Search NASA⌕ Search

SEARCH · Search NASA

Results for “lithium morphology evolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Li Morphology Evolution during Initial Cycles in a Gel Composite Polymer Electrolyte

Understanding and controlling lithium morphology evolution and lithium dendrite formation and growth during cycling is one of the key challenges for high-energy lithium metal batteries. This challenge applies to liquid electrolyte batteries as well as solid-state and semi-solid-state batteries. Our current knowledge about the evolution of the Li morphology is mostly obtained from liquid electrolyte-based studies in a Li–Li symmetrical cell configuration. The knowledge obtained in such conditions may not readily transfer into solid-state or semi-solid-state batteries. In this work, Li morphology evolution during initial cycling in a full cell configuration with the LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC 622) cathode and a semi-solid-state gel composite electrolyte is monitored via post-mortem photographs and scanning electron microscopy at multiple length scales. The gel composite electrolyte contains a cross-linked poly(ethylene oxide)-based polymer electrolyte, ceramic fillers, and a liquid plasticizer. The results show that severe surface pitting occurs as early as the second stripping cycle. Pit formation and continuous dissolution during the stripping process are the main cause of the Li surface roughening and dendrite growth mechanism in the model gel composite electrolyte. Comparing Li dendrite growth mechanisms in liquid, polymer, and ceramic solid electrolytes, the dendrite growth mechanism observed in this model electrolyte resembles that of the liquid electrolyte the most. This study suggests that strategies to control Li morphology and prevent dendrite growth in a gel composite electrolyte should be similar to strategies applicable to liquid electrolytes.

25 ENERGY STORAGE↗

Interface morphogenesis with a deformable secondary phase in solid-state lithium batteries

Here, the complex morphological evolution of lithium metal at the solid-state electrolyte interface limits performance of solid-state batteries, leading to inhomogeneous reactions and contact loss. Inspired by biological morphogenesis, we developed an interfacial self-regulation concept in which a deformable secondary phase dynamically aggregates at the interface in response to local electro-chemo-mechanical stimuli, enhancing contact. The stripping of a lithium electrode that contains 5 to 20 mole % electrochemically inactive sodium domains causes spontaneous sodium accumulation across the interface, with the sodium deforming to attain intimate electrical contact without blocking lithium transport. This process, characterized with operando x-ray tomography and electron microscopy, mitigates voiding and improves cycling at low stack pressures. The counterintuitive strategy of adding electrochemically inactive alkali metal to improve performance demonstrates the utility of interfacial self-regulation for solid-state batteries.

Yoon, Sun Geun [Georgia Institute of Technology, A↗

The Crucial Role of Vacancy Concentration in Enabling Superatomic Diffusion in Lithium Intermetallics

Anode-free solid-state Li batteries promise significant increases in energy densities compared to current commercial batteries that rely on liquid electrolytes. Major challenges persist in controlling morphological evolution during the plating and stripping of lithium metal at the anode current collector. Elemental additives that alloy with lithium have been found to modify the plating and stripping behavior of lithium. Many alloying elements form intermetallics with lithium and the mobility of Li through these intermetallics is believed to have an important effect on morphological evolution. This study shows that Li transport coefficients through intermetallics span a wide range in values, with the B32 LiAl intermetallic predicted to have a Li tracer diffusion coefficient as high as 10 –6 cm 2 /s at room temperature, which is 8 orders of magnitude larger than that of isostructural B32 LiZn. This work demonstrates the crucial role of vacancy concentration in controlling the mobility of Li atoms through intermetallics. While the migration barriers for Li-vacancy exchanges in both LiAl and LiZn are remarkably low, the superatomic conductivity in LiAl is shown to arise from the unique electronic structure of the B32 LiAl compound, which favors high concentrations of vacancies.

25 ENERGY STORAGE↗

Discharge Rate‐Driven Li 2 O 2 Growth Exhibits Unconventional Morphology Trends in Solid‐State Li‐O 2 Batteries

Solid-state lithium oxygen batteries (LOBs) are known for their enhanced safety, higher electrochemical stability, and improved energy density compared to liquid-state LOBs. However, the investigation of solid-state LOBs is limited with little understanding of their discharge and charge processes. In this work, a polymer-based solid-state LOB is used to investigate the effect of discharge rate on lithium peroxide (Li 2 O 2 ) formation, the oxygen evolution reaction (OER), and cycle performance. Notably, we observe a counterintuitive trend: Li 2 O 2 particle size increases with increasing discharge current density, in contrast to liquid systems. This behavior arises from inherent space charge layers that restrict Li⁺ transport under high current, and spatially heterogeneous active sites at the solid electrolyte–cathode interface, directly evidenced by small angle X-ray scattering (SAXS), which govern nucleation accessibility and promote site-selective Li 2 O 2 growth. Furthermore, higher current densities improve ORR and OER efficiency but accelerate anode degradation, while lower currents promote side reactions. These opposing effects result in a trade-off that defines an optimal discharge rate (0.1 mA cm -2 ) for maximizing cycle life. This study provides a new mechanistic perspective on discharge-driven processes in solid-state LOBs and offers practical guidelines for performance optimization in future high-energy battery systems.

Discharge current density↗

Transient Chemo‐Mechanical Model of Lithium Plating Impacted by External Pressure

Abstract Lithium anodes show great promise in commercial applications, but are hindered by lithium plating and dendrite growth which cause safety concerns during long‐term cell operation. Stack pressure is experimentally observed to improve cell lifetime; however, the relationship between stress and lithium deposition has remained difficult to elucidate. In this work, a transient, 3D, finite‐element model of the evolution of a lithium anode due to stripping and plating is developed. The evolution of a microscale protrusion on the anode surface is tracked over one charge‐discharge cycle with respect to stack pressure and lithium yield strength. Lithium plastic deformation, nonconformal anode‐separator contact, and separator porosity effects are accounted for. Over the course of several hours of stripping/plating, the anode surface evolves to a similar morphology under pressure regardless of the initial conditions due to lithium plastic deformation and hardening. The rate of this evolution highly depends on the applied pressure and assumed lithium yield strength.

25 ENERGY STORAGE↗

Study of Void Formation at the Lithium|Solid Electrolyte Interface

There is growing recognition of the critical role of void formation in lithium metal anodes in solid-state batteries and its impact on electrochemical performance. While experimental studies have demonstrated the challenges ensuing from void formation at the lithium metal interface with the solid electrolyte, there is a need to understand and quantify the role of intrinsic transport properties in lithium metal and the impact of external stimuli, such as temperature, pressure, and current density. Here, we develop this understanding by constructing a phase field-based model that captures the evolution of void domains at the lithium-solid electrolyte interface. Growth of the pores is driven by the fast removal of lithium from the interface during stripping at high current densities. Relative magnitudes of the bulk and surface lithium diffusivities, along with the applied current density, dictate the final pore morphology. Increasing the temperature results in faster diffusion, while external applied pressure causes creep flow of lithium, both of which help to mitigate the evolution of voids by quickly transporting metal from the bulk to the interface. Finally, a phase map as a function of temperature and pressure is developed as a guide to determine the regions that can lead to the stable cycling of lithium metal.

25 ENERGY STORAGE↗

In-situ visualization of the transition metal dissolution in layered cathodes

Transition metal dissolution in layered cathodes is one of the most intractable issues that deteriorates the battery performance and lifetime. It not only aggravates the structure degradation in cathode, but also damages the solid electrolyte interphase in anode and even induce the formation of lithium dendrites. In this work, we investigate the dissolution behaviors of polycrystalline and single-crystalline layered cathode via operando X-ray imaging techniques. The described cathode particle morphology appears to have a significant impact on the evolution of the dissolution dynamics. As a mitigation strategy, we reveal that doping with trace amount of Zr in the layered cathode could improve its robustness against the transition metal dissolution. Our finding provides valuable insights for designing the next-generation highly-stable layered battery cathodes.

25 ENERGY STORAGE↗

Strain-retardant coherent perovskite phase stabilized Ni-rich cathode

The use of state-of-the-art Ni-rich layered oxides (LiNi x Co y Mn 1-x-y O 2 , x > 0.5) as the cathode material for lithium-ion batteries can push the energy and power density to a higher level than is currently available. However, volume variation associated with anisotropic lattice strain and stress that is being developed during lithium (de) intercalation induces severe structural instability and electrochemical decay of the cathode materials, which is amplified further when the battery is operating at a high voltage (above 4.5 V), which is essential for unlocking its high energy. Even after much effort by the research community, an intrinsic strain-retardant method for directly alleviating the continuous accumulation of lattice strain remains elusive. By introducing a coherent perovskite phase into the layered structure functioning as a ‘rivet’, we significantly mitigate the pernicious structural evolutions by a pinning effect. The lattice strain evolution in every single cycle is markedly reduced by nearly 70% when compared with conventional materials, which significantly enhances morphological integrity leading to a notable improvement in battery cyclability. This strain-retardant approach broadens the perspective for lattice engineering to release the strain raised from lithium (de)intercalation and paves the way for the development of high-energy-density cathodes with long durability.

25 ENERGY STORAGE↗

SEI formation mechanisms and Li + dissolution in lithium metal anodes: Impact of the electrolyte composition and the electrolyte-to-anode ratio

The lithium metal battery is one of today's most promising high-energy-density storage devices. Its full-scale implementation depends on solving operational and safety issues intrinsic to the Li metal high reactivity leading to uncontrolled electrolyte decomposition and uneven Li deposition. In this work, we study the spontaneous formation of the solid electrolyte interphase (SEI) upon contact of Li metal with the electrolyte and describe the heterogeneous SEI morphological features. Multiple electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethoxyethane (DME), dimethyl carbonate (DMC), 1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) and bis(2,2,2-trifluoroethyl) ether (BTFE) are used. Findings include the description of the SEI evolution from dispersed LiO, LiS, LiN, and LiF clusters to a continuous and compact inorganic phase in which the LiO and LiF content depend on the presence of fluorine diluents. Further, the role of the DME ether solvent helping the growth of a “wet-SEI” is compared to that of the highly unstable carbonate DMC, which decomposes into complex radical oligomers that might contribute to further electrolyte decomposition. The impact of the electrolyte-to-anode ratio on LiFSI decomposition is highlighted. Finally, we suggest the existence of a critical LiFSI concentration and electrolyte-to-anode ratio that could potentially balance the rate of electrolyte depletion and lithium consumption.

25 ENERGY STORAGE↗

Probing the Impact of Vacancy Diffusion on Void Dynamics at the Lithium Metal–Solid Electrolyte Interface

Lithium (Li) metal-based solid-state batteries (SSBs) are considered promising candidates for next-generation energy storage due to their superior energy density and enhanced safety compared to conventional Li-ion systems. However, their practical application is limited by challenges such as void formation at the Li-solid electrolyte (SE) interface, which disrupts ion transport and accelerates interfacial degradation. This work investigates how the coupled effects of electro-dissolution kinetics and surface diffusion at the Li metal surface govern the evolution of interfacial morphology during stripping. This work examines the influence of three distinct surface diffusion modes, which are terrace diffusion, step diffusion, and interlayer diffusion, on maintaining interfacial stability. In addition, how the dominant surface diffusion mechanism can overcome the contact loss due to high reaction kinetics is explored. Furthermore, the roughness of the Li metal anode surface is quantified, and the influence of different diffusion mechanisms on the evolution of the dynamic solid–solid interface is examined. The critical role of temperature in enhancing Li surface diffusivity and expanding the regime of stable contact is highlighted. By identifying distinct regimes of interface stability, this study analyzes how non-uniform electrochemical dynamics dictate void morphology evolution and interfacial contact. These insights offer guiding principles for engineering robust Li–SE interfaces in SSBs.

lithium metal anode↗

Effects of dose rate on the microstructure and deuterium retention in γ-LiAlO 2 pellets

This report presents experimental findings obtained from November 2024 to September 2025. Defect accumulation and microstructural evolution during ion irradiation at elevated temperatures are governed by two competing processes: defect production, driven by dose rate, and defect recovery, controlled by defect diffusion, interaction, and annihilation. At a given dose, the resulting microstructural evolution depends on both the dose rate and irradiation temperature. As a continuation of our FY24 tritium science project, which investigated temperature effects at a fixed dose rate, this study focuses on dose-rate effects at a fixed temperature to provide deeper insights into the irradiated microstructure and compositional changes in γ-LiAlO 2 pellets. The study aims to elucidate the impact of dose rate on microstructure, precipitate morphology, deuterium retention, and lithium volatility in γ-LiAlO 2 pellets under sequential 120 keV He + and 80 keV D 2 + ion irradiation. Three dose rates of 7.3×10 4 , 2.9×10 4 and 6.8×10 5 dpa/s were applied to achieve the same total ion fluence of 2×10 17 (He + +D + )/cm 2 at 500 °C, corresponding to a maximum combined dose of 7.55 dpa at ~255 nm. The irradiated pellets were subsequently characterized using scanning transmission electron microscopy (STEM) and time-of-flight secondary ion mass spectrometry (ToF-SIMS). The microstructural response of γ-LiAlO 2 to ion irradiation was found to be strongly dose-rate dependent. At medium and high dose rates, irradiation produced a surface amorphized layer and an underlying crystalline layer containing LiAl 5 O 8 precipitates, with implanted gases accumulating and forming blisters at the crystalline-amorphous interface. It remains to be investigated whether the amorphized layer was produced by He + ion irradiation prior to D 2 + ion irradiation. In contrast, at low dose rates, the material remained crystalline, with cavities, likely gas-filled, distributed around precipitates, within the γ-LiAlO 2 matrix, and along grain boundaries. While precipitate morphology exhibited anisotropy, their size showed little sensitivity to dose rate in the applied range of this study. This result, however, does not rule out the possibility that further reductions in dose rate could influence precipitate size. High dose-rate irradiation enhanced protonium–deuterium isotopic exchange and lithium depletion in the amorphized region. Collectively, the results show that dose rate governs amorphization, gas redistribution, isotopic exchange, and lithium depletion, providing important insights into the mechanisms underlying structural evolution in γ-LiAlO 2 pellets under reactor-relevant irradiation conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE↗

Synergistic Co-Ir/Ru Composite Electrocatalysts Impart Efficient and Durable Oxygen Evolution Catalysis in Acid

Exploring highly active and robust catalysts, which have low precious metal content, to boost the kinetically sluggish oxygen evolution reaction (OER) is a key concern for hydrogen production via proton exchange membrane water electrolysis (PEMWE). Here, in this work, rational engineering of the morphology and the local geometric ligand environment of Ir and Ru catalysts are presented by using defect-rich, lanthanum- and lithium-doped Co 3 O 4 nanofiber (LLCF) as substrate that promotes the electrocatalytic OER. Two catalysts, IrCoOx@LLCF and RuCoOx@LLCF, achieve mass activities of 1013.5 A g Ir –1 and 1911.4 A g Ru –1 in 0.1 M HClO 4 at 300 mV overpotential, respectively, which are 26 and 50 times higher than that of commercial IrO 2 and RuO 2 . Operando X-ray absorption spectroscopy unveils the reversible structure of IrCoOx during the OER and the suppression of over-oxidation of Co and Ir, giving rise to high stability. Density functional theory calculations reveal that the local geometric ligand engineering optimizes the binding of oxygenated species to the active sites, resulting in strongly enhanced catalytic activity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Perspective—Lithium Metal Nucleation and Growth on Conductive Substrates: A Multi-Scale Understanding from Atomistic, Nano-, Meso-, to Micro-Scales

Reversible lithium (Li) deposition and stripping on conductive substrates like copper is vital for long-life high-energy rechargeable Li batteries. The reversibility is believed hindered by solid electrolyte interphase (SEI) formation and Li dendritic growth. Via in situ, operando cryo-microscopy and molecular dynamics simulation, we discovered amorphous Li before a disorder-order phase transition to bcc phase. The kinetics plays a significant role in Li nucleation and morphology evolution. This perspective on Li nucleation and growth from atomistic to nano- (<20 nm), meso- (20–100 nm), and micro-scales (>100 nm) provides a practical guidance on regulating dense Li deposits reversibly for long life performance.

25 ENERGY STORAGE↗

Cohesive phase-field chemo-mechanical simulations of inter- and trans- granular fractures in polycrystalline NMC cathodes via image-based 3D reconstruction

The optimal design and durable utilization of lithium-ion batteries necessitates an objective modeling approach to understand fracture and failure mechanisms. This paper presents a comprehensive chemo-mechanical modeling study focused on elucidating fracture-induced damage and degradation phenomena in the polycrystalline Li $\mathcal{x}$ Ni 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) cathode. An innovative approach that utilizes image-based reconstructed 3D geometry as finite element (FE) mesh input is employed to enhance the precision in capturing the convoluted architecture and morphological features. For accurately representing the intricate crack configurations within the polycrystalline system, we adopted the cohesive phase-field fracture (CPF) model. Through the integration of advanced image-based geometry reconstruction technique and the promising CPF modeling approach, lithium (de)intercalation induced crack evolution (e.g., nucleation, propagation, branching and diverse modes including inter-/trans-(intra-) granular patterns) and the resulting chemical degradation can be precisely captured, which is also compared and validated with numerical predictions using a continuum damage model. In particular, this model predicts fracture induced degradation under varying fracture properties of grain boundaries and charging rates; the conclusion that NMC particles comprised of larger grains are predicted to have less degradation than those with smaller grains can also be drawn. This comprehensive analysis provides valuable insights into the fracture and degradation within polycrystalline NMC cathodes.

25 ENERGY STORAGE↗

Physicochemical Heterogeneity in Silicon Anodes from Cycled Lithium-Ion Cells

The severe capacity fade of lithium-ion cells with silicon-dominant anodes has hindered their widescale commercialization. In this work, we link cell capacity fade to the heterogeneous physicochemical evolution of silicon anodes during battery cycling. Through a multi-length scale characterization approach, we demonstrate that silicon particles near the anode surface react differently than those near the copper current collector. In particular, near the anode surface we find an amorphized wispy silicon encased in a highly fluorinated matrix of electrolyte-reduction products. In contrast, closer to the current collector, the silicon retains more of its initial morphology and structure, suggesting the presence of isolated particles. Here, the results show that accessibility of active silicon to lithium-ions varies across the anode matrix. Material and cell designs, which minimize electrode expansion resulting from the in-filling of pores with the solid electrolyte interphase (SEI), are needed to enhance anode homogeneity during the electrochemical cycling.

25 ENERGY STORAGE↗

Defect Chemistry in High‐Voltage Cathode Materials for Lithium‐Ion Batteries

High-voltage cathodes (HVCs) have emerged as a paramount role for the next-generation high-energy-density lithium-ion batteries (LIBs). However, the pursuit of HVCs comes with inherent challenges related to defective structures, which significantly impact the electrochemical performance of LIBs. The current obstacle lies in the lack of a comprehensive understanding of defects and their precise effects. This perspective aims to provide insights into defect chemistry for governing HVCs. The classifications, formation mechanisms, and evolution of defects are outlined to explore the intricate relationship between defects and electrochemical behavior. The pressing need for cutting-edge characterization techniques that comprehensively investigate defects across various temporal and spatial scales is emphasized. Building on these fundamental understandings, engineering strategies such as composition tailoring, morphology design, interface modification, and structural control to mitigate or utilize defects are thoroughly discussed for enhanced HVCs performance. Furthermore, these insights are expected to provide vital guidelines for developing high-performance HVCs for next-generation high-energy lithium-ion batteries.

cross-scale characterization↗

Multidimensional visualization of the dynamic evolution of Li metal via in situ/operando methods

The growing demands for high-energy density electrical energy storage devices stimulate the coupling of conversion-type cathodes and lithium (Li) metal anodes. While promising, the use of these “Li-free” cathodes brings new challenges to the Li anode interface, as Li needs to be dissolved first during cell operation. In this study, we have achieved a direct visualization and comprehensive analysis of the dynamic evolution of the Li interface. The critical metrics of the interfacial resistance, Li growth, and solid electrolyte interface (SEI) distribution during the initial dissolution/deposition processes were systematically investigated by employing multidimensional analysis methods. They include three-electrode impedance tests, in situ atomic force microscopy, scanning electrochemical microscopy, and cryogenic scanning transmission electron microscopy. The high-resolution imaging and real-time observations show that a loose, diffuse, and unevenly distributed SEI is formed during the initial dissolution process. This leads to the dramatically fast growth of Li during the subsequent deposition, deviating from Fick’s law, which exacerbates the interfacial impedance. The compactness of the interfacial structure and enrichment of electrolyte species at the surface during the initial deposition play critical roles in the long-term stability of Li anodes, as revealed by operando confocal Raman spectroscopic mapping. In conclusion, our observations relate to ion transfer, morphological and structural evolution, and Li (de)solvation at Li interfaces, revealing the underlying pathways influenced by the initial dissolution process, which promotes a reconsideration of anode investigations and effective protection strategies.

25 ENERGY STORAGE↗