At least 19 records

Thermal characteristics of Lithium-ion batteries

Lithium-ion batteries have a very promising future for space applications. Currently they are being used on a few GEO satellites, and were used on the two recent Mars rovers Spirit and Opportunity. There are still problem that exist that need to be addressed before these batteries can fully take flight. One of the problems is that the cycle life of these batteries needs to be increased. battery. Research is being focused on the chemistry of the materials inside the battery. This includes the anode, cathode, and the cell electrolyte solution. These components can undergo unwanted chemical reactions inside the cell that deteriorate the materials of the battery. During discharge/ charge cycles there is heat dissipated in the cell, and the battery heats up and its temperature increases. An increase in temperature can speed up any unwanted reactions in the cell. Exothermic reactions cause the temperature to increase; therefore increasing the reaction rate will cause the increase of the temperature inside the cell to occur at a faster rate. If the temperature gets too high thermal runaway will occur, and the cell can explode. The material that separates the electrode from the electrolyte is a non-conducting polymer. At high temperatures the separator will melt and the battery will be destroyed. The separator also contains small pores that allow lithium ions to diffuse through during charge and discharge. High temperatures can cause these pores to close up, permanently damaging the cell. My job at NASA Glenn research center this summer will be to perform thermal characterization tests on an 18650 type lithium-ion battery. High temperatures cause the chemicals inside lithium ion batteries to spontaneously react with each other. My task is to conduct experiments to determine the temperature that the reaction takes place at, what components in the cell are reacting and the mechanism of the reaction. The experiments will be conducted using an accelerating rate calorimeter (ARC), which uses a heat-wait-search mode until an exothermic reaction is detected. After an exotherm is found the calorimeter maintains an adiabatic environment around a bomb which holds the test sample. The ARC will help identify important reactions and what temperature these exothermic reactions take place at. In order fully understand the battery, we are first going to take apart the battery and test the individual components of the battery using the ARC. I will first conduct a test on the electrolyte solution by itself. We will then test the electrolyte solution with the anode. We would like to see how the electrolyte solution reacts with the anode and its binder material. The next would be the same test using the cathode instead of the anode. By comparing the results of the electrolyte, electrolyte with anode, and the electrolyte with the cathode we can determine the reactions that are taking place due to each component. Using the heat capacity of the each individual sample and the temperature by which the sample increases, kinetic and thermo-dynamical information can then be found. A Gas chromatograph could be used to help with the task of identifying the by-products at the end of each test. One way of increasing the cycle life is to increase the stability of the materials inside the

Hauser, Dan↗

Kinetics of intercalation of lithium into NbSe3 and TiS2 cathodes

Titanium disulfide and niobium triselenide are two well-studied candidate materials for positive electrodes in rechargeable lithium cells. A comparative study of the kinetics of intercalation of lithium in both the cathodes is made here based on various electrochemical techniques, i.e., linear polarization, potentiodynamic polarization, and ac impedance under different experimental conditions such as prismatic or disk configuration of fresh, partially discharged, or cycled electrode. Further, the diffusion coefficients of lithium ions in these cathodes are estimated under these conditions using conventional techniques, i.e., ac impedance, chronocoulometry, chronoamperometry, and current pulse relaxation. Based on the values of the diffusion coefficients, the applicability of these methods for the determination of diffusion coefficients is discussed.

Ratnakumar, B. V.↗

Predicting Thermal Response in a Li-ion Cell on a UAV Fight Profile

As the energy storage devices continue to "pack" more energy in a small space, any damage, battery component failure, manufacturing defect, or electrically abusing the battery can lead to catastrophic thermal runaway events. A catastrophic thermal event in a cell leads to high temperature, in some instances spewing of battery materials due to gas development from side reactions initiated due to high internal temperatures. Also, a thermal runaway event can propagate from a single "failed" cell to the pack in a battery pack, leading to a more significant event. Mitigating a thermal runaway event is important in the commercial and automotive sectors. However, preventing such events in an electric aircraft (or air taxis) is paramount due to the lack of alternatives in the event of a failure. Battery prognostics algorithms allow the prediction of state-of-charge (SOC) and end-of-life (EOL) of a Li-ion battery in a UAV (unmanned air vehicle) [1]. For this presentation, we will extend this two-level battery predictive algorithm to predict SOC, EOL, and estimated maximum temperature during a simulated flight. The model is extended by integrating a lumped physics-driven thermal model for high current densities [2]. The parameters used to control SOC and EOL are maximum storable charge, time constant for Li-ion diffusivity in the carbon particles, and internal cell resistance. Cycling leads to an increase in the heat generated by an aged Li-ion cell with a LiyCoO2 (LCO) cathode and a LixC6 (MCMB) anode. The aging of a cell leads to increase in SEI layer thickness, the diffusion time for the lithium ions inside the electrodes, and the local reaction rates, in addition to the thermodynamic abuse caused by fixed cycling voltages controlled by a Battery Management System. As the battery ages, the cell resistance increases, while the onset temperature of the thermal runaway decreases (depends on the cell chemistry and cell abuse history). Any large deviation of the cell temperature from the estimated (expected) value can identify a faulty cell. Since SEI decomposition has the lowest onset temperature in the series of reactions leading to thermal runaway, the model considers the self-heating rate of the SEI decomposition as onset temperature (similar to Ref. [3]). The parameters in the Arrhenius equation for the SEI heating rate depend on the number of cycles, the cell's operating temperature, and the cell's abuse history [4,5]. Coupling the electrochemical, thermal, and aging model allow the prognostic algorithm to estimate a typical cell voltage and temperature as a function of age (cycling and calendar), whose departure from measured values from the BMS is used to identify a safety event. In addition, we will present the results from two simulated flight scenarios for a UAV: typical and extreme, since the power requirements vary significantly during take-off, landing, and changing altitudes, while the power requirements remain low during the cruise. For this presentation, the power requirement for a battery pack in a UAV is scaled to a single cell. This cell is cycled through a simulated profile, and the data is collected and used to predict a safety event.

Li-ion↗

Electrochemical impedance spectroscopy of lithium-titanium disulfide rechargeable cells

The two-terminal alternating current impedance of Li/TiS2 rechargeable cells was studied as a function of frequency, state-of-charge, and extended cycling. Analysis based on a plausible equivalent circuit model for the Li/TiS2 cell leads to evaluation of kinetic parameters for the various physicochemical processes occurring at the electrode/electrolyte interfaces. To investigate the causes of cell degradation during extended cycling, the parameters evaluated for cells cycled 5 times were compared with the parameters of cells cycled over 600 times. The findings are that the combined ohmic resistance of the electrolyte and electrodes suffers a tenfold increase after extended cycling, while the charge-transfer resistance and diffusional impedance at the TiS2/electrolyte interface are not significantIy affected. The results reflect the morphological change and increase in area of the anode due to cycling. The study also shows that overdischarge of a cathode-limited cell causes a decrease in the diffusion coefficient of the lithium ion in the cathode.

Narayanan, S. R.↗

Flexible Hybrid Battery/Pseudocapacitor

Batteries keep devices working by utilizing high energy density, however, they can run down and take tens of minutes to hours to recharge. For rapid power delivery and recharging, high-power density devices, i.e., supercapacitors, are used. The electrochemical processes which occur in batteries and supercapacitors give rise to different charge-storage properties. In lithium ion (Li+) batteries, the insertion of Li+, which enables redox reactions in bulk electrode materials, is diffusion controlled and can be slow. Supercapacitor devices, also known as electrical double-layer capacitors (EDLCs) store charge by adsorption of electrolyte ions onto the surface of electrode materials. No redox reactions are necessary, so the response to changes in potential without diffusion limitations is rapid and leads to high power. However, the charge in EDLCs is confined to the surface, so the energy density is lower than that of batteries.

Tucker, Dennis S.↗

3D Printed TiO 2 Negative Electrodes for Sodium-Ion and Lithium-ion Batteries using Vat Photopolymerization

Additive manufacturing, also called 3D printing, represents a unique approach to develop three dimensional shape-conformable batteries with enhanced electrodes, specific surface area, improved ion diffusion, and power. For the first time, the formulation of a composite photocurable resin loaded with battery electrochemically active components was designed to feed a vat photopolymerization (VPP) 3D printer. In direct alignment with NASA’s Artemis mission goals to develop sustainable lunar energy storage infrastructure necessary to support long-term human operations, TiO 2 was here selected as an active material for the negative electrode for sodium-ion and lithium-ion batteries due to its abundance on the lunar surface. The TiO 2 loading in the composite photocurable resin and in the resulting VPP-printed negative electrode was increased as high as possible to enhance the electrochemical performance, while simultaneously ensuring the printability and acceptable mechanical strength for sample handling. The effect of thermal post-processing on the electrical, electrochemical and mechanical performance is reported. Finally, a configurational study is implemented to identify the impact of two different electrode designs (cubic and gyroid lattice unit cells) on the electrochemical performance. This work addresses the difficulties related to the introduction of solid particles within a VPP photocurable resin and the need for a compromise between the electrochemical performances and printability to obtain fully functional VPP-printed electrodes.

sodium-ion battery↗

Active experiments in the distant magnetosphere - The AMPTE program

The Active Magnetospheric Particle Tracer Explorers (AMPTE) program consists of three spacecraft that will be launched to inject tracer ions (lithium and barium) inside and outside the earth's magnetosphere and to detect and monitor these ions as they convect and diffuse through the inner magnetosphere. The principal objectives of the program are: (1) to investigate the transfer of mass from the solar wind to the magnetosphere and its further transport and energization within the magnetosphere; (2) to study the interaction between artificially injected and cosmical plasmas; (3) to establish the elemental and charge composition and dynamics of the charged particle population in the magnetosphere over a broad energy range; and (4) to explore further the structure and dynamics of ambient plasmas in the magnetosphere. The implementation of the above objectives is discussed, with emphasis placed on the tracer aspect of the program.

Krimigis, S. M.↗

Engineering experimental program on the effects of near-space radiation on lithium doped solar cells

The results of an experimental evaluation of the real-time degradation characteristics of lithium-diffused silicon solar cells are reported. A strontium-90 radioisotope was used for simulation of a typical earth-orbital electron environment. The experiment was performed in an ion pump vacuum chamber with samples maintained at -50, +20, +50, and +80 C. Samples were illuminated during the 6-month exposure run with solar cell 1-5 characteristics measured periodically in situ. This 6-month exposure corresponded to a 1 MeV equivalent fluence of approximately 10 to the 14th power electrons/sq cm. Several types of lithium cells were irradiatied and compared directly with conventional N/P cells. The best lithium cells compared favorably with N/P cells, particularly at the higher test temperatures. With a slight improvement of initial performance characteristics, lithium cells appear feasible for 5 to 10 year missions at synchronous altitude. Based on the reported results and those of other irradiation experiments, lithium cells would appear to be superior to N/P cells in proton-dominated earth-orbital environments. Another important conclusion of the effort was that illuminated/loaded cells degrade more rapidly than do dark/unloaded cells. The irradiation experiment provided data of high quality with a high degree of confidence because of the experimental and statistical analysis techniques utilized.

Source record↗

Radiation Damage Workshop

The availability of data regarding the radiation behavior of GaAs and silicon solar cells is discussed as well as efforts to provide sufficient information. Other materials are considered too immature for reasonable radiation evaluation. The lack of concern over the possible catastrophic radiation degradation in cascade cells is a potentially serious problem. Lithium counterdoping shows potential for removing damage in irradiated P-type material, although initial efficiencies are not comparable to current state of the art. The possibility of refining the lithium doping method to maintain high initial efficiencies and combining it with radiation tolerant structures such as thin BSF cells or vertical junction cells could provide a substantial improvement in EOL efficiencies. Laser annealing of junctions, either those formed ion implantation or diffusion, may not only improve initial cell performance but might also reduce the radiation degradation rate.

Stella, P. M.↗

Nanostructured MnO2-Based Cathodes for Li-Ion/Polymer Cells

Nanostructured MnO2-based cathodes for Li-ion/polymer electrochemical cells have been investigated in a continuing effort to develop safe, high-energy-density, reliable, low-toxicity, rechargeable batteries for a variety of applications in NASA programs and in mass-produced commercial electronic equipment. Whereas the energy densities of state-of-the-art lithium-ion/polymer batteries range from 150 to 175 W h/kg, the goal of this effort is to increase the typical energy density to about 250 W h/kg. It is also expected that an incidental benefit of this effort will be increases in power densities because the distances over which Li ions must diffuse through nanostructured cathode materials are smaller than those through solid bulk cathode materials.

Skandan, Ganesh↗

Li-Ion Cells Employing Electrolytes With Methyl Propionate and Ethyl Butyrate Co-Solvents

Future NASA missions aimed at exploring Mars and the outer planets require rechargeable batteries that can operate at low temperatures to satisfy the requirements of such applications as landers, rovers, and penetrators. A number of terrestrial applications, such as hybrid electric vehicles (HEVs) and electric vehicles (EVs) also require energy storage devices that can operate over a wide temperature range (i.e., -40 to +70 C), while still providing high power capability and long life. Currently, the state-of-the-art lithium-ion system has been demonstrated to operate over a wide range of temperatures (-30 to +40 C); however, the rate capability at the lower temperatures is very poor. These limitations at very low temperatures are due to poor electrolyte conductivity, poor lithium intercalation kinetics over the electrode surface layers, and poor ionic diffusion in the electrode bulk. Two wide-operating-temperature-range electrolytes have been developed based on advances involving lithium hexafluorophosphate-based solutions in carbonate and carbonate + ester solvent blends, which have been further optimized in the context of the technology and targeted applications. The approaches employed include further optimization of electrolytes containing methyl propionate (MP) and ethyl butyrate (EB), which are effective co-solvents, to widen the operating temperature range beyond the baseline systems. Attention was focused on further optimizing ester-based electrolyte formulations that have exhibited the best performance at temperatures ranging from -60 to +60 C, with an emphasis upon improving the rate capability at -20 to -40 C. This was accomplished by increasing electrolyte salt concentration to 1.20M and increasing the ester content to 60 percent by volume to increase the ionic conductivity at low temperatures. Two JPL-developed electrolytes 1.20M LiPF6 in EC+EMC+MP (20:20:60 v/v %) and 1.20M LiPF6 in EC+EMC+EB (20:20:60 v/v %) operate effectively over a wide temperature range in MCMB-LiNiCoAlO2 and Li4Ti5O12-LiNi-CoAlO2 prototype cells. These electrolytes have enabled high rate performance at low temperature (i.e., up to 2.0C rates at -50 C and 5.0C rates at -40 C), and good cycling performance over a wide temperature range (i.e., from -40 to +70 C). Current efforts are focused upon improving the high temperature resilience of the methyl propionatebased system through the use of electrolyte additives, which are envisioned to improve the nature of the solid electrolyte interphase (SEI) layers.

Smart, Marshall C.↗

Study of beryllium and beryllium-lithium complexes in single-crystal silicon.

When beryllium is thermally diffused into silicon, it gives rise to acceptor levels 191 and 145 meV above the valence band. Quenching and annealing studies indicate that the 145-meV level is due to a more complex beryllium configuration than the 191-meV level. When lithium is thermally diffused into a beryllium-doped silicon sample, it produces two new acceptor levels at 106 and 81 meV. Quenching and annealing studies indicate that these new levels are due to lithium forming a complex with the defects responsible for the 191- and 145-meV beryllium levels, respectively. Electrical measurements imply that the lithium impurity ions are physically close to the beryllium impurity atoms. The ground state of the 106-meV beryllium-lithium level is split into two levels, presumably by internal strains. Tentative models are proposed to explain these results.

Crouch, R. K.↗

A study of beryllium and beryllium-lithium complexes in single crystal silicon

When beryllium is thermally diffused into silicon, it gives rise to acceptor levels 191 MeV and 145 meV above the valence band. Quenching and annealing studies indicate that the 145-MeV level is due to a more complex beryllium configuration than the 191-MeV level. When lithium is thermally diffused into a beryllium-doped silicon sample, it produces two acceptor levels at 106 MeV and 81 MeV. Quenching and annealing studies indicate that these levels are due to lithium forming a complex with the defects responsible for the 191-MeV and 145-MeV beryllium levels, respectively. Electrical measurements imply that the lithium impurity ions are physically close to the beryllium impurity atoms. The ground state of the 106-MeV beryllium level is split into two levels, presumably by internal strains. Tentative models are proposed.

Crouch, R. K.↗

Lithium-ion drifting: Application to the study of point defects in floating-zone silicon

The use of lithium-ion (Li(+)) drifting to study the properties of point defects in p-type Floating-Zone (FZ) silicon crystals is reported. The Li(+) drift technique is used to detect the presence of vacancy-related defects (D defects) in certain p-type FZ silicon crystals. SUPREM-IV modeling suggests that the silicon point defect diffusivities are considerably higher than those commonly accepted, but are in reasonable agreement with values recently proposed. These results demonstrate the utility of Li(+) drifting in the study of silicon point defect properties in p-type FZ crystals. Finally, a straightforward measurement of the Li(+) compensation depth is shown to yield estimates of the vacancy-related defect concentration in p-type FZ crystals.

Silicon↗

The limits of low-temperature performance of Li-ion cells

The results of electrode and electrolyte studies reveal that the poor low-temperature (<-30 degrees C) performance of Li-ion cells is mainly caused by the carbon electrodes and not the organic electrolytes and solid electrolyte interphase, as previously suggested. It is suggested that the main causes for the poor performance in the carbon electrodes are (i) the low value and concentration depedence of the Li diffusivity and (ii) limited Li capacity.

Diffusion Electrolytes Lithium Secondary cells↗

Electron cyclotron harmonic waves observed by the AMPTE-IRM plasma wave experiment following a lithium release in the solar wind

An unexpected occurrence following the second lithium release by the AMPTE-IRM spacecraft in the solar wind on September 20, 1984, was the appearance of electron cyclotron harmonic emissions. These emissions began about 50 s after the release and continued for several minutes. Narrow-band emissions polarized perpendicular to the magnetic field with amplitudes of approximately 0.00001 V/m were observed in each of the first five harmonic bands. The diffuse emissions extended from below the lowest measured frequency channel to above the highest narrow-band emission with a maximum below the electron cyclotron frequency. It will be shown that these observations are inconsistent with their generation by several ion beam instabilities.

Roeder, J. L.↗

Thermal diffuse X-ray scattering in simple metals

Calculations are reported for the ionic structure factor and X-ray scattering cross section of sodium (at T=0 K and 90 K) and lithium (both isotopes at T=0 K) within the harmonic approximation. An evaluation of the appropriate displacement- displacement correlation function by the special point method circumvents the need for a multiphonon expansion. In the case of sodium, the structure in the one-phonon scattering was straightforwardly accounted for, and an approximate expansion was obtained for all multiphonon scattering. By treating core and conduction electrons on an equal footing, it is shown that information on the conduction electron system is present in the forward scattering component. In lithium the one-phonon cross section at small angles aids in the determination of the effective electron-ion interaction.