Search NASA⌕ Search

SEARCH · Search NASA

Results for “lithium pulverization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Quantitative insights for diagnosing performance bottlenecks in lithium–sulfur batteries

Lithium–sulfur (Li–S) batteries hold significant promise for electric vehicles and aviation due to their high energy density and cost-effectiveness. However, understanding the root causes of performance degradation remains a formidable challenge, as the interplay of multiple factors obscures key failure mechanisms. A major limitation has been the inability to quantify soluble sulfur species within practical detection limits accurately and to correlate electrochemical processes with associated physical inventory changes. Here, we introduce the high-performance liquid chromatography-ultraviolet spectroscopy and gas chromatography sequential characterization (HUGS) toolkit, capable of precisely quantifying seven distinct sulfur and polysulfide species at concentrations as low as 40 ppb. HUGS has been successfully applied to practical coin and pouch cells without requiring cell modification. Furthermore, our self-developed software, Dr HUGS, enhanced the data analysis speed by over 30 times, enabling multi-source data integration and delivering comprehensive analysis results within minutes. Using HUGS, we identify significant capacity losses from inactive lithium and sulfur during initial cycles and sulfide-rich solid–electrolyte interphase (SEI) formation on the anode during later cycles. Notably, our findings reveal that soluble polysulfides have minimal contributions to capacity loss, challenging long-standing assumptions. Moreover, HUGS demonstrates that constant-pressure setups in Li–S pouch cells improve compositional uniformity compared to constant-gap configurations. For sulfurized polyacrylonitrile (SPAN) cathodes, unique issues such as non-sulfide SEI formation and lithium pulverization are observed, which can be mitigated through localized high-concentration electrolytes to enhance lithium inventory retention. By enabling precise quantification of critical inventory components, HUGS provides transformative insights into failure mechanisms across various electrolytes and cathode chemistries, guiding rational design strategies for next-generation energy storage systems.

25 ENERGY STORAGE↗

Good Practice for Safe Handling of Lithium Metal Anode and High Energy Rechargeable Lithium Metal Batteries

High-energy rechargeable lithium metal batteries have been intensively revisited in recent years. Since more researchers started to use pouch cell as the platform to study the fundamentals at relevant scales, safe testing and handling of lithium metal and high-energy lithium metal batteries have become critical. Cautions and safety procedures are needed when handling cycled pouch cells with pulverized lithium particles inside. From cell design, electrode preparation, cell fabrication to testing procedure, this work aims to discuss all possible root causes that may initiate cell internal shorting and raise safety concerns. Safe transfer and disposal of cycled pouch cells are also discussed. The insights provided in this article are applicable for the research on high-energy lithium-ion batteries as well and may inspire more safety strategies to accelerate research innovation by using large-format batteries as the testing vehicle and conduct the research safely.

25 ENERGY STORAGE↗

Composite Lithium Metal Structure to Mitigate Pulverization and Enable Long‐Life Batteries

In lithium metal batteries, non‐uniform stripping of lithium results in pit formation, which promotes subsequent non‐uniform, dendritic deposition. This viscous cycle leads to pulverization of lithium which promotes cell shorting or capacity degradation, symptoms further exaggerated by high electrode areal loading and lean electrolytes. Here, to address this challenge, a composite lithium metal anode is engineered that contains uniformly distributed, nanometer‐sized carbon particles. This composite lithium is shown to strip more uniformly since the growth of non‐uniform pits is intercepted by the carbon particles. This mechanism is corroborated by a continuum electrochemical model. Subsequent lithium deposition on carbon particles is also found to be more uniform than on the surface with irregular pits. Notably, the pulverization rate of composite lithium is 26 times slower than that of commercial lithium. Moreover, in a Li‐S battery with sulfurized polyacrylonitrile cathode, the use of the composite anode extends the cycle life by three times when the areal capacity is 8 mAh cm −2 . The approach of using an engineered lithium composite structure to address challenges during both stripping and plating can inform future designs of lithium metal anodes for high areal capacity operations.

high areal capacity↗

Maximizing Calendering Effects Through the Mechanical Pulverization of Co-Free Nickel-Rich Cathodes in Lithium-Ion Cells

Calendering is a technique used to maximize the volumetric energy density of battery electrodes. However, higher amounts of calendering result in increased tortuosity and particle cracking. We propose a novel packing structure of electrode particles to maximize calendering benefits while minimizing particle fracture. Cobalt-free layered oxide cathode LiNi0.92Mn0.04Al0.04O2 (NMA) particles are pulverized through ball-milling and coated with lithium phosphate. Pulverized and pristine NMA are fabricated into “bimodal” electrodes, whereas “unimodal” electrodes consist of only pristine NMA. Each electrode type was made into 30% porosity, 40% porosity, and uncalendered coin cell samples. X-ray diffraction suggests that the unimodal samples suffer from more particle fracture than the bimodal samples when calendered to the same porosity of 30%. Electrochemical impedance spectroscopy suggests that the bimodal electrodes exhibit lower surface film resistance. This is supported by enhanced capacity retention for the bimodal samples after 100 cycles.

25 ENERGY STORAGE↗

Nucleation-promoting and growth-limiting synthesis of disordered rock-salt Li-ion cathode materials

Disordered rock-salt oxides and oxyfluorides are promising positive electrode materials for high-performance lithium-ion batteries free of nickel and cobalt. However, conventional synthesis methods rely on post-synthesis pulverization to achieve cycling-appropriate particle sizes, offering limited control over particle microstructure and crystallinity. This accelerates degradation and complicates secondary particle processing. Here we present a synthesis strategy that enhances nucleation while suppressing particle growth and agglomeration across various disordered rock-salt compositions, including lithium–manganese–titanium oxide, lithium–manganese–niobium oxide, and lithium–nickel–titanium oxide systems. Applied to Li 1.2 Mn 0.4 Ti 0.4 O 2 , this method yields highly crystalline, well-dispersed sub-200 nm particles that form homogeneous electrode films with stable cycling behavior. Tested in cells with lithium metal as the counter electrode, these electrodes deliver ~200 mAh/g with 85% capacity retention relative to the first cycle after 100 cycles (20 mA/g, 1.5–4.8 V), and an average discharge voltage loss of 4.8 mV per cycle, compared to 38.6% retention and 7.5 mV loss per cycle for electrodes derived from pulverized solid-state particles. This approach suggests a route to enhance the performance and durability of disordered rock-salt electrodes for sustainable lithium-ion batteries.

Batteries↗

Lithium-Ion Battery Life Model with Electrode Cracking and Early-Life Break-in Processes

This paper develops a physically justified reduced-order capacity fade model from accelerated calendar- and cycle-aging data for 32 lithium-ion (Li-ion) graphite/nickel-manganese-cobalt (NMC) cells. The large data set reveals temperature-, charge C-rate-, depth-of-discharge-, and state of charge (SOC)-dependent degradation patterns that would be unobserved in a smaller test matrix. Model structure is informed by incremental capacity analysis that shows loss of lithium inventory and cathode-material loss as the dominant capacity fade mechanisms. The model includes terms attributable to solid-electrolyte interface (SEI) growth, electrode cracking, cycling-driven acceleration of SEI growth, and "break-in" mechanisms that slightly decrease or increase available Li inventory early in life. The study explores what mathematical couplings of these mechanisms best describe calendar aging, cycle aging, and mixed calendar/cycle aging. Various approaches are discussed for extracting relevant stress factors from complex cycling profiles to predict lifetime during real-world battery loads using models trained on constant-current laboratory test results. The complexity of the present human-driven model identification process motivates future work in machine learning to more widely search and statistically discern the optimal model that correctly extrapolates capacity fade based on physical knowledge.

25 ENERGY STORAGE↗

Hierarchical porous silicon structures with extraordinary mechanical strength as high-performance lithium-ion battery anodes

Abstract Porous structured silicon has been regarded as a promising candidate to overcome pulverization of silicon-based anodes. However, poor mechanical strength of these porous particles has limited their volumetric energy density towards practical applications. Here we design and synthesize hierarchical carbon-nanotube@silicon@carbon microspheres with both high porosity and extraordinary mechanical strength (>200 MPa) and a low apparent particle expansion of ~40% upon full lithiation. The composite electrodes of carbon-nanotube@silicon@carbon-graphite with a practical loading (3 mAh cm −2 ) deliver ~750 mAh g −1 specific capacity, <20% initial swelling at 100% state-of-charge, and ~92% capacity retention over 500 cycles. Calendered electrodes achieve ~980 mAh cm −3 volumetric capacity density and <50% end-of-life swell after 120 cycles. Full cells with LiNi 1/3 Mn 1/3 Co 1/3 O 2 cathodes demonstrate >92% capacity retention over 500 cycles. This work is a leap in silicon anode development and provides insights into the design of electrode materials for other batteries.

25 ENERGY STORAGE↗

Diffusional lithium trapping as a failure mechanism of aluminum foil anodes in lithium-ion batteries

Aluminum foils are an appealing anode for lithium-ion batteries due to high capacity and low-cost, but their viability has been limited due to poor cyclability arising from pulverization and solid-electrolyte interphase growth. Here, we show that significant capacity degradation of aluminum foil anodes during electrochemical cycling also occurs due to diffusional lithium trapping. Scanning electron microscopy of cross-sectioned, cycled foils in the delithiated state reveals large regions of β-LiAl that are passivated by a surface layer of α-Al, which has poor Li + diffusivity. It is found that lithium diffusion occurs preferentially along the β-LiAl grain boundaries, so the grain structure after initial lithiation significantly affects the trapping behavior. Diffusional lithium trapping is exacerbated by both higher delithiation rates and higher areal capacity, presenting a challenge towards commercialization of aluminum foil anodes. We further demonstrate that diffusional trapping in aluminum foil anodes can be mitigated through alloy design, with the addition of 2–3 wt% Li yielding improved first cycle efficiency, and the addition of 1 wt% Si yielding improved cycle life. These results provide a mechanistic understanding of diffusional lithium trapping in aluminum foil anodes and highlight compositional design of alloys as a promising strategy to overcome it.

25 ENERGY STORAGE↗

Influence of Calendering on the Electrochemical Performance of LiNi 0.9 Mn 0.05 Al 0.05 O 2 Cathodes in Lithium-Ion Cells

Electrode calendering is a necessary process used in industry to improve the volumetric capacity of lithium-ion batteries. However, calendering high-nickel cathodes leads to electrode particle pulverization, raising concerns of a reduced cycle life due to parasitic side reactions. We present here an investigation of the impact of calendering on the morphology and electrochemical performance of the cobalt-free layered oxide cathode LiNi 0.9 Mn 0.05 Al 0.05 O 2 (NMA-90). We find that secondary particle pulverization and fusion simultaneously occur at sufficiently high pressures. The initial surface area of the cathode is shown to increase with the degree of calendering, despite the higher likelihood of secondary particle fusion. Long-term cycling of full coin cells assembled with the NMA-90 cathode and the graphite anode indicates that cells with higher degrees of cathode calendering exhibit lower capacity fade compared to uncalendered cathodes. Hybrid pulse-power tests demonstrate that the usable capacity range of cells with calendered cathodes far exceeds those with uncalendered cells after long-term cycling. The improved capacity retention and pulse-power performance are attributed to the enhanced mechanical properties of the electrode after calendering that prevents loss of the primary particle contact during long-term cycling. As a result, we find that calendering high-nickel NMA-90 to industrially relevant densities does not have a detrimental effect on capacity fade, marking an important step toward commercial adoption.

25 ENERGY STORAGE↗

Size effect on the growth and pulverization behavior of Si nanodomains in SiO anode

Silicon monoxide (SiO) as a promising silicon-based anode electrode of lithium-ion batteries (LIBs) has been the subject of many recent investigations. However, the complex microstructural features of SiO hinder attempts to link the microstructure changes in SiO with its electrochemical performances upon electrochemical cycling. This study employs X-ray pair distribution function (PDF), with a high-resolution transmission electron microscope (HRTEM), to investigate the microstructure of Si nanodomains in SiO and its structural evolution over the electrochemical cycling process. The experiment results reveal the size evolution of Si nanodomains in SiO during the electrochemical cycling and find it highly dependent on the initial Si domain size in SiO. If the initial Si domain size is too large, the average size of Si nanodomains would increase at first and then decrease after a certain number of cycles, which indicates the pulverization of Si domains after the electrochemical-driven growth of Si nanodomains reaches a critical point. Furthermore, these results suggest that an optimal initial Si nanodomain size of 4-6 nm for SiO anode materials is essential to retard the growth and subsequent pulverization process of Si nanodomains and thus to improve the cyclability of SiO during long-term cycling.

25 ENERGY STORAGE↗

Large Scale Synthesis of Manganese Oxide/Reduced Graphene Oxide Composites as Anode Materials for Long Cycle Lithium Ion Batteries

Manganese oxides have been frequently used as cathodes in primary batteries. Applications of manganese oxides in secondary batteries are limited by low electrical conductivity and rapid capacity fading because of electrode pulverization and aggregation. In this study, a solid-state synthetic strategy is presented that successfully combines nanosize (~ 50 nm) nickel doped α-MnO 2 with reduced graphene oxides as highly stable composite anodes in lithium ion batteries. The synthesis approach is easy to scale up and suitable for industrial applications. Here, the rationally designed Ni-α-MnO 2 /RGO was tested in galvanostatic half coin cells for Li + charge-discharge studies. The results show that this composite maintains a high capacity of 615 mAh g -1 even after 200 cycles at a high current rate of 1 C (830 mA g -1 ), and with a high Coulombic efficiency near 99%. The anodes exhibit excellent rate capability in a wide range of rate testing from 0.2 to 10 C, without showing capacity decay. This superior anode performance is ascribed to the reduced size of α-MnO 2 domains that are well dispersed in an RGO matrix, which affords good ionic/elec. cond., low charge transfer resistance and mitigates issues of vol. expansion of the anodic active materials. This study opens up an avenue for developing the manufacturing of high-performance electrodes for real applications, such as batteries in electrical vehicles.

25 ENERGY STORAGE↗

Unravelling fast-charging degradation in NMC/Gr pouch cells: Lithium plating and SEI properties

As fast-charging technology expands across the electric vehicle and emerging energy-storage applications, understanding its impact on battery performance and longevity is critical. In this study, 1.8 Ah LiNi 0.6 Mn 0.2 Co 0.2 O 2 /graphite pouch cells were charged at various charging rates (0.5C, 2C, 4C, and 6C) to investigate the degradation mechanisms. Our results showed that well-designed NMC/Gr pouch cells could reach over 1000 cycles with a 2C charging rate, while only reaching around 500 cycles with 4C and 6C charging rates. Fast-charging effects on NMC and graphite electrodes were obtained through a series of post-mortem characterizations, including electrochemical impedance spectroscopy (EIS), Raman spectroscopy, X-ray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS). Although higher charging rates cause pulverization of NMC secondary particles, the dominant degradation mechanism driving the fading of fast-charging-related performance lies in the graphite anode, where lithium plating and LiF-rich solid electrolyte interphase (SEI) formation result in Li inventory loss and impedance growth. The postmortem results suggest that the formation of a LiF-rich SEI, which exacerbates anode impedance and some irreversible Li + ion loss, is likely driven by the substantial decomposition of PF 6 − during fast charging, an effect often overlooked in smaller laboratory-scale studies.

Luo, Mei [Argonne National Laboratory (ANL), Argon↗

Re-Engineering Poly(Acrylic Acid) Binder toward Optimized Electrochemical Performance for Silicon Lithium-Ion Batteries: Branching Architecture Leads to Balanced Properties of Polymeric Binders

Silicon is a promising anode material for lithium-ion batteries with its superior capacity. However, the drastic volume changes during lithiation/delithiation cycles hinder the cycling performance, resulting in particle pulverization, conductivity loss, and an unstable electrode-electrolyte interface. In this work, a series of synthetic polymeric binders, poly(acrylic acid-co-tetra(ethylene glycol) diacrylate)-featuring a poly(acrylic acid) (PAA) backbone branched via tetra(ethylene glycol) diacrylate (TEGDA)-are developed that edge toward evidencing well-balanced properties to confront capacity fading in Si-based electrodes. The incorporation of ether chain not only leads to the branching architecture of the PAA backbone, thus affecting its mechanical properties, but also promotes the conductivity of Li ions. As a result, a synergistic performance improvement is observed in both half and full cells. The best-performing cell using a branched PAA binder (bPAA) with a feeding molar ratio ([TEGDA]:[acrylic acid(AA)]) of 0.2 results in a 10% increase in initial capacity and a 31% increase in capacity retention over 100 cycles compared to the linear PAA cell. The cross-sectional microscopic images of the cycled electrodes reveal that bPAA binders can drastically reduce the electrode expansion. This improvement results from the well-balanced properties of the polymer design, which could guide further development for more advanced binder materials.

25 ENERGY STORAGE↗

1000 Wh L−1 lithium-ion batteries enabled by crosslink-shrunk tough carbon encapsulated silicon microparticle anodes

Abstract Microparticulate silicon (Si), normally shelled with carbons, features higher tap density and less interfacial side reactions compared to its nanosized counterpart, showing great potential to be applied as high-energy lithium-ion battery anodes. However, localized high stress generated during fabrication and particularly, under operating, could induce cracking of carbon shells and release pulverized nanoparticles, significantly deteriorating its electrochemical performance. Here we design a strong yet ductile carbon cage from an easily processing capillary shrinkage of graphene hydrogel followed by precise tailoring of inner voids. Such a structure, analog to the stable structure of plant cells, presents ‘imperfection-tolerance’ to volume variation of irregular Si microparticles, maintaining the electrode integrity over 1000 cycles with Coulombic efficiency over 99.5%. This design enables the use of a dense and thick (3 mAh cm–2) microparticulate Si anode with an ultra-high volumetric energy density of 1048 Wh L–1 achieved at pouch full-cell level coupled with a LiNi0.8Co0.1Mn0.1O2 cathode.

25 ENERGY STORAGE↗

Interface-engineered (CrMnTiZnCo) 3 O 4 @polypyrrole nano-hybrids for superior lithium storage

High-entropy oxides (HEO) have emerged as promising anode materials for lithium-ion batteries (LIBs) due to their high theoretical specific capacity. However, their practical application is hindered by several challenges, including significant volume expansion, electrode pulverization, and substantial irreversible capacity loss during initial cycles. To address these limitations, this study designed a novel core-shell composite material, denoted as HEO@PPy, which consists of a (CrMnTiZnCo) 3 O 4 -based HEO core and a polypyrrole (PPy) shell. This composite demonstrates remarkable electrochemical performance: it maintains a specific capacity of 1090.1 mAh/g after 100 cycles at 100 mA/g and retains 521.8 mAh/g after 1000 cycles at 1 A/g, highlighting its superior cycling stability. Furthermore, it exhibits excellent rate capability, delivering a capacity of 372.1 mAh/g even at a high current density of 5 A/g. These findings confirm that the strategic compositional and structural design of HEOs, combined with hybridization with conductive polymers like PPy, provides a viable pathway for developing advanced anode materials for next-generation, high-performance lithium-ion batteries.

25 ENERGY STORAGE↗

Novel One-Step Production of Carbon-Coated Sn Nanoparticles for High-Capacity Anodes in Lithium-Ion Batteries

Lithium-ion batteries offer the highest energy density of any currently available portable energy storage technology. By using different anode materials, these batteries could have an even greater energy density. One material, tin, has a theoretical lithium capacity (994 mAh/g) over three-times higher than commercial carbon anode materials. Unfortunately, to achieve this high capacity, bulk tin undergoes a large volume expansion, and the material pulverizes during cycling, giving a rapid capacity fade. To mitigate this issue, tin must be scaled down to the nano-level to take advantage of unique micromechanics at the nanoscale. Synthesis techniques for Sn nanoparticle anodes are costly and overly complicated for commercial production. A novel one-step process for producing carbon-coated Sn nanoparticles via spark plasma erosion (SPE) shows great promise as a simple, inexpensive production method. The SPE method, characterization of the resulting particles, and their high-capacity reversible electrochemical performance as anodes are described. With only a 10% addition of these novel SPE carbon-coated Sn particles, one anode composition demonstrated a reversible capacity of ~460 mAh/g, achieving the theoretical capacity of that particular electrode formulation. These SPE carbon-coated Sn nanoparticles are drop-in ready for present commercial lithium-ion anode processing and would provide a ~10% increase in the total capacity of current commercial lithium-ion cells.

25 ENERGY STORAGE↗

Facile Synthesis of Micrometer-sized Hierarchical Porous Si@C Anodes for High-Performance Lithium-Ion Batteries

Extensive studies have been conducted to determine if replacing graphite anodes with silicon is feasible since silicon possesses a high capacity and is an abundant resource; however, Si anodes suffer significant volume changes during cycling, which pulverizes its structure and subsequently causes rapid capacity fading. We used SiO2 nanoparticles (nSiO2) and low-cost coal-derived humic acid as a feedstock to synthesize high performance Si-C anodes for Li-ion Batteries through spray drying, calcination, and magnesiothermic reductions. Our Si-C anodes features micrometer-sized porous Si coated with a graphitized carbon shell (mpSi@C). The hierarchical graphitized carbon shell and porous silicon structure relieve the mechanical stress of the Si phase upon cycling, which stabilizes the structure. This mpSi@C composite design allows for a high initial discharge capacity of 2199.9 mAh g-1 at 0.1 A g-1 and a cycling performance of 68% capacity retention after 100 cycles at 1.0 A g-1. The multipoint contact between the Si anode and C structure allows for a remarkable performance rate of 566.3 mAh g-1 at 5.0 A g-1.

01 COAL, LIGNITE, AND PEAT↗