaway. In this work, we present a detailed electrochemical-thermal model to investigate the physical behavior during an internal short-circuit. Simulations at wide range of heat transfer coefficients and short-circuit resistances are conducted to illustrate electrochemical and thermal behavior under a wide range of conditions. The Joule heating at the shorted region promotes electrochemical reactions nearby, causing in-plane non-uniformity of electrolyte and active material transport. Furthermore, it is found that diffusion in solid active materials plays a significant role at very high shorting currents (~20 C), as electrochemical reactions rate are being controlled progressively more by availability of Li + at the interface, due to limitations in diffusion through the active material with increasing discharge rates. This diffusion limitation causes a drop in available energy, and subsequently a decrease in cell equilibrium potential and the heat generation rate at the location of the short. On the other hand, rapid depletion of lithium concentration in the electrolyte and accumulation on the electrode surface results in highly non-uniform transport properties resulting in higher heat generation rates. Hence, the heating regime shifts from "local heating" to "global heating". Based on the findings, important design parameters for battery safety are discussed.

25 ENERGY STORAGE↗

In Situ Measurement of Temperature Distributions in a Li-ion Cell during Internal Short Circuit and Thermal Runaway

Here we report in situ measurement of temperature distributions in a 2.5-Ah pouch format Li-ion cell during internal short circuit (ISC) and thermal runaway. The ISC and thermal runaway were triggered by nail penetration. The local temperatures were measured by embedded K type micro thermocouples in the middle layer of the experimental Li-ion cell. Highly non-uniform temperature distributions were observed during ISC and thermal runaway as compared with those during constant current discharging and external short circuit. The in situ measurement also captured details of how thermal runaway started from the ISC location and spread to the entire cell in a few seconds. Moreover, the comparison between ISC without thermal runaway and ISC with thermal runaway suggests that internal short circuit resistance plays a critical role in the risk of thermal runaway.

Huang, Shan↗

On-Demand Cell Internal Short Circuit Device

A device implantable in Li-ion cells that can generate a hard internal short circuit on-demand by exposing the cell to 60C has been demonstrated to be valuable for expanding our understanding of cell responses. The device provides a negligible impact to cell performance and enables the instigation of the 4 general categories of cell internal shorts to determine relative severity and cell design susceptibility. Tests with a 18650 cell design indicates that the anode active material short to the aluminum cathode current collector tends to be more catastrophic than the 3 other types of internal shorts. Advanced safety features (such as shutdown separators) to prevent or mitigate the severity of cell internal shorts can be verified with this device. The hard short success rate achieved to date in 18650 cells is about 80%, which is sufficient for using these cells in battery assemblies for field-failure-relevant, cell-cell thermal runaway propagation verification tests

Darcy, Eric↗

Detection of an internal short circuit in a battery

An electrical device comprises a battery cell; a pressure sensor for measuring swelling forces of the battery cell, optionally with voltage, temperature and current sensors, and a battery management system including a controller. The controller executes a program to: (i) determine a reference swelling force corresponding to a reference electrical signal received from the pressure sensor at an earlier reference time, (ii) determine a second swelling force corresponding to a second electrical signal received from the pressure sensor at a later second time, and (iii) determine whether a risk of internal short circuit of the battery cell exists by comparing a reference level of the reference electrical signal and a signal representative of the second electrical signal. When the signal representative of the second electrical signal exceeds the reference level of the reference electrical signal by a threshold amount, a risk of internal short circuit of the cell exists.

Stefanopoulou, Anna G.↗

Internal short circuit and failure mechanisms of lithium-ion pouch cells under mechanical indentation abuse conditions: An experimental study

Electromechanical structural integrity and thermal stability dictate the safety performance of lithium-ion batteries. Progressive deformation and failure across microscopic and macroscopic lengths scales that are responsible for internal short circuit (ISC) in lithium-ion cells under mechanical abuse conditions remains elusive. In this study, a series of indentation tests were conducted on lithium-ion cells with different capacities up to the occurrence of ISC. The external response and internal configuration of these cells were investigated. It is discovered that cells with different capacities and state of charges exhibited different behaviors. Maximum temperature, which is often regarded as the most important parameter related to thermal runaway (TR), varied considerably due to the complicated contact configurations. X-ray computed tomography (XCT) showed that ISC was a collective result of shear band or other strain-localization modes in the electrode assembly, shear offsets in the granular coatings of electrodes, and the accompanying ductile fracture in the metal foils. We believe that the irregular strain-localization modes (kinks, cusps, and buckles), radical mismatches in mechanical properties of different layers, and geometric features of the indenter eventually lead to the tearing/puncture of cell separator at various locations. Furthermore, the results could provide useful guidance for the micromechanical modeling of lithium-ion cells.

25 ENERGY STORAGE↗

Understanding Li-Ion Cell Internal Short Circuit and Thermal Runaway through Small, Slow and In Situ Sensing Nail Penetration

Here we report a small, slow and in situ sensing (3S) nail penetration test method to understand Li-ion cell internal short circuit (ISC) and thermal runaway. The method not only keeps conventional nail penetration's advantage of simple implementation, but also enhances its relevance to field failures and enables detailed in situ diagnosis. It was applied to 3-Ah pouch cells and revealed insights that could not be captured by conventional methods. Most interestingly, multiple in situ temperature peaks were observed during a period of over 100 s before thermal runaway. These initial peaks exceeded safety limit but the temperature rapidly decreased after each peak instead of causing immediate thermal runaway. Further investigation suggested that the initial temperature peaks occurred when nail tip reached aluminum foil current collector to form a low resistance ISC between anode and aluminum foil. The rapid temperature decrease after each peak can be attributed to sudden drop of ISC current, which can be further attributed to rupture of aluminum foil and increase of contact resistance. The findings show that 3S nail penetration test can separate processes of ISC from thermal runaway and provide details of ISC at the level of individual electrode and current collector.

25 ENERGY STORAGE↗

Improved internal short circuit models for thermal runaway simulations in lithium-ion batteries

Thermal runaway (TR) modeling is one of the primary tools that can be used to overcome challenges associated with lithium-ion battery (LIB) safety. Among all LIB accidents that have occurred over the past decade, Internal Short Circuit (ISC) remains the most common trigger mechanism. Many available models in the literature either use a simplified approach to simulate ISC or completely ignore its contribution. The aim of this study is to understand the nature of the heat released for different types of ISC scenarios, including aluminum-anode, anode–cathode, and copper-cathode ISC. We study ISC behavior using a coupled electrochemical–thermal model with an integrated TR chemical kinetics solver built in the COMSOL Multiphysics framework. The time duration of heat release and the magnitude of the peak ISC current are studied as functions of parameters such as the size of the penetrating filament and the capacity of the cell. The numerical results are used to build an empirical model validated against the published experimental TR propagation data. Our model can be successfully used as a viable low-cost substitute in lower order (lumped) TR simulations to enable TR prevention and mitigation.

Singh, Bakhshish Preet (ORCID:0000000264751992)↗

Simultaneously Blocking Chemical Crosstalk and Internal Short Circuit via Gel-Stretching Derived Nanoporous Non-Shrinkage Separator for Safe Lithium-Ion Batteries

The separator, an ionic permeable and electronic insulating membrane between cathode and anode, plays a crucial role in the electrochemical and safety performance of batteries. However, the commercial polyolefin separators not only suffer from inevitable thermal shrinkage at elevated temperature, but also fail to inhibit the hidden chemical crosstalk of reactive gases such as O 2 , leading to often reported thermal runaway (TR) and hence preventing large-scale implementation of high-energy-density lithium-ion batteries. Herein, a nanoporous non-shrinkage separator (GS-PI) was fabricated via a novel gel-stretching orientation approach to eliminate TR. In situ synchrotron small angle X-ray scattering during heating clearly showed that the as-prepared thin GS-PI separator exhibits superior mechanical tolerance at high temperature, thus effectively preventing internal short circuit. Meanwhile, the unique nanoporous structure design further blocks chemical crosstalk and the associated exothermic reactions. Accelerating Rate Calorimetry test revealed that the practical 1 Ah LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622)/graphite pouch cell using GS-PI nanoporous separator show a maximum temperature rise (dT/dt max ) of only 3.7 °C s -1 compared to 131.6 °C s -1 in the case of Al 2 O 3 @PE macroporous separator. Furthermore, despite the reduced pore size, the GS-PI separator demonstrates better cycling stability than conventional Al 2 O 3 @PE separator at high temperature without sacrificing specific capacity and rate capability.

25 ENERGY STORAGE↗

Quantifying and modeling of stress-driven short-circuits in lithium-ion batteries in electrified vehicles

Despite the huge expansion of electric vehicle sales in the market, customers are discouraged by the possible catastrophic consequences brought by the safety issues of lithium-ion batteries, such as internal short circuits, especially in crash scenarios. Herein, we reveal the quantitative relationship between the deformations of the battery and the internal short circuit. By in situ and ex situ observations and post mortem characterization of the component materials, we quantify the stress-driven internal short circuit and failure behavior of the component material. With the aid of a validated numerical computational model as well as the in situ characterization of the global-field temperature, we successfully identify the minor and major short circuits of the cells upon various mechanical abusive loadings. Finally, we establish the internal short circuit criteria for typical formats of batteries. Furthermore, this discovery also provides a fundamental understanding of both internal and external stress-driven short circuits in a much broader context.

25 ENERGY STORAGE↗

Investigating the Ability of Plastic Current Collectors to Isolate Internal Shorts

Metallized plastic current collectors in Li-ion cells reduce mass and reduce the internal short circuit hazard compared to aluminum and copper foils. Shorts induced by nail and by our internal short circuit device were performed on control 18650 cells and on cells with the collectors replaced with metallized polyester and aramid films. Tests were performed inside our fractional thermal runaway calorimeter to quantify the heat transferred and its distributions and those runs done at a synchrotron yielded fascinating very high speedX-ray videography. These show tolerance to nail penetration and activation of defect internal shorts and when thermally forced into thermal runaway, the heat output is significantly reduced. Very high resolutionCT scans, cross sections, and cell tear downs give insights into the thermal and mechanism for these plastic collectors.

Plastic Current Collectors↗

Performance and Safety Tests on Samsung 18650 Li-ion Cells: Two Cell Designs

In order to meet the applications for space shuttle in future, two types of Samsung cells, with capacity 1800 mAh and 2000 mAh, have been investigated. The studies focused on: (1) Performance tests: completed 250 cycles at various combinations of charge/discharge C rates and discharge capacity measurements at various temperatures; and (2) Safety tests: overcharge and overdischarge, heat abuse, short circuit, internal and external short, and vibration, vacuum, and drop tests

Deng, Yi↗

Prevention of lithium-ion battery thermal runaway using polymer-substrate current collectors

Isolating electronically conducting material from internal short circuits is a promising way to prevent the onset of thermal runaway within lithium-ion cells. Here, a metal-coated polymer current collector, which is designed to disconnect internal short circuits by withdrawing from the heating region, is tested in 18650 cells. In addition to having lower mass and manufacturing costs, cells with metal-coated polymer current collectors demonstrate a reduced risk of thermal runaway during nail penetration. High-speed synchrotron X-ray radiography of 18650 cells during nail-penetration testing, in tandem with pre- and post-mortem X-ray computed tomography, provides insights into the function of the current collectors. The results are compared with those of 18650 cells with standard commercial aluminum and copper current collectors. Cells with aluminum-coated polymer current collectors demonstrated 100% success in thermal runaway prevention during nail penetration, retaining a cell voltage >4.00 V, while standard cells consistently experienced thermal runaway.

25 ENERGY STORAGE↗

Composite Thermal Switch

Lithium primary and lithium ion secondary batteries provide high specific energy and energy density. The use of these batteries also helps to reduce launch weight. Both primary and secondary cells can be packaged as high-rate cells, which can present a threat to crew and equipment in the event of external or internal short circuits. Overheating of the cell interior from high current flows induced by short circuits can result in exothermic reactions in lithium primary cells and fully charged lithium ion secondary cells. Venting of the cell case, ejection of cell components, and fire have been reported in both types of cells, resulting from abuse, cell imperfections, or faulty electronic control design. A switch has been developed that consists of a thin layer of composite material made from nanoscale particles of nickel and Teflon that conducts electrons at room temperature and switches to an insulator at an elevated temperature, thus interrupting current flow to prevent thermal runaway caused by internal short circuits. The material is placed within the cell, as a thin layer incorporated within the anode and/or the cathode, to control excess currents from metal-to-metal or metal-to-carbon shorts that might result from cell crush or a manufacturing defect. The safety of high-rate cells is thus improved, preventing serious injury to personnel and sensitive equipment located near the battery. The use of recently available nanoscale particles of nickel and Teflon permits an improved, homogeneous material with the potential to be fine-tuned to a unique switch temperature, sufficiently below the onset of a catastrophic chemical reaction. The smaller particles also permit the formation of a thinner control film layer (<50 m), which can be incorporated into commercial high-rate lithium primary and secondary cells. The innovation permits incorporation in current lithium and lithium-ion cell designs with a minimal impact on cell weight and volume. The composite thermal switch (CTS(TradeMark)) coating can be incorporated in either the anode or cathode or both. The coating can be applied in a variety of different processes that permits incorporation in the cell and electrode manufacturing processes. The CTS responds quickly and halts current flow in the hottest parts of the cell first. The coating can be applied to metal foil and supplied as a cell component onto which the active electrode materials are coated.

McDonald, Robert↗

Gas-driven short disconnection mitigates thermal runaway in Li-ion batteries under mechanical abuse

Mechanical abuse poses a critical safety risk to Li-ion batteries by inducing internal short circuits that initiate thermal runaway. Remarkably, voltage recovery frequently emerges during thermal runaway initiation, a phenomenon that conventional theories fail to explain. Here, our study develops a new multiphysics mechanism to explain voltage recovery, termed gas-driven short disconnection, whereby internal gas pressure mechanically disengages short-circuit contacts and causes the cell voltage to rebound. This mechanism incorporates gas generation and its structural impact on the short circuit. Real-time optical and thermal imaging and X-ray computed tomography reveal fluid-structure interaction between internal gas flow and adjacent shorting contacts. We establish a mechanistic framework linking gas-driven short disconnection to cell-level voltage and temperature responses, elucidating the extension–truncation pattern of voltage recovery. Furthermore, thermal regime maps show that a voltage recovery duration exceeding 5 s correlates with limited temperature rise below 150 °C, indicating that sustained short-circuit disconnection suppresses Joule heating. Additionally, a dimensionless criterion is deduced from scaling analysis for physical plausibility of gas-driven short disconnection in mechanically abused cells. This finding inspires smart venting control, which regulates gas release to maintain the internal pressure while dissipating gas enthalpy, thereby providing a device-level strategy for thermal runaway mitigation.

Gas-driven short disconnection↗

Thermal Runaway of Li-Ion Cells: How Internal Dynamics, Mass Ejection, and Heat Vary with Cell Geometry and Abuse Type

Thermal runaway of lithium-ion batteries can involve various types of failure mechanisms each with their own unique characteristics. Using fractional thermal runaway calorimetry and high-speed radiography, the response of three different geometries of cylindrical cell (18650, 21700, and D-cell) to different abuse mechanisms (thermal, internal short circuiting, and nail penetration) are quantified and statistically examined. Correlations between the geometry of cells and their thermal behavior are identified, such as increasing heat output per amp-hour (kJ Ah −1 ) of cells with increasing cell diameter during nail penetration. High-speed radiography reveals that the rate of thermal runaway propagation within cells is generally highest for nail penetration where there is a relative increase in rate of propagation with increasing diameter, compared to thermal or internal short-circuiting abuse. For a given cell model tested under the same conditions, a distribution of heat output is observed with a trend of increasing heat output with increased mass ejection. Finally, internal temperature measurements using thermocouples embedded in the penetrating nail are shown to be unreliable thus demonstrating the need for care when using thermocouples where the temperature is rapidly changing. All data used in this manuscript are open access through the NREL and NASA Battery Failure Databank.

25 ENERGY STORAGE↗