Search NASA⌕ Search

SEARCH · Search NASA

Results for “lithium morphology”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Study of Stable Cathodes and Electrolytes for High Specific Density Lithium-Air Battery

Future NASA missions require high specific energy battery technologies, greater than 400 Wh/kg. Current NASA missions are using "state-of-the-art" (SOA) Li-ion batteries (LIB), which consist of a metal oxide cathode, a graphite anode and an organic electrolyte. NASA Glenn Research Center is currently studying the physical and electrochemical properties of the anode-electrolyte interface for ionic liquid based Li-air batteries. The voltage-time profiles for Pyr13FSI and Pyr14TFSI ionic liquids electrolytes studies on symmetric cells show low over-potentials and no dendritic lithium morphology. Cyclic voltammetry measurements indicate that these ionic liquids have a wide electrochemical window. As a continuation of this work, sp2 carbon cathode and these low flammability electrolytes were paired and the physical and electrochemical properties were studied in a Li-air battery system under an oxygen environment.

cathodes↗

Chemical and morphological characteristics of lithium electrode surfaces

Lithium electrode surfaces were analyzed for chemical and morphological characteristics, using electron spectroscopy chemical analysis (ESCA) and scanning electron microscopy (SEM). Samples included lithium metal and lithium electrodes which were cycled in a 1.5 M lithium arsenic hexafluoride/two-methyl tetrahydrofuran electrolyte. Results show that the surface of the as-received lithium metal was already covered by a film composed of LiO2 and an Li2O/CO2 adduct with a thickness of approximately 100-200 A. No evidence of Ni3 was found. Upon exposure of the lithium electrode to a 1.5 M LiAsF6/2-Me-THF electrochemical environment, a second film was observed to form on the surface, consisting primarily of As, Si, and F, possibly in the form of lithium arsenic oxyfluorides or lithium fluorosilicates. It is suggested that the film formation may be attributed to salt degradation.

Yen, S. P. S.↗

The observation of structural defects in neutron-irradiated lithium-doped silicon solar cells

Electron microscopy has been used to observe the distribution and morphology of lattice defects introduced into lithium-doped silicon solar cells by neutron irradiation. Upon etching the surface of the solar cells after irradiation, crater-like defects are observed that are thought to be associated with the space charge region around vacancy clusters. Thermal annealing experiments showed that the crater defects were stable in the temperature range 300 to 1200 K in all of the lithium-doped samples. Some annealing of the crater defects was observed to occur in the undoped cells which were irradiated at the lowest doses.

Sargent, G. A.↗

Internal strain analysis of ceramics using scanning laser acoustic microscopy

Quantitative studies of material behavior characteristics are essential for predicting the functionality of a material under its operating conditions. A nonintrusive methodology for measuring the in situ strain of small dimeter (to 11 microns) ceramic fibers under uniaxial tensile loading and the local internal strains of ceramics and ceramic composites under flexural loading is introduced. The strain measurements and experimentally observed mechanical behavior are analyzed in terms of the microstructural development and fracture behavior of each test specimen evaluated. Measurement and analysis of Nicalon silicon carbide (SiC) fiber (15 microns diameter) indicate that the mean elastic modulus of the individual fiber is 185.3 GPa. Deviations observed in the experimentally determined elastic modulus values between specimens were attributed to microstructural variations which occur during processing. Corresponding variations in the fracture surface morphology were also observed. The observed local mechanical behavior of a lithium alumino-silicate (LAS) glass ceramic, a LAS/SiC monofilament composite, and a calcium alumino-silicate (CAS)/SiC fully reinforced composite exhibits nonlinearities and apparent hysteresis due to the subcritical mechanical loading. Local hysteresis in the LAS matrices coincided with the occurrence of multiple fracture initiation sites, localized microcracking, and secondary cracking. The observed microcracking phenomenon was attributed to stress relaxation of residual stresses developed during processing, and local interaction of the crack front with the microstructure. The relaxation strain and stress predicted on apparent mechanical hysteresis effects were defined and correlated with the magnitude of the measured fracture stress for each specimen studied. This quantitative correlation indicated a repeatable measure of the stress at which matrix microcracking occurred for stress relief of each material system. Stress relaxation occurred prior to the onset of steady state cracking conditions. The relaxation stress occurred at 18.5 percent of the fracture stress in LAS and 11.0 percent of the yield stress in CAS/SiC. The relaxation stress ratio was dependent upon the dominant fracture mode of the LAS/SiC specimens. Relaxation stress ratios greater than 0.30 were observed for specimens which fractured due to shear at the fiber matrix interface; specimens which fracture due to tensile cracking had relaxation stress ratios less than 0.30. The stress relaxation ratio appeared to be a specific characteristic of the glass ceramic material. The measured stress relaxation for LAS indicated a measure of the inherent residual stresses in the material due to processing and suggested localized toughening mechanisms for brittle material structures.

Kent, Renee M.↗

Attachment of Single-wall Carbon Nanotubes (SWNTs) on Platinum Surfaces by Self-Assembling Techniques

Single-wall carbon nanotubes (SWNTs) are very interesting materials because of their morphology, electronic and mechanical properties. Its morphology (high length-to-diameter ratio) and electronic properties suggest potential application of SWNTs as anode material for lithium ion secondary batteries. The introduction of SWNTs on these types of sources systems will improve their performance, efficiency, and capacity to store energy. A purification method has been applied for the removal of iron and amorphous carbon from the nanotubes. Unpurified and purified SWNTs were characterized by transmission electron microscopy (TEM), and thermogravimetric analysis (TGA). In order to attach carbon nanotubes on platinum electrode surfaces, a self-assembled monolayer (SAM) of 4-aminothiophenol (4-ATP) was deposited over the electrodes. The amino-terminated SAM obtained was characterized by cyclic voltammetry, X-ray photoelectron spectroscopy (XPS), and Fourier-transforms infrared (FTIR) spectroscopy. Carbon nanotubes were deposited over the amino-terminated SAM by an amide bond formed between SAM amino groups and carboxylic acid groups at the open ends of the carbon nanotubes.This deposition was characterized using Raman spectroscopy and Scanning Electron microscopy (SEM).

Rosario-Castro, Belinda I.↗

Electrochemical impedance spectroscopy of lithium-titanium disulfide rechargeable cells

The two-terminal alternating current impedance of Li/TiS2 rechargeable cells was studied as a function of frequency, state-of-charge, and extended cycling. Analysis based on a plausible equivalent circuit model for the Li/TiS2 cell leads to evaluation of kinetic parameters for the various physicochemical processes occurring at the electrode/electrolyte interfaces. To investigate the causes of cell degradation during extended cycling, the parameters evaluated for cells cycled 5 times were compared with the parameters of cells cycled over 600 times. The findings are that the combined ohmic resistance of the electrolyte and electrodes suffers a tenfold increase after extended cycling, while the charge-transfer resistance and diffusional impedance at the TiS2/electrolyte interface are not significantIy affected. The results reflect the morphological change and increase in area of the anode due to cycling. The study also shows that overdischarge of a cathode-limited cell causes a decrease in the diffusion coefficient of the lithium ion in the cathode.

Narayanan, S. R.↗

Electrolytic Co-deposition Neutron Production Evaluation

Co-deposition electrochemical cells are a simple means to examine novel nuclear reactions. In this study, palladium and deuterium atoms were co-deposited on a cathode at stoichiometric densities, forming dendritic morphologies. Bubble detector neutron dosimeters were used to measure equivalent dose levels during electrolytic deposition. Standard configuration cells expected to produce excess neutrons were denoted as experimental cells and contained an electrolyte consisting of palladium(II) chloride, lithium chloride, and heavy water. The control cells used copper(II) chloride, lithium chloride, and heavy water electrolyte. Experimental and control cells were supplied current, increasing from 0.1 to 100.0 mA over a period of 20 days. For test days 9 through 20, the standard configuration experimental cells exhibited significantly higher average neutron radiation than the controls at a 99% confidence level. Alternative configurations involving more increasing current over a shortened time scale, substitutions of water in place of heavy water or potassium chloride for lithium chloride, as well as inclusion of depleted uranium near the cell cathodes all resulted in inconclusive evidence for promoting neutron production.

neutron↗

Advanced Lithium-ion Batteries with High Specific Energy and Improved Safety for Nasa's Missions

High Energy Materials ( Cathodes, anodes and high voltage and safe electrolyte are required to meet the needs of the future space missions. A. Cathodes: The layered layered composites of of Li2MnO3 and LiMO2 are promising Power capability of the materials, however requires further improvement. Suitable morphology is critical for good performance and high tap (packing) density. Surface coatings help in the interfacial kinetics and stability. B. Electrolytes: Small additions of Flame Retardant Additives improves flammability without affecting performance (Rate and cycle life). 1.0 M in EC+EMC+TPP was shown to have good performance against the high voltage cathode; Performance demonstrated in large capacity prototype MCMB- LiNiCoO2 Cells. Formulations with higher proportions are looking promising. Still requires further validation through abuse tests (e.g., on 18650 cells).

NASA Missions↗

Optimization of the lithium/thionyl chloride battery

A 1-D math model for the lithium/thionyl chloride primary cell is used in conjunction with a parameter estimation technique in order to estimate the electro-kinetic parameters of this electrochemical system. The electro-kinetic parameters include the anodic transfer coefficient and exchange current density of the lithium oxidation, alpha sub a,1 and i sub o,i,ref, the cathodic transfer coefficient and the effective exchange current density of the thionyl chloride reduction, alpha sub c,2 and a sup o i sub o,2,ref, and a morphology parameter, Xi. The parameter estimation is performed on simulated data first in order to gain confidence in the method. Data, reported in the literature, for a high rate discharge of an experimental lithium/thionyl chloride cell is used for an analysis.

White, Ralph E.↗

Microstructural analysis of the 2195 aluminum-lithium alloy welds

The principal objective of this research was to explain a tendency of 2195 Al-Li alloy to crack at elevated temperature during welding. Therefore, a study was made on the effect of welding and thermal treatment on the microstructure of Al-Li Alloy 2195. The critical roles of precipitates, boundaries, phases, and other features of the microstructure were inferred from the crack propagation paths and the morphology of fracture surface of the alloy with different microstructures. Particular emphasis was placed on the microstructures generated by the welding process and the mechanisms of crack propagation in such structures. Variation of the welding parameters and thermal treatments were used to alter the micro/macro structures, and they were characterized by optical and scanning electron microscopy. A theoretical model is proposed to explain changes in the microstructure of welded material. This model proposes a chemical reaction in which gases from the air (i.e., nitrogen) release hydrogen inside the alloy. Such a reaction could generate large internal stresses capable to induce porosity and crack-like delamination in the material.

Talia, George E.↗

Environmental fatigue in aluminum-lithium alloys

Aluminum-lithium alloys exhibit similar environmental fatigue crack growth characteristics compared to conventional 2000 series alloys and are more resistant to environmental fatigue compared to 7000 series alloys. The superior fatigue crack growth behavior of Al-Li alloys 2090, 2091, 8090, and 8091 is due to crack closure caused by tortuous crack path morphology and crack surface corrosion products. At high R and reduced closure, chemical environment effects are pronounced resulting in accelerated near threshold da/dN. The beneficial effects of crack closure are minimized for small cracks resulting in rapid growth rates. Limited data suggest that the 'chemically small crack' effect, observed in other alloy system, is not pronounced in Al-Li alloys. Modeling of environmental fatigue in Al-Li-Cu alloys related accelerated fatigue crack growth in moist air and salt water to hydrogen embrittlement.

Piascik, Robert S.↗

Survival of epiphytic bacteria from seed stored on the Long Duration Exposure Facility (LDEF)

This study was designed to determine the survival of microorganisms exposed to the relatively harsh conditions found in low Earth orbit (LEO). Seed of corn, sunflower, canteloupe, zucchini, bean, pea, and pumpkin cultivars were packaged in two 18 x 2.5 cm aluminum tubes; wall thickness for each tube was 1.33 mm. One seed tube was attacked to payload M0006, tray C-2; a second tube was stored at room temperature in a lab on Earth. Five lithium fluoride thermoluminescent dosimetry wafers (TLD-100 wafers) were placed in each aluminum tube. The total mean dosages for flight and ground-control TLD wafers were 210.0 and 0.9 rads, respectively. Seeds were washed for 2 hrs in a phosphate buffered saline solution. Bacteria were isolated by plating samples of the seed-washings onto dilute tryptic soy agar. Pure isolates of morphologically distinct bacteria were obtained by standard microbiological procedures. Bacteria were grouped according to colony-type and preliminary identification was completed using a fatty-acid analysis system. Bacillus spp. were the primary microoganisms that survived on seed during the experiment. Bacterial diversity and relative abundance were similar for the ground flight seed. Bacillus subtilus, B. pumilus, B. licheniformis, B. polymyxa, B. megaterium, and B. pabuli were isolated most frequently. Members of the genera Kurthia, Listeria, Micrococcus, and Arthrobacter were also isolated from flight and ground control seed. Results support the hypothesis that terrestrial microorganisms can survive long periods of time in the relatively harsh LEO environment.

Schuerger, Andrew C.↗

The relative stress-corrosion-cracking susceptibility of candidate aluminum-lithium alloys for aerospace structural applications

The microstructure and tensile properties of two powder metallurgy processed aluminum-lithium alloys were determined. Strength properties of 480 MPa yield and 550 MPa ultimate tensile strength with 5% strain to fracture were attained. Very little reduction in area was observed and fracture characteristics were brittle. The magnesium bearing alloy exhibited the highest strength and ductility, but fracture was intergranular. Recrystallization and grain growth, as well as coarse grain boundary precipitation, occurred in Alloy 2. The fracture morphology of the two alloys differed. Alloy 1 fractured along a plane of maximum shear stress, while Alloy 2 fractured along a plane of maximum tensile stress. It is found that a fixed orientation relationship exists between the shear fracture plane and the rolling direction which suggests that the PM alloys are strongly textured.

Pizzo, P. P.↗

High-Capacity, High-Voltage Composite Oxide Cathode Materials

This SBIR project integrates theoretical and experimental work to enable a new generation of high-capacity, high-voltage cathode materials that will lead to high-performance, robust energy storage systems. At low operating temperatures, commercially available electrode materials for lithium-ion (Li-ion) batteries do not meet energy and power requirements for NASA's planned exploration activities. NEI Corporation, in partnership with the University of California, San Diego, has developed layered composite cathode materials that increase power and energy densities at temperatures as low as 0 degC and considerably reduce the overall volume and weight of battery packs. In Phase I of the project, through innovations in the structure and morphology of composite electrode particles, the partners successfully demonstrated an energy density exceeding 1,000 Wh/kg at 4 V at room temperature. In Phase II, the team enhanced the kinetics of Li-ion transport and electronic conductivity at 0 degC. An important feature of the composite cathode is that it has at least two components that are structurally integrated. The layered material is electrochemically inactive; however, upon structural integration with a spinel material, the layered material can be electrochemically activated and deliver a large amount of energy with stable cycling.

Hagh, Nader M.↗

Characterization of Al-Cu-Li Alloy 2090 Near Net Shape Extrusion

Aluminum-lithium (Al-Li) alloys near net shape extrusions are being evaluated for potential application in launch vehicle structures. The objective of this study was to determine tensile and fracture properties, corrosion resistance, and weldability of integrally stiffened panels of Al-Cu-Li alloy 2090 in the T8 temper. The microstructure was pre-dominantly unrecrystallized. Texture analyses revealed the presence of fiber components in the stiffeners and a combination of fiber and rolling components in the skin. Variations in grain morphology and texture through the extruded cross section were correlated with the tensile, fracture, and corrosion behavior. Tensile strengths at room and cryogenic temperatures of the 2090 extrusions were similar to other 2090 product forms and were higher than 2219-T87, the primary structural material in the Space Shuttle external tank; however, ductilities were lower. The fracture resistance of the 2090 extrusion was lower than 2219-T87 plate at room temperature. At cryogenic temperatures, tensile ductility and fracture behavior of the 2090 extrusion were similar to other 2090 product forms but were lower than 2219-T87 plate. The exfoliation and stress corrosion resistance of the 2090 extrusion compared favorably with the characteristics of other 2090 product forms. The weldability and weldment properties of the extrusions were similar to 2090 and 2219 plates.

Birt, M. J.↗

Fatigue crack initiation and small crack growth in several airframe alloys

The growth of naturally-initiated small cracks under a variety of constant amplitude and variable amplitude load sequences is examined for several airframe materials: the conventional aluminum alloys, 2024-T3 and 7075-T6, the aluminum-lithium alloy, 2090-T8E41, and 4340 steel. Loading conditions investigated include constant amplitude loading at R = 0.5, 0, -1 and -2 and the variable amplitude sequences FALSTAFF, Mini-TWIST and FELIX/28. Crack growth was measured at the root of semicircular edge notches using acetate replicas. Crack growth rates are compared on a stress intensity factor basis, to those for large cracks to evaluate the extent of the small crack effect in each alloy. In addition, the various alloys are compared on a crack initiation and crack growth morphology basis.

Swain, M. H.↗

Fatigue crack initiation and small crack growth in several airframe alloys

The growth of naturally-initiated small cracks under a variety of constant amplitude and variable amplitude load sequences is examined for several airframe materials: the conventional aluminum alloys, 2024-T3 and 7075-T6, the aluminum-lithium alloy, 2090-T8E41 and 4340 steel. Loading conditions investigated include constant amplitude loading at R = 0.5, 0, -1 and -2 and the variable amplitude sequences FALSTAFF, Mini-TWIST, and FELIX/28. Crack growth was measured at the root of semicircular edge notches using acetate replicas. Crack growth rates are compared on a stress intensity factor basis, to those for large cracks to evaluate the extent of the small crack effect in each alloy. In addition, the various alloys are compared on a crack initiation and crack growth morphology basis.

Swain, M. H.↗

Electrodeposition of Metals in Microgravity Conditions

Metal electrodeposition may introduce various morphological variations depending on the electrolytic conditions including cell configurations. For liquid electrolytes, a precise study of these deposits may be complicated by convective motion due to buoyancy. Zero-gravity (0-G) condition provided by drop shaft or parabolic flight gives a straightforward mean to avoid this effect: we present here 0-G electrodeposition experiments, which we compare to ground experiments (1-G). Two electrochemical systems were studied by laser interferometry, allowing to measure the concentration variations in the electrolyte: copper deposition from copper sulfate aqueous solution and lithium deposition from an ionic liquid containing LiTFSI. For copper, concentration variations were in good agreement with theory. For lithium, an apparent induction time was observed for the concentration evolution at 1-G: due to this induction time and to the low diffusion coefficient in ionic liquid, the concentration variations were hardly measurable in the parabolic flight 0-G periods of 20 seconds.

Nishikawa, K.↗