Search NASA⌕ Search

SEARCH · Search NASA

Results for “investment casting”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

The High-Temperature Mechanical Properties of EN 1.4509 Stainless Steel Cast Using Investment Casting

The high-temperature (600-900 °C) mechanical properties of EN 1.4509 stainless steel made by investment casting were studied by changing the Nb content based on this stainless steel composition standard. The results indicate that with an increase in tensile temperature, the high-temperature strength shows a downward trend and the high-temperature plasticity increases. The results also indicate that with an increase in Nb content, the high-temperature strength rises continually and the high-temperature plasticity decreases; for example, the tensile strengths at 900 °C of Steel A, Steel B and Steel C are 21, 25 and 31 MPa, respectively, and the yield strengths are 15, 20 and 22 MPa, respectively, and the elongations are 97.7, 85.3 and 73.7%, respectively. The high-temperature tensile strength of the investment casting EN 1.4509 stainless steel sample is closely related to the bulk (Ti, Nb) (C, N) and the Laves phase (Fe{sub 2}Nb) at the ferritic grain boundaries and in the ferritic grains. These are the main factors for improvement in the high-temperature strength of the tested steels; additionally, the coarse ferritic grains also play a certain role in improving the mechanical properties. The Nb content of the investment casting EN 1.4509 stainless steel can be reduced to 0.25 wt.%, and at this content, a combination of good high-temperature mechanical properties and higher room-temperature plasticity is obtained.

36 MATERIALS SCIENCE↗

Energy Saving Melting andRevert Reduction Technology (E0SMARRT): Predicting Pattern Tooling and Casting Dimension for Investment Casting

The investment casting process is an expendable mold process where wax patterns of the part and rigging are molded, assembled, shelled and melted to produce a ceramic mold matching the shape of the component to be cast. Investment casting is an important manufacturing method for critical parts because of the ability to maintain dimensional shape and tolerances. However, these tolerances can be easily exceeded if the molding components do not maintain their individual shapes well. In the investment casting process there are several opportunities for the final casting shape to not maintain the intended size and shape, such as shrinkage of the wax in the injection tool, the modification of the shape during shell heating, and with the thermal shrink and distortion in the casting process. Studies have been completed to look at the casting and shell distortions through the process in earlier phases of this project. Dr. Adrian Sabau at Oak Ridge National Labs performed characterizations and validations of 17-4 PH stainless steel in primarily fused silica shell systems with good agreement between analysis results and experimental data. Further tasks provided material property measurements of wax and methodology for employing a viscoelastic definition of wax materials into software. The final set of tasks involved the implementation of the findings into the commercial casting analysis software ProCAST, owned and maintained by ESI Group. This included: o the transfer of the wax material property data from its raw form into separate temperature-dependent thermophysical and mechanical property datasets o adding this wax material property data into an easily viewable and modifiable user interface within the pre-processing application of the ProCAST suite, namely PreCAST o and validating the data and viscoelastic wax model with respect to experimental results

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Predicting Pattern Tooling and Casting Dimensions for Investment Casting, Phase III

Efforts during Phase III focused mainly on the shell-alloy systems. A high melting point alloy, 17-4PH stainless steel, was considered. The experimental part of the program was conducted at ORNL and commercial foundries, where wax patterns were injected, molds were invested, and alloys were poured. Shell molds made of fused-silica and alumino-silicates were considered. A literature review was conducted on thermophysical and thermomechanical properties alumino-silicates. Material property data, which were not available from material suppliers, was obtained. For all the properties of 17-4PH stainless steel, the experimental data available in the literature did not cover the entire temperature range necessary for process simulation. Thus, some material properties were evaluated using ProCAST, based on CompuTherm database. A comparison between the predicted material property data and measured property data was made. It was found that most material properties were accurately predicted only over several temperature ranges. No experimental data for plastic modulus were found. Thus, several assumptions were made and ProCAST recommendations were followed in order to obtain a complete set of mechanical property data at high temperatures. Thermal expansion measurements for the 17-4PH alloy were conducted during heating and cooling. As a function of temperature, the thermal expansion for both the alloy and shell mold materials showed different evolution on heating and cooling. Numerical simulations were performed using ProCAST for the investment casting of 17-4PH stainless steel parts in fused silica molds using the thermal expansion obtained on heating and another one with thermal expansion obtained on cooling. Since the fused silica shells had the lowest thermal expansion properties in the industry, the dewaxing phase, including the coupling between wax-shell systems, was neglected. The shell mold was considered to be a pure elastic material. The alloy dimensions were obtained from numerical simulations. For 17-4PH stainless steel parts, the alloy shrinkage factors were over-predicted, as compared with experimental data. Additional R&D focus was placed on obtaining material property data for filled waxes, waxes that are common in the industry. For the first time in the investment casting industry, the thermo-mechanical properties of unfilled and filled waxes were measured. Test specimens of three waxes were injected at commercial foundries. Rheometry measurement of filled waxes was conducted at ORNL. The analysis of the rheometry data to obtain viscoelastic properties was not completed due to the reduction in the budget of the project (approximately 50% funds were received).

36 MATERIALS SCIENCE↗

Effects of process variables on the properties of YBa2Cu3O(7-x) ceramics formed by investment casting

An investment casting process has been developed to produce net-shape, superconducting ceramics. In this work, a factorial experiment was performed to determine the critical process parameters for producing cast YBa2Cu3O7 ceramics with optimum properties. An analysis of variance procedure indicated that the key variables in casting superconductive ceramics are the particle size distribution and sintering temperature. Additionally, the interactions between the sintering temperature and the other process parameters (e.g., particle size distribution and the use of silver dopants) were also found to influence the density, porosity, and critical current density of the fired ceramics.

Hooker, M. W.↗

Alloy Shrinkage factors for the investment casting of 17-4PH stainless steel parts

In this study, the alloy shrinkage factors were obtained for the investment casting of 17-4PH stainless steel parts. For the investment casting process, unfilled wax and fused silica with a zircon prime coat were used for patterns and shell molds, respectively. Dimensions of the die tooling, wax pattern, and casting were measured using a Coordinate Measurement Machine. For all the properties, the experimental data available in the literature did not cover the entire temperature range necessary for process simulation. A comparison between the predicted material property data measured property data is made. It was found that most material properties were accurately predicted over the most of the temperature range of the process. Several assumptions were made in order to obtain a complete set of mechanical property data at high temperatures. Thermal expansion measurements for the 17-4PH alloy were conducted at heating and cooling. As a function of temperature, the thermal expansion for both the alloy and shell mold materials showed different evolution at heating and cooling. Thus, one generic simulation were performed with thermal expansion obtained at heating and another one with thermal expansion obtained at cooling. The alloy dimensions were obtained from numerical simulation results of solidification, heat transfer, and deformation phenomena. As compared with experimental results, the numerical simulation results for the shrinkage factors were slightly over-predicted.

36 MATERIALS SCIENCE↗

Cryogenic Fracture Toughness Evaluation of an Investment Cast Al-Be Alloy for Structural Applications

Aluminum-Beryllium metal matrix composite materials are useful due to their desirable performance characteristics for aerospace applications. Desirable characteristics of this material includes light-weight, dimensional stability, stiffness, good vibration damping characteristics, low coefficient of thermal expansion, and workability, This material is 3.5 times stiffer and 22% lighter than conventional aluminum alloys. electro-optical systems, advanced sensor and guidance components for flight and satellite systems, components for light-weight high-performance aircraft engines, and structural components for helicopters. Aluminum-beryllium materials are now available in the form of near net shape investment castings. In this materials properties characterization study, the cryogenic tensile and fracture properties of an investment casting alloy, Beralcast 363, were determined. Tensile testing was performed at 21 C (70 F), -73.3 C (-100 F), -195.5 C (-320 F) and -252.8 C (-423 F), and fracture (K(sub lc) and da/dN) testing was performed at -73.3 C (-100 F), -195.5 C (-320 F) and -252.8 C (-423 F). Their use is attractive for weight critical structural applications such as advanced

Gamwell, W. R.↗

Characterization of Al-Mn particles in AZ91D investment castings

Manganese is currently added to Mg-Al alloys in order to improve the corrosion behavior of cast components. A part of this manganese is dissolved in the magnesium matrix and the balance is found as fine Al(Mn,Fe) particles dispersed within castings. For AZ91D specimens prepared using the plaster mould investment casting process, these particles were observed in very large quantity at the surface of castings. These particles were characterized by scanning electron microscopy and electron probe microanalysis. It was found that they consist of Al{sub 8}Mn{sub 5} phase and that their morphology and size depend on local solidification conditions. Their presence at the surface of the castings is related to low solidification rates and reduced thermal gradients at the mould/metal interface.

36 MATERIALS SCIENCE↗

Coating composition embodiments for use in investment casting methods

Disclosed herein are embodiments of a coating composition for use in investment casting. The coating composition embodiments provide a solidified coat that can be as a mold for casting castable materials and that is easily removed from the casted material using water. The coating composition embodiments disclosed herein are reusable and are non-toxic and exhibit high thermal stability.

Cluff, Kyle↗

The Impact of Ceramic Shell Strength on Hot Tearing during Investment Casting

The effect of ceramic shell strength on hot tearing susceptibility during solidification was inspected practicing investment casting of the cobalt-base superalloy samples with the same casting conditions, but different ceramic shell systems. Results showed that the lower the ceramic shell strength upon using polymer additives, the lower the hindered contraction rate, and the lower the hindered contraction rate, the smaller the hot tearing tendency. Optical microscopy and electron microscopy scanning revealed that the hot tear propagated along the last solidified interdendritic phase, and that the hot tear surface had two major modes: (1) the ductile region in the outer layer; and (2) the inner region of liquid embrittlement.

36 MATERIALS SCIENCE↗

Application of Rapid Prototyping to the Investment Casting of Test Hardware (MSFC Center Director's Discretionary Fund Final Report, Project No. 98-08)

Investment casting masters of a selected propulsion hardware component, a fuel pump housing, were rapid prototyped on the several processes in-house, along with the new Z-Corp process acquired through this project. Also, tensile samples were prototyped and cast using the same significant parameters. The models were then shelled in-house using a commercial grade zircon-based slurry and stucco technique. Next, the shelled models were fired and cast by our in-house foundry contractor (IITRI), with NASA-23, a commonly used test hardware metal. The cast models are compared by their surface finish and overall appearance (i.e., the occurrence of pitting, warping, etc.), as well as dimensional accuracy.

Cooper, K. G.↗

Nonaqueous slip casting of high temperature ceramic superconductors using an investment casting technique

A process for slip casting ceramic articles that does not employ parting agents and affords the casting of complete, detailed, precision articles that do not possess parting lines is presented. This process is especially useful for high temperature superconductors and water-sensitive ceramics. A wax pattern for a shell mold is provided, and an aqueous mixture of a calcium sulfate-bonded investment material is applied as a coating to the wax pattern. The coated wax pattern is then dried, followed by curing to vaporize the wax pattern and leave a shell mold of the calcium sulfate-bonded investment material. The shell mold is cooled to room temperature, and a ceramic slip, created by dispersing a ceramic powder in an organic liquid, is poured therein. After a ceramic shell of desired thickness or a solid article has set up in the shell mold, excess ceramic slip is poured out. The shell mold is misted with water and peeled away from the ceramic article, after which the ceramic is fired to provide a complete, detailed, precision, high temperature superconductive ceramic article without parting lines. The casting technique may take place in the presence of a magnetic field to orient the ceramic powders during the casting process.

Hooker, Matthew W.↗

CoCrFeNi Multi-principal Element Alloy Prepared Via Self-propagating High-Temperature Synthesis Plus Investment Casting Method

A CoCrFeNi multi-principal element alloy was successfully prepared via the combination of self-propagating high-temperature synthesis and investment casting. The phase identification, the as-cast microstructure, and the solidification phenomena were investigated. Unlike the dendrite morphology obtained by arc melting, cellular growth in the as-cast alloy was observed as a consequence of the rapid solidification. The solidification process is discussed with regard to the rate of advance of the liquid–solid interface, the equilibrium melting range, and the interface temperature gradient.

36 MATERIALS SCIENCE↗

Gating System Design Optimization for Investment Casting Process

This article aims to optimize specific castings, characterized as an element of the continuous track for armored vehicle. During the primary melts, defects in the form of oxide films and shrinkage porosity occurred. Steel 20ChGSNM described by the Russian GOST standard was used as a batch material, and the investment casting method was selected for production. To eliminate the above-mentioned defects, only changes in the gating system were allowed, because the interference with an ongoing production regarding technical and technological parameters was unacceptable by the manufacturer. Numerical simulation, x-ray, macro-structural and micro-structural analysis were used during the optimization process. The three variants were analyzed, and the achieved results demonstrated that it is possible to significantly affect the casting internal homogeneity by modifying the gating system individual parts. The final variant ensured a decrease in defects by up to 90% and the production of casting having the quality required by the customer.

36 MATERIALS SCIENCE↗

Effect of Friction Stir Processing on Fatigue Behavior of an Investment Cast Al-7Si-0.6 Mg Alloy

Cast aluminum alloys in general show poor fatigue performance due to presence of defects. Friction stir processing (FSP) can be used as a tool for enhancing mechanical properties of cast alloys by eliminating such defects. In the present study FSP led to a five times improvement in fatigue life of an investment cast Al-7Si-0.6Mg hypoeutectic alloy. The reason for such enhancement was linked to closure of casting porosity which acted as crack nucleation sites in the as-cast condition. Porosity acted as notches in the as-cast alloy and led to an order of magnitude higher crack growth rate. As FSP eliminated the porosity and refined Si particles, crack growth rate dropped due to the elimination of the notch effect together with increased crack path tortuosity. Finally, short crack behavior was noted in both cast and FSP specimens. The critical crack length where transition from short crack to long crack behavior took place is related to respective microstructural characteristic dimensions.

36 MATERIALS SCIENCE↗

Effect of Friction Stir Processing on Microstructure and Tensile Properties of an Investment Cast Al-7Si-0.6Mg Alloy

Friction stir processing (FSP) is emerging as a promising tool for microstructural modification. The present study assesses the effects of FSP on the microstructure and mechanical properties of an investment cast Al-7Si-Mg alloy. FSP eliminates porosity and significantly refines eutectic Si particles. The extent of particle refinement varied with changes in processing conditions. High tool rotation rate and low to intermediate tool traverse speed generated a higher volume fraction of finer particles. Tensile ductility changed significantly as a result of FSP, whereas UTS improved only marginally. Yield strength was similar in both cast and FSPed samples under various heat treated conditions, with the highest value obtained after a T6 heat treatment. Further, FSP caused significant grain refinement in the stir zone, subsequently transforming into very coarse grains as abnormal grain growth (AGG) occurred during solution treatment at high temperature.

36 MATERIALS SCIENCE↗

Interaction Between Ceramic Molds and High-Speed Steel during Gravity and Vacuum Investment Casting

Ceramic molds containing the ZrSiO{sub 4}/SiO{sub 2} primary face coat with and without addition of cobalt aluminate were produced. After firing, the surface and the cross sections of the face coats were subjected to detailed characterization using XRD, SEM and EDS. The interaction between the mold systems and 0.9C-6W-5Mo-4Cr-2V high-speed steel was studied during the gravity and vacuum investment casting. During casting, the isostructural transformation of the initial ZrSiO{sub 4} filler occurred. For the mold without addition of the cobalt aluminate, two different types of interaction products [multicomponent phase containing O, Al, Zr, Fe, W and V and (Fe, W,Mo,Cr){sub 2}Al{sub 2}O{sub 6})] were revealed. An interaction layer of a depth in the range of 5-30 μm was thoroughly studied after casting into the mold containing the cobalt aluminate. Addition of the cobalt aluminate into the ceramic system provided significant refinement of the high-speed steel microstructure.

36 MATERIALS SCIENCE↗