Maximum energy product at elevated temperatures for hexagonal strontium ferrite (SrFe12O19) magnet

The electronic structure of hexagonal strontium ferrite (SrFe12O19) was calculated based on the density functional theory (DFT) and generalized gradient approximation (GGA). The GGA+U method was used to improve the description of localized Fe 3d electrons. Three different effective U (U-eff) values of 3.7, 7.0, and 10.3 eV were used to calculate three sets of exchange integrals for 21 excited states. We then calculated the temperature dependence of magnetic moments m(T) for the five sublattices (2a, 2b, 12k, 4f(1), and 4f(2)) using the exchange integrals. The m(T) of the five sublattices are inter related to the nearest neighbors, where the spins are mostly anti-ferromagnetically coupled. The five sublattice m(T) were used to ()brain the saturation magnetization M-s(T) of SrFe12O19, which is in good agreement with the experimental values. The temperature dependence of maximum energy product. ((BII)(max)(T)) was calculated using the calculated M-s(T). (C) 2013 Elsevier B.V. All rights reserved.

Park, J↗

Nano-Magnets and Additive Manufacturing for Electric Motors

High power density is required for application of electric motors in hybrid electric propulsion. Potential path to achieve high power density in electric motors include advanced materials, lightweight thermal management, lightweight structural concepts, high power density power electronics, and advanced manufacturing. This presentation will focus on two key technologies for achieving high power density, advanced magnets and additive manufacturing. The maximum energy product in current magnets is reaching their theoretical limits as a result of material and process improvements. Future improvements in the maximum energy product for magnets can be achieved through development of nanocomposite magnets combining the hard magnetic phase and soft magnetic phase at the nanoscale level. The presentation will provide an overview of the current state of development for nanocomposite magnets and the future path for doubling the maximum energy product. The other part of the presentation will focus on the role of additive manufacturing in fabrication of high power density electric motors. The presentation will highlight the potential opportunities for applying additive manufacturing to fabricate electric motors.

materials↗

Hard Magnetic, Low Neodymium Nd-Fe-B Melt-Spun Alloys Containing Refractory Metals

The effect of selected refractory metals addition on the structure and magnetic properties was studied for the nanocomposite Nd{sub 9}Fe{sub 77-x}B{sub 14}M{sub x}(M = Ti, Mo, Nb, Mn), Nd{sub 8}Fe{sub 78-x}B{sub 14}M{sub x}(M = Ti, Mo, Nb, Mn) and Nd{sub 7}Fe{sub 79-x}B{sub 14}Ti{sub x} systems. It was found that the addition of 2 and 4 at % of refractory metals leads to a substantial increase of the coercivity and maximum energy product for each of the nanocomposite systems while maintaining the remanence unchanged. The highest properties were obtained for the alloys containing 4-5 at% of the refractory metals. The maximum energy product of 143 kJ/m{sup 3} was achieved for the Nd{sub 8}Fe{sub 74}B{sub 14}Ti{sub 4} alloy.

36 MATERIALS SCIENCE↗

New anisotropic MnBi permanent magnets by field-annealing of compacted melt-spun alloys modified with Mg and Sb

A technique has been designed for manufacturing rare-earth-free MnBi-based magnets capable of filling the existing "gap" between the ferrite and rare-earth permanent magnets. Whereas the earlier approaches relied on sintering of fine and easily degrading single-crystal MnBi particles, the new method achieves refinement of the key α-MnBi phase through melt-spinning combined with appropriate alloying. Modification of the MnBi alloys with Mg and Sb generates a high-coercivity nanostructure of the metastable β' phase. A subsequent compaction at 150 °C produces fully dense materials while converting the β' phase into the stable α phase. Lastly, a short annealing at 265–300 °C in a magnetic field of 3 T increases the fraction of the α phase to 97–98% and aligns the c axes of the α crystallites. A maximum energy product (BH) max of 11.5 MGOe and an intrinsic coercivity Hc of 5.6 kOe have been obtained in a magnet with the nominal composition Mn 50 Bi 46.5 Mg 3 Sb 0.5 . Because the coercivity increases with temperature, the maximum energy product of this magnet is still as high as 8.9 MGOe at 175 °C. Increasing the Sb content to 1.5 at.% increases the H c to 9.3 kOe, but at the same time inhibits the development of the texture thus decreasing the (BH) max . The addition of Mg was found to increase the c lattice parameter of the α phase resulting in an unusually large ratio c/a ≈1.432.

36 MATERIALS SCIENCE↗

Microstructure and Hard Magnetic Properties of Sm 1-x Zr x (Fe,Co) 11.3-y Ti 0.7 By Ingots and Thick Melt-Spun Ribbons

Permanent magnets made from Sm(Fe,Co) 12 -based compounds are being actively pursued through nanostructuring and powder metallurgy. This study was aimed at the development of hard magnetic properties in bulk as-cast alloys and in melt-spun alloys for very low wheel speeds. Slower solidification rates and alloying with Zr promote the tetragonal ThMn 12 -type crystal structure, whereas higher solidification rates and alloying with B replace the ThMn 12 structure type with the TbCu 7 structure type. When introduced simultaneously, Zr and B dramatically reduce the alloy solidification rates required for both the refinement of the 1:12 crystallites and their replacement with the 1:7 phase. In bulk arc-melted alloys, this allowed for a microstructure of separated 1:12 crystallites 1–3 μm in size, although, because of the ferromagnetic nature of a minority phase, the coercivity of these fine-grained alloys reached only 0.73 kOe. A moderately accelerated solidification further refined the 1:12 crystallites and increased the coercivity; a Sm 0.7 Zr 0.4 (Fe,Co) 10.8 Ti 0.7 B 0.5 alloy exhibited a coercivity of 1.5 kOe and a maximum energy product of 3.4 MGOe when it was melt-spun into a 0.26-mm-thick ribbon. A more rapid solidification suppressed the 1:12 phase and after annealing at 800–850 °C, the alloys modified with Zr and B developed reasonably high coercivity and maximum energy product even when melt-spun at a wheel speed of 6 m/s. For the above-mentioned alloy, these values were 4.1 kOe and 7.8 MGOe, respectively. Further, a similarly processed very-Sm-lean Sm 0.5 Zr 0.6 (Fe,Co) 10.6 Ti 0.7 B 0.7 alloy exhibited a remanence of 8.8 kG and an energy product of 7.4 MGOe.

36 MATERIALS SCIENCE↗

Microstructure refinement of hot deformed Dy-free NdFeB magnets through a novel cold sintering approach by pressure-assisted spark plasma sintering

Anisotropic fine-grained Dy-free NdFeB high-performance magnets were produced using a novel cold sintering approach by pressure-assisted spark plasma sintering (SPS). The NdFeB nanocrystalline ribbon powders were subjected to cold sintering below 450 °C using pressure-assisted SPS, followed by hot deformation at 710 °C and 810 °C via SPS. Results indicate that cold sintering below 450 °C effectively restricts grain growth in the NdFeB magnets, yielding sub-100 nm scale grains across both fine-grained regions and most coarse-grained regions. The refined grain structure achieved through cold sintering allows for a lower hot deformation temperature as compared with the magnet by conventional sintering, as finer grains allow easier deformation and grain sliding/rotation. This process produces a highly fine-grained and anisotropic microstructure to achieve high magnetic performance (i.e., high intrinsic coercivity, remanence, and maximum energy product) in the magnets. The cold sintering (at 350 °C) and lower hot deformation temperatures required (e.g., 710 °C) help control grain coarsening and limit grain size that is commensurate with the size of a single magnetic domain of the Nd 2 Fe 14 B magnetic matrix phase, resulting in high intrinsic coercivity (H ci =11.4 kOe). Furthermore, the reduced hot deformation temperature mitigates the formation of coarse grain bands, leading to improved magnetic properties, specifically an increased remanence (B r = 14.3 kGs) and a high maximum energy product ((BH) max = 48 MGOe). In conclusion, cold sintered hot deformed NdFeB magnet also shows good thermal stability with reversible temperature coefficient α(B r )= -0.097 %/K and α(H ci )= -0.616 %/K at elevated temperatures up to 400 K.

Cold Sintering↗

Evolution of structural and magnetic properties due to nanocrystallization of mechanically milled amorphous Pr-Co-B powders

Pr{sub 2}Co{sub 14}B permanent magnet powders were prepared by mechanical milling of an arc-melted ingot. X-ray diffraction analysis revealed the presence of the 2:14:1 phase after 1 h of milling which transformed into an amorphous phase with additional milling time. Increasing the milling time also lowered the intrinsic coercivity while the saturation magnetization increased up to 105 emu/g. Differential scanning calorimetry measurements revealed a crystallization temperature of around 560 °C. Upon annealing 30 h of as-milled amorphous powders between 500 and 900 °C, we observed the precipitation of the 2:14:1 phase. The optimum post-milling annealing temperature was 600 °C with an intrinsic coercivity of 7 kOe and maximum energy product of 6 MGOe.

36 MATERIALS SCIENCE↗

High performance Nd-Fe-B permanent magnets without critical elements

Scanning electron microscopy, and magnetization measurements reveal that as cast (Nd 1–x Ce x ) 2 Fe 14 B alloys contain significant amounts of α-Fe that can be dramatically reduced by annealing the alloys at 1000 °C for 3 days. The room temperature intrinsic coercivity, Hci, of (Nd 0.8 Ce 0.2 ) 2.2 Fe 14 B melt spun ribbons was found to be 11 kOe, which is ~32 to ~10% higher in comparison to that of Nd 2 Fe 14 B (Hci = 8.3 kOe), and (Nd 0.8 Ce 0.2 ) 2.0 Fe 14 B (Hci = 10 kOe), respectively. The substitution of Co for Fe in (Nd 0.8 Ce 0.2 ) 2 Fe 14–z Co z B significantly increases both TC and the maximum energy product, (BH)max. Our study shows that both Co-containing and Co-free Ce-substituted Nd 2 Fe 14 B alloys have excellent magnetic properties at room temperature and above. As a result, the experimental results also demonstrate the potential of Nd-Ce-Fe-TM-B based alloys as alternative to expensive Dy-containing high performance rare earth magnets.

36 MATERIALS SCIENCE↗

Extracting the mass dependence and quantum numbers of short-range correlated pairs from A ( e , e ' p ) and A ( e , e ' p p ) scattering

The addition of Molybdenum was used to modify the nanostructure and enhance coercivity of rare-earth-free Zr 2 Co 11 -based nanocrystalline permanent magnets. The effect of Mo addition on magnetic domain structures of melt spun nanocrystalline Zr 16 Co 84- x Mo x ( x = 0 , 0.5, 1, 1.5, and 2.0) ribbons has been investigated. It was found that magnetic properties and local domain structures are strongly influenced by Mo doping. The coercivity of the samples increases with the increase in Mo content ( x ≤ 1.5 ). The maximum energy product ( B H ) max increases with increasing x from 0.5 MGOe for x = 0 to a maximum value of 4.2 MGOe for x = 1.5 . The smallest domain size with a relatively short magnetic correlation length of 128 nm and largest root-mean-square phase shift Φ rms value of 0.66° are observed for the x = 1.5 . The optimal Mo addition promotes magnetic domain structure refinement and thus leads to a significant increase in coercivity and energy product in this sample. MDH is primarily a dimer in solution, although an oligomeric species with a molecular mass of ~450–560 kDa forms at higher protein concentrations. A new measurement of the rare, doubly radiative decay eta->pi 0 γγ was conducted with the Crystal Ball and TAPS multiphoton spectrometers together with the photon tagging facility at the Mainz Microtron MAMI.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Magnetic Force Microscopy Study of Zr 2 Co 11 -Based Nanocrystalline Materials: Effect of Mo Addition

The addition of Molybdenum was used to modify the nanostructure and enhance coercivity of rare-earth-free Zr 2 Co 11 -based nanocrystalline permanent magnets. The effect of Mo addition on magnetic domain structures of melt spun nanocrystalline Zr 16 Co 84- x Mo x ( x = 0 , 0.5, 1, 1.5, and 2.0) ribbons has been investigated. It was found that magnetic properties and local domain structures are strongly influenced by Mo doping. The coercivity of the samples increases with the increase in Mo content ( x ≤ 1.5 ). The maximum energy product ( B H ) max increases with increasing x from 0.5 MGOe for x = 0 to a maximum value of 4.2 MGOe for x = 1.5 . The smallest domain size with a relatively short magnetic correlation length of 128 nm and largest root-mean-square phase shift Φ rms value of 0.66° are observed for the x = 1.5 . The optimal Mo addition promotes magnetic domain structure refinement and thus leads to a significant increase in coercivity and energy product in this sample.

Yue, Lanping (ORCID:0000000304060206)↗

Exchange-spring mechanism of soft and hard ferrite nanocomposites

Graphical abstract: - Highlights: • Exchange-spring behaviour of soft and hard ferrites was studied. • XRD patterns indicated soft and hard ferrites as fcc and hcp structure. • Hysteresis loops indicate wide difference in coercivity of soft and hard phases. • Nanocomposites produced convex hysteresis loop characteristic of single-phase. - Abstract: The paper reports exchange-spring soft and hard ferrite nanocomposites synthesized by chemical co-precipitation with or without the application of ultrasonic vibration. The composites contained BaFe{sub 12}O{sub 19} as the hard phase and CoFe{sub 2}O{sub 4}/MgFe{sub 2}O{sub 4} as the soft phase. X-ray diffraction patterns of the samples in the optimum calcined condition indicated the presence of soft ferrites as face-centred cubic (fcc) and hard ferrites as hexagonal close packed (hcp) structure respectively. Temperature dependence of magnetization in the range of 20–700 °C demonstrated distinct presence of soft and hard ferrites as magnetic phases which are characterized by wide difference in magnetic anisotropy and coercivity. Exchange-spring mechanism led these nanocomposite systems to exchange-coupled, which ultimately produced convex hysteresis loops characteristic of a single-phase permanent magnet. Fairly high value of coercivity and maximum energy product were observed for the samples in the optimum calcined conditions with a maximum applied field of 1600 kA/m (2 T)

36 MATERIALS SCIENCE↗

Enhancement of hard magnetism and chemical order of synthetic L 1 0 -FeNi

An ordered tetragonal L 1 0 -FeNi, also known as meteoritic mineral tetrataenite – a promising rare-earth-free hard-magnetic compound – has been synthesized starting from a mechanochemically-activated disordered cubic A1-FeNi via formation of a chemically-ordered FeNiN intermediate and its subsequent denitrogenation and further purification of the product. The nature of a process control agent employed during the mechanochemical activation of A1-FeNi and ammonia flow velocity during the synthesis of the intermediate are two of the main factors controlling the nitrogenation. Denitrogenation with hydrogen at elevated pressures and at temperatures substantially below the order-disorder L 1 0 -FeNi → A1-FeNi transition preserves the chemical order established in the intermediate nitride. Further, post-synthesis refinement of the L 1 0 -FeNi product includes the removal of residual nitrides with a dilute acid to further improve hard-magnetic properties of the material. The L 1 0 -FeNi powders synthesized using this method exhibit a coercivity as high as 2.3 kOe and a maximum energy product reaching 6 MGOe – the highest values ever reported for a synthetic tetrataenite.

36 MATERIALS SCIENCE↗

Chloride Molten Salt Electrolysis Enables Integrated and Energy-Efficient Process for NdFeB Magnet Fabrication

Rare-earth elements (REEs) have been identified by NATO, the USDOE, and USGS as critical materials, i.e., materials which have significant demand yet pose supply-chain risks. Many of the existing processes for separations, metallization, and final parts production used across the REE supply chain involve energy intensive steps. For example, neodymium (Nd or NdPr) is produced using oxyfluoride electrolysis of Nd 2 O 3 , which requires hydrofluoric acid to produce a key electrolyte component (NdF 3 ) and generates undesired perfluorocarbon (PFC) gases. Such challenges make securing a resilient supply chain for NdFeB permanent magnets in countries like the United States prohibitively difficult. Here, we propose a chloride-based MSE process that circumvents these challenges, delivering high-purity NdPr from a (NdPr)Cl 3 feed from upstream REE separations. This eliminates environmentally-damaging steps of oxalate or carbonate precipitation and calcination, and enables superior production rates due to greater solubility of (NdPr)Cl 3 in chloride melts compared to Nd 2 O 3 . We show that CMSE generates high-purity NdPr (99.4 wt.%) while being energy-efficient (~ 6 kWh/kg-Nd). NdPr from CMSE was used to fabricate a NdFeB magnet with an excellent maximum energy product (> 40 MGOe), comparable to commercially available NdFeB magnets. This establishes CMSE as a leading approach for integrated, energy-efficient NdFeB magnet production.

Materials science↗

Minimizing particle aggregation in Sm 2 Fe 17 N 3 powders: A CaO-assisted reduction-diffusion approach

We report a novel synthesis of Sm 2 Fe 17 N 3 powders using a CaO-assisted reduction-diffusion (RD) approach. CaO plays a crucial role during mechanochemical processing – acting both as a dispersant and a surface coating agent, which helps to prevent agglomeration due to sintering of Sm 2 Fe 17 particles during the RD step. Together with the added dispersant, the CaO by-product formed during RD can be easily removed in the washing step resulting in fewer aggregated Sm 2 Fe 17 N 3 particles and lower oxygen contamination in the final product. The impact of varying CaO amounts was examined, and synthesis conditions were optimized to achieve phase-pure Sm 2 Fe 17 N 3 powders with less aggregation of magnetic particles. The powders synthesized with addition of 1 wt% CaO as dispersant exhibited the highest hard-magnetic properties: a coercivity (H c ) of 10.7 kOe and a maximum energy product ((BH) max ) of 17.3 MGOe. By densifying the Sm 2 Fe 17 N 3 powders using high-pressure spark plasma sintering, a bulk magnet with a (BH) max of 21.1 MGOe with 88 % of theoretical density was produced. In conclusion, reducing aggregation of the Sm 2 Fe 17 N 3 increases coercivity and remanence of these magnets.

36 MATERIALS SCIENCE↗

Development of rare-earth-free bulk magnets with energy product up to 12 MGOe in field annealed Mn–Bi–Mg–In–Sb alloys

A treatment consisting of annealing in a moderately strong, ≤30 kOe, magnetic field was applied to arc-melted ingots and compacted melt-spun alloys with composition Mn 50 Bi 50-x-y-z Mg x In y Sb z . The high degree of texture of the magnetic α phase induced with annealing of the ingot samples (except the Mn–Bi–Sb one) allowed for accurate determination of the phase anisotropy field. Alloying was found to increase the anisotropy field from 45 kOe in the Mn 50 Bi 50 alloy to 65 kOe in the Mn 50 Bi 45 Mg 3 In 0.5 Sb 1.5 alloy. In the compacted melt-spun alloys subjected to field annealing, a higher degree of texture could be achieved after compaction which had involved less heating, when a smaller fraction of the metastable β' phase had been converted into the α phase; compaction at room temperature allowed for the highest degree of texture in the Mn 50 Bi 45 Mg 3 In 0.5 Sb 1.5 magnet. The addition of indium was found to decrease the solidus temperatures of the alloys, facilitating the development of the α phase during the field annealing and modifying the properties of the resulting magnets. Introduction of indium resulted in a higher coercivity H c of the Mn–Bi–Mg–In magnets and in a better texture of the Mn–Bi–Mg–Sn–In magnets. The former effect allowed, in particular, for a viable maximum energy product ( BH ) max of 10 MGOe to be developed in the Mn 50 Bi 46.5 Mg 3 In 0.5 magnet through annealing in a relatively low field of 15 kOe, whereas the latter effect allowed for an excellent combination of ( BH ) max = 11.6 MGOe and H c = 8.5 kOe in the Mn 50 Bi 45 Mg 3 In 0.5 Sb 1.5 magnet. The highest ( BH ) max of 12 MGOe was realized in the Mn 50 Bi 46 Mg 3 In 0.5 Sb 0.5 magnet.

36 MATERIALS SCIENCE↗

Permanent Electride Magnets Induced by Quasi‐Atomic Non‐Nucleus‐Bound Electrons

Abstract Interstitial quasi‐atomic electrons (IQEs) in the quantized energy levels of positively charged cavities possess a substantial own magnetic moment and control the magnetism of crystalline electrides depending on the interaction with surrounding cations. However, weak spin‐orbit coupling and gentle exchange interaction restricted by the IQEs preclude a large magnetic anisotropic, remaining a challenge for a hard magnetism. It is reported that 2D [ Re 2 C] 2+ ·2e − electrides (Re = Er, Ho, Dy, and Tb) show the permanent magnetism in a ferrimagnetic ground state, mimicking the ferrites composed of magnetic sublattices with different spin polarizations. Magnetic interaction between Re‐spin lattice and IQE‐spin lattice in the [ Re 2 C] 2+ ·2e − electrides results in a large magnetocrystalline anisotropy and high coercivity, giving a maximum energy product of 15 MGOe. It is demonstrated that the spontaneous breaking of magnetic IQE‐sublattice through substitution with paramagnetic elements produces a crossover into an antiferromagnetic spin ordering of Re‐sublattice, implying that the magnetic sublattice of IQEs drives the permanent magnetism.

Hwang, Jeong Yun [Department of Materials Science ↗

3D printing of anisotropic Sm–Fe–N nylon bonded permanent magnets

Abstract Fabricating a bonded magnet with a near‐net shape in suitable thermoplastic polymer binders is of paramount importance in the development of cost‐effective energy technologies. In this work, anisotropic Sm 2 Fe 17 N 3 (Sm–Fe–N) bonded magnets are additively printed using SmFeN anisotropic magnetic particles in a polymeric binder polyamide‐12 (PA12). The anisotropic SmFeN bonded magnets are fabricated by Big Area Additive Manufacturing followed by post‐printing alignment in a magnetic field. Optimal post‐alignment results in an enhanced remanence of ∼0.68 T in PA12 reflected in a parallel‐oriented (aligned) measured direction. The maximum energy product achieved for the additively printed anisotropic bonded magnet of Sm–Fe–N in PA12 polymer is 78.8 KJ m −3 . Our results show advanced processing flexibility with 3D printing of the development of SmFeN nylon bonded magnets designed for applications with no critical rare earth magnets.

42 ENGINEERING↗

Low-Temperature Short-Time SPS Processes to Produce Fine-Grained High-Coercivity Barium Hexaferrite Ceramics from Polyol Nanoparticles

Barium hexaferrite (BaFe{sub 12}O{sub 19}) ceramics were obtained by combination of polyol-synthesized precursors subsequently consolidated by spark plasma sintering (SPS) at a low temperature (800 {sup ∘}C). X-ray powder diffraction studies showed the influence of the experimental parameters to produce a virtually single- or multiphase material. The room temperature magnetic properties exhibited interesting variety of properties, including exchange coupling (spring magnet) between hexaferrite and other magnetic phases. The saturation magnetization and coercive field, at room temperature, are in the 34–70 emu/g and 4.1–5.0 kOe ranges, respectively. The combination of strong coercive field and magnetization resulted in a maximum energy product [(BH)max] = 10.9 kJ/m{sup 3} for the sample with the highest BaFe{sub 12}O{sub 19} content.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗