Three-dimensional morphology of an ultrafine Al-Si eutectic produced via laser rapid solidification

Al-Si alloys processed by laser rapid solidification yield eutectic microstructures with ultrafine and interconnected fibers. Such fibrous structures have long been thought to bear resemblance to those formed in impurity-doped alloys upon conventional casting. Here, we show that any similarity is purely superficial. By harnessing high-throughput characterization and computer vision techniques, we perform a three-dimensional analysis of the branching behavior of the ultrafine eutectic and compare it against an impurity-modified eutectic as well as a random fractal (as a benchmark). Differences in the branching statistics point to different microstructural origins of the impurity- and quench-modified eutectic. Finally, our quantitative approach is not limited to the data presented here but can be used to extract abstract information from other volumetric datasets, without customization.

36 MATERIALS SCIENCE↗

Models of Rapid Solidification

Laser annealing studies provide much information on various consequences of rapid solidification, including the trapping of impurities in the crystal, the generation of vacancies and twins, and on the fundamental limits to the speed of the crystal-melt interface. Some results obtained by molecular dynamics methods of the solidification of a Lennard-Jones liquid are reviewed. An indication of the relationship of interface speed to undercooling for certain materials can be derived from this model. Ising model simulations of impurity trapping in silicon are compared with some of the laser annealing results. The consequences of interface segregation and atomic strain are discussed.

Gilmer, G. H.↗

Interface velocity dependent solute trapping and phase selection during rapid solidification of laser melted hypo-eutectic Al-11at.%Cu alloy

Microstructure formation of a hypo-eutectic Al-11Cu (atom percent) alloy during solidification after laser melting has been studied by transmission electron microscopy (TEM). The evolution of the solid-liquid-interface velocity, V SL , during the solidification process has been determined from direct observation by in-situ TEM. This enabled correlating V SL with development of four distinct microstructure zones. Crystal growth mode transitions from planar to cellular, cellular to dendritic, dendritic to cellular, and cellular to planar, have been observed for the accelerating solid-liquid-interface. The transition from coupled two-phase growth to the single-phase growth occurred for V SL = V a = (0.80±0.05) m/s, where V a is the velocity of absolute stability, at the onset of banded morphology grain formation. The in-situ and post-mortem TEM uniquely permitted determination of the non-equilibrium solidus for the rapidly solidifying Al-11Cu alloy. Experimental evidence for solute clustering and chemical ordering tendencies at length scales on the order of ≤ 5nm has been detected in the single-phase regions of the banded grains. The structural features of the single-phase bands have been interpreted as signatures of ‘frozen in’ configurations present in the liquid boundary layer adjacent to the growing crystal, which has a width of about 3nm. Finally, the nano-scale spatiotemporal resolution experimental TEM studies performed here provided quantitative metrics, e.g. the solidification interface velocity dependent solute concentration of the α-Al phase and the near-atomic scale structure in the single-phase bands, that are uniquely suitable for comparison with theory and model predictions for solidification microstructure development in multicomponent alloys after laser melting.

36 MATERIALS SCIENCE↗

Systematic discovery of new nano-scale metastable intermetallic eutectic phases in laser rapid solidified Aluminum-Germanium alloy

Laser surface remelting of as-cast Al-Ge eutectic alloy is shown to produce ultrafine lamellar eutectic morphology with interlamellar spacing refined up to ∼60 nm and composed of FCC Al solid solution and unusual Al x Ge y intermetallic phases that do not form during near-equilibrium solidification. The microstructures are characterized and analyzed using a combination of selected area electron diffraction, high-resolution scanning transmission electron microscopy, energy dispersive X-ray spectroscopy to obtain high-resolution elemental maps, and atomistic modeling using density functional theory followed by atomic-scale image simulation. Depending on the local solidification conditions, the crystallography of the Al x Ge y intermetallic phases in the eutectic microstructure is either monoclinic (C 2/c) or monoclinic (P 2 1 ), with high densities of defects in both cases. This is in sharp contrast to the as-cast alloys that showed nominally pure Al and Ge phases with significant solute partitioning and equilibrium FCC and diamond cubic crystal structures, respectively. Corresponding kinetic phase diagrams are proposed to interpret the evolution of nano-lamellar eutectic morphologies with equilibrium Al and metastable Al x Ge y phases, and to explain increased solid solubility in the Al phases manifested by precipitation of ultrafine clusters of Ge. Furthermore, the reasons for the formation of these metastable eutectics under laser rapid solidification are discussed from the perspective of the competitive growth criterion.

Al-Ge eutectic↗

Mechanical Behavior of Al–Al2Cu–Si and Al–Al2Cu Eutectic Alloys

In this study, laser rapid solidification technique was used to refine the microstructure of ternary Al–Cu–Si and binary Al–Cu eutectic alloys to nanoscales. Micropillar compression testing was performed to measure the stress–strain response of the samples with characteristic microstructure in the melt pool regions. The laser-remelted Al–Al2Cu–Si ternary alloy was observed to reach the compressive strength of 1.59 GPa before failure at a strain of 28.5%, which is significantly better than the as-cast alloy with a maximum strength of 0.48 GPa at a failure strain of 4.8%. The laser-remelted Al–Cu binary alloy was observed to reach the compressive strength of 2.07 GPa before failure at a strain of 26.5%, which is significantly better than the as-cast alloy with maximum strength of 0.74 GPa at a failure strain of 3.3%. The enhanced compressive strength and improved compressive plasticity were interpreted in terms of microstructural refinement and hierarchical eutectic morphology.

36 MATERIALS SCIENCE↗

Plastic homogeneity in nanoscale heterostructured binary and multicomponent metallic eutectics: An overview

Heterostructured materials comprised of relatively soft/hard disparate phases typically exhibit composite strengthening but lack plastic deformability at ambient temperatures. However, heterostructured systems comprised of nanoscale phases can simultaneously enhance yield strength and strain hardening, thereby promoting uniform distribution of plastic flow. In this review, the atomic-scale deformation mechanisms in model systems of eutectic alloys, Al-Al 2 Cu and Al-Si, refined to nanoscales via laser rapid solidification are discussed, and compared with literature on multi-component (high entropy) eutectics such as Ni-Al-Fe-based with Cr and/or Co additions. The nano-lamellar Al-Al 2 Cu structures exhibit unit defect mechanisms not reported in monolithic Al 2 Cu intermetallic: localized shear on {0 1 1} and shear-induced faults on {1 2 1} planes, constrained by closely-spaced dislocation arrays in Al confined by Al/Al 2 Cu interfaces. The unexpected plasticity mechanisms are enabled by slip continuity in nanoscale Al-Al 2 Cu eutectics associated with the orientation relationship and interface habit planes. In nano-fibrous Al-Si eutectic, tensile ductility at strength approaching 600 MPa is observed resulting from dislocation plasticity in the nano-Al channels and cracking in Si nanofibers. Molecular dynamics simulations show that Al dislocations easily cross-slip (screw) or climb (edge) along Al-Si interfaces, making slip transmission difficult. The propagation of nano-cracks is suppressed by surrounding strain hardening Al, retaining good ductility of the sample, in spite of lack of direct slip transmission. Finally, the critical unit mechanisms of slip transmission and interface-enabled plasticity observed in nanoscale eutectic binary systems can also explain the strength-ductility relationship in multi-component eutectics and homogeneously distributed plastic flow with increasing microstructural heterogeneity.

36 MATERIALS SCIENCE↗

Ultrahigh strength and plasticity in laser rapid solidified Al–Si nanoscale eutectics

As-cast Al–20wt.% Si alloys were processed via laser rapid solidification (LRS) techniques to create eutectic microstructures with nanoscale interconnected, nanotwinned Si fibers. LRS morphologies exhibit higher flow stress, exceeding 800 MPa and uniform plastic deformation above 20% compared to as-cast alloy that fractures at strains below 8% at flow strength of approximately 200 MPa. The strengthening mechanisms of LRS morphologies are interpreted in terms of the interfacial constraints: increase in yield strength as well as strain hardening rate due to nanoscale confined slip in fibrous Al–Si eutectic, and load transfer and eventual plasticity in the nanoscale Si fibers.

36 MATERIALS SCIENCE↗

Transmission electron microscopy of the rapid solidification microstructure evolution and solidification interface velocity determination in hypereutectic Al-20at.%Cu after laser melting

The evolution of rapid solidification (RS) microstructure and solidification interface velocity has been studied experimentally by in-situ transmission electron microscopy and postmortem characterization for hypereutectic Al-20at.%Cu (37 wt.%Cu) after laser melting. Four morphologically distinct regions formed via growth modes changing from θ-Al 2 Cu phase dendrites to eutectic cell growth, possibly α-Al dendrite growth (α-cell), banded growth, and α-Al plane front growth. Tendency for faceting and low capacity for solute trapping limited the θ-phase dendrite growth to solidification interface velocity v < 0.07 m/s. Consequently, formation of pro-eutectic micro-constituent was suppressed, and RS microstructure formation was dominated by eutectic, α-cell, and banded morphology grains for the Al-20at.%Cu alloy. Eutectic growth operated for interface velocity of 0.1 m/s ≤ v < 0.3 m/s, with a transition from regular lamellar, 2-λ and 1-λ mode to a dense irregular morphology dominated by α-phase at v = 0.3 m/s. Interface temperature calculations indicated feasibility of α-cell growth mode for 0.3 m/s ≤ v < 0.7 m/s. Banded growth occurred for 0.7 m/s ≤ v < 1.3 m/s. Plane front α-phase growth was evident for interface velocities v ≥ 1.3 m/s. Previous work on rapid solidification microstructure development in hypereutectic Al-Cu alloys reported a regime of α-cell growth subsequently to eutectic and prior to transition to banded growth for Al-19at.%Cu (36 wt.%Cu), while for Al-22at.%Cu (40 wt.%Cu) eutectic growth transitioned directly to α-plane front growth without emergence of a banded regime. Finally, based on the current study the disappearance of the banded growth regime occurs for a composition larger than 20at.%Cu.

36 MATERIALS SCIENCE↗

Laser‐Powder Melt Pool Solidification Dynamics and Microstructural Engineering of Ti‐5553 Microlattices

The fine geometric and topological control afforded by additive manufacturing technologies has enabled the manufacture of architected materials across length scales, and enabling tunable mechanical performance as a function of local and global design. Progress has been made to tune the mechanical response of architected materials through geometry, but understanding how the geometry and processing conditions will inform the microstructure remains a challenge due to the rapid solidification in laser powder bed fusion. This study uses in situ X-ray imaging and electron backscatter diffraction microscopy to demonstrate that the melt pool size, microstructure morphology, and elastic strain distribution is influenced by a combination of lattice geometry and laser processing conditions. These results indicate that within larger melt pools the local thermal gradients are sufficient to enable a columnar-to-equiaxed transition across the melt pool. Furthermore, the solidification mechanisms producing these microstructures are examined across the first 5 ms of melting and solidification, described via in situ high-speed X-ray imaging and mirrored via multiphysics simulation.

additive manufacturing↗

Localized orientation gradients in additively manufactured stainless steel 316H structures

The high solidification rates during additive manufacturing cause highly localized thermal and strain gradients. The effect of these gradients on the evolution of local orientation misorientations within a grain is not well understood. In this study, stainless steel 316H parts were fabricated via laser powder bed fusion using three different energy densities: 43, 71, and 135 J/mm 3 . Electron backscatter diffraction showed that the maximum misorientations of the grains can be up to 25° along the build direction. Misorientation gradients (RM g ) within grains are process-dependent and can change from 0.036°/μm to 0.015°/μm with increased volumetric energy densities. In conclusion, the characterized misorientation gradients are an indication of the level of dislocations and, to an extent, the plastic deformation resulting from the rapid solidification during laser powder bed fusion.

316H↗

Laser powder bed fusion of Inconel 718 on 316 stainless steel

The joining of Inconel 718 and 316 stainless steel has notable industrial importance. However, traditional arc-welding has many issues. In particular, the formation of the detrimental Nb-rich Laves phase in the heat affected zone can promote crack initiation and propagation, which leads to poor mechanical properties. The small heat input and the rapid solidification of laser powder bed fusion (PBF) has the potential to suppress this problem. Despite the infancy of the multi-material PBF, it is of interest to investigate the relationship among the process parameter, the microstructure at the materials joining point, and the mechanical performance. In this study, we used high-speed x-ray imaging to in-situ monitor the printing of Inconel 718 tracks on a 316H SS substrate via laser powder bed fusion, followed by post-build characterization and testing with SEM, XRD and nanoindentation. We observed that a higher linear energy density resulted in a more diffused interface and a smaller compositional gradient, but as a trade-off, generated more keyhole pores and thermal cracks. Furthermore, we also showed that the built layer exhibited chemical inhomogeneity at two length scales: a tens-of-mu m-scale compositional vortex due to the melt flow, and a sub-mu m-scale Nb-rich dendritic structure due to the non-equilibrium solidification that led to the formation of the Laves phase. It was inferred that the chemical inhomogeneity may benefit the mechanical properties at the interface by providing more interlocking between the two materials and also by limiting the effect of the brittle Laves phase to potentially short range.

36 MATERIALS SCIENCE↗

Beyond the eutectic paradigm: nanolamellar patterns in a rapidly solidified peritectic alloy

Peritectic transformations are central to many structural alloys, yet pattern formation remains poorly understood due to complex growth dynamics and limited three-dimensional data. Here, we report an unusual two-phase microstructure in a Zn–Ag peritectic alloy subjected to rapid solidification by laser surface remelting. Synchrotron X-ray nanotomography reveals a lamellar structure of primary 𝜀-AgZn 3 and peritectic Zn with ∼700 nm spacing. Although resembling a eutectic morphology, this pattern forms without a eutectic reaction through non-steady coupled growth from the liquid. SEM and TEM-EDS confirm interface shapes and phase compositions. These findings expand the design space of peritectics for refined microstructural control.

36 MATERIALS SCIENCE↗

A Comparison of Solidification Structures and Submicroscale Cellular Segregation in Rapidly Solidified Stainless Steels Produced via Two-Piston Splat Quenching and Laser Powder Bed Fusion

Fusion-based additive manufacturing techniques leverage rapid solidification (RS) conditions to create parts with complex geometries, unique microscale/nanoscale morphological features, and elemental segregation. Three custom composition stainless steel alloys with varying chromium equivalence to nickel equivalence ratio (Cr eq /Ni eq ) between 1.53 and 1.95 were processed using laser powder bed fusion (LPBF) and/or two-piston splat quenching (SQ) to produce solidification rates estimated between 0.4 and 0.8 m/s. Both scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were utilized to collect high-resolution images, electron backscatter diffraction (EBSD) phase identification, and measure cellular segregation. Similar features were observed in both LPBF and SQ samples including phase and microstructure, nanoscale oxide particles, cell size, and segregation behavior. However, dislocation pileup was observed along the cell boundaries only in the LPBF austenite solidified microstructure. Targeted adjustment of the SQ feedstock Cr and Ni concentrations, within the ASTM A240 specification for 316L resulted in no observable impact on the cell size, oxide particle size, or magnitude of segregation. Also, the amount of Ni segregation in the ferrite solidified microstructures did not significantly differ, regardless of Cr/Ni eq or processing technique. Here, SQ is demonstrated as capable of simulating RS rates and microstructures similar to LPBF for use as an alternative screening tool for new RS alloy compositions.

42 ENGINEERING↗

A high strength Al-2Ni-0.5Zr conductor alloy fabricated via laser powder bed fusion

There is a current need for new aluminum alloy design strategies to target applications requiring high strength and conductivity with reductions in mass. A new lightweight Al-2Ni-0.5Zr (wt. %) conductor alloy was fabricated using laser powder bed fusion. A design of experiments probed the alloy's solidification cracking susceptibility. It was observed that solidification cracking was generally reduced with fast scan speeds, above 1500 mm/s, and smaller hatch spacings. The different cooling rates throughout the melt pool produced a heterogeneous distribution of cellular and equiaxed Al 3 Ni precipitates in the as-printed alloy. Additionally, the rapid solidification characteristic of laser powder bed fusion created a super-saturated Zr solid solution. An aging heat treatment at 375 °C for 24 h imparted strengthening through the precipitation of L1 2 -Al 3 Zr nanoprecipitates, which counteracted the softening caused by the fragmentation and coarsening of Al 3 Ni precipitates. The yield strength increased from 138 MPa in the as-printed condition to 168 MPa after aging, while the ductility remained constant at ∼21%. The aging treatment simultaneously increased the electrical conductivity from 40.8% IACS (International Annealed Copper Standard) to 53.5% IACS. Modeling of the strengthening mechanisms and electrical conductivity contributions rationalized the simultaneous increase in strength and conductivity upon aging. Furthermore, the strengthening efficacy of the Al 3 Ni and L1 2 -Al 3 Zr precipitates, combined with the low Ni and Zr solubility in the FCC Al matrix, facilitated both high strength and electrical conductivity. Overall, the combination of strength and electrical conductivity positions this alloy as a suitable choice for additively manufactured lightweight conductors.

Additive manufacturing↗

Refining Microstructures in Additively Manufactured Al/Cu Gradients Through TiB 2 Inclusions

Here, the additive manufacture of compositionally graded Al/Cu parts by laser engineered net shaping (LENS) is demonstrated. The use of a blue light build laser enabled deposition on a Cu substrate. The thermal gradient and rapid solidification inherent to selective laser melting enabled mass transport of Cu up to 4 mm from a Cu substrate through a pure Al deposition, providing a means of producing gradients with finer step sizes than the printed layer thicknesses. Divorcing gradient continuity from layer or particle size makes LENS a potentially enabling technology for the manufacture of graded density impactors for ramp compression experiments. Printing graded structures with pure Al, however, was prevented by the growth of Al 2 Cu 3 dendrites and acicular grains amid a matrix of Al 2 Cu. A combination of adding TiB 2 grain refining powder and actively varying print layer composition suppressed the dendritic growth mode and produced an equiaxed microstructure in a compositionally graded part. Material phase was characterized for crystal structure and nanoindentation hardness to enable a discussion of phase evolution in the rapidly solidifying melt pool of a LENS print.

36 MATERIALS SCIENCE↗