Disentangling cation effects on ion mobility and structure in ionic liquid electrolytes
Ionic liquids (ILs) are low-temperature molten salts, where ion transport is primarily governed by ion–ion interactions. Yet, the impact of organic IL cations on critical electrolyte properties such as ion dissociation and overall transport behavior in lithium-salt-doped ILs remains poorly understood. Moreover, despite their critical role in designing IL-based electrolytes for energy storage applications, ion–ion interactions and ion-specific transport under an applied electrical potential are seldom quantified, largely due to the unique experimental and computational challenges involved. Herein, we compare transport properties obtained using 1 H, 7 Li, and 19 F pulsed-field gradient nuclear magnetic resonance (NMR) and electrophoretic NMR (eNMR) with those measured by electrochemical impedance spectroscopy. Non-equilibrium molecular dynamics (MD) simulations and eNMR confirm the presence of negatively charged [Li(TFSI) n ] (1−n) aggregates that migrate towards the positive electrode, resulting in negative lithium transference numbers. Equilibrium MD simulations reveal a vehicular Li ion transport mechanism facilitated by long-lived aggregates with Li + cations strongly bound to multiple TFSI − anions. Finally, we observe an inverse relationship between the apparent charge of the TFSI − anion in the neat IL, which is dictated by the IL cation, and Li + transport in the salt-doped systems. This highlights the opportunity to tune electrolyte performance by tailoring cation chemistry.
Improved Stability of Oxysulfide Solid-State Electrolytes in Li(G3)TFSI Solvate Ionic Liquid Electrolyte
The performance of all solid-state batteries is limited by poor interfacial contact between active material and solid-state electrolyte (SSE) particles. Semi-solid batteries utilize a secondary electrolyte phase to wet the SSE/AM interface to improve cell performance. Solvate ionic liquids (SILs) are one class of liquid electrolytes under consideration for use in semi-solid batteries. This paper focuses on the Li(G3)TFSI SIL consisting of the bis(trifluoromethanesulfonyl)imide (TFSI − ) anion coupled to a [Li(G3)] + solvate cation. Sulfide SSEs are normally subject to nucleophilic attack by trigylme (G3), however, strong coordination of Li + to G3 in the [Li(G3)] + solvate cation prevents this reaction from taking place. Consequently, the stability of sulfide SSE depends on the ideal 1:1 molar ratio of G3 to TFSI, which may be difficult to maintain. We studied the chemical stability of 70Li 2 S·(30-x)P 2 S 5 ·xP 2 O 5 (x = 0, 2, 5, 10) (oxy)sulfide solid-state electrolyte in Li(G3)TFSI SIL. By physical measurement, UV–vis spectroscopy, electrochemical evaluation, X-ray photoelectron spectroscopy, and first principles calculation it is shown that increased oxygen content improves the stability of SSE in various Li(G3) x TFSI (x = 1, 2, 3, 4) liquid electrolytes. The results suggest that an oxysulfide SSE + SIL semi-solid electrolyte is a good choice for future semi-solid battery designs.
Insight into the Solid Electrolyte Interphase Formation in Bis(fluorosulfonyl)Imide Based Ionic Liquid Electrolytes
The formation of the solid electrolyte interphase (SEI) in an ionic liquid electrolyte of 0.5 m lithium bis(fluorosulfonyl)imide (LiFSI) in 1-ethyl-3-methylimidazolium bis(fluorosulfonyl)imide at high cell voltages (1.7–1.9 V) is investigated in ordered mesoporous carbon (OMC) based Li metal cells using an operando small-angle neutron scattering (SANS) technique coupled with electrochemical impedance spectroscopy and ex situ X-ray photoelectron spectroscopy (XPS). It is demonstrated that discharging the OMC Li metal cells to ≈2 V and holding the cell voltage constant induces a rapid current increase with time, confirming extensive reduction and SEI formation. XPS analysis reveals that LiF is formed at open cell voltage (OCV), which is attributed to the carbenes generated at the lithium negative electrode because of its reaction with EMIm cation diffusing to and initiating the reaction with FSI - anions at the carbon positive electrode. It is confirmed that the chemical reaction at OCV and electrochemical reduction at high cell voltage of the FSI - anion plays a protective role against EMIm cation co-intercalation into the carbon positive electrode during the initial discharge. Operando SANS studies also suggest that slight differences occur in the surface composition and reaction mechanism as a function of cell voltage.
The passivity of lithium electrodes in liquid electrolytes for secondary batteries
Rechargeable Li metal batteries are currently limited by electrolyte decomposition and rapid Li consumption. Li plating and stripping greatly depend on the solid electrolyte interphase formed at the Li metal-liquid electrolyte interface. This Review discusses the reactions occurring at this interface from a corrosion science perspective, highlighting the requirements for an ideal passivation layer. Rechargeable Li metal batteries are currently limited by safety concerns, continuous electrolyte decomposition and rapid consumption of Li. These issues are mainly related to reactions occurring at the Li metal-liquid electrolyte interface. Additionally, the formation of a passivation film (that is, a solid electrolyte interphase) determines ionic diffusion and the structural and morphological evolution of the Li metal electrode upon cycling. In this Review, we discuss spontaneous and operation-induced reactions at the Li metal-electrolyte interface from a corrosion science perspective. We highlight that the instantaneous formation of a thin protective film of corrosion products at the Li surface, which acts as a barrier to further chemical reactions with the electrolyte, precedes film reformation, which occurs during subsequent electrochemical stripping and plating of Li during battery operation. Finally, we discuss solutions to overcoming remaining challenges of Li metal batteries related to Li surface science, electrolyte chemistry, cell engineering and the intrinsic instability of the Li metal-electrolyte interface.
Investigation of Structure and Transport in Li-Doped Ionic Liquid Electrolytes: [pyr14][TFSI], [pyr13][FSI], [EMIM][BF4]
Ionic liquid electrolytes have been proposed as a means of improving the safety and cycling behavior of advanced lithium batteries; however, the properties of these electrolytes under high lithium doping are poorly understood. Here, we employ both polarizable molecular dynamics simulation and experiment to investigate the structure, thermodynamics and transport of three potential electrolytes, N-methyl-N-butylpyrrolidinium bis(trifluoromethylsufonyl)imide ([pyr14][TFSI]), N- methyl-N-propylpyrrolidinium bis(fluorosufonyl)imide ([pyr13][FSI]), and 1-ethyl-3-- methylimidazolium boron tetrafluoride ([EMIM][BF4]), as a function of Li (-) salt concentration and temperature. Structurally, Li(+) is shown to be solvated by three anion neighbors in [pyr14][TFSI] and four anion neighbors in both [pyr13][FSI] and [EMIM][BF4], and at all levels of xLi we find the presence of lithium aggregates. Furthermore, the computed density, diffusion, viscosity, and ionic conductivity show excellent agreement with experimental data. While the diffusion and viscosity exhibit a systematic decrease and increase, respectively, with increasing xLi, the contribution of Li(+) to ionic conductivity increases until reaching a saturation doping level of xLi 0.10. Comparatively, the Li(+) conductivity of [pyr14][TFSI] is an order of magnitude lower than that of the other liquids, which range between 0.1-0.3 mScm. The differences in Li(+) transport are reflected in the residence times of Li(+) with the anions, which are revealed to be much larger for [pyr14][TFSI] (up to 100 ns at the highest doping levels) than in either [EMIM][BF4] or [pyr13][FSI]. Finally, we comment on the relative kinetics of Li(+) transport in each liquid and we present strong evidence for transport through anion exchange (hopping) as opposed to the net motion of Li(+) with its solvation shell (vehicular).
Dendrite-free Al recycling via electrodeposition using ionic liquid electrolytes: The effects of deposition temperature and cathode surface roughness
In this report, the electrodeposition of Al from aluminum scrap alloys (A2020) on copper cathode substrates with varied surface roughness under different deposition temperatures was studied using low-temperature AlCl 3 -1-butyl-3-methyl-imidazolium chloride (BMIC) ionic liquid electrolytes. The bulk electrodeposition of Al was carried out under a voltage of 1.5 V at a stirring rate of 120 rpm using a fixed ionic liquid electrolyte concentration (molar ratio AlCl 3 : BMIC = 2:1). The effects of deposition temperature (range from 80 °C to 140 °C) and surface roughness of Cu cathode substrates (polished by 320, 600, 800, 1200 grits SiC sandpapers and mirror polishing process) on the morphology of deposited Al, current density, current efficiency and energy consumption, were investigated. The Al deposits were characterized using scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD), profilometer, and electrochemical measurements for current density, current efficiency, and energy consumption. It is demonstrated that the deposition temperature and surface roughness of Cu electrodes play a critical role in the nucleation and growth of Al deposits. Higher deposition temperature promotes the diffusion and/or migration of Al 2 Cl 7 - ions and then enhances the current density and efficiency during the electrodeposition of Al. Smoother surface of Cu electrodes is preferred for the formation of dendrite-free Al deposits. Typically, on the mirror polished Cu electrode, no Al dendrite structure was observed, and only plate-like Al deposits were formed at the deposition temperature of 100 °C. Pure metallic Al was successfully deposited on Cu electrodes in AlCl 3 + BMIC ionic liquid electrolytes for all experiments with a current efficiency range from 72% to 99% and energy consumption of 4.6–6.3 kW h/kg Al.
Incorporating the Nanoscale Encapsulation Concept from Liquid Electrolytes into Solid-State Lithium–Sulfur Batteries
Solid-state Li–S batteries are attractive due to their high energy density and safety. However, it is unclear whether the concepts from liquid electrolytes are applicable in the solid state to improve battery performance. Here, we demonstrate that the nanoscale encapsulation concept based on Li 2 S@TiS 2 core–shell particles, originally developed in liquid electrolytes, is effective in solid polymer electrolytes. Using in situ optical cell and sulfur K-edge X-ray absorption, we find that polysulfides form and are well-trapped inside individual particles by the nanoscale TiS 2 encapsulation. We see that this TiS 2 encapsulation layer also functions to catalyze the oxidation reaction of Li 2 S to sulfur, even in solid-state electrolytes, proven by both experiments and density functional theory calculations. A high cell-level specific energy of 427 W·h·kg –1 is achieved by integrating the Li 2 S@TiS 2 cathode with a poly(ethylene oxide)-based electrolyte and a lithium metal anode. This study points to the fruitful direction of borrowing concepts from liquid electrolytes into solid-state batteries.
Balancing solvation: stabilizing lithium metal batteries via optimized cosolvents for ionic-liquid electrolytes
In this study, we examined three cosolvents with distinct solvation capabilities for ionic-liquid electrolytes based on 1-methyl-1-propyl pyrrolidinium bis(fluorosulfonyl)imide (Py13FSI). We demonstrate that 1,1,1-trifluoro-2-(2-(2-(2,2,2-trifluoroethoxy)ethoxy)ethoxy)ethane (FDG) notably enhances the cycle life of Py13FSI-based electrolytes, outperforming 1,1,2,2-tetrafluoroethyl 2,2,3,3-tetrafluoropropylether (TTE) and diglyme (DG). Electrochemical and surface analyses showed that this improvement could be attributed to the formation of a favorable cathode interphase, promoting efficient Li+ transport with reduced overpotential. Spectroscopic techniques (FTIR, Raman, and NMR spectroscopy) and molecular dynamics simulations revealed that cosolvents with varying solvation abilities can influence the solvation structures in Py13FSI-based electrolytes. The mild solvating strength and lithium stability of FDG are key contributors to its effectiveness. Conversely, DG, a strong solvating solvent, destabilized the Py13FSI-DG electrolyte at the lithium metal anode, while TTE, a non-solvating solvent, failed to enhance lithium transport or form a stable cathode interphase. Our findings highlight that balanced solvation exerted by the cosolvents is critical for forming a stable electrolyte–cathode interface, potentially through FSI decomposition. This study offers valuable insights into the development of durable ionic-liquid electrolytes, emphasizing the importance of selecting cosolvents with optimal solvation properties.
Solid Electrolyte Interphase Formation at the Ionic Liquid Electrolyte—Lithium-Metal Interface Using an Ab Initio Molecular Dynamics Approach
An interfacial study is performed using ab initio molecular dynamics (AIMD) simulations to elucidate the electrochemical interfacial stability of an ionic liquid (IL) as component of an electrolyte in contact with a Li-metal anode when an additive, vinylene carbonate (VC), is added to the electrolyte. The IL electrolyte is composed of 1-butyl-1-methylpyrrolidinium bis(fluoro-sulfonyl)-imide (PYR14 + FSI − ) with lithium bis(trifluoromethane-sulfonyl)imide salt (Li + TFSI − ) in a 8:2 concentration ratio. Reactions observed at the interface electrolyte/Li-metal during the AIMD simulations are verified by electronic structure calculations using density functional theory calculations considering a continuum solvent model. We found that the addition of VC to the IL prevents further reduction of the counter-ion TFSI − and retards reduction of FSI − in comparison to the case when the additive VC is absent. The PYR14 + reduction is never observed with or without the additive. The 1st, 2nd, and 3rd electron affinities of the PYR14 + are −0.08, −0.36 and −3.65 eV, indicating little to large repulsive behavior against electrons. The opposite is observed for the two negative ions, FSI − and TFSI − , which yield 1st electron affinities of 1.73 and 1.83 eV, respectively. Reactions obtained under open circuit conditions. Dissociation mechanisms are presented for all IL components reduced at the IL/Li-metal interface.
Investigation of Structure and Transport in Li-Doped Ionic Liquid Electrolytes: [pyr14][TFSI], [pyr13][FSI], [EMIM][BF4]
Ionic liquid electrolytes have been proposed as a means of improving the safety and cycling behavior of advanced lithium batteries; however, the properties of these electrolytes under high lithium doping are poorly understood. Here, we employ both polarizable molecular dynamics simulation and experiment to investigate the structure, thermodynamics and transport of three potential electrolytes, N-methyl-N-butylpyrrolidinium bis(trifluoromethylsufonyl)imide ([pyr14][TFSI]), N- methyl-N-propylpyrrolidinium bis(fluorosufonyl)imide ([pyr13][FSI]), and 1-ethyl-3-- methylimidazolium boron tetrafluoride ([EMIM][BF4]), as a function of Li (-) salt concentration and temperature. Structurally, Li(+) is shown to be solvated by three anion neighbors in [pyr14][TFSI] and four anion neighbors in both [pyr13][FSI] and [EMIM][BF4], and at all levels of xLi we find the presence of lithium aggregates. Furthermore, the computed density, diffusion, viscosity, and ionic conductivity show excellent agreement with experimental data. While the diffusion and viscosity exhibit a systematic decrease and increase, respectively, with increasing xLi, the contribution of Li(+) to ionic conductivity increases until reaching a saturation doping level of xLi 0.10. Comparatively, the Li(+) conductivity of [pyr14][TFSI] is an order of magnitude lower than that of the other liquids, which range between 0.1-0.3 mScm. The differences in Li(+) transport are reflected in the residence times of Li(+) with the anions, which are revealed to be much larger for [pyr14][TFSI] (up to 100 ns at the highest doping levels) than in either [EMIM][BF4] or [pyr13][FSI]. Finally, we comment on the relative kinetics of Li(+) transport in each liquid and we present strong evidence for transport through anion exchange (hopping) as opposed to the net motion of Li(+) with its solvation shell (vehicular).
Liquid electrolytes for low-temperature lithium batteries: main limitations, current advances, and future perspectives
Lithium-ion batteries (LIBs) can now be used in almost all modern electronic devices and electric vehicles. However, as the range of applications increases, the challenges increase as well, especially at very low temperatures. Many individual processes could result in capacity loss of LIBs at low temperatures; however, most of them are associated with the liquid electrolyte inside the battery. In this review, we first discuss the main limitations in developing liquid electrolytes used in low-temperature LIBs, and then we summarize the current advances in low-temperature electrolytes, including lithium salts, solvents, additives, and new strategies. Finally, we present some perspectives on the current state of low-temperature electrolytes for LIBs, outlining the most promising research areas in this field. In conclusion, this review will provide useful insights into the design of cryogenic electrolytes and the path forward to the widespread use of LIBs in cryogenic environments.
Insights into the Nanostructure, Solvation, and Dynamics of Liquid Electrolytes through Small-Angle X-Ray Scattering
The fundamental understanding of nanostructures of liquid electrolytes is expected to enable transformative gains in electrochemical energy storage capacities. However, the solvation structures and molecular dynamics in electrolytes are hard to probe, which limits further performance improvements in macroscopic properties such as ionic conductivity, viscosity, and stability. Small-angle X-ray scattering (SAXS), a non-destructive method for nanostructures characterization in liquids, offers a unique perspective on molecular clusters, anion-cation pairs, solvation sheath, percolating network, aggregates, and domain sizes of electrolytes. Notably, the SAXS method has excellent time-resolution, enabling the study of molecular dynamics by operando characterization. This review focuses on the microscopic understanding of liquid electrolytes by SAXS and operando SAXS. The unique capabilities of X-ray scattering for intra- and inter-molecular relationship and nanostructure characterization of electrolytes are highlighted.
A comprehensive review on liquid electrolyte design for low-temperature lithium/sodium metal batteries
Lithium/sodium metal batteries (LMBs/SMBs) possess immense potential for various applications due to their high energy density. Nevertheless, LMBs/SMBs are highly susceptible to the detrimental effects of an unstable solid electrolyte interphase (SEI) and dendrites during practical applications, particularly pronounced in low-temperature environments. Furthermore, sluggish ion transportation further compromises the cycling stability of LMBs/SMBs at low temperatures. To achieve stable operation of LMBs/SMBs at low temperatures, researchers have made numerous efforts including electrolyte optimization aimed at creating stable SEIs and suppressing the metal dendrites under low temperature conditions. Despite the significant advancements made recently in the liquid electrolyte design, there remains considerable hurdle in electrolyte engineering for practical low-temperature, high energy density LMBs/SMBs, calling for a profound comprehension of the intricate interplay between the electrochemical reaction kinetics and electrolyte compositions. Here, this review provides a thorough overview of various strategies in optimizing liquid electrolytes covering weakly solvating electrolytes, concentration-designed electrolytes, and solvation structure-designed electrolytes, to address the challenges faced by LMBs/SMBs at low temperatures, including slow reaction kinetics and the difficulties in Li + /Na + solvation/desolvation. Furthermore, this review discusses future prospects for the advancement of this field, intending to provide valuable insights and support for subsequent research undertakings.
Investigation of Structure and Transport in Li-Doped Ionic Liquid Electrolytes: [pyr14][TFSI], [pyr13][FSI] and [EMIM][BF4]
Ionic liquid electrolytes have been proposed as a means of improving the safety and cycling behavior of advanced lithium batteries; however, the properties of these electrolytes under high lithium doping are poorly understood. Here, we employ both polarizable molecular dynamics simulation and experiment to investigate the structure, thermodynamics and transport of three potential electrolytes, N-methyl-Nbutylpyrrolidinium bis(trifluoromethylsufonyl)imide ([pyr14][TFSI]), N- methyl-Npropylpyrrolidinium bis(fluorosufonyl)imide ([pyr13][FSI]), and 1-ethyl-3-- methylimidazolium boron tetrafluoride ([EMIM][BF4]), as a function of Li-salt concentration and temperature. Structurally, Li(+) is shown to be solvated by three anion neighbors in [pyr14][TFSI] and four anion neighbors in both [pyr13][FSI] and [EMIM][BF4], and at all levels of x(sub Li) we find the presence of lithium aggregates. Furthermore, the computed density, diffusion, viscosity, and ionic conductivity show excellent agreement with experimental data. While the diffusion and viscosity exhibit a systematic decrease and increase, respectively, with increasing x(sub Li), the contribution of Li(+) to ionic conductivity increases until reaching a saturation doping level of x(sub Li) is approximately 0.10. Comparatively, the Li(+) conductivity of [pyr14][TFSI] is an order of magnitude lower than that of the other liquids, which range between 0.1 - 0.3 mS/cm. The differences in Li(+) transport are reflected in the residence times of Li(+) with the anions, which are revealed to be much larger for [pyr14][TFSI] (up to 100 ns at the highest doping levels) than in either [EMIM][BF4] or [pyr13][FSI]. Finally, we comment on the relative kinetics of Li(+) transport in each liquid and we present strong evidence for transport through anion exchange (hopping) as opposed to the net motion of Li(+) with its solvation shell (vehicular).
Hollow-core optical fibre sensors for operando Raman spectroscopy investigation of Li-ion battery liquid electrolytes
Improved analytical tools are urgently required to identify degradation and failure mechanisms in Li-ion batteries. However, understanding and ultimately avoiding these detrimental mechanisms requires continuous tracking of complex electrochemical processes in different battery components. Here, we report an operando spectroscopy method that enables monitoring the chemistry of a carbonate-based liquid electrolyte during electrochemical cycling in Li-ion batteries with a graphite anode and a LiNi 0.8 Mn 0.1 Co 0.1 O 2 cathode. By embedding a hollow-core optical fibre probe inside a lab-scale pouch cell, we demonstrate the effective evolution of the liquid electrolyte species by background-free Raman spectroscopy. The analysis of the spectroscopy measurements reveals changes in the ratio of carbonate solvents and electrolyte additives as a function of the cell voltage and show the potential to track the lithium-ion solvation dynamics. The proposed operando methodology contributes to understanding better the current Li-ion battery limitations and paves the way for studies of the degradation mechanisms in different electrochemical energy storage systems.